Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Study of functionally modified carbon nanotubes with respect to carbon dioxide

I.V. Zaporotskova, S.V. Boroznin, E.S. Dryuchkov, A.R. El Zanin, P.A. Zaporotskov, N.P. Boroznina

Volgograd State University

DOI: 10.26456/pcascnn/2026.18.842

Original article

Abstract: In this study, the sensory properties towards carbon dioxide of nanocomposites, which are carbon nanotubes with metal oxides attached to it, was studied. The study focused on the geometry and stability of adsorption complexes and the changes in the physicochemical properties (the energy gap and charge distribution) of nanostructures caused by adsorption processes. This research was conducted using computer experiments based on calculations performed with density functional theory methods and a quasi-molecular approach. The results of the computer experiment allowed us to estimate the change in the adsorption energy and the band gap. Based on this analysis, presented below, iron oxide was selected as the most effective material in terms of the adsorption energy (from 0,17 to 0,23 eV), this materials have a sufficiently strong response (in the best case the energy gap decreases from 1,644 to 1,622 eV) and, consequently, a high sensitivity to carbon dioxide. Response in the case of the carbon nanotubes (6,6)-cobalt oxide is significantly stronger (the energy gap decreases from 1,54 to 1,45 or 1,34 eV depending on the adsorption distance), but the strong interaction between composite and carbon dioxide could cause poisoning the sensor. The carbon nanotubes-copper oxide composite is characterized by weak response and, consequently, low sensitivity towards carbon dioxide. The results obtained reveal important physicochemical patterns of interaction between carbon nanotubes and metal oxides composites and carbon dioxide. These findings are significant in terms of the sensitivity and reproducibility of chemical sensors measurements, making them crucial for the development of nanoscale gas sensors.

Keywords: carbon nanotubes, metal oxides, carbon dioxide, gas sensing, density functional theory, energy gap, charge distribution

  • Irina V. Zaporotskova – Dr. Sc., Professor, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0002-9486-2482
  • Sergey V. Boroznin – Dr. Sc., Head of the Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0003-0110-2271
  • Evgeny S. Dryuchkov – Senior Lecturer, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0002-8995-9773
  • Anton R. El Zanin – Engineer, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0009-0005-3897-9490
  • Pavel A. Zaporotskov – Ph. D., Associate Professor, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0003-3122-8801
  • Natalia P. Boroznina – Dr. Sc., Professor, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0003-0813-6888

For citation:

Zaporotskova I.V., Boroznin S.V., Dryuchkov E.S., El Zanin A.R., Zaporotskov P.A., Boroznina N.P. Issledovanie funktsionalno modifitsirovannykh uglerodnykh nanotrubok v otnoshenii k dioksidu ugleroda [Study of functionally modified carbon nanotubes with respect to carbon dioxide], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 842-856. DOI: 10.26456/pcascnn/2026.18.842. ⎘

Full article (in Russian): download PDF file

References:

1. Capurso T., Stefanizzi M., Torresi M., Camporeale S.M. Perspective of the role of hydrogen in the 21st century energy transition, Energy Conversion and Management, 2022, vol. 251, art. no. 114898, 17 p. DOI: 10.1016/j.enconman.2021.114898.
2. Adebayo T.S. Environmental consequences of fossil fuel in Spain amidst renewable energy consumption: a new insight from the wavelet-based Granger causality approach, International Journal of Sustainable Development and World Ecology, 2022, vol. 29, issue 7, pp. 579-592. DOI: 10.1080/13504509.2022.2054877.
3. Voumik L.C., Islam M.A., Ray S. et al. CO2 emissions from renewable and non-renewable electricity generation sources in the G7 countries: static and dynamic panel assessment, Energies, 2023, vol. 16, issue 3, art. no. 1044, 14 p. DOI: 10.3390/en16031044.
4. Hamad T.A., Agll A.A., Hamad Y.M., Sheffield J.W. Solid waste as renewable source of energy: current and future possibility in Libya, Case Studies in Thermal Engineering, 2014, vol. 4, pp. 144-152. DOI: 10.1016/j.csite.2014.09.004.
5. Rabbi M.F., Popp J., Máté D., Kovács S. Energy security and energy transition to achieve carbon neutrality, Energies, 2022, vol. 15, issue 21, art. no. 8126, 18 p. DOI: 10.3390/en15218126.
6. Ping D., Li Y., Wu S. et al. Designing cobalt–nickel dual-atoms on boron, nitrogen-codoped carbon nanotubes for carbon dioxide electroreduction to syngas, Journal of Colloid and Interface Science, 2025, vol. 683, issue 1, pp. 446-456. DOI: 10.21203/rs.3.rs-2790800/v1.
7. Guo H., Jiang J., Li Y. et al. An aging giant at the center of global warming: population dynamics and its effect on CO2 emissions in China, Journal of Environmental Management, 2023, vol. 327, art. no. 116906, 12 p. DOI: 10.1016/j.jenvman.2022.116906.
8. Feng J.C., Sun L., Yan J. Carbon sequestration via shellfish farming: a potential negative emissions technology, Renewable and Sustainable Energy Reviews, 2023, vol. 171, art. no. 113018, 10 p. DOI: 10.1016/j.rser.2022.113018.
9. Scheiblehner D., Neuschitzer D., Wibner S. et al. Hydrogen production by methane pyrolysis in molten binary copper alloys, International Journal of Hydrogen Energy, 2023, vol. 48, issue 16, pp. 6233-6243. DOI: 10.1016/j.ijhydene.2022.08.115
10. Conley K., Karttunen A.J. Bridging the junction: electrical conductivity of carbon nanotube networks, Journal of Physical Chemistry C, 2022, vol. 126, issue 40, pp. 17266-17274. DOI: 10.1021/acs.jpcc.2c03904.
11. Tang D.M., Cretu O., Ishihara S. et al. Chirality engineering for carbon nanotube electronics, Nature Reviews Electrical Engineering, 2024, vol. 1, issue 3, pp. 149-162. DOI: 10.1038/s44287-023-00011-8.
12. Rashko M.N., Hamad S.M., Barzinjy A.A., Hamad A.H. Mechanical properties of carbon nanotubes (CNTs): a review, Eurasian Journal of Science and Engineering, 2022, vol. 8, issue 2, pp. 54-68.
13. Pitroda, J., Jethwa, B., Dave, S.K. A critical review on carbon nanotubes, International Journal of Construction Research in Civil Engineering, 2016, vol. 2, issue 5, pp. 36-42.
14. Kashyap K.T., Patil R.G. On Young’s modulus of multi-walled carbon nanotubes, Bulletin of Materials Science, 2008, vol. 31, issue 2, pp. 185-187. DOI: 10.1007/s12034-008-0032-2.
15. Guo S.Y., Hou P.X., Zhang F. et al. Gas sensors based on single-wall carbon nanotubes, Molecules, 2022, vol. 27, issue 17, art. no. 5381, 22 p. DOI: 10.3390/molecules27175381.
16. Liu D., Shi L., Dai Q. et al. Functionalization of carbon nanotubes for multifunctional applications, Trends in Chemistry, 2024, vol. 6, issue 4, pp. 186-210. DOI: 10.1016/j.trechm.2024.02.002.
17. Xue X., Gu D., Xia X. et al. Solar bipolar cell facilitating carbon dioxide for efficient coproduction of electricity and syngas, Journal of Power Sources, 2022, vol. 521, art. no. 230985, 10 p. DOI: 10.1016/j.jpowsour.2022.230985.
18. Wu Y., Zhao X., Shang Y. et al. Application-driven carbon nanotube functional materials, ACS Nano, 2021, vol. 15, issue 5, pp. 7946-7974. DOI: 10.1039/d4cs00390j.
19. Wang Z., Feng J., Liu X., Guo H. Preparation methods and performance analysis of polyanthraquinone/carbon nanotube composites for capturing carbon dioxide, Atmosphere, 2022, vol. 13, issue 4, art. no. 543, 11 p. DOI: 10.3390/atmos13040543.
20. Hsan N., Dutta P.K., Kumar S. et al. Capture and chemical fixation of carbon dioxide by chitosan grafted multi-walled carbon nanotubes, Journal of CO2 Utilization, 2020, vol. 41, art. no 101237, 12 p. DOI: 10.1016/j.jcou.2020.101237.
21. Kumar S., Bera R., Das N., Koh J. Chitosan-based zeolite-Y and ZSM-5 porous biocomposites for H2 and CO2 storage, Carbohydrate Polymers, 2020, vol. 232, art. no. 115808, 8 p. DOI: 10.1016/j.carbpol.2019.115808.
22. Babu D.J., Bruns M., Schneider J.J. Unprecedented CO2 uptake in vertically aligned carbon nanotubes, Carbon, 2017, vol. 125, pp. 327-335. DOI: 10.1016/j.carbon.2017.09.047.
23. Romero-Guzmán L., Reyes-Gutiérrez L.R., Romero-Guzmán E.T., Savedra-Labastida E. Carbon nanotube filters for removal of air pollutants from mobile sources, Journal of Minerals and Materials Characterization, 2017, vol. 6, issue 1, pp. 105-118. DOI: 10.4236/jmmce.2018.61009.
24. Mkhondo N., Magadzu T. Surface properties of metal oxides and their role on electrochemical hydrogen storage of carbon nanotubes, Digest Journal of Nanomaterials and Biostructures, 2018, vol. 13, issue 4, pp. 921-929.
25. Rodrigues J., Mata D., Pimentel A. et al. One-step synthesis of ZnO decorated CNT buckypaper composites and their optical and electrical properties, Materials Science and Engineering: B, 2015, vol. 195, pp. 38-44. DOI: 10.1016/j.mseb.2015.01.009.
26. Lozano-Rosas R., Bravo-Arredondo J.M., Karthik-Tangirala V.K., Robles-Águila M.J. Development and evaluation of ZnO and ZnO/MWCNT composite as CO₂ gas sensors, Applied Physics A, 2023, vol. 129, issue 11, art. no. 788, 10 p. DOI: 10.1007/s00339-023-07061-7.
27. Hannon A., Li J. Solid state electronic sensors for detection of carbon dioxide, Sensors, 2019, vol. 19, issue 18, art. no. 3848, 14 p. DOI: 10.3390/s19183848.
28. Sonkar P.K., Ganesan V. Metal oxide‑carbon nanotubes nanocomposite‑modified electrochemical sensors for toxic chemicals, Metal Oxides, 2021, pp. 235-261. DOI: 10.1016/B978-0-12-820727-7.00006-9.
29. Hussain M.M., Rahman M.M., Asiri A.M. Ultrasensitive and selective 4-aminophenol chemical sensor development based on nickel oxide nanoparticles decorated carbon nanotube nanocomposites for green environment, Journal of Environmental Sciences, 2017, vol. 53, pp. 27-38. DOI: 10.1016/j.jes.2016.03.028.
30. Amirzadeh Z., Javadpour S., Shariat M.H., Knibbe R. Non-enzymatic glucose sensor based on copper oxide and multi-wall carbon nanotubes using PEDOT:PSS matrix, Synthetic Metals, 2018, vol. 245, pp. 160-166. DOI: 10.1016/j.synthmet.2018.08.021.
31. Peng X., Luan Z., Zechao D. et al. Carbon nanotubes‑iron oxides magnetic composites as adsorbent for removal of Pb(II) and Cu(II) from water, Carbon, 2005, vol. 43, issue 4, pp. 880-883. DOI: 10.1016/j.carbon.2004.11.009.
32. Cardoso E.R., Tverdokhleb N., Eising M. et al. Hydrogen gas sensing performance of iron oxide‐decorated carbon nanotubes: the influence of iron oxide species and concentration, Analysis & Sensing, 2025, vol. 5, issue 3, art. no. e202400092, 9 p. DOI: 10.1002/anse.202400092.
33. Tan Q., Fang J., Liu W. et al. Acetone sensing properties of a gas sensor composed of carbon nanotubes doped with iron oxide nanopowder, Sensors, 2015, vol. 15, issue 11, pp. 28502-28512. DOI:10.3390/s151128502.
34. Moon S., Vuong N.M., Lee D. et al Co3O4–SWCNT composites for H₂S gas sensor application, Sensors and Actuators B: Chemical, 2016, vol. 222, pp. 166-172. DOI: 10.1016/j.snb.2015.08.072.
35. Li W., Jung H., Hoa N.D. et al. Nanocomposite of cobalt oxide nanocrystals and single-walled carbon nanotubes for a gas sensor application, Sensors and Actuators B: Chemical, 2010, vol. 150, issue 1, pp. 160-166. DOI:10.1016/j.snb.2010.07.023
36. Davidson E.R., Clark A.E. A viewpoint on population analyses, International Journal of Quantum Chemistry, 2022, vol. 122, issue 8, art. no. e26860, 10 p. DOI: 10.1002/qua.26860.
37. Khan F., Julien C.M., Islam S.S. Fabrication of multiwalled carbon nanotubes/MoS₂ nanocomposite: application as temperature sensor, FlatChem, 2023, vol. 40, art. no 100521, 11 p. DOI: 10.1016/j.flatc.2023.100521.

Content |