Phase-structural design of TiSiBN nanocomposite coating synthesized by vacuum-arc plasma-assisted method
Y.F. Ivanov1, A.A. Klopotov2, N.A. Prokopenko1, E.A. Petrikova1
1 Institute of High Current Electronics of the Siberian Branch of RAS
2 Tomsk State University of Architecture and Building
DOI: 10.26456/pcascnn/2026.18.634
Original article
Abstract: The paper considers the phase and structural conditions of the formation of a nanostructured TiSiBN coating synthesized by the vacuum-arc plasma-assisted method on a 321 steel substrate. It is shown that analysis of the ternary systems Ti-Si-N, Ti-B-N and Ti-Si-B allows one to predict in advance the limited solubility of the components and the predominant formation of some individual nitride phases. Based on the size factor, Pauling electronegativity and valence of the elements, it was established that nitrogen and boron have a significant size mismatch with titanium, which prevents the formation of extended substitutional solid solutions and enhances the tendency to form TiN- and BN-containing phases. Experimental data obtained by electron microscopy confirm the formation of a multilayer coating without a pronounced columnar structure. The main volume of the coating is represented by TiN and BN nanocrystallites 2,5-3,5 nm in size, and a transition layer up to 100 nm thick is revealed between the coating and the substrate. The average coating hardness is 32 GPa, with a range of 21-49 GPa. A physical interpretation of the hardening is proposed, based on a modified Hall-Petch dependence, suppression of dislocation nucleation in nanocrystallites, and consideration of the contribution of interphase and intraphase boundaries.
Keywords: film/substrate system, vacuum-arc plasma-assisted method, phase composition, defect substructure, phase diagram
- Yuri F. Ivanov – Dr. Sc., Chief Researcher, Laboratory of Plasma Emission Electronics, Institute of High Current Electronics of the Siberian Branch of RAS, ORCID: 0000-0001-8022-7958
- Anatoly A. Klopotov – Dr. Sc., Professor, Department of Applied Mechanics and Materials Science, Tomsk State University of Architecture and Building, ORCID: 0000-0002-3690-0436
- Nikita A. Prokopenko – Junior Researcher, Laboratory of Plasma Emission Electronics, Institute of High Current Electronics of the Siberian Branch of RAS, ORCID: 0000-0002-9381-872X
- Elizaveta A. Petrikova – Junior Researcher, Laboratory of Plasma Emission Electronics, Institute of High Current Electronics of the Siberian Branch of RAS, ORCID: 0000-0002-1959-1459
For citation:
Ivanov Y.F., Klopotov A.A., Prokopenko N.A., Petrikova E.A. Fazovo-strukturnoe proektirovanie nanokompozitnogo pokrytiya TiSiBN, sintezirovannogo vakuumno-dugovym plazmenno-assistirovannym metodom [Phase-structural design of TiSiBN nanocomposite coating synthesized by vacuum-arc plasma-assisted method], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 634-645. DOI: 10.26456/pcascnn/2026.18.634. ⎘
Full article (in Russian): download PDF file
References:
1. Hocking M.G., Vasantasree V., Sidky P.S. Metallic and ceramic coatings: production, high temperature properties and applications.London, Longman Scientific & Technical, 1989, 516 p.
2. Barvinok V.A., Bogdanovich V.I. Fizicheskiye osnovy i matematicheskoye modelirovaniye protsessov vakuumnogo ionno-plazmennogo napyleniya [Physical principles and mathematical modeling of vacuum ion-plasma spraying processes]. Moscow, Mashinostroyeniye Publ., 1999, 309 p. (In Russian).
3. Vintizenko L.G., Grigoriev S.V., Koval N.N. et al. Dugovyye razryady nizkogo davleniya s polym katodom i ikh primeneniye v generatorakh plazmy i istochnikakh zaryazhennykh chastits [Low-pressure hollow-cathode arc discharges and their application in plasma generators and charged particle sources], Izvestiya vysshikh uchebnykh zavedeniy. Fizika [Russian Physics Journal], 2001. vol. 44, issue 9, pp. 28-35. (In Russian).
4. Vepřek S., Reiprich S., Shizhi L. Superhard nanocrystalline composite materials: the TiN/Si3N4 system, Applied Physics Letters, 1995, vol. 66, issue 20, pp. 2640-2642. DOI: 10.1063/1.113110.
5. Zhang S., Sun D., Fu Y., Du H. Recent advances of superhard nanocomposite coatings: a review, Surface and Coatings Technology, 2003, vol. 167, issue 2-3, pp. 113–119. DOI: 10.1016/S0257-8972(02)00903-9.
6. Sambasivan S., Petuskey W.T. Phase chemistry in the Ti–Si–N system: thermochemical review with phase stability diagrams, Journal of Materials Research, 1994, vol. 9, issue 9, pp. 2362-2369. DOI: 10.1557/JMR.1994.2362.
7. Ma X., Li C., Zhang W. The thermodynamic assessment of the Ti–Si–N system and the interfacial reaction analysis, Journal of Alloys and Compounds, 2005, vol. 394, pp. 138-147. DOI: 10.1016/j.jallcom.2004.09.027.
8. Ma X., Li C., Zhang W. Study on the phase diagram of the Ti–B–N system and the interfacial reaction of the Ti/BN joints, Materials Science and Engineering A, 2005, vol. 392, issue 1-2, pp. 394-402. DOI: 10.1016/j.msea.2004.10.018.
9. Yang Y., Chang Y.A., Tan L. Thermodynamic modeling and experimental investigation of the Ti-rich corner of the B–Si–Ti system, Intermetallics, 2005, vol. 13, issue 10, pp. 1110-1115. DOI: 10.1016/j.intermet.2005.02.001.
10. Hall E.O. The deformation and ageing of mild steel: III. Discussion of results, Proceedings of the Physical Society. Section B, 1951, vol. 64, no. 9, pp. 747-753. DOI: 10.1088/0370-1301/64/9/303.
11. Petch N.J. The cleavage strength of polycrystals, Journal of the Iron and Steel Institute, 1953, vol. 174, pp. 25-28.
12. Naik S.N., Walley S.M. The Hall–Petch and inverse Hall–Petch relations and the hardness of nanocrystalline metals, Journal of Materials Science, 2020, vol. 55, issue 7, pp. 2661-2681. DOI: 10.1007/s10853-019-04160-w.
13. Ivanov Yu.F., Klopotov A.A., Shugurov V.V. at al. Amorfno-kristallicheskiye borsoderzhashchiye pokrytiya, sformirovannyye ionno-plazmennym metodom [Amorphous-crystalline boron-containing coatings formed by the ion-plasma method] // Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 725-735. DOI: 10.26456/pcascnn/2023.15.725. (In Russian).
14. Prokopenko N.A., Petrikova Ye.A., Tolkachev O.S. et al. Fazoobrazovaniye v sisteme Nb–Cu–Ti, sformirovannoy na podlozhke vakuumno-dugovym plazmenno-assistirovannym metodom [Phase formation in the Nb–Cu–Ti system formed on a substrate by the vacuum-arc plasma-assisted method] Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 135-147. DOI: 10.26456/pcascnn/2025.17.135. (In Russian).
15. Klopotov A.A., Ivanov Yu.F., Petrikova E.A. et al. Strukturno-fazovyye sostoyaniya poverkhnostnogo sloya splava Al–Si posle elektronno-ionno-plazmennoy obrabotki [Structural and phase states of the surface layer of Al–Si alloy after electron-ion-plasma processing], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2014, issue 6, pp. 162-170. DOI: 10.26456/pcascnn/2014.6.162. (In Russian).
16. Leyland A., Matthews A. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behavior, Wear, 2000, vol. 246, issue 1-2, pp. 1-11. DOI: 10.1016/S0043-1648(00)00488-9.
17. Musil J. Hard nanocomposite coatings: thermal stability, oxidation resistance and toughness, Surface and Coatings Technology, 2012, vol. 207, pp. 50–65. DOI: 10.1016/j.surfcoat.2012.05.073.
18. Musil J., Jirout M. Toughness of hard nanostructured ceramic thin films // Surface and Coatings Technology, 2007, vol. 201, issue 9–11, pp. 5148-5152. DOI: 10.1016/j.surfcoat.2006.07.020.
19. Pshyk O., Nakonechna O., Coy E. Current view of nanoindentation: recent developments and application in material characterization, ACS Applied Materials & Interfaces, 2025, vol. 17, issue 25, pp. 36275-36300. DOI: 10.1021/acsami.5c05434.
20. Zhu Y. T., Langdon T. G. Influence of grain size on deformation mechanisms: An extension to nanocrystalline materials, Materials Science and Engineering: A, 2005, vol. 409, issue 1-2, pp. 234-242. doi:10.1016/j.msea.2005.05.111.