On the possibility of using a graphene membrane as a mass sensor
Z.A. Akhmatov1,2,3, Z.A. Akhmatov1
1 Kabardino-Balkarian State University named after H.M. Berbekov
2 Institute for Nuclear Research of the RAS
3 Kabardino-Balkar Scientific Center of the RAS
DOI: 10.26456/pcascnn/2026.18.214
Original article
Abstract: Detection of chemical and biological molecules with high sensitivity and selectivity is crucial in various fields of science and medicine. Highly sensitive mass sensors are used for environmental monitoring, detecting trace amounts of toxic substances or explosive gases. In addition, such sensors can be used to weigh individual protein, DNA, and RNA molecules to understand the mechanisms of their interactions. An important role of mass sensors is in monitoring the growth of thin films, nanowires, and fullerenes, where precision must be at the atomic level. With the development of nanotechnology, a new class of sensors based on the use of graphene and carbon nanotubes has been proposed. Graphene-based sensors are expected to have ultra-high sensitivity to adsorbed atoms and molecules. In this regard, this study examines the possibility of using edge-clamped graphene membrane as an ultra-sensitive mass sensor. A molecular dynamics simulation of oscillations of a free-standing rectangular graphene membrane and a rectangular graphene membrane loaded by iron nanodroplet was performed. The added mass was determined from obtained values of the fundamental frequencies of vibrations of the free and loaded membranes. It has been shown that the use of formulas for the vibrations of a classical membrane gives a difference in mass of more than 5 times. For thin carbon membranes such as graphene, bending stiffness must be taken into account to obtain a sufficiently accurate result when determining the load mass.
Keywords: graphene membrane, mass sensor, molecular dynamics simulation, vibrational mode, bending stiffness
- Zeitun A. Akhmatov – Ph. D., Senior Researcher, Institute of Mathematics and Natural Sciences, Kabardino-Balkarian State University named after H.M. Berbekov, Senior Researcher, Laboratory of Astrophysics and Cosmic Ray Physics Institute for Nuclear Research of the RAS, Senior Researcher, Institute of Informatics and Regional Management Problems Kabardino-Balkar Scientific Center of the RAS, ORCID: 0000-0002-3859-0056
- Zarif A. Akhmatov – Senior Lecturer at the Institute of Mathematics and Natural Sciences, Kabardino-Balkarian State University named after H.M. Berbekov
For citation:
Akhmatov Z.A., Akhmatov Z.A. O vozmozhnosti ispolzovaniya grafenovoj membrany v kachestve datchika massy [On the possibility of using a graphene membrane as a mass sensor], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 214-222. DOI: 10.26456/pcascnn/2026.18.214. ⎘
Full article (in Russian): download PDF file
References:
1. Sadeghzadeh S. Nanoparticle mass detection by single and multilayer graphene sheets: Theory and simulations, Applied Mathematical Modelling, 2016, vol. 40, issue 17-18, pp. 7862-7879. DOI: 10.1016/j.apm.2016.03.051.
2. Lee H.-L., Yang Y.-C., Chan W.-J. Mass detection using a graphene-based nanomechanical resonator, Japanese Journal of Applied Physics, 2013, vol. 52, no. 2R, pp. 025101-1-025101-4. DOI: 10.7567/JJAP.52.025101.
3. Chu L., Shi J., de Cursi E.S Vibration analysis of vacancy defected graphene sheets by monte carlo based finite element method, Nanomaterials, 2018, vol. 8, issue 7, art. no. 489, 21 p. DOI: 10.3390/nano8070489.
4. Akhmatov Z. A., Akhmatov Z. A., Dependence of the vibrational frequencies of a graphene sheet on the ratio of its sides and the number of vacancy defects, Letters to Journal of Experimental and Theoretical Physics, 2025, vol. 121, issue 9, pp. 702-708. DOI: 10.1134/S0021364024605438.
5. Eringen A.C. On differential equations of nonlocal elasticity and solutions of screw dislocation and surface waves, Journal of Applied Physics, 1983, vol. 54, issue 9, pp. 4703-4710. DOI: 10.1063/1.332803.
6. Peddieson J., Buchanan G.R., McNitt R.P. Application of nonlocal continuum models to nanotechnology, International Journal of Engineering Science, 2003, vol. 41, issue 3-5, pp. 305-312. DOI: 10.1016/S0020-7225(02)00210-0.
7. Lee H.-L., Hsu J.-C., Chang W.-J. Frequency shift of carbon-nanotube-based mass sensor using nonlocal elasticity theory, Nanoscale Research Letters, 2010, vol. 5, issue 11, pp. 1774-1778. DOI: 10.1007/s11671-010-9709-8.
8. Nazemnezhad R., Zare M., Hosseini-Hashemi S., Shokrollahi H. Molecular dynamics simulation for interlayer interactions of graphene nanoribbons with multiple layers, Superlattices and Microstructures, 2016, vol. 98, pp. 228-234. DOI: 10.1016/j.spmi.2016.08.036.
9. Gupta S.S., Batra R.C. Elastic properties and frequencies of free vibrations of single-layer graphene sheets, Journal of Computational and Theoretical Nanoscience, 2010, vol. 7, issue 10, pp. 2151-2164. DOI: 10.1166/jctn.2010.1598.
10. Neek-Amal M., Peeters F.M. Linear reduction of stiffness and vibration frequencies in defected circular monolayer graphene, Physical Review B. 2010, vol. 81, issue 23, pp. 235437-1-235437-6. DOI: 10.1103/PhysRevB.81.235437.
11. Hoover W.G. Canonical dynamics: equilibrium phase-space distributions, Physical Review. A, 1985, vol. 31, issue 3, pp. 1695-1697. DOI: 10.1103/PhysRevA.31.1695.
12. Liu R., Wang L., Jiang J. Thermal vibration of a single-layered graphene with initial stress predicted by semiquantum molecular dynamics, Materials Research Express, 2016, vol. 3, no. 9, art. no. 095601, 10 p.. DOI: 10.1088/2053-1591/3/9/095601.
13. Kornhauser E.T., Mintzer D. On the vibration of mass-loaded membranes, Journal of the Acoustical Society of America, 1953, vol. 25, issue 5, pp. 903-906. DOI: 10.1121/1.1907216.
14. Natsuki T., Shi J. X., Ni Q.-Q. Vibration analysis of nanomechanical mass sensor using double-layered graphene sheets resonators, Journal of Applied Physics, 2013, vol. 114, issue 9, pp. 094307-1-094307-5. DOI: 10.1063/1.4820522.
15. Murmu T., Adhikari S. Nonlocal mass nanosensors based on vibrating monolayer graphene sheets, Sensors and Actuators B, 2013, vol. 188, pp. 1319-1327. DOI: 10.1016/j.snb.2013.07.051.
16. Zhang Z., Lan L., Wang Y., Wang C. Vibration frequency analysis of rippled single-layered graphene sheet: Toward the nano resonant devices design, Physica E: Low-dimensional Systems and Nanostructures, 2019, vol. 114, art. no. 113580, 22 p. DOI: 10.1016/j.physe.2019.113580.