Imprint effect in spherulitic lead zirconate titanate thin films

S.V. Senkevich1,2, V.P. Pronin2, I.V. Ryzhov2, M.V. Staritsyn3, A.R. Dunkabash4, E.Yu. Kaptelov1, I.P. Pronin1

1 Ioffe Institute
2 The Herzen State Pedagogical University of Russia
3 NRC Kurchatov Institute, CRISM Prometey
4 Saint Petersburg State University of Industrial Technologies and Design

DOI: 10.26456/pcascnn/2026.18.133

Original article

Abstract: We investigated the microstructure and imprint (internal field) of spherulitic lead zirconate titanate thin films formed via a two-stage radio frequency magnetron sputtering process on Pt/TiO2/SiO2/Si substrates at various perovskite phase crystallization temperatures (Tann = 580–650°C). The films were subjected to a thermal treatment and application of a strong external field, and prolonged aging. Microstructural analysis using scanning electron microscopy revealed that increasing Tann led to a sharp increase (by a factor of 5-10) in the crystal lattice rotation rate; this effect is attributed to the recrystallization of the perovskite phase, accompanied by an increase in its density. It was found that the magnitude and orientation of the internal field in the films, determined from dielectric hysteresis loops, depended on the «phase» state of the films. Long-term aging (~ 108 s) had little effect on the internal field in the loose phase. In the dense phase, aging led to a significant change in the magnitude and direction of the internal field vector. The observed changes are attributed to strong bending deformation of the crystal lattice and the resulting directed diffusion of charged oxygen vacancies toward the upper film interface. The study discusses the role of the electronic subsystem and charged oxygen vacancies in the formation of the imprint (internal field) and in charge redistribution across the film thickness under the influence of external factors and the passage of time.

Keywords: radio frequency magnetron sputtering, lead zirconate titanate thin films, spherulitic microstructure, oxygen vacancies, Gorsky effect

  • Stanislav V. Senkevich – Ph. D., Senior Researcher, Ioffe Institute, Herzen State Pedagogical University of Russia, ORCID: 0000-0002-4503-1412
  • Vladimir P. Pronin – Dr. Sc., Professor, The Herzen State Pedagogical University of Russia, ORCID: 0000-0003-0997-1113
  • Igor V. Ryzhov – PhD, Associate Professor, The Herzen State Pedagogical University of Russia, ORCID: 0000-0002-9878-4338
  • Mikhail V. Staritsyn – Ph. D., Senior Researcher, NRC Kurchatov Institute, CRISM Prometey, ORCID: 0000-0002-0088-4577
  • Anife R. Dunkabash – Assistant, Department of Physics, Saint Petersburg State University of Industrial Technologies and Design, ORCID: 0000-0003-0202-1502
  • Evgeny Yu. Kaptelov – Ph. D., Senior Researcher, Ioffe Institute, ORCID: 0000-0002-7423-6943
  • Igor P. Pronin – Dr. Sc., Leading Researcher, Ioffe Institute, ORCID: 0000-0003-3749-8706

For citation:

Senkevich S.V., Pronin V.P., Ryzhov I.V., Staritsyn M.V., Dunkabash A.R., Kaptelov E.Yu., Pronin I.P. Effekt imprinta v tonkikh sferolitovykh plenkakh tsirkonata-titanata svintsa [Imprint effect in spherulitic lead zirconate titanate thin films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 133-143. DOI: 10.26456/pcascnn/2026.18.133. ⎘

Full article (in Russian): download PDF file

References:

1. Warren W.L., Dimos D., Pike G.E. et al. Voltage shifts and imprint in ferroelectric capacitors, Applied Physical Letters, 1995, vol. 67, issue 6, pp. 866-868. DOI: 10.1063/1.115531.
2. Akkopru-Akgun B. Trolier-McKinstry S. Tuning Nb solubility, electrical properties, and imprint through PbO stoichiometry in PZT films, Materials, 2023, vol. 16, issue 11, art. no. 3970, 17 p. DOI: 10.3390/ma16113970.
3. Shen G.Y., Zhu L.W., Wang Z.G. et al. Tuning self-polarization of epitaxial BiFeO3 thin films through Interface effects, ACS Applied Materials & Interfaces, 2024, vol. 16, issue 50, pp. 70038-70046. DOI: 10.1021/acsami.4c14995.
4. Xie M., Yu H., Zhang B. et al. Role of domain walls on imprint and fatigue in HfO2-based ferroelectrics, Physical Review B, 2025, vol. 111, issue 18, art. no. 184108, 7 p. DOI: 10.1103/PhysRevB.111.184108.
5. Foster N.F. The deposition and piezoelectric characteristics of sputtered lithium niobate films, Journal of Applied Physics, 1969, vol. 40, issue 1, pp. 420-423. DOI: 10.1080/10584580215468.
6. Sviridov E. Sem I., Alyoshin V. et al. Ferroelectric film self-polarization, MRS Online Proceedings Library, 1994, vol. 361, issue 1, pp. 141-146. DOI: 10.1557/PROC-361-141.
7. Frey J., Schlenkrich F., Schönecker A. Self-polarization and texture of wet chemically derived lead zirconate titanate thin films, Integrated Ferroelectrics, 2001, vol. 35, issue 1-4, pp. 195-113. DOI: 10.1080/10584580108016892.
8. Kholkin A.L. Brooks K.G., Taylor D.V. et al. Self-polarization effect in Pb(Zr,Ti)O3 thin films, Integrated Ferroelectrics, 1998, vol. 22, issue 1-4, pp. 525-533. DOI: 10.1080/10584589808208071.
9. Pronin I.P., Kaptelov E.Yu., Tarakanov E.A. et al. Self-polarization and migratory polarization in thin-film ferroelectric capacitor, Integrated Ferroelectrics, 2002, vol. 49, issue 1, pp. 285-294. DOI: 10.1080/10584580215468.
10. Bursian E.V., Zaikovski O.I., Makarov K.V. Polyarizatsiya segnetoelektricheskoj plastiny izgibom [Polarization of a ferroelectric plate by bending], Izvestiya AN SSSR, seriya fizicheskaya [Bulletin of the Academy of Sciences of the USSR. Physical Series], 1969, vol. 33, issue 7, pp. 1098-1101. (In Russian).
11. Yudin P.V., Tagantsev A.K. Fundamentals of flexoelectricity in solids, Nanotechnology, 2013, vol. 24, issue 43, art. no. 432001, 36 p. DOI: 10.1088/0957-4484/24/43/432001.
12. Bruchhaus R., Pitzer D., Schreiter M. et al. Optimized PZT thin films for pyroelectric IR detector arrays, Journal of Electroceramics, 1999, vol. 3, issue 2, pp. 151-162. DOI: 10.1023/A:1009995126986.
13. Staritsyn M.V., Kiselev D.A., Pronin V.P. et al. Osobennosti mikrostructury I svoistv tonkych sferolitovych plyonok PZT sformirovannych dvuchstadiinym vysokochastotnym metodom [Peculiarities of the microstructure and properties of thin spherulitic PZT films formed by a two-stage radio-frequency magnetron method], Fiziko-khimicheskie aspect izuchenya klasterov, nanostructure I nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, vol. 15, pp. 196-206. DOI: 10.26456/pcascnn/2023.15.196. (In Russian).
14. Hiboux S., Muralt P. Origin of voltage offset and built-in polarization in in-situ sputter deposited PZT thin films, Integrated Ferroelectrics, 2001, vol. 36, issue 1-4, pp. 83-92. DOI: 10.1080/10584580108015530.
15. Afanasjev V.P., Mosina G.N., Petrov A.A. et al. Specific properties of the PZT-based thin-film capacitor structures with excess lead oxide, Technical Physics Letters, 2001, vol. 27, issue 6, pp. 467-469. DOI: 10.1134/1.1383827.
16. Krupanidhi S.B. Resent advances in the deposition of ferroelectric thin films, Integrated Ferroelectrics, 1992, vol. 1, issue 2-4, pp. 161-180. DOI: 10.1080/10584589208215709.
17. Pronin V.P., Senkevich S.V., Kaptelov E.Yu., Pronin I.P. Features of the formation of a perovskite phase in thin polycrystalline Pb(Zr,Ti)O3 films, Journal of Surface Investigation. X-ray, Synchrotron and Neutron Techniques. 2010, vol. 4, issue 5, pp. 703-708. DOI: 10.1134/S1027451010050010.
18. Kolosov V.Yu., Tholen A.R. Transmission electron microscopy studies of the specific structure of crystals formed by phase transition in iron oxide amorphous films, Acta Materialia, 2000, vol. 48, issue 8, p. 1829-1840. DOI: 10.1016/S1359-6454(99)00471-1.
19. Osipov V.V., Kiselev D.A. et al. Internal field and self-polarization in lead zirconate titanate thin films, Physics of the Solid State, 2015, vol. 57, issue 9, pp. 1793-1799. DOI: 10.1134/S1063783415090267.
20. Gorsky W.S. Theorie des elastischen Nachwirkung in ungeordneten Mischkristallen (elastische Nachwirkung zweiter Art). Physikalische Zeitschrift Der Sowjetunion, 1935, vol. 8, p. 457-471.
21. Kosevich A.M. How a crystal flows, Soviet Physics Uspekhi, 1975, vol. 17, issue 6, pp. 920-930. DOI: 10.1070/PU1975v017n06ABEH004405.
22. Pronin I.P., Kukushkin S.A., Spirin V.V. et al. Formation mechanisms and the orientation of self-polarization in PZT polycrystalline thin films, Materials Physics and Mechanics, 2017, vol. 30, issue 1, pp. 20-34.

Content |