Size effect in the formation of fractal nickel films
V.A. Anofriev1, A.S. Antonov1, E.M. Semenova1, M.S. Afanasiev2,3, N.Yu. Sdobnyakov1
1 Tver State University
2 Fryazino Branch of V.A. Kotelnikov Institute of Radio Engineering and Electronics of RAS
3 MIREA – Russian Technological University
DOI: 10.26456/pcascnn/2026.18.007
Original article
Abstract: In this paper, we examine the size effect to describe the patterns of fractal relief formation using nanoscale nickel films (50-100 nm thick). Two alternative imaging methods were employed: atomic force microscopy and scanning tunneling microscopy. By analyzing a series of images at a scale of 500 nm, which provides the best surface resolution and image quality for both methods, we obtained the size dependences of the fractal dimension on film thickness. We have described the formation of fractal relief depending on the location of the studied region on the film surface using both methods: varying the film thickness and selecting specific, statistically identical regions of the nickel film. The non-linear change in the fractal dimension for nickel films with increasing thickness can be explained by two parallel processes: the formation of a «new» fractal relief and the degradation of the «formed» fractal relief during the deposition process, which distinguishes this effect from some classical dimensional effects for nanoscale films, for example, the dependence of their melting temperature on thickness.
Keywords: size effect, degradation and growth, atomic force microscopy, scanning tunneling microscopy, fractal relief, nickel films
- Vitaly A. Anofriev – 4th year postgraduate student, General Physics Department, Tver State University
- Alexander S. Antonov – Ph. D., Researcher, Tver State University, ORCID: 0000-0003-1709-8078
- Elena M. Semenova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University, ORCID: 0000-0003-2755-6933
- Mikhail S. Afanasiev – Dr. Sc., Docent, Professor, Leading Researcher, Fryazino Branch of V.A. Kotelnikov Institute of Radio Engineering and Electronics of RAS, Professor, Department of Metrology and Standardization MIREA – Russian Technological University, ORCID: 0000-0001-5475-8616
- Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336
For citation:
Anofriev V.A., Antonov A.S., Semenova E.M., Afanasiev M.S., Sdobnyakov N.Yu. Razmernyj effekt pri formirovanii fraktalnykh plenok nikelya [Size effect in the formation of fractal nickel films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 7-20. DOI: 10.26456/pcascnn/2026.18.007. ⎘
Full article (in Russian): download PDF file
References:
1. Ivanov G.S., Brylkin Yu.V. Fraktal'naya geometricheskaya model' mikropoverkhnosti [Fractal geometric microsurface model], Geometriya i grafika [Geometry & Graphics], 2016, vol. 4, no. 1, pp. 4-11. DOI: 10.12737/18053. (In Russian).
2. Brylkin Yu.V., Kusov A.L., Florov A.V. Testirovanie algoritma modelirovaniya rel'efa sherokhovatoj poverkhnosti na osnove teorii fraktalov [Testing a rough surface relief modeling algorithm based on fractal theory, Izvestiya Kabardino-Balkarskogo gosudarstvennogo universiteta], [Proceedings of the Kabardino-Balkarian State University], 2014, vol. IV, no. 5, pp. 86-89. (In Russian).
3. Belko A.V., Nikitin A.V., Strekal' N.D., German A.E. Fractal structure of gold clusters formed under vacuum deposition on dielectric substrates, Journal of Surface Investigation. X-ray, Synchrotron and Neutron Techniques, 2009, vol. 3, issue 3, pp. 338-342. DOI: 10.1134/S1027451009030021.
4. Van Put A., Vertes A., Wegrzynek D. et al. Quantitative characterization of individual particle surfaces by fractal analysis of scanning electron microscope images, Fresenius' Journal of Analytical Chemistry, 1994, vol. 350, issue 7-9, pp. 440-447. DOI: 10.1007/BF00321787.
5. Mannelquist A., Almquist N., Fredriksson S. Influence of tip geometry on fractal analysis of atomic force microscopy images, Applied Physics A, 1998, vol. 66, supplement issue 1, pp. S891-S895. DOI: 10.1007/s003390051262.
6. Douketis C., Haslett T.L., Wang Z. et al. Rough silver films studied by surface enhanced Raman spectroscopy and low temperature scanning tunnelling microscopy, Progress in Surface Science, 1995, vol. 50, issue 1-4, pp. 187-195. DOI: 10.1016/0079-6816(95)00053-4
7. Zahn W., Zösch A. The dependence of fractal dimension on measuring conditions of scanning probe microscopy, Fresenius' Journal of Analytical Chemistry, 1995, vol. 365, issue 1-3, pp. 168-172. DOI: 10.1007/s002160051466.
8. Anofriev V.A., Sdobnyakov N.Yu., Antonov A.S. et al. Fractal relief on the surface of molybdenum films, Proceedings of the 2025 Conference of Young Researchers in Electrical and Electronic Engineering (2025 ElCon), January 28-29, 2025, St. Petersburg, Russia. St. Petersburg, Saint Petersburg Electrotechnical University «LETI», 2025, pp. 958-963.
9. Sdobnyakov N.Yu., Zykov T.Yu., Bazulev A.N., Antonov A.S. Opredelenie fraktal'noi razmernosti ostrovkovykh plenok zolota na slyude [Determination of the fractal dimension of island films of gold on mica], Vestnik TvGU, seriya «Fizika» [Herald of Tver State University, series «Physics»], 2009, issue 6, pp. 112-119. (In Russian).
10. Ivanov D.V., Antonov A.S., Semenova E.M. et al. Poluchenie nanorazmernykh plenok platiny, obladayushchikh fraktal'nymi svojstvami [Obtaining nanosized platinum films with fractal properties], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 73-88. DOI: 10.26456/pcascnn/2020.12.073. (In Russian).
11. Ivanov D.V., Antonov A.S., Semenova E.M. et al. Determination of the fractal size of titanium films at different scales, Journal of Physics: Conference Series, 2021, vol. 1758, art. no. 012013, 6 p. DOI: 10.1088/1742-6596/1758/1/012013.
12. Anofriev V.A., Antonov A.S., Semenova E.M. et al. Patterns of formation of relief of titanium and molybdenum nanofilms: fractal approach, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2025, vol. 19, issue 6, pp. 1683-1690. DOI: 10.1134/S1027451025702362.
13. Anofriev V.A., Sdobnyakov N.Yu., Antonov A.S. et al. Fractal relief on the surface of molybdenum films, Materials Letters, 2026, vol. 421, art. no. 141198, 5 p. DOI: 10.1016/j.matlet.2026.141198.
14. Sdobnyakov N.Yu., Antonov A.S., Ivanov D.V. Morfologicheskie kharakteristiki i fraktal'nyj analiz metallicheskikh plenok na dielektricheskikh poverkhnostyakh: monografiya [Morphological characteristics and fractal analysis of metal films on dielectric substrates: monography]. Tver: Tver State University Publ., 2019, 168 p. (In Russian).
15. Antonov A.S., Sdobnyakov N.Yu., Ivanov D.V. et al. Issledovanie fraktal'nykh svojstv nanorazmernykh plenok zolota, serebra i medi: atomno-silovaya i tunnel'naya mikroskopiya [Investigation of fractal properties of nanosized gold, silver and copper films: atomic force and tunnelling microscopy], Khimicheskaya fizika i mezoskopiya [Chemical Physics and Mesoscopy], 2017, vol. 19, no. 3, pp. 473-486. (In Russian).
16. Zahn W., Zösch A. Characterization of thin-film surfaces by fractal geometry, Fresenius' Journal of Analytical Chemistry, 1997, vol. 358, issue 1-2, pp. 119-121. DOI: 10.1007/s002160050360.
17. Barabásy A.L., Stanley H.E. Fractal concepts in surface growth. Cambridge, Cambridge University Press, 1995, XX, 366 p.
18. Persson B.N.J. On the fractal dimension of rough surfaces, Tribology Letters, 2014, vol. 54, issue 1, pp. 99-106. DOI: 10.1007/s11249-014-0313-4.
19. Antonov A.S., Sdobnyakov N.Yu., Anofriev V.A. et al. Kompleksnyj podkhod k izucheniyu fraktalnykh struktur na poverkhnosti zheleza [Comprehensive approach to studying fractal structures on iron surfaces], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 7-23. DOI: 10.26456/pcascnn/2024.16.007. (In Russian).
20. DigitalSurf. Available at: www.url: https://www.digitalsurf.com (accessed 31.07.2026).
21. Anofriev V.A., Antonov A.S., Vasilyev S.A. et al. Sravnitelnyj analiz protsessa formirovaniya fraktalnykh metallicheskikh plenok: atomisticheskoe modelirovanie [Comparative analysis of the process of formation of fractal metal films: atomistic simulation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 339-352. DOI: 10.26456/pcascnn/2025.17.339. (In Russian).
22. Howland R., Benatar L. A practical guide to scanning probe microscopy. Sunnyvale, Park Scientific Instruments, 1996, 74 p.
23. Nguyen V.T.A., Gabdullin P.G., Arkhipov A.V. Transformatsiya morfologii tonkikh plenok nikelya i tsirkoniya na estestvenno okislennykh kremnievykh podlozhkakh pri otzhige v vakuume [Modification of morphology of thin nickel and zirconium films on naturally oxidized silicon substrates by annealing in vacuum], Nauchno-tekhnicheskie vedomosti SPbGPU. Fiziko-matematicheskie nauki [St. Petersburg State Polytechnical University Journal. Physics and Mathematics], 2025, vol. 18, no. 4, pp. 139-150. DOI: 10.18721/JPM.18410.
24. Gromov D.G., Zhigal’skii G.P., Karev A.V. et al. Fluctuation phenomena in nanoscale nickel films near the melting point, Semiconductors, 2011, vol. 45, issue 13, pp. 1689-1693. DOI: 10.1134/S1063782611130136.
25. Neyts E.C., Bogaerts A. Numerical study of the size-dependent melting mechanisms of nickel nanoclusters, The Journal of Physical Chemistry C, 2009, vol. 113, issue 7, pp. 2771-2776. DOI: 10.1021/jp8058992.
26. Torkhov N.A., Bozhkov V.G., Ivonin I.V., Novikov V.A. Determination of the fractal dimension for the epitaxial n-GaAs surface in the local limit, Semiconductors, 2009, vol. 43, issue 1, pp. 33-41. DOI: 10.1134/S1063782609010084.
27. Harada S., Hua Y., Nakanishi S. et al. Electrodeposition of fractal structured nickel for hydrogen evolution reaction in alkaline, ChemElectroChem, 2024, vol. 11, issue 9, art. no. e202400005, 7 p. DOI 10.1002/celc.202400005.
28. Lewis A.E., Roberts M. Using fractal structure to describe nickel crystal morphology, JOM, 2003, vol. 55, issue 2, pp. 59-61. DOI: 10.1007/s11837-003-0229-1.