Comparative atomistic simulation of structural stability/instability of ternary double-shell nanoparticles Pd@X@Pt, X@Pd@Pt, Pt@X@Pd and X@Pt@Pd (X – Ni, Cu)
A.Yu. Kolosov, K.G. Savina, D.N. Sokolov, E.S. Mitinev, I.A. Vzglyadov, I.S. Dmitriev, N.Yu. Sdobnyakov
Tver State University
DOI: 10.26456/pcascnn/2026.18.363
Original article
Abstract: Ternary double-shell nanoparticles with a total number of 5100 atoms were investigated via comparative atomistic simulations using molecular dynamics and Monte Carlo methods to study their structural stability and phase transformations. Employing the many-body tight-binding potential, the caloric curves of the nanoparticles were calculated during sequential heating and cooling cycles within a temperature range of 300-1500 K. Based on the analysis of melting and crystallization intervals, it is shown that the layer ordering critically affects the thermal stability of the particles. It was established that configurations with an outer nickel layer lose their structural stability upon heating and undergo a rearrangement into asymmetric multipod structures. The Pd@Ni@Pt configuration proved to be the most stable, with its crystalline core preserving fcc symmetry at temperatures above 1500 K. The analysis of local density distributions showed that after full recrystallization of the nanoparticles, palladium atoms tend to exhibit surface segregation; furthermore, if copper was included in the composition, all three components are distributed almost uniformly throughout the volume, whereas nickel atoms occupy the central part of the nanoparticle, platinum forms the sub-surface layer, and palladium forms the outer shell.
Keywords: molecular dynamics method, Monte-Carlo method, MDSym, Metropolis, tight-binding potential, ternary double-shell nanoparticles, segregation, local structure
- Andrei Yu. Kolosov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-3805-0567
- Kseniya G. Savina – 4th year postgraduate student, General Physics Department, Tver State University, ORCID: 0000-0002-4916-4968
- Denis N. Sokolov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-2411-0143
- Egor S. Mitinev – 2nd year postgraduate student, General Physics Department, Tver State University
- Ivan A. Vzglyadov – 4th year student, General Physics Department, Tver State University
- Ivan S. Dmitriev – 4th year student, General Physics Department, Tver State University
- Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336
For citation:
Kolosov A.Yu., Savina K.G., Sokolov D.N., Mitinev E.S., Vzglyadov I.A., Dmitriev I.S., Sdobnyakov N.Yu. Sravnitelnoe atomisticheskoe modelirovanie strukturnoj stabilnosti/nestabilnosti ternarnykh dvukhobolochechnykh nanochastits Pd@X@Pt, X@Pd@Pt, Pt@X@Pd i X@Pt@Pd (X – Ni, Cu) [Comparative atomistic simulation of structural stability/instability of ternary double-shell nanoparticles Pd@X@Pt, X@Pd@Pt, Pt@X@Pd and X@Pt@Pd (X – Ni, Cu)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 363-379. DOI: 10.26456/pcascnn/2026.18.363. ⎘
Full article (in Russian): download PDF file
References:
1. Bogdanov S.S., Sdobnyakov N.Yu. [Zakonomernosti strukturoobrazovaniya v binarnykh nanochastitsakh GTSK-metallov pri termicheskom vozdeystvii: atomisticheskoe modelirovanie: monografiya] Regularities of structure formation in binary nanoparticles of FCC metals under thermal impact: atomistic simulation: monograph. Tver, Tver State University Publ., 2023, 144 p. DOI: 10.26456/bs.2023.144. (In Russian).
2. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI: 10.26456/sny.2025.408. (In Russian).
3. Samsonov V.M., Talyzin I.V., Kartoshkin A.Yu., Vasilyev S.A. Surface segregation in binary Cu–Ni and Au–Co nanoalloys and the core–shell structure stability/instability: thermodynamic and atomistic simulations, Applied Nanoscience, 2019, vol. 9, issue 1, pp. 119-133. DOI: 10.1007/s13204-018-0895-5.
4. Samsonov V.M., Talyzin I.V., Kartoshkin A.Yu. et al. On the problem of stability/instability of bimetallic core–shell nanostructures: molecular dynamics and thermodynamic simulations, Computational Materials Science, 2021, vol. 199, art. no. 110710, 11 p. DOI: 10.1016/j.commatsci.2021.110710.
5. Bogdanov S., Samsonov V., Sdobnyakov N. et al. Molecular dynamics simulation of the formation of bimetallic core–shell nanostructures with binary Ni–Al nanoparticle quenching, Journal of Materials Science, 2022, vol. 57, issue 28, pp. 13467–13480. DOI: 10.1007/s10853-022-07476-2.
6. Samsonov V., Romanov A., Talyzin I. et al. Puzzles of surface segregation in binary Pt–Pd nanoparticles: molecular dynamics and thermodynamic simulations, Metals, 2023, vol. 13, issue 7, art. no. 1269, 20 p. DOI: 10.3390/met13071269.
7. Kolosov A.Yu., Savina K.G., Nepsha N.I. et al. Comparative atomistic simulation of structure and structural transformations in Ni–Ag and Ni–Cu nanoalloys, Physics of the Solid State, 2024, vol. 66, issue 12, pp. 2027-2032. DOI: 10.61011/PSS.2024.12.60180.6394PA.
8. Nepsha N.I., Sokolov D.N., Kolosov A.Yu. et al. O probleme ustojchivosti/neustojchivosti v ternarnykh nanochastitsakh Cu–Fe–Ni tipa yadro–obolochka [On the problem of stability/instability in core–shell ternary Cu–Fe–Ni nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical-Chemical Aspects of the Study of Clusters, Nanostructures and Nanomaterials], 2024, issue 16, pp. 517–531. DOI: 10.26456/pcascnn/2024.16.517. (In Russian).
9. Nepsha N.I., Sdobnyakov N.Yu., Samsonov V.M. et al. Atomistic simulation of segregation in ternary Pt–Pd–Ni nanoalloy, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2024, vol. 18, issue 6, pp. 1388-1394. DOI: 10.1134/S1027451024701295.
10. Samsonov V., Nepsha N., Sdobnyakov N. et al. Chemical and structural segregation in Pt–Pd–Ni ternary nanosystems: molecular dynamics simulation, Materials Chemistry and Physics, 2025, vol. 340, art. no. 130827, 11 p. DOI: 10.1016/j.matchemphys.2025.130827.
11. Samsonov V.M., Talyzin I.V., Romanov A.A. et al. On the relation between spontaneous segregation of components in ternary Pt–Pd–Ni nanoparticles and stability of core–shell nanostructures: molecular dynamics study, Colloid Journal, 2025, vol. 87, issue 4, pp. 398-413. DOI: 10.7868/S3034543X25040111. (In Russian).
12. Ryu J., Choi J., Lim D.-H. et al. Morphology-controlled synthesis of ternary Pt–Pd–Cu alloy nanoparticles for efficient electrocatalytic oxygen reduction reactions, Applied Catalysis B: Environmental, 2015, vol. 174–175, pp. 526–532. DOI: 10.1016/j.apcatb.2015.03.019.
13. Wu Z.-P., Caracciolo D.T., Maswadeh Y. et al. Alloying–realloying enabled high durability for Pt–Pd-3d-transition metal nanoparticle fuel cell catalysts, Nature Communications, 2021, vol. 12, art. no. 859, 14 p. DOI: 10.1038/s41467-021-21017-6.
14. Zhang Y., Li H., Yan X. et al. Composition-controlled synthesis of Pt–Pd–Cu ternary metal nanoparticles for an enhanced electrocatalytic hydrogen evolution reaction, Nanoscale, 2025, vol. 17, issue 23, pp. 14415-14423. DOI: 10.1039/D5NR01065A.
15. de Souza M.K.R., Cardoso E.S.F., Fortunato G.V. et al. Combination of Cu–Pt–Pd nanoparticles supported on graphene nanoribbons decorating the surface of TiO2 nanotube applied for CO2 photoelectrochemical reduction, Journal of Environmental Chemical Engineering, 2021, vol. 9, art. no. 105803, 11 p. DOI: 10.1016/j.jece.2021.105803.
16. Shi W., Park A.H., Kwon Y.U. Scalable synthesis of (Pd,Cu)@Pt core–shell catalyst with high ORR activity and durability, Journal of Electroanalytical Chemistry, 2022, vol. 918, art. no. 116451, 9 p. DOI: 10.1016/j.jelechem.2022.116451.
17. Takeuchi Y., Lee H.-J., Dao A.T.N. et al. Formation of multishell Au@Ag@Pt nanoparticles by coreduction method: a microscopic study, Materials Today Chemistry, 2021, vol. 21, art. no. 100515, 7 p. DOI: 10.1016/j.mtchem.2021.100515.
18. Samsonov V., Lutsay A., Zhigunov D. et al. Self-assembly of three-shell nanostructures in initially homogeneous binary metallic nanoparticles: hybrid molecular dynamics/Monte Carlo simulations, Physica B: Condensed Matter, 2025, vol. 718, art. no. 417898, 12 p. DOI: 10.1016/j.physb.2025.417898.
19. Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N., Savina K.G. MDSym. Certificate RF, no. 2025683621, 2025. (In Russian).
20. Cleri F., Rosato V. Tight-binding potentials for transition metals and alloys, Physical Review B, 1993, vol. 48, issue 1, pp. 22-33. DOI: 10.1103/PhysRevB.48.22.
21. Nosé S. A unified formulation of the constant temperature molecular dynamics methods, The Journal of Chemical Physics, 1984, vol. 81, issue 1, pp. 511-519. DOI: 10.1063/1.447334.
22. Leimkuhler B., Noorizadeh E., Theil F. A gentle stochastic thermostat for molecular dynamics, Journal of Statistical Physics, 2009, vol. 135, issue 2, pp. 261-277. DOI: 10.1007/s10955-009-9734-0.
23. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
24. Sokolov D.N., Sdobnyakov N.Yu., Kolosov A.Yu., Ershov P.M., Bogdanov S.S. Metropolis. Certificate RF, no. 2019661915, 2019. (In Russian).
25. Ferrando R., Jellinek J., Johnston R.L. Nanoalloys: From theory to applications of alloy clusters and nanoparticles, Chemical Reviews, 2008, vol. 108, issue 3, pp. 845-910. DOI: 10.1021/cr040090g.
26. Samsonov V.M., Romanov A.A., Talyzin I.V. et. al. Surface segregation in binary metallic nanoparticles: atomistic simulation and thermodynamic modeling, Bulletin of the Russian Academy of Sciences: Physics, 2024, vol. 88, issue 5, pp. 739-744. DOI: 10.1134/s1062873824706512.
27. Samsonov V.M., Talyzin I.V., Zhigunov D.V. Segregatsiya komponentov kak neobkhodimoe uslovie ehvtekticheskoi prirody splava i nanosplava [Segregation of components as a necessary condition for the eutectic nature of an alloy and nanoalloy], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical-Chemical Aspects of the Study of Clusters, Nanostructures and Nanomaterials], 2024, issue 16. pp. 387-398. DOI: 10.26456/pcascnn/2024.16.387. (In Russian).
28. Eom N., Messing M.E., Johansson J., Deppert K. General trends in core–shell preferences for bimetallic nanoparticles, ACS Nano, 2021, vol. 15, issue 5, pp. 8883-8895. DOI: 10.1021/acsnano.1c01500.