On the energetics of vacancy formation and diffusion in mesoporous materials
A.V. Shishulin, A.V. Shishulina
Nizhny Novgorod State Technical University named after R.E. Alekseev
DOI: 10.26456/pcascnn/2026.18.304
Short communication
Abstract: This paper examines the dependence of the vacancy formation energy and the activation energy of volume diffusion in the «skeleton» of a mesoporous material on the geometric characteristics (volume and shape) of the pores distributed within the material. The geometric features of the pores were defined within a fractal-geometric approach by their effective diameter and fractal dimension. The presented estimates indicate that the effect characteristic of nanoparticles, associated with the significant dependence of the vacancy formation energy and the activation energy of volume diffusion on the particle size and shape, can also occur in mesoporous materials (with a characteristic pore size from 5 to 50 nm), even though the mesoporous objects themselves can have macroscopic dimensions. Using porous gold as an example, it is shown that a decrease in the pore volume and a «complication» of their morphology lead to a noticeable reduction in the considered energy characteristics. The results were obtained within the framework of the cohesive energy-based model.
Keywords: vacancy formation energy, volume diffusion activation energy, mesoporous materials, fractal dimension, cohesion, size distribution, Hardy-Ramanujan-Rademacher formula
- Alexander V. Shishulin – Ph. D., Associate Professor, Nizhny Novgorod State Technical University named after R.E. Alekseev, ORCID: 0000-0003-2370-5313
- Anna V. Shishulina – Ph. D., Associate Professor, Nizhny Novgorod State Technical University named after R.E. Alekseev, ORCID: 0009-0000-0681-5022
For citation:
Shishulin A.V., Shishulina A.V. K voprosu ob energii obrazovaniya vakansii i energii aktivatsii diffuzii v mezoporistykh materialakh [On the energetics of vacancy formation and diffusion in mesoporous materials], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 304-312. DOI: 10.26456/pcascnn/2026.18.304. ⎘
Full article (in Russian): download PDF file
References:
1. Lu K. Nanoparticulate materials: synthesis, characterization, and processing. Hoboken, Wiley, 2012, 464 p. DOI: 10.1002/9781118408995.
2. New Frontiers in nanoparticles and nanocomposite materials, ed by. A. Öchsner, A. Shokuhfar. Berlin, Heidelberg, Springer, 2013, 371 p. DOI: 10.1007/978-3-642-14697-8.
3. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI:10.26456/sny.2025.408. (In Russian).
4. Essajai R., Benhouria Y., Rachadi A. et al. Shape-dependent structural and magnetic properties of Fe nanoparticles studied through simulation methods, RSC Advances, 2019, vol. 9, issue 38, pp. 22057-22063. DOI: 10.1039/C9RA03047F.
5. Guisbiers G. αshape, birth of one universal parameter? Key Engineering Materials, 2010, vol. 444, pp. 69-80. DOI: 10.4028/www.scientific.net/KEM.444.69.
6. Guisbiers G. Size-dependent material properties towards a universal equation, Nanoscale Research Letters, 2010, vol. 5, issue 7, art. no. 1132, 5 p. DOI: 10.1007/s11671-010-9614-1.
7. Bogdanov S.S., Sdobnyakov N.Yu. Zakonomernosti strukturoobrazovaniya v binarnykh nanochastitsakh GTsK-metallov pri termicheskom vozdejstvii: atomisticheskoe modelirovanie [Patterns of structure formation in binary nanoparticles of FCC metals under thermal exposure: atomistic simulation]. Tver, Tver State University Publ., 2023, 144 p. DOI: 10.26456/bs.2023.144. (In Russian).
8. Sdobnyakov N.Yu, Kolosov A.Yu, Sokolov D.N. et al. Kompleksnyj podkhod k modelirovaniyu plavleniya i kristallizatsii v pyatikomponentnykh metallicheskikh nanochastitsakh: molekulyarnaya dinamika i metod Monte-Karlo [Complex approach to the simulation of melting and crystallization in five-component metallic nanoparticles: molecular dynamics and the Monte Carlo method], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 589-601. DOI: 10.26456/pcascnn/2023.15.589 (in Russian).
9. Shishulin A.V., Shishulina A.V. Vliyanie iskhodnogo sostava na fazovye ravnovesiya pri tverdofaznom rasslaivanii v nanochastitsakh binarnykh splavov (na primere sistemy W-Cr) [Influence of the initial composition on the phase equilibria in the case of the solid phase separation in binary alloy nanoparticles (exemplifying on the W-Cr system)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 299-307. DOI: 10.26456/pcascnn/2023.15.299 (In Russian).
10. Shishulin A.V., Shishulina A.V., Kuptsov A.V. Osobennosti fazovykh ravnovesij «zhidkost’ – tverdoe telo» v nanochastitsakh sistemy Six-Ge1-x pri razlichnom vzaimnom raspolozhenii faz [Peculiarities of «liquid – solid» phase equilibria in Six-Ge1-x nanoparticles for various mutual arrangement of phases], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 437-447. DOI: 10.26456/pcascnn/2024.16.437 (In Russian).
11. Shishulin A.V., Shishulina A.V. One more parameter determining the stratification of solutions in small-volume droplets, Journal of Engineering Physics and Thermophysics, 2022, vol. 95, issue 6, pp. 1374-1382. DOI: 10.1007/s10891-022-02606-8.
12. Shishulin A.V., Potapov A.A., Shishulina A.V. On the transition between ferromagnetic and paramagnetic states in mesoporous materials with fractal morphology, Eurasian Physical Technical Journal, 2021, vol. 18, issue 2(36), pp. 6-11. DOI: 10.31489/2021NO2/6-11.
13. Shishulin A.V., Shishulina A.V. K voprosu ob uprugikh kharakteristikakh mezoporistykh materialov [Several notes on the elastic properties of mesoporous materials], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 308-316. DOI: 10.26456/pcascnn/2023.15.308 (in Russian).
14. Shishulin A.V., Shishulina A.V., Kuptsov A.V. K voprosu o plavlenii mezoporistykh materialov [Several notes on the melting behavior of mesoporous materials], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostructur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 427-436. DOI: 10.26456/pcascnn/2024.16.427 (in Russian).
15. Shishulin A.V., Shishulina A.V. O shirine zapreshchennoj zony v mezoporistykh poluprovodnikakh [On the energy bandgap in mesoporous semiconductors], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 317-327. DOI: 10.26456/pcascnn/2025.17.317 (In Russian).
16. Goyal M., Goyal V. Effects of size and temperature on the vacancy concentration in nanomaterials, Pramana, 2021, vol. 95, art. no. 99, 8 p. DOI: 10.1007/s12043-021-02127-8.
17. Yu X., Zhan Z. The effects of the size of nanocrystalline materials on their thermodynamic and mechanical properties, Nanoscale Research Letters, 2014, vol. 9, art. no. 616, 6 p. DOI: 10.1186/1556-276X-9-516.
18. Attarian Shandiz M. Effective coordination number model for the size dependency of physical properties of nanocrystals, Journal of Physics: Condensed Matter, 2008, vol. 20, no. 32, art. no. 325237, 9 p. DOI: 10.1088/0953-8984/20/32/325237.
19. Tiwari G.P., Patil R.V. A correlation between vacancy formation energy and cohesive energy, Scripta metallurgica, 1975, vol. 9, issue 8, pp. 833-836. DOI: 10.1016/0036-9748(75)90564-5.
20. Guisbiers G. Schottky defects in nanoparticles, The Journal of Physical Chemistry C, 2011, vol. 115, issue 6, pp. 2616-2621. DOI: 10.1021/jp108041q.
21. Yu X., Zhan Z., Rong J. et al. Vacancy formation energy and size effects, Chemical Physics Letters, 2014, vol. 600, pp. 43-45. DOI: 10.1016/j.cplett.2014.03.046.
22. Aqra F., Ayyad A. Surface free energy of alkali and transition metal nanoparticles, Applied Surface Science, 2014, vol. 324, pp. 308-313. DOI: 10.1016/j.apsusc.2014.07.004.
23. Ivanov D.V., Antonov A.S., Semenova E.M. et al. Razlichnye skhemy polucheniya fraktal'nogo rel'efa nanorazmernykh plenok platiny [Different schemes for obtaining fractal relief of nanosized platinum films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 156-165. DOI: 10.26456/pcascnn/2021.13.156.
24. Anofriev V.A., Antonov A.S., Ivanov D.V., Semenova E.M., Ivanova A.I., Tretiakov S.A., Afanasiev M.S., Sdobnyakov N.Yu. Pattern formirovaniya fraktal'nogo rel'efa dlya nanorazmernykh plyonok molibdena [Formation pattern of fractal relief for nanosized molybdenum films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 17-31. DOI: 10.26456/pcascnn/2023.15.017 (In Russian).
25. Fedoseev V.B., Shishulin A.V. On the size distribution of dispersed fractal particles, Technical Physics, 2021, vol. 66, issue 1, pp. 34-40. DOI: 10.1134/S1063784221010072.
26. Chuvil’deev V.N., Nokhrin A.V., Kopylov V.I. et al. Spark plasma sintering for high-speed diffusion bonding of the ultrafine-grained near-α Ti-5Al-2V alloy with high strength and corrosion resistance for nuclear engineering, Journal of Materials Science, 2019, vol. 54, issue 24, pp. 14926-14949. DOI: 10.1007/s10853-019-03926-6.
27. Fedoseev V.B. Vliyaniye temperatury i davleniya na fraktal’nuyu razmernost’ defektov kristallicheskoy struktury [Influence of the temperature and pressure on the fractal dimension of crystal structure defects], Butlerosvkiye soobscheniya [Butlerov Communications], 2010, vol. 23, issue 14, pp. 26-42 (in Russian).
28. Fedoseev V.B. The use of fractal geometry for the thermodynamic description of the thre-dimensional crystal structure elements, Pis’ma o materialakh [Letters on Materials], 2012, vol. 2, issue 2, pp. 78-83. DOI: 10.22226/2410-3535-2012-2-78-83.