Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Atomistic simulation of segregation in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations

K.G. Savina, S.V. Serov, A.Yu. Kolosov, D.N. Sokolov, D.A. Kravchenko, R.E. Grigoryev, S.S. Bogdanov, E.E. Arakcheev, N.Yu. Sdobnyakov

Tver State University

DOI: 10.26456/pcascnn/2026.18.466

Original article

Abstract: In this work, the molecular dynamics method was used to study modeling quaternary Ni-Cu-Fe-Co nanoparticles (containing 4000 atoms) with different initial configurations: a particle with a mixed three-component core and a nickel shell, a four-shell structure with concentric shells, a nanoalloy with a uniform distribution of components, a four-layer planar structure, two symmetrical variants with seven layers of atoms. The interatomic interaction was described by the tight-binding potential. The molecular dynamics experiment was carried out according to the following scheme: 1) heating from 300 to 1800 K, and then cooling to 300 K with relaxation at each step of 10 ps, 2) relaxation for 100 ps at temperature 300 K. For the first stage, two rates of thermally induced action were selected. The temperature ranges of hysteresis of the melting and crystallization processes were determined. Segregation patterns in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations are described using radial density distributions. The temperature parameters of the hysteresis associated with melting and crystallization processes have been evaluated. The obtained results demonstrate the variability of the properties of multicomponent nanoparticles, determined by both the initial conditions (morphology, composition, size) and the conditions of the molecular dynamics experiment (rate of thermally induced action).

Keywords: molecular dynamics, MDSym, tight-binding potential, quaternary nanoparticles, segregation, nickel, copper, cobalt, iron, local density

  • Kseniya G. Savina – 4th year postgraduate student, General Physics Department, Tver State University, ORCID: 0000-0002-4916-4968
  • Sergei V. Serov – 2nd year postgraduate student, General Physics Department, Tver State University, ORCID: 0009-0004-6219-6309
  • Andrei Yu. Kolosov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-3805-0567
  • Denis N. Sokolov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-2411-0143
  • Daria A. Kravchenko – 3rd year postgraduate student, General Physics Department, Tver State University
  • Roman E. Grigoryev – 4th year postgraduate student, General Physics Department, Tver State University
  • Sergei S. Bogdanov – Ph. D., Researcher, General Physics Department, Tver State University
  • Evgenii E. Arakcheev – 3rd year student, General Physics Department, Tver State University
  • Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336

For citation:

Savina K.G., Serov S.V., Kolosov A.Yu., Sokolov D.N., Kravchenko D.A., Grigoryev R.E., Bogdanov S.S., Arakcheev E.E., Sdobnyakov N.Yu. Atomisticheskoe modelirovanie segregatsii v chetyrekhkomponentnykh nanochastitsakh Ni-Cu-Fe-Co s razlichnymi nachalnymi konfiguratsiyami [Atomistic simulation of segregation in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 466-483. DOI: 10.26456/pcascnn/2026.18.466. ⎘

Full article (in Russian): download PDF file

References:

1. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI:10.26456/sny.2025.408. (In Russian).
2. Veresov S.A., Savina K.G., Veselov A.D. et al. K voprosu izucheniya protsessov strukturoobrazovaniya v chetyrekhkomponentnykh nanochastitsakh [To the problem of investigating the processes of structure formation in four-component nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 371-382. DOI: 10.26456/pcascnn/2022.14.371. (In Russian).
3. Sdobnyakov N.Yu., Samsonov V.M., Serov S.V. et al. Atomistic simulation of thermoinduced structural transformations in four-component Cu–Au–Pt–Pd nanoalloys with different morphologies, Colloid Journal, 2025, vol. 87, issue 4, pp. 560-571. DOI: 10.1134/S1061933X25600526.
4. Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N. et al. Kompleksnyj podkhod k modelirovaniyu plavleniya i kristallizatsii v pyatikomponentnykh metallicheskikh nanochastitsakh: molekulyarnaya dinamika i metod Monte-Karlo [Complex approach to the simulation of melting and crystallization in five-component metallic nanoparticles: molecular dynamics and the Monte Carlo method], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 589-601. DOI: 10.26456/pcascnn/2023.15.589. (In Russian).
5. Kolosov A.Yu., Savina K.G., Veresov S.A. et al. Stsenarii strukturoobrazovaniya v chetyrekhkomponentnykh nanochastitsakh: atomisticheskoe modelirovanie [Scenarios of structure formation in quaternary nanoparticles: atomistic modeling], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 432-443. DOI: 10.26456/pcascnn/2023.15.432. (In Russian).
6. Kolosov A.Yu., Veresov S.A., Serov S.V. et al. Razmernyi effekt v chetyrekhkomponentnykh nanochastitsakh Au–Cu–Pd–Pt i ikh stabil’nost’ [Size effect in quaternary Au–Cu–Pd–Pt nanoparticles and their stability], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 361-372. DOI: 10.26456/pcascnn/2024.16.361. (In Russian).
7. Serov S.V., Nepsha N.I., Kolosov A.Yu. et al. Strukturnye prevrashcheniya v chetyrekhkomponentnykh nanosplavakh Cu-Au-Pt-Pd razlichnoj morfologii pri posledovatelnykh termoindutsirovannykh tsiklakh [Structural transformations in quaternary nanoalloys Cu-Au-Pt-Pd of different morphology under successive thermally induced cycles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 466-484. DOI: 10.26456/pcascnn/2025.17.466. (In Russian).
8. Dahale C., Srinivasan S., Mishra S. et al. Surface segregation in AgAuCuPdPt high entropy alloy: insights from molecular simulations, Molecular Systems Design & Engineering, 2022, vol. 7, issue 8, pp. 878-888. DOI: 10.1039/D2ME00045H.
9. Kolosov A.Yu., Nepsha N., Sokolov D.N. et al. Chemical and structural segregation in quaternary Ni-Cu-Fe-Co nanoparticles: atomistic simulation and experiment, ACS Physical Chemistry Au, 2026, vol. 6, issue 1, pp. 163-173. DOI: 10.1021/acsphyschemau.5c00102.
10. Ferrando R., Jellinek J., Johnston R.L. Nanoalloys: from theory to applications of alloy clusters and nanoparticles, Chemical Reviews, 2008, vol. 108, issue 3, pp. 845-910. DOI: 10.1021/cr040090g.
11. Eom N., Messing M.E., Johansson J. et al. General trends in core–shell preferences for bimetallic nanoparticles, ACS Nano, 2021, vol. 15, issue 5, pp. 8883–8895. DOI: 10.1021/acsnano.1c01500.
12. Samsonov V.M., Talyzin I.V., Kartoshkin A.Y. et al. Prediction of segregation in binary metal nanoparticles: thermodynamic and atomistic simulations, Physics of Metals and Metallography, 2019, vol. 120, issue 6, pp. 578-583. DOI: 10.1134/S0031918X19060115.
13. Samsonov V., Romanov A., Talyzin I. et al. Puzzles of surface segregation in binary Pt–Pd nanoparticles: molecular dynamics and thermodynamic simulations, Metals, 2023, vol. 13, issue 7, art. no. 1269, 20 p. DOI: 10.3390/met13071269.
14. Samsonov V.M., Romanov A.A., Talyzin I.V. et al. Surface segregation in binary metallic nanoparticles: atomistic simulation and thermodynamic modeling, Bulletin of the Russian Academy of Sciences: Physics, 2024, vol. 88, issue 5, pp. 739-744. DOI: 10.1134/s1062873824706512.
15. Romanovskii V.I., Kolosov A.Yu., Khort A.A. et al. Osobennosti sinteza nanochastits Cu-Ni: eksperiment i kompyuternoe modelirovanie [Features of Cu-Ni nanoparticle synthesis: experiment and computer simulation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2020, issue 12, pp. 293-309. DOI: 10.26456/pcascnn/2020.12.293.
16. Romanovski V., Sdobnyakov N., Roslyakov S. et al. Bimetallic CuNi nanoparticle formation: solution combustion synthesis and molecular dynamic approaches, Inorganic Chemistry, 2024, vol. 63, issue 52, pp. 24844-24854. DOI: 10.1021/acs.inorgchem.4c04260.
17. Sdobnyakov N., Khort A., Myasnichenko V., Podbolotov K., Romanovskaia E., Kolosov A., Sokolov D., Romanovski V. Solution combustion synthesis and Monte Carlo simulation of the formation of CuNi integrated nanoparticles, Computational Materials Science, 2020, vol. 184, art. no 109936, 12 p. DOI: 10.1016/j.commatsci.2020.109936.
18. Kolosov A.Yu., Savina K.G., Nepsha N.I. et al. Comparative atomistic simulation of structure and structural transformations in Ni-Ag and Ni-Cu nanoalloys, Physics of the Solid State, 2024, vol. 66, issue 12, pp. 2027-2032. DOI: 10.61011/PSS.2024.12.60180.6394PA.
19. Liao H., Fisher A., Xu Z.J. Surface segregation in bimetallic nanoparticles: A critical issue in electrocatalyst engineering, Small, 2015, vol. 11, issue 27, pp. 3221-3246. DOI: 10.1002/smll.201403380.
20. Bohra M., Grammatikopoulos P., Diaz R.E. et al. Surface segregation in chromium-doped NiCr alloy nanoparticles and its effect on their magnetic behavior, Chemistry of Materials, 2015, vol. 27, issue 9, pp. 3216-3225. DOI: 10.1021/acs.chemmater.5b00837.
21. Jia M., Liang D., Du Q. et al. Fe-Co-Ni-Cu high entropy magnetic nanoparticles with high magnetothermal properties, Scripta Materialia, 2024, vol. 247, art. no. 116119, 6 p. DOI: 10.1016/j.scriptamat.2024.116119.
22. Mao A., Xiang H., Ran X. et al. Plasma arc discharge synthesis of multicomponent Co-Cr-Cu-Fe-Ni nanoparticles, Journal of Alloys and Compounds, 2019, vol. 775, pp. 1177-1183. DOI: 10.1016/j.jallcom.2018.10.170.
23. Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N., Savina K.G. MDSym. Certificate RF, no. 2025683621, 2025. (In Russian).
24. Leimkuhler B., Noorizadeh E., Theil F. A gentle stochastic thermostat for molecular dynamics, Journal of Statistical Physics, 2009, vol. 135, issue 2, pp. 261-277. DOI: 10.1007/s10955-009-9734-0.
25. Cleri F., Rosato V. Tight-binding potentials for transition metals and alloys, Physical Review B, 1993, vol. 48, issue 1, pp. 22-33. DOI: 10.1103/PhysRevB.48.22.
26. Karolewski M.A. Tight-binding potentials for sputtering simulations with fcc and bcc metals, Radiation Effects and Defects in Solids, 2001, vol. 153, issue 3, pp. 239-255. DOI: 10.1080/10420150108211842.
27. Paz Borbón L.O. Computational studies of transition metal nanoalloys. Berlin, Heidelberg, Springer-Verlag, 2011, 155 p. DOI: 10.1007/978-3-642-18012-5.
28. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.

Content |