Influence of the nature of the organo-ligand complex of transition metals and thermochemical activation on the effectiveness of metal oxide catalysts for carbon nanotube growth in the CVD process
A.P. Prudchenko, O.Yu. Poliakova, J.S. Protasevich
L.M. Litvinenko Institute of Physical Organic and Coal Chemistry
DOI: 10.26456/pcascnn/2026.18.917
Original article
Abstract: This paper presents the results of a study of the effect of the nature of organic ligands, the composition of organo-ligand complexes of 3d-metals, and the conditions of their thermal degradation in the synthesis of metal oxide catalysts for the growth of carbon nanotubes on their effectiveness of the processes of catalytic chemical deposition of carbon from the gas phase. Metal oxide catalysts were synthesized using a technique combining the approaches of polymerized complex precursors, the chelation method of sol-gel technology, as well as thermal decomposition and thermochemical activation of the carrier. It has been established that the effectiveness of catalysts of the general composition Me2CO/CaCO3 (Me–Fe, Ni) in the CCVD synthesis of carbon nanotubes depends both on the nature of organic ligands of transition metal complexes and on the composition of active metals. The effect of the structure of the ligands used in the synthesis of metal oxide catalysts for both the Fe–Co and Ni–Co combinations is similar and consists in increasing the effectiveness in the following sequence: glycols < polyglycols < polyalcohols < carbohydrates (mono- and disaccharides) < branched polyalcohols (pentaerythritol). Replacing Fe with Ni in the organo-ligand complex can significantly reduce the optimal process temperature from 800°С to 500°С, as well as increase the specific yield of the carbon product. Based on the results of the analysis of temperature dependences using the example of catalysts where the ligands were sucrose, fructose, pentaerythritol and citric acid, it was assumed that the decrease in productivity observed with increasing temperature may be due to an increase in the mobility of catalytic particles, their agglomeration, sintering and, as a result, loss of activity. It has been established that, in case of significant excess, organic ligands can play the role of additional fuel in the process of thermochemical activation of the carrier, affecting its morphology, composition, surface texture, and energy efficiency.
Keywords: carbon nanotubes, metal oxide catalysts, organic ligands, chelates, CVD synthesis, carbon nanomaterials
- Anatoliy P. Prudchenko – Ph. D., Senior Researcher, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0002-5664-4932
- Oksana Yu. Poliakova – Junior Researcher, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0002-4189-4947
- Julia S. Protasevich – Leading Engineer, Department of Supramolecular Chemistry, L.M. Litvinenko Institute of Physical Organic and Coal Chemistry, ORCID: 0009-0001-8704-887X
For citation:
Prudchenko A.P., Poliakova O.Yu., Protasevich J.S. Vliyanie prirody organo-ligandnogo kompleksa perekhodnykh metallov i termokhimicheskoj aktivatsii na effektivnost metalloksidnykh katalizatorov rosta uglerodnykh nanotrubok v CVD protsesse [Influence of the nature of the organo-ligand complex of transition metals and thermochemical activation on the effectiveness of metal oxide catalysts for carbon nanotube growth in the CVD process], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 917-925. DOI: 10.26456/pcascnn/2026.18.917. ⎘
Full article (in Russian): download PDF file
References:
1. Bulyarsky S.V. Uglerodnye nanotrubki: tekhnologiya, upravlenie svojstvami, primenenie [Carbon nanotubes: technology, property control, and applications]. Ulyanovsk, Strezhen Publ., 2011, 479 p. (In Russian).
2. Mishchenko S.V., Tkachev A.G. Uglerodnye nanomaterialy. Proizvodstvo, svojstva, primenenie [Carbon nanomaterials. Production, properties, and applications]. Moscow: Mechanical Engineering Publ., 2008, 320 p. (In Russian).
3. Lim X.X., Low S.C., Oh W.D. A critical review of heterogeneous catalyst design for carbon nanotubes synthesis: functionalities, performances, and prospects, Fuel Processing Technology, 2023, vol. 241, art. no. 107624, 28 p. DOI: 10.1016/j.fuproc.2022.107624.
4. Allaedini Gh. Siti M.T., Aminayi P. et al Carbon nanotubes via different catalysts and the important factors that affect their production: A review on catalyst preferences, International Journal of Nano Dimension, 2016, vol. 7, no 3, pp. 186–200. DOI: 10.7508/ijnd.2016.03.002.
5. Shah K.A., Tali B.A. Synthesis of carbon nanotubes by catalytic chemical vapour deposition: A review оn carbon sources, catalysts and substrates, Materials Science in Semiconductor Processing, 2016, vol. 41, pp. 67-82. DOI: 10.1016/j.mssp.2015.08.013.
6. Prima D.O., Vatsadze S.Z. Cocktail-type catalysis: an emerging concept in metal-mediated transformations, Organometallics, 2025, vol. 44, issue 13, pp. 1337-1357. DOI: 10.1021/acs.organomet.5c00117.
7. Galushko A.S., Cherepanova V.A., Ananikov V.P. Totally defined catalysis as a new paradigm for describing catalytic systems by combining advanced analytics and machine learning techniques, Advances in Organometallic Chemistry, 2025, vol. 84, pp. 255-285. DOI: 10.1016/bs.adomc.2025.09.005.
8. Li Z., Dervishi E., Xu Y. et al. Carbon nanotube growth on calcium carbonate, Catalysis Letters, 2009, vol. 131, issue 3-4, pp. 356-363. DOI: 10.1007/s10562-009-0061-5.
9. Magrez A., Seo J.W., Smajda R. et al. Catalytic CVD synthesis of carbon nanotubes: towards high yield and low temperature growth, Materials, 2010, vol. 3, issue 11, pp. 4871-4891. DOI: 10.3390/ma3114871.
10. Burakova E.A., Besperstova G.S., Neverova M.A. et al. Vliyanie termoobrabotki na svojstva katalizatora sinteza uglerodnykh nanotrubok [Influence of heat treatment on the properties of a catalyst for the synthesis of carbon nanotubes], Vestnik Voronezhskogo gosudarstvennogo universiteta inzhenernykh tekhnologij [Proceedings of the Voronezh State University of Engineering Technologies], 2020, vol. 82, no 1, pp. 237-246. DOI: 10.20914/2310-1202-2020-1-237-246.
11. Poliakova O.Yu., Prudchenko A.P., Protasevich Yu.S. Influence of the nature of chelating agents on the activity and structural pre-organization of metal oxide catalysts for the growth of carbon nanotubes synthesized by the method of polymerized complex precursors, Physics of Particles and Nuclei Letters, 2024, vol. 21, issue 4, pp. 761-763. DOI: 10.1134/S1547477124701280.
12. Lobiak E.V., Shlyakhova E.V., Bulusheva L.G. et al. Ni–Mo and Co–Mo alloy nanoparticles for catalytic chemical vapor deposition synthesis of carbon nanotubes, Journal of Alloys and Compounds, 2015, vol. 621, pp. 351-356. DOI: 10.1016/j.jallcom.2014.09.220.
13. Lobiak E.V., Shlyakhova E.V., Gusel’nikov A.V. et al. Сarbon nanotube synthesis using Fe-Mo/MgO catalyst with different ratios of CH4 and H2 gases, Physica status solidi (b), 2017, vol. 255, issue 1, art. no. 1700274, 6 p. DOI: 10.1002/pssb.201700274.
14. Prudchenko A.P., Polyakova O.Yu., Protasevich Yu.S. Metal oxide catalysts for low-temperature template CCVD synthesis of carbon nanotubes, Journal of Advanced Materials and Technologies, 2024, vol. 9, no. 1, pp. 12-22. DOI: 10.17277/jamt 01.pp.012-022.