Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Modeling the temperature dependence of the energy gap of a subnanocluster of titanium dioxide

G.P. Mikhailov1, Yu.G. Voronova2

1 Ufa University of Science and Technology
2 Ufa State Petroleum Technological University

DOI: 10.26456/pcascnn/2026.18.418

Original article

Abstract: Using quantum-chemical modeling methods, the temperature dependence of the energy gap of the (TiO2)15 subnanocluster was studied in the range from 10 to 900 K. Within the framework of density functional theory (M06/6-31G(d,p) approximation), it was found that the (TiO2)15 subnanocluster has a quasi-spherical shape (C2h symmetry, diameter of 0,9 nm), and its inner core exhibits the atomic order of rutile. Thermostable structures (TiO2)15 were obtained by the non-empirical molecular dynamics method using the Atom-Centered Density Matrix Propagation scheme. For each temperature, the energy gap Egap between the lowest vacant and highest occupied molecular orbitals was calculated using the M06/6-31G(d,p) approximation. The obtained data were analyzed using the Eg(T) model dependencies developed for crystalline solids. The qualitative similarity of the temperature dependencies of Eg(T) for the (TiO2)15 cluster and bulk semiconductors has been established, namely, a non-linear monotonic decrease of the Eg with increasing temperature. As the temperature increases, significant anharmonicity of the (TiO2)15 cluster vibrations is observed, and the temperature sensitivity of the O 2p (highest occupied molecular orbital) and Ti 3d (lowest unoccupied molecular orbital) molecular orbitals is different, with the titanium orbitals showing a weak dependence. The most adequate and physically interpretable results are obtained using the O’Donnell-Chen model, which takes into account the quantum nature of the subnanocluster vibrations and allows us to determine the average energy of the vibrational modes that determine the temperature dependence of the energy gap.

Keywords: nanocluster, titanium dioxide, density functional theory, energy gap

  • Gennady P. Mikhailov – Dr.Sc., Professor, Department of Materials Science and Physics of Metals, Ufa University of Science and Technology, ORCID: 0000-0002-2299-0450
  • Yulia G. Voronova – Ph.D., Associate Professor of the Department of Information Technologies and Applied Mathematics, Ufa State Petroleum Technological University

For citation:

Mikhailov G.P., Voronova Yu.G. Modelirovanie temperaturnoj zavisimosti energeticheskogo zazora subnanoklastera dioksida titana [Modeling the temperature dependence of the energy gap of a subnanocluster of titanium dioxide], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 418-427. DOI: 10.26456/pcascnn/2026.18.418. ⎘

Full article (in Russian): download PDF file

References:

1. Lee, C., Rock, N. D., Islam, A. et al. Electron–phonon effects and temperature-dependence of the electronic structure of monoclinic β-Ga2O3, Applied Physics Letters Materials, 2023, vol. 11, issue 1, art. no. 011106, 7 p. DOI: 10.1063/5.0131453.
2. Yang K., Dai Y., Huang B. (2020). Review of first-principles studies of TiO2: nanocluster, bulk, and material interface, Catalysts, 2020, vol. 10, issue 9, art. no. 972, 33 p. DOI: 10.3390/catal10090972.
3. Zavatski S., Neilande E., Bandarenka H. et al. Density functional theory for doped TiO2: current research strategies and advancements. Nanotechnology, 2024, vol. 35, no. 19, art. no. 192001, 28 p. DOI: 10.1088/1361-6528/ad272e.
4. Pugachevskii M.A. Ultraviolet absorption spectrum of laser-ablated titanium dioxide nanoparticles, Technical Physics Letters, 2013, vol. 39, issue 1, pp. 36-38 DOI: 10.1134/S1063785013010239.
5. Qu Z.-w., Kroes G.-J. Theoretical study of stable, defect-free (TiO2)n nanoparticles with n=10-16, The Journal of Physical Chemistry C, 2007, vol. 111, issue 45, pp.16808-16817. DOI: 10.1021/jp073988t.
6. Schlegel H.B., Millam J.M., Iyengar S.S. et al. Ab initio molecular dynamics: Propagating the density matrix with Gaussian orbitals, Journal of Chemical Physics, 2001, vol. 114, issue 22, pp. 9758-9763. DOI: 10.1063/1.1372182.
7. Zhao Y., Truhlar D.G. The M06 suite of density functionals for main group thermochemistry, thermochemical kinetics, noncovalent interactions, excited states, and transition elements: two new functionals and systematic testing of four M06-class functionals and 12 other functionals, Theoretical Chemistry Accounts, 2008, vol. 120, issue 1-3, pp. 215-241. DOI: 10.1007/s00214-007-0310-x.
8. Frisch M.J., Trucks G.M. et al. Gaussian 09 (Revision D.01). Wallingford, Gaussian Inc., 2013.
9. Chemcraft – graphical software for visualization of quantum chemistry computations. Version 1.6. Available at: chemcraftprog.com (accessed 01.06.2026).
10. Mikhailov G.P. Raschyot temperaturnoj zavisimosti magnitnoj vospriimchivosti subnanorazmernykh klasterov dioksida titana [Calculation of the temperature dependence of the magnetic susceptibility of subnanosized titanium dioxide clusters]. Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 284-292. DOI: 10.26456/pcascnn/2025.17.284.
11. Burdett J.K., Hughbanks T., Miller G.J. et al. Structural-electronic relationships in inorganic solids: powder neutron diffraction studies of the rutile and anatase polymorphs of titanium dioxide at 15 and 295 K, Journal of the American Chemical Society, 1987, vol. 111, issue 12, pp. 3639-3646. DOI: 10.1021/ja00246a021.
12. Zanatta A. R. Temperature-dependent optical bandgap of TiO2 under the Anatase and Rutile phases, Results in Physics, 2024, vol. 60, art. no. 107653, 5 p. DOI: 10.1016/j.rinp.2024.107653.
13. Varshni Y.P. Temperature dependence of the energy gap in semiconductors, Physica, 1967, vol. 34, issue 2, pp. 149-154. DOI: 10.1016/0031-8914(67)90062-6.
14. Pässler R. Semi-empirical descriptions of temperature dependences of band gaps in semiconductors, Physica Status Solidi (b), 2003, vol. 236, issue 3, pp. 710-728. DOI: 10.1002/pssb.200301752.
15. O’Donnell K.P., Chen X. Temperature dependence of semiconductor band gaps, Applied Physics Letters, 1991, vol. 58, issue 23, pp. 2924-2926. DOI: 10.1063/1.104723.
16. Rayimjonova U., El-Sayed Kh., Kitamura T. et al. Evaluation of electron–phonon coupling strength and average phonon energy in MoS2 thin film, Japanese Journal of Applied Physics, 2024, vol. 63, no. 12, pp. 12SP25-1- 12SP25-6. DOI: 10.35848/1347-4065/ad9c86.

Content |