Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Formation of supramolecular particles of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer: interaction of components and properties

M.O. Tonkushina, I.D. Gagarin, B.T.M.A.. Sharadgah, A.A. Ostroushko

Ural Federal University

DOI: 10.26456/pcascnn/2026.18.171

Original article

Abstract: Polyoxometalate nanoclusters are capable of interacting with various compounds and forming multicomponent supramolecular systems. Fine-tuning the properties of such a system, based on the tasks of future practical application, can be carried out by selecting its components. In this work, three-component supramolecular systems of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer, which form without the involvement of additional crosslinking reagents, were investigated. It was found that upon interaction with polyethylene glycol, the {Mo72Fe30}(doxorubicin)12 complex forms hydrogen bonds with the ether oxygen and terminal groups of the polymer, whereas in {Mo72Fe30}(doxorubicin)12-polyvinylpyrrolidone system, the nitrogen in the lactam ring of the polymer is electrostatically attracted to the negatively charged surface of the polyoxometalate. The presence of polymers does not affect the release rate of doxorubicin from the {Mo72Fe30}(doxorubicin)12 complex in a solution at pH 7,4 (blood pH). The difference in the nature of interaction of the two polymers with the polyoxometalate is manifested in the sizes of the particles formed in solution; specifically, in the system with polyethylene glycol, the particle size distribution did not differ from that of the solution in the absence of the polymer (average size 22 nm), whereas in the system with polyvinylpyrrolidone, a broad particle size distribution ranging from 30 nanometers to several micrometers was observed.

Keywords: {Mo72Fe30}, doxorubicin, polyethylene glycol, polyvinylpyrrolidone, particle size, supramolecular systems

  • Margarita O. Tonkushina – Ph. D., Senior Researcher, Department of Chemical Materials Science in Scientific Research Institute of Physics and Applied Mathematics, Ural Federal University, ORCID: 0000-0003-4371-3900
  • Ilya D. Gagarin – Ph. D., Researcher, Department of Chemical Materials Science in Scientific Research Institute of Physics and Applied Mathematics, Ural Federal University, ORCID: 0000-0002-8545-927X
  • Barah T.M.A.. Sharadgah – 3rd postgraduate student, Department of Medical Biochemistry and Biophysics, Ural Federal University
  • Alexander A. Ostroushko – Dr. Sc., Professor, Head of Department of Chemical Materials Science in Scientific Research Institute of Physics and Applied Mathematics, Ural Federal University, ORCID: 0000-0003-0206-5513

For citation:

Tonkushina M.O., Gagarin I.D., Sharadgah B.T.M.A.., Ostroushko A.A. Formirovanie supramolekulyarnykh chastits polioksometallat {Mo72Fe30}-doksorubitsin-biosovmestimyj polimer: vzaimodejstvie komponentov i svojstva [Formation of supramolecular particles of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer: interaction of components and properties], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 171-184. DOI: 10.26456/pcascnn/2026.18.171. ⎘

Full article (in Russian): download PDF file

References:

1. Liu Y., Wang Q., Li F., Ling D. Nature-inspired supramolecular assemblies for precise biomedical imaging and therapy, Acta Pharmaceutica Sinica B, 2022, vol. 12, issue 10, pp. 4008-4010. DOI: 10.1016/j.apsb.2022.06.014.
2. Li Y., Tian R., Zou Y. et al. Strategies and applications for supramolecular protein self‐assembly, Chemistry – A European Journal, 2024, vol. 30, issue 66, art. no. e202402624, 13 p. DOI: 10.1002/chem.202402624.
3. Peng S., Wang K., Guo D.-S., Liu Y. Supramolecular polymeric vesicles formed by p-sulfonatocalix[4]arene and chitosan with multistimuli responses, Soft Matter, 2015, vol. 11, issue 2, pp. 290-296. DOI: 10.1039/C4SM02170C.
4. Datta L.P., Mukherjee R., Biswas S., Das T.K. Peptide-based polymer–polyoxometalate supramolecular structure with a differed antimicrobial mechanism, Langmuir, 2017, vol. 33, issue 49, pp. 14195-14208. DOI: 10.1021/acs.langmuir.7b02916.
5. Raza A., Rasheed T., Nabeel F. et al. Endogenous and exogenous stimuli-responsive drug delivery systems for programmed site-specific release, Molecules, 2019, vol. 24, issue 6, art. no. 1117, 21 p. DOI: 10.3390/molecules24061117.
6. Bellavita R., Braccia S., Falanga A., Galdiero S. An overview of supramolecular platforms boosting drug delivery, Bioinorganic Chemistry and Applications, 2023, vol. 2023, art. id 608428, 15 p. DOI: 10.1155/2023/8608428.
7. Webber M.J., Appel E.A., Meijer E.W., Langer R. Supramolecular biomaterials, Nature Materials, 2016, vol. 15, issue 1, pp. 13-26. DOI: 10.1038/nmat4474.
8. Veselov V.V., Nosyrev A.E., Jicsinszky L. et al. Targeted delivery methods for anticancer drugs, Cancers, 2022, vol. 14, issue 3, art. no. 622, 28 p. DOI: 10.3390/cancers14030622.
9. Balli M.V., Biedermann F., Prodi L., Picchetti P. Supramolecular chemistry for optical detection and delivery applications in living plants, Chemical Society Reviews, 2025, vol. 54, issue 17, pp. 7769-7869. DOI: 10.1039/D4CS00500G.
10. Tripathy D., Gadtya A.S., Moharana S. Supramolecular gel, its classification, preparation, properties, and applications: a review, Polymer-Plastics Technology and Materials, 2023, vol. 62, issue 3, pp. 306-326. DOI: 10.1080/25740881.2022.2113892.
11. Gareev K., Tagaeva R., Bobkov D. et al. Passing of nanocarriers across the histohematic barriers: current approaches for tumor theranostics, Nanomaterials, 2023, vol. 13, issue 7, art. no. 1140, 33 p. DOI: 10.3390/nano13071140.
12. Korolev D., Postnov V., Aleksandrov I., Murin I. The combination of solid-state chemistry and medicinal chemistry as the basis for the synthesis of theranostics platforms, Biomolecules, 2021, vol. 11, issue 10, art. no. 1544, 22 p. DOI: 10.3390/biom11101544.
13. Walha S., Hussein R.K., Roisnel T., Ben Ahmed A. Imidazolium versus phenylalaninium hybrid salts: supramolecular control of electronic, nonlinear optical and bioactive properties, RSC Advances, 2026, vol. 16, issue 11, pp. 10230-10242. DOI: 10.1039/D5RA09394E.
14. Kataria M., Seki S. Responsive chirality: tailoring supramolecular assemblies with external stimuli as future platforms for electronic/spintronic materials, Chemistry – A European Journal, 2025, vol. 31, issue 1, art. no. e202403460, 29 p. DOI: 10.1002/chem.202403460.
15. Yamamoto Y., Yamagishi H., Huang J.-S., Lorke A. Molecular and supramolecular designs of organic/polymeric micro-photoemitters for advanced optical and laser applications, Accounts of Chemical Research, 2023, vol. 56, issue 12, pp. 1469-1481. DOI: 10.1021/acs.accounts.3c00084.
16. Jiang D., Ni D., Rosenkrans Z.T. et al. Nanozyme: new horizons for responsive biomedical applications, Chemical Society Reviews, 2019, vol. 48, issue 14, pp. 3683-3704. DOI: 10.1039/C8CS00718G.
17. Filippova A.D., Sozarukova M.M., Baranchikov A.E. et al. Peroxidase-like activity of CeO2 nanozymes: particle size and chemical environment matter, Molecules, 2023, vol. 28, issue 9, art. no. 3811, 18 p. DOI: 10.3390/molecules28093811.
18. Xu D., Sheng B., Lin Z.-H. et al. Fe3O4 nanozyme as a novel plant growth promoter for enhancing salt tolerance in cucumber seedlings: integrated analysis of growth physiology and transcriptional metabolism, Environmental Science: Nano, 2026, vol. 13, issue 4, pp. 2092-2111. DOI: 10.1039/D5EN00970G.
19. Ma X., Xiao Y., Li S. et al. Recent advances in supramolecular systems for precision medicine: structural design, functional integration, and clinical translation challenges, Pharmaceutics, 2025, vol. 17, issue 9, art. no. 1192, 28 p. DOI: 10.3390/pharmaceutics17091192.
20. Finbloom, J.A., Francis, M.B. Supramolecular strategies for protein immobilization and modification, Current Opinion in Chemical Biology, 2018, vol. 46, pp. 91-98. DOI: 10.1016/j.cbpa.2018.05.023.
21. Romanovska, A., Schmidt, M., Brandt, V. et al. Controlling the function of bioactive worm micelles by enzyme-cleavable non-covalent inter-assembly cross-linking, Journal of Controlled Release, 2024, vol. 368, pp. 15-23. DOI: 10.1016/j.jconrel.2024.02.013.
22. Doan L., Nguyen T.M.D., Le Q.N. et al. Surface modifications of superparamagnetic iron oxide nanoparticles with citric acid, selenium, and silver combining with polymer blend as antibacterial agent, Discover Nano, 2025, vol. 20, issue 1, art. no. 186, 25 p. DOI: 10.1186/s11671-025-04372-x.
23. Stuckart M., Monakhov K.Y. Polyoxometalates as components of supramolecular assemblies, Chemical Science, 2019, vol. 10, issue 16, pp. 4364-4376. DOI: 10.1039/C9SC00979E.
24. Budych, M.J.W., Staszak, K., Bajek, A. et al. The future of polyoxymetalates for biological and chemical applications, Coordination Chemistry Reviews, 2023, vol. 493, art. no. 215306, 25 p. DOI: 10.1016/j.ccr.2023.215306.
25. Taghiyar H., Yadollahi B., Kajani A.A. Controlled drug delivery and cell adhesion for bone tissue regeneration by Keplerate polyoxometalate (Mo132)/metronidazole/PMMA scaffolds, Scientific Reports, 2022, vol. 12, issue 1, art. no. 14443, 12 p. DOI: 10.1038/s41598-022-18622-w.
26. Bijelic A., Rompel A. Polyoxometalates: more than a phasing tool in protein crystallography, ChemTexts, 2018, vol. 4, issue 3, art. no. 10, 27 p. DOI: 10.1007/s40828-018-0064-1.
27. Müller A., Sarkar S., Shah S.Q.N. et al. Archimedean synthesis and magic numbers: «sizing» giant molybdenum-oxide-based molecular spheres of the Keplerate type, Angewandte Chemie International Edition, 1999, vol. 38, issue 21, pp. 3238-3241. DOI: 10.1002/(SICI)1521-3773(19991102)38:21<3238::AID-ANIE3238>3.0.CO;2-6.
28. Grzhegorzhevskii K.V., Zelenovskiy P.S., Koryakova O.V., Ostroushko A.A. Thermal destruction of giant polyoxometalate nanoclusters: a vibrational spectroscopy study, Inorganica Chimica Acta, 2019, vol. 489, pp. 287-300. DOI: 10.1016/j.ica.2019.01.016.
29. Tonkushina M.O., Grzhegorzhevskii K.V., Ermoshin A.A. et al. The electrostatic‐mediated formation of a coordination complex: the trapping and release of an antitumor drug with an anthracycline core from {Mo72Fe30}‐based ensembles, ChemistrySelect, 2022, vol. 7, issue 45, art. no. 202203684, 8 p. DOI: 10.1002/slct.202203684.
30. Tonkushina M., Gagarin I., Guseynova A. et al. Molecular recognition on the multisite binding surface of the keplerate {Mo72 Fe30} giving supramolecular texturing and modulating the function of guest molecules, Inorganic Chemistry, 2024, vol. 63, issue 38, pp. 17388-17405. DOI: 10.1021/acs.inorgchem.4c01338.
31. Das G., Nicastri A., Coluccio M.L. et al. FT‐IR, Raman, RRS measurements and DFT calculation for doxorubicin, Microscopy Research and Technique, 2010, vol. 73, issue 10, pp. 991-995. DOI: 10.1002/jemt.20849.
32. Brogly M., Bistac S., Bindel D. Adsorption and structuration of PEG thin films: influence of the substrate chemistry, Polymers, 2024, vol. 16, issue 9, art. no. 1244, 18 p. DOI: 10.3390/polym16091244.
33. K.V. Anasuya, Harlapur S.F., Harlapur S.F., Patil R.D. Studies on metal complexes of poly (vinylpyrrolidone) (PVP): formation, characterisation and antimicrobial manganese (II) and iron (II) complexes, African Journal of Biomedical Research, 2024, vol. 27, pp. 10007-10018. DOI: 10.53555/AJBR.v27i5S.5594.
34. Sasaki K., Hussan K.P.S., Kita R. et al. Fundamental insights into bulk polyvinylpyrrolidone (PVP): Combining DFT, molecular dynamics, and spectroscopic techniques, Chemical Physics, 2026, vol. 603, art. no. 113053, 11 p. DOI: 10.1016/j.chemphys.2025.113053.
35. Tonkushina M.O., Gagarin I.D., Terziyan T.V. et al. Giant polyoxometalates in albumin solutions: particle size, zeta potential and cells response, Journal of Solution Chemistry, 2026, 21 p. DOI: 10.1007/s10953-026-01596-y.
36. Grzhegorzhevskii,K., Tonkushina, M., Gushchin P. et al. Association of keplerate-type polyoxometalate {Mo72Fe30} with tetracycline: nature of binding sites and antimicrobial action, Inorganics, 2022, vol. 11, issue 1, art. no. 9, 12 p. DOI: 10.3390/inorganics11010009.
37. Tonkushina M.O., Gagarin I.D., Russkikh O.V., Belozerova K.A., Ostroushko A.A. Destruktsiya polioksometallata {Mo72Fe30} kak transportnogo agenta v sredakh, modeliruyushchikh krov, ego stabilizatsiya albuminom [Destruction of polyoxometalate {Mo72Fe30} as a transport agent in blood simulating media, its stabilization by albumin], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 885-892. DOI: 10.26456/pcascnn/2020.12.885. (In Russian).
38. Sciortino G., Aureliano M., Garribba E. Rationalizing the decavanadate(V) and oxidovanadium(IV) binding to G-actin and the competition with decaniobate(V) and ATP, Inorganic Chemistry, 2021, vol. 60, issue 1, pp. 334-344. DOI: 10.1021/acs.inorgchem.0c02971.

Content |