Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Synthesis and thermal stability of high-entropy oxide (CuZnNiCoFeCrAl)xOy nanoparticles obtained by joint exploding wires

A.V. Pervikov, A.I. Sagun, E.E. Ryumin, K.V. Suliz, M.I. Lerner

National Research Tomsk State University

DOI: 10.26456/pcascnn/2026.18.751

Original article

Abstract: For the first time, a high-entropy oxide nanoparticle-based powder was synthesized via a single-step method based on the co-electrical explosion of various metal/alloy wires in an oxygen-containing atmosphere. The particle size distribution and crystal structure were characterized using transmission electron microscopy and X-ray diffraction analysis. It was shown that particle sizes varied from 10 nm to 3 μm. The particles exhibited a spherical morphology with a relatively uniform distribution of metals throughout their volume. Their crystal structure was represented by spinel and rock-salt phases. Thermal stability of the powder was also investigated. Sintering at 800°C was found to lead to the emergence of weak reflections of the CuO phase. Increasing the sintering temperature to 1000°C resulted in grain growth up to 2-5 μm and the formation of distinct copper-enriched grains. The synthesized powder was used to prepare polymer pellets for the extrusion-based 3D printing of high-entropy oxide ceramic products. The obtained pellets were applied to print a block structure with gyroidal channels. The results of this study demonstrate that co-electrical explosion of wires made of different metals/alloys enables the production of particles with a controlled structure and elemental composition. Tailoring the structure, elemental composition, and metal segregation both during particle synthesis and during sintering of the extrusion-printed part opens new avenues for developing ceramic products with novel or enhanced functional properties.

Keywords: nanoparticles, high-entropy oxide, aluminum oxide, thermal stability, segregation, electrical explosion of wires, current, spinel, rock-salt, gyroid structure

  • Alexander V. Pervikov – Ph. D., Senior Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-7593-0710
  • Anton I. Sagun – Research Engineer, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0009-0001-9537-4878
  • Egor E. Ryumin – Engineer, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0009-0005-2303-9519
  • Konstantin V. Suliz – Research Engineer, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-5556-2113
  • Marat I. Lerner – Dr. Sc., Principal Researcher, Laboratory of metallurgy nanotechnology, Faculty of physics and technology, National Research Tomsk State University, ORCID: 0000-0001-8565-1344

For citation:

Pervikov A.V., Sagun A.I., Ryumin E.E., Suliz K.V., Lerner M.I. Sintez i termicheskaya stabilnost nanochastits vysokoentropijnogo oksida (CuZnNiCoFeCrAl)xOy, poluchennykh sovmestnym elektricheskim vzryvom provolok [Synthesis and thermal stability of high-entropy oxide (CuZnNiCoFeCrAl)xOy nanoparticles obtained by joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 751-760. DOI: 10.26456/pcascnn/2026.18.751. ⎘

Full article (in Russian): download PDF file

References:

1. Hamza A., Umar Azam M., Raza A., et al. Additive manufacturing of ceramic composite cellular structures by spontaneous infiltration of copper oxide in alumina, Journal of Materials Research and Technology, 2025, vol.34, pp.1539-1548. DOI: 10.1016/j.jmrt.2024.12.152.
2. С. Heuer, B. Bock-Seefeld, P. Kaiser et al. 3D printing of alumina components via Fused Granulate Fabrication technology and solvent-free debinding of highly filled feedstocks comprising (LD)-polyethylene and cellulos, Ceramics International. 2025, vol..51, issue.28, pp. 58287-58296. DOI: 10.1016/j.ceramint.2025.10.048.
3. Kerber F., Malczyk P., Hubálková J. et al. Effect of heating rate on powder-bed pre-debinding of thermal-shock-resistant 3D-printed alumina for hydrogen-combustion applications, Ceramics International, 2026, vol.52.issue.20, pp. 36093-36103. DOI: 10.1016/j.ceramint.2026.06.117.
4. Wu V., Liu L., Wang Y., et al. Recent advances in high-entropy oxides: Composition modulation, morphology control, and catalytic applications, Green Energy & Environment, 2026. In Press, Corrected Proof. DOI: 10.1016/j.gee.2026.05.001.
5. Pervikov A.V., Suliz K.V., Sagun A.I., et al. Elektrovzryvnoy sintez dispersnykh poroshkov oksida alyuminiya dlya ekstruzionnoy 3D pechati poristykh izdeliy [Exploding wires synthesis of dispersed aluminum oxide powders for extrusion 3D printing of porous product], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 125-134. DOI: 10.26456/pcascnn/2025.17.125. (In Russian).
6. Suliz K.V., Agafonov G.O., Shmakov V.V. et al. One-step novel synthesis of multicomponent oxide nanoparticles via joint exploding wires of dissimilar metals/alloys, Ceramics International, 2025, vol.51, issue.18, pp. 25632-25643. DOI: 10.1016/j.ceramint.2025.03.245.
7.Suliz K.V., Shmakov V.V., Pervikov A.V. et al. Kristallicheskaya struktura i dispersnyy sostav nanochastits mnogokomponentnogo (NiFeCoCuZn)xOy oksida, poluchennykh sovmestnym elektricheskim vzryvom provolok[Crystal structure and dispersed composition of multicomponent (NiFeCoCuZn)XOY oxide nanoparticles obtained by joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 203-210. DOI: 10.26456/pcascnn/2025.17.203. (In Russian).
8. Suliz K.V., Pustovalov A.V., Pervikov A.V. Kristallicheskaya struktura i dispersnyy sostav nanochastits mnogokomponentnogo (NiCoCrFeAl)xOy oksida, poluchennykh sovmestnym elektricheskim vzryvom provolochek [Crystal structure and dispersed composition of multicomponent oxide (NiCoCrFeAl)xOy nanoparticles obtained via joint exploding wires], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 916-927. DOI: 10.26456/pcascnn/2025.17.916. (In Russian).
9. Liu S., Liu K., Qi L., Yang L. Synthesis of high-entropy oxide nanopowders with different crystal structures by electrical explosion of wires, Nanomaterials, 2025, vol.15, issue.8, art. no 571, 17 p. DOI: 10.3390/nano15080571.
10. Dabrowa J., Stygar M., Mikula A. et al. Synthesis and microstructure of the (Co,Cr,Fe,Mn,Ni)3O4 high entropy oxide characterized by spinel structure, Materials Letters, 2018, vol.216, pp. 32-36. DOI: 10.1016/j.matlet.2017.12.148.
11. Haynes W.M. CRC handbook of chemistry and physics, 95th ed. Boca Raton, CRC Press, 2014, 2704 p. DOI: 10.1201/b17118.
12. Kvartskhava I.F., Bondarenko V.V., Pliutto A.A., Chernov A.A. Oscillographic determination of energy of electric explosion of wires, Journal of Experimental and Theoretical Physics, 1957, vol. 4, issue 5, pp. 623-629.
13. Berardan D., Meena A.K., Franger S. et al. Controlled Jahn-Teller distortion in (MgCoNiCuZn)O-based high entropy oxides, Journal of Alloys and Compounds, 2017, vol.704, pp.693-700. DOI: 10.1016/j.jallcom.2017.02.070.
14. Suliz K.V., Gusarenko A.A., Pervikov A.V. Characteristic formation of the structure composite nanoparticles high entropy oxide/Ag obtained by joint exploding wires, Powder Technology, 2026, vol.469, art.no. 121951, 9 p. DOI: 10.1016/j.powtec.2025.121951.