On the phase separation in nanoscale particle systems: the role of external environment (exemplified on W-Cr pseudo-alloy)

A.V. Shishulin, E.A. Vyalkova, A.V. Shishulina

Nizhny Novgorod State Technical University named after R.E. Alekseev

DOI: 10.26456/pcascnn/2026.18.313

Short communication

Abstract: Due to their unique combination of physicochemical properties, heavy tungsten-based pseudo-alloys with an ultrafine-grained structure produced from nanoparticles by advanced powder metallurgy techniques have become a subject of considerable research interest. In this work, within the framework of a thermodynamic approach, we simulate the features of the phase composition in core-shell nanoparticles formed from a phase-separating solid solution, using the heavy W-Cr pseudo-alloy as a model system. For a binary system with limited solid-state solubility, a specific effect is demonstrated: in contrast to macroscopic systems, the equilibrium composition and volume fraction of the coexisting nanophases vary significantly depending on the chemical nature of the external environment. The environment dictates the surface energy of the outer interface. The set of considered modellin dispersion media includes argon (a common sintering atmosphere), hydrogen (an annealing atmosphere), and several others. For two distinct heterogeneous states of the core-shell structure, temperature dependences of the equilibrium phase composition in each state were obtained. A thermodynamic interpretation of the observed regularities is provided, based on three possible mechanisms for reducing the free energy of the system.

Keywords: nanoparticles, solution decomposition, chemical thermodynamics, solubility, core-shell structure, tungsten, chromium

  • Alexander V. Shishulin – Ph. D., Associate Professor, Nizhny Novgorod State Technical University named after R.E. Alekseev, ORCID: 0000-0003-2370-5313
  • Evgeniya A. Vyalkova – 4th-year undergraduate student, Nizhny Novgorod State Technical University named after R.E. Alekseev
  • Anna V. Shishulina – Ph. D., Associate Professor, Nizhny Novgorod State Technical University named after R.E. Alekseev, ORCID: 0009-0000-0681-5022

For citation:

Shishulin A.V., Vyalkova E.A., Shishulina A.V. O tverdofaznom rasslaivanii v nanochastitsakh binarnykh splavov: rol vneshnej sredy (na primere psevdosplava W-Cr) [On the phase separation in nanoscale particle systems: the role of external environment (exemplified on W-Cr pseudo-alloy)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 313-321. DOI: 10.26456/pcascnn/2026.18.313. ⎘

Full article (in Russian): download PDF file

References:

1. Vilémová M., Illková K., Lukáš F. et al. Microstructure and phase stability of W-Cr alloy prepared by spark plasma sintering, Fusion Engineering and Design, 2018, vol. 127, pp. 173-178 DOI: 10.1016/j.fusengdes.2018.01.012.
2. Hou Q.-Q., Huang K., Luo L.-M. et al. Microstructure and its high temperature oxidation behavior in W-Cr alloys prepared by spark plasma sintering, Materialia, 2019, vol. 6, art. no. 100332, 8 p. DOI: 10.1016/j.mtla.2019.100332.
3. Cordero Z.C., Carpenter R.R., Schuh C.A., Schuster B.E. Sub-scale ballistic testing of an ultrafine grained tungsten alloy into concrete targets, International Journal of Impact Engineering, 2016, vol. 91, pp. 1-5. DOI: 10.1016/j.ijimpeng.2015.11.013.
4. Chookajorn T., Park M., Schuh C.A. Duplex nanocrystalline alloys: entropic nanostructure stabilization and a case study on W-Cr, Journal of Materials Research, 2015, vol. 30, issue 2, pp. 151-162. DOI: 10.1557/jmr.2014.385.
5. Bose A., Schuh C.A., Tobia J.C. et al. Traditional and additive manufacturing of a new tungsten heavy alloy alternative, International Journal of Refractory Metals and Hard Materials, 2018, vol. 73, pp. 22-28. DOI: 10.1016/j.ijrmhm.2018.01.019.
6. Knowles A.J., Cheng T.Y.S., Ma K. et al. Spinodally reinforced W-Cr fusion armour, Applied Materials Today, 2024, vol. 41, art. no. 102430, 7 p. DOI: 10.1016/j.apmt.2024.102430.
7. Sdobnyakov N.Yu., Kolosov A.Yu, Bogdanov S.S. Modelirovaniye protsessov koalestsentsii i spekaniya v mono- i bimetallichenkikh nanosistemakh [Simulation of the processes of coalescence and sintering in mono- and bimetallic nanosystems]. Tver, Tver State University Publ., 2021, 168 p. DOI: 10.26456/skb.2021.168. (In Russian).
8. Shishulin A.V., Fedoseev V.B. Size effect in the phase separation of Cr-W solid solutions, Inorganic Materials, 2018, vol. 54, issue 6, pp. 546-549. DOI: 10.1134/S0020168518050114.
9. Shishulin A.V., Potapov A.A., Shishulina A.V. Fractal nanoparticles of phase-separating solid solutions: morphology-dependent phase equilibria in tungsten heavy pseudo-alloys, Eurasian Physical Technical Journal, 2023, vol. 20, issue 4(46), pp. 125-132. DOI: 10.31489/2023no4/125-132.
10. Tilmann W., Fehr A., Heringhaus M. Mechanical milling to foster the solid solution formation and densification in Cr-W-Si for hot-pressing of PVD target materials, Advanced Powder Technology, 2021, vol. 32, issue 6, pp. 1927-1934. DOI: 10.1016/j.apt.2021.04.001.
11. Shishulin A.V., Fedoseev V.B. Effect of initial composition on the liquid-solid phase transition in Cr-W alloy nanoparticles, Inorganic Materials, 2019, vol. 55, issue 1, pp. 14-18. DOI: 10.1134/S0020168519010138.
12. Shishulin A.V., Potapov A.A., Shishulina A.V. Fractal nanoparticles of phase-separating solid solutions: nanoscale effects on phase equilibria, thermal conductivity, thermoelectric performance, Springer Proceedings in Complexity, ed. by C.H. Skiadas, Y. Dimotikalis. Cham, Springer, 2022, pp. 421-432. DOI: 10.1007/978-3-030-96964-6_30.
13. Savina K.G., Veselov A.D., Grigoryev R.E. et al. Strukturnye prevrascheniya v binarnykh nanochastistakh Ti-V: razmernyj effect i effect izmeneniya sostava [Structural transformations in binary Ti-V nanopartivles: size effect and effect of composition change], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 532-542. DOI: 10.26456/pcascnn/2024.16.532 (In Russian).
14. Shishulin A.V., Shishulina A.V. Ravnovensnyj fazovyj sostav i vzaimnaya rastvorimost’ komponentov v nanochastitsakh fraktal’noj formy tyazhelogo psevdosplava W-Cr [Equilibrium phase composition and mutual solubility in fractal nanoparticles of the W-Cr heavy pseudo-alloy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 380-388. DOI: 10.26456/pcascnn/2019.11.380 (In Russian).
15. Serov S.V. Nepsha N.I., Kolosov A.Yu., Sokolov D.N., Savina K.G., Veresov S.A., Sdobnyakov N.Yu. Strukturnyje prevrashchenija v chetyrekhkomponentnykh nanosplavakh Cu-Au-Pt-Pd razlichnoj morfologii pri posledovatel’nykh termoindutsirovannykh tsiklakh [Structural transformations in quaternary nanoalloys Cu-Au-Pt-Pd of different morphology under successive thermally induced cycles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 466-484. DOI: 10.26456/pcascnn/2025.17.466 (In Russian).
16. Shishulin A.V., Shishulina A.V. Vliyanie iskhodnogo sostava na fazovye ravnovesiya pri tverdofaznom rasslaivanii v nanochastitsakh binarnykh splavov (na primere sistemy W-Cr) [Influence of the initial composition on the phase equilibria in the case of the solid phase separation in binary alloy nanoparticles (exemplifying on the W-Cr system)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 299-307. DOI: 10.26456/pcascnn/2023.15.299 (In Russian).
17. Shishulin A.V., Shishulina A.V. O eshche odnoj osobennosti vysokotemperaturnykh fazovykh ravnovesij v nanochastitsakh tyazhelogo psevdosplava Crx-W1-x [One more peculiarity of high-temperature phase equilibria in nanoparticles of the Crx-W1-x heavy pseudo-alloy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 328-338. DOI: 10.26456/pcascnn/2025.17.328 (in Russian).
18. Sdobnyakov N.Yu. Modelirovanie strukturnykh prevrascheniy v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh [Simulation of structural transformations in monokomponent and multicomponent metal nanosystems]. Tver, Tver State University Publ., 2025, 408 p. DOI: 10.26456/sny.2025.408. (In Russian).
19. Samsonov V.M., Demenkov D.E., Karacharov V.I., Bembel’ A.G. Fluctuation approach to the problem of thermodynamics’ applicability to nanoparticles, Bulletin of the Russian Academy of Sciences: Physics, 2011, vol. 75, issue 8, pp. 1073-1077. DOI: 10.3103/S106287381108034X.
20. Shishulin A.V., Fedoseev V.B., Shishulina A.V. O vliyanii vneshnej sredy na fazovye ravnovesiya v sisteme malogo ob"ema na primere raspada tverdogo rastvora Bi-Sb [Environment-dependent phase equilibria in a small-volume system in the case of the decomposition of Bi-Sb solid solutions], Butlerovskiye soobscheniya [Butlerov Communications], 2017, vol. 51, issue 7, pp. 31-37.(In Russian).
21. Shishulin A.V., Shishulina A.V. O shirine zapreshchennoj zony v mezoporistykh poluprovodnikakh [On the energy bandgap in mesoporous semiconductors], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 317-327. DOI: 10.26456/pcascnn/2025.17.317 (In Russian).
22. Fedoseev V.B., Shishulin A.V. On the size distribution of dispersed fractal particles, Technical Physics, 2021, vol. 66, issue 1, pp. 34-40. DOI: 10.1134/S1063784221010072.

Content |