Modeling of light propagation in silicon nitride and zinc selenide photonic integrated circuit elements with a switchable phase-change material film
A.A. Burtsev1, V.V. Ionin1, A.V. Kiselev1, A.A. Nevzorov1,2, V.A. Mikhalevsky1, N.N. Eliseev1, A.A. Lotin1
1 National Research Centre «Kurchatov Institute»
2 University of Science and Technology MISIS
DOI: 10.26456/pcascnn/2026.18.354
Short communication
Abstract: This work presents a comparative analysis of two technological platforms for photonic integrated circuits: silicon nitride (Si₃N₄) and zinc selenide (ZnSe). Using numerical modeling, we demonstrate transmission characteristics of waveguides made of these materials upon switching of an active Ge2Sb2Te5 phase-change cell. Comparison of the two waveguide platforms with an integrated phase-change layer reveals fundamental differences in modulation physics, governed by the choice of operating wavelength. The silicon nitride waveguide (near-infrared range) exhibits strong field localization near the interface and supports several hybrid modes, some of plasmon-polariton nature. This results in a superlinear dependence of losses on the active film thickness, requiring precise optimization (20 nm) to achieve maximum contrast (246%). In contrast, the zinc selenide waveguide (mid- and far-infrared range) shows a reduced plasmonic contribution, a depleted modal composition (close to single-mode), and a quasi-linear increase in losses with film thickness. This provides a wider range of permissible active film thicknesses (20-50 nm) and stable modulation characteristics (contrast up to 112%).
Keywords: photonic integrated circuits, optical waveguides, phase-change materials, thin films
- Anton A. Burtsev – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0280-7943
- Vitaly V. Ionin – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-1253-2261
- Alexey V. Kiselev – Ph. D., Senior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0292-9553
- Alexey A. Nevzorov – Ph. D., Researcher, National Research Centre «Kurchatov Institute», Researcher at Laboratory of Photonic Gas Sensors University of Science and Technology MISIS, ORCID: 0000-0001-5602-6355
- Vladimir A. Mikhalevsky – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-6234-1084
- Nikolay N. Eliseev – Junior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-8864-3961
- Andrey A. Lotin – Dr. Sc, Deputy Head of the branch, National Research Centre «Kurchatov Institute», ORCID: 0000-0001-9051-7158
For citation:
Burtsev A.A., Ionin V.V., Kiselev A.V., Nevzorov A.A., Mikhalevsky V.A., Eliseev N.N., Lotin A.A. Modelirovanie rasprostraneniya izlucheniya v elemente fotonnoj integralnoj skhemy na osnove nitrida kremniya i selenida tsinka i pereklyuchaemoj plenki fazoizmenyaemogo materiala [Modeling of light propagation in silicon nitride and zinc selenide photonic integrated circuit elements with a switchable phase-change material film], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 354-362. DOI: 10.26456/pcascnn/2026.18.354. ⎘
Full article (in Russian): download PDF file
References:
1. Atabaki A.H., Moazeni S., Pavanello F., et al. Integrating photonics with silicon nanoelectronics for the next generation of systems on a chip, Nature, 2018, vol. 556, issue. 7701, pp. 349-354. DOI: 10.1038/s41586-018-0028-z.
2. Thomson D., Zilkie A., Bowers J. E. et al. Roadmap on silicon photonics, Journal of Optics, 2016, vol. 18, issue 7, art. no. 073003, 20 p. DOI: 10.1088/2040-8978/18/7/073003.
3. Shekhar S, Bogaerts W., Chrostowski L. et. al. Roadmapping the next generation of silicon photonics, Nature Communications, 2024, vol. 15, art. no. 751, 15 p. DOI: 10.1038/s41467-024-44750-0.
4. Liu Q., Bian Y., Xiong J. Progress in passive silicon photonic devices: a review, Photonics, 2025, vol. 12, issue 9, art. no. 928, 27 p. DOI: 10.3390/photonics12090928.
5. Blumenthal D.J., Heideman R., Geuzebroek D. et al. Silicon nitride in silicon photonics, Proceedings of the IEEE, 2018, vol. 106, issue 12, pp. 2209-2231. DOI: 10.1109/JPROC.2018.2861576.
6. Sharma T., Wang J., Kaushik B.K. et. al. Review of recent progress on silicon nitride-based photonic integrated circuits, IEEE Access, 2020, vol. 8, pp. 195436-195446. DOI: 10.1109/ACCESS.2020.3032186.
7. Urick V.J., Mckinney J.D., Williams K.J. Fundamentals of microwave photonics. New York: John Wiley & Sons, 2015, 496 p. DOI:10.1002/9781119029816.
8. Rahman T., Pappu M.A.H., Mondal B.K. et.al. Synthesis of ZnSe thin films by solution-processed spin coating method for photonic integration applications, Journal of Materials Science: Materials in Engineering, 2025, vol. 20, issue 1, art. no. 71, 12 p. DOI: 10.1186/s40712-025-00299-4.
9. Ren D., Dong C., Høvik J., et. al. Low-loss hybrid germanium-on-zinc selenide waveguides in the longwave infrared, Nanophotonics, 2024, vol. 13, issue 10, pp. 1815-1822. DOI: 10.1515/nanoph-2023-0698.
10. Phase change materials: science and applications, ed. by S. Raoux and M. Wutting. New York, Springer Science+Business Media, LLC, 2009, 450 p. DOI: 10.1007/978-0-387-84874-7.
11. Kolobov A.V., Tominaga J. Chalcogenides: metastability and phase change phenomena. Berlin Heidelberg, Springer-Verlag, 2012, XVI, 284 p. DOI: 10.1007/978-3-642-28705-3.
12. Abdollahramezani S., Hemmatyar O., Taghinejad H. et al. Tunable nanophotonics enabled by chalcogenide phase-change materials, Nanophotonics, 2020, vol. 9, issue 5, pp. 1189-1241. DOI: 10.1515/nanoph-2020-0039.
13. Guo P., Sarangan A. M., Agha I. A review of germanium-antimony-telluride phase change materials for non-volatile memories and optical modulators, Applied Sciences, 2019, vol. 9, issue 3, art. no. 530, 26 p. DOI: 10.3390/app9030530.
14. Kozyukhin S.A., Lazarenko P.I., Popov A.I., Eremenko I.L. Phase change memory materials and their applications, Russian Chemical Reviews, 2022, vol. 91, issue 9, art. no. RCR5033, 37 p. DOI: 10.1070/RCR5033.
15. Han S.-T., Zhou Y. Photo-electroactive non-volatile memories for data storage and neuromorphic computing. Duxford: Woodhead Publishing, 2020, 352 p. DOI: 10.1016/C2019-0-00530-4.
16. Wuttig M., Yamada N. Phase-change materials for rewriteable data storage, Nature materials, 2007, vol. 6, issue 11, pp. 824-832. DOI: 10.1038/nmat2009.
17. Ionin V.V., Kiselev A.V., Burtsev A.A. et al. An optical synapse based on a polymer waveguide with a GST225 active layer, Applied Physics Letters, 2021, vol. 119, issue 8, art. no. 081105, 5 p. DOI: 10.1063/5.0063349.
18. Kawano K, Kitoh Т. Introduction to optical waveguide analysis: solving Maxwell's equation and the Schrodinger equation. New York: John Wiley & Sons, 2001, XIII+275 p. DOI: 10.1002/0471221600.
19. Kalluri D.K. Electromagnetic waves, materials, and computation with MATLAB. Boca Raton, CRC Press, 2012, 886 p. DOI: 10.1201/b11793.
20. Shalaev V.M. Optical negative-index metamaterials, Nature Photonics, 2007, vol. 1, pp. 41-48. DOI: 10.1038/nphoton.2006.49.
21. Maier S.A. Plasmonics: fundamentals and applications. New York, Springer, 2007, XXVI+224 p. DOI: 10.1007/0-387-37825-1.