A planar array of GST225-based memristor elements
V.A. Mikhalevsky1, A.A. Burtsev1, V.V. Ionin1, A.A. Nevzorov1,2, A.V. Kiselev1, N.N. Eliseev1, A.A. Lotin1,3
1 National Research Centre «Kurchatov Institute»
2 National University of Science and Technology MISIS
3 Mendeleev University of Chemical Technology
DOI: 10.26456/pcascnn/2026.18.705
Original article
Abstract: This paper presents a modeling study of the electrical resistance in a memristor structure based on the phase-change Ge₂Sb₂Te₅ material. The changes in resistance are driven by some structural transformations in the active region of the memory cell under the influence of electrical control pulses. A novel planar architecture for memristor structures has been demonstrated. Using the simulation data for this architecture, temperature dynamics and phase transitions are analyzed within the framework of the classical Stefan problem. Optimal parameters for the electrical control pulses are identified. The results demonstrate that once the phase transition threshold is reached, the resistance switching time becomes essentially independent of the control parameters. The proposed memristor architecture exhibits advantages in both power efficiency and the capability for multilevel resistance states, positioning it as a key component for next-generation memristive technologies.
Keywords: memristor, chalcogenides, phase change materials, thin films, amorphization
- Vladimir A. Mikhalevsky – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-6234-1084
- Anton A. Burtsev – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0280-7943
- Vitaly V. Ionin – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-1253-2261
- Alexey A. Nevzorov – Ph. D., Researcher, National Research Centre «Kurchatov Institute», Researcher, Laboratory of Photonic Gas Sensors National University of Science and Technology MISIS, ORCID: 0000-0001-5602-6355
- Alexey V. Kiselev – Ph. D., Senior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0292-9553
- Nikolay N. Eliseev – Junior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-8864-3961
- Andrey A. Lotin – Dr. Sc., Deputy Head of the branch, National Research Centre «Kurchatov Institute», Deputy Director of the Department of Scientific and Technical Policy Mendeleev University of Chemical Technology, ORCID: 0000-0001-9051-7158
For citation:
Mikhalevsky V.A., Burtsev A.A., Ionin V.V., Nevzorov A.A., Kiselev A.V., Eliseev N.N., Lotin A.A. Planarnyj massiv memristornykh elementov na osnove GST225 [A planar array of GST225-based memristor elements], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 705-713. DOI: 10.26456/pcascnn/2026.18.705. ⎘
Full article (in Russian): download PDF file
References:
1. Phase change materials. science and applications, ed. by S. Raoux and M. Wutting. New York, Springer Science+Business Media, LLC, 2009, 450 p. DOI: 10.1007/978-0-387-84874-7.
2. Kolobov A.V., Tominaga J. Chalcogenides: Metastability and Phase Change Phenomena. Berlin Heidelberg, Springer-Verlag, 2012, XVI, 284 p. DOI: 10.1007/978-3-642-28705-3.
3. Kozyukhin S.A., Lazarenko P.I., Popov A.I., Eremenko I.L. Phase change memory materials and their applications, Russian Chemical Reviews, 2022, vol. 91, issue 9, art. no. RCR5033, 37 p. DOI: 10.1070/RCR5033.
4. Zhang W., Mazzarello R., Wuttig M., Ma E. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing, Nature Reviews Materials, 2019, vol. 4, issue 3, pp. 150-168. DOI: 10.1038/s41578-018-0076-x.
5. Papandreou N., Pantazi A., Sebastian A. et al. Multilevel phase-change memory, 17th IEEE International Conference on Electronics, Circuits and Systems, 12-15 December 2010 Athens, Greece. New York, IEEE Publ., 2010, pp. 1017-1020. DOI: 10.1109/ICECS.2010.5724687.
6. Burr G.W., Breitwisch M.J., Franceschini M. et al. Phase change memory technology, Journal of Vacuum Science & Technology B, 2010, vol. 28, issue 2, pp. 223-262. DOI: 10.1116/1.3301579.
7. Terao M., Morikawa T., Ohta T. Electrical phase-change memory: fundamentals and state of the art, Japanese Journal of Applied Physics, 2009, vol. 48, issue 8R, art. no. 080001, 14 p. DOI: 10.1143/JJAP.48.080001.
8. Fong S.W., Neumann C.M., Wong H.S.P. Phase-change memory – Towards a storage-class memory, IEEE Transactions on Electron Devices, 2017, vol. 64, issue 11, pp. 4374-4385. DOI: 10.1109/TED.2017.2746342.
9. Le Gallo M., A. Sebastian A. An overview of phase-change memory device physics, Journal of Physics D: Applied Physics, 2020, vol. 53, issue 21, art. no. 213002, 27 p. DOI: 10.1088/1361-6463/ab7794.
10. Burr G.W., Brightsky M.J., Sebastian A. et al. Recent progress in phase-change memory technology, IEEE Journal on Emerging and Selected Topics in Circuits and Systems, 2016, vol. 6, issue 2, pp. 146-162. DOI: 10.1109/JETCAS.2016.2547718.
11. Burtsev A.A., Eliseev N.N., Mikhalevsky V.A., et a. Physical properties’ temperature dynamics of GeTe, Ge2Sb2Te5 and Ge2Sb2Se4Te1 phase change materials, Materials Science in Semiconductor Processing, 2022, vol. 150, art. no. 106907, 8 p. DOI: 10.1016/j.mssp.2022.106907.
12. Lazarenko P.I., Sherchenkov A.A., Kozyukhin S.A. et al. Electrical properties of the Ge2Sb2Te5 thin films for phase change memory application, AIP Conference Proceedings, 2016, vol. 1727, issue 1, art. no. 020013, 6 p. DOI: 10.1063/1.4945968.
13. Xiong W. Applications of Comsol multiphysics software to heat transfer processes: degree thesis. Helsinki: Arcada University of Applied Sciences, 2010, 64 p.
14. Gupta S.C. The classical Stefan problem. Basic concepts, modelling and analysis, 2nd ed. Elsevier, 2017, II+726 p. DOI: 10.1016/C2017-0-02306-6.
15. Kiselev A.V., Mikhalevsky V.A., Burtsev A.A. et al. Transmissivity to reflectivity change delay phenomenon observed in GeTe thin films at laser-induced reamorphization, Optics & Laser Technology, 2021, vol. 143, art. no. 107305, 6 p. DOI: 10.1016/j.optlastec.2021.107305.
16. Kiselev A.V., Ionin V.V., Burtsev A.A. et al. Dynamics of reversible optical properties switching of Ge2Sb2Te5 thin films at laser-induced phase transitions, Optics & Laser Technology, 2022, vol. 147, art. no. 107701, 6 p. DOI: 10.1016/j.optlastec.2021.107701.