Dielectric properties of Pt/0,91NaNbO3-0,09SrZrO3/SrRuO3/MgO(001) antiferroelectric thin films
D.S. Pavlenko1, A.L. Bulanova1, A.V. Pavlenko1,2
1 Southern Federal University
2 Southern Scientific Center of the RAS
DOI: 10.26456/pcascnn/2026.18.112
Original article
Abstract: In this work, 0,91NaNbO3-0,09SrZrO3 (NZNO-0,09) thin films were grown on SrRuO3/MgO(001) substrates using the high-frequency magnetron sputtering method in an O2 atmosphere. A comprehensive study of their crystal structure, dielectric response, and polarization characteristics was carried out using X-ray diffraction analysis, dielectric spectroscopy, and measurements of dielectric hysteresis loops. It was established that the obtained films are single-phase, impurity-free, and at room temperature they exist in the antiferroelectric phase. At the same time, in contrast to ceramics of the same composition, they exhibit relaxor behavior in terms of the temperature–frequency dependence of the relative permittivity ε and dielectric loss tangent tg δ. Analysis of the dispersion of ε and tan δ in the temperature range T = 305-460 K and frequency range f = 0,2-500 kHz revealed the presence of contributions from two relaxation processes associated with different polarization mechanisms. A model describing the observed spectra is proposed. The paper discusses the origins of the observed features in the formation of dielectric properties, as well as the high energy efficiency of the NZNO-0,09 films. The obtained results are important for understanding the mechanisms governing the property formation in antiferroelectric nanoscale thin films in view of their application in modern functional electronics.
Keywords: antiferroelectric, dielectric properties, thin films, polarization, high-frequency magnetron sputtering method
- Danil S. Pavlenko – 1st year graduate student, Research Institute of Physics, Southern Federal University, ORCID: 0009-0008-9069-7302
- Anna L. Bulanova – Senior Lecturer, Department of General Physics, Southern Federal University
- Anatoly V. Pavlenko – Dr. Sc., Leading Researcher, Research Institute of Physics, Southern Federal University, Head of the Department of Physics, Chemistry, and Computer Science Southern Scientific Center of the RAS, ORCID: 0000-0002-4257-2950
For citation:
Pavlenko D.S., Bulanova A.L., Pavlenko A.V. Dielektricheskie svojstva tonkikh plenok antisegnetoelektrika Pt/0,91NaNbO3-0,09SrZrO3/SrRuO3/MgO(001) [Dielectric properties of Pt/0,91NaNbO3-0,09SrZrO3/SrRuO3/MgO(001) antiferroelectric thin films], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 112-121. DOI: 10.26456/pcascnn/2026.18.112. ⎘
Full article (in Russian): download PDF file
References:
1. Lui Z., Lu Z., Ye J. et al Antiferroelectrics for energy storage applications: a review, Advanced Materials Technologies, 2018, vol. 3, issue 9, art. no. 1800111, 21 p. DOI: 10.1002/admt.201800111.
2. Setter N., Damjanovic D., Eng L. et al. Ferroelectric thin films: review of materials, properties, and applications, Journal of Applied Physics, 2006, vol. 100, issue 5, pp. 051606-1-051606-46. DOI: 10.1063/1.2336999.
3. Smirnova E.P., Passet R.S., Sotnikova G.Yu. et al. Evolution of phase transitions and the energy conservation effect in SrTiO3−PbZrO3 solid solutions, Solid State Physics, 2023, vol. 65, no. 5, pp. 828-832. DOI: 10.21883/PSS.2023.05.56057.30.
4. Vakhrushev S.B., Bronvald Yu.A., Petroukhno K.A. et al. Antiferrodistortive soft mode in PbZr0.024Ti0.976O3 crystal, Physics of the Solid State, 2021, vol. 63, issue 12, pp. 1840-1846. DOI: 10.1134/S1063783421100383.
5. Ueda R., Shirane G. X-ray study on phase transition of lead zirconate, PbZrO3, Journal of the Physical Society of Japan, 1951, vol. 6, issue 3, pp. 209-210. DOI: 10.1143/jpsj.6.209.
6. Htet C.S., Nayak S., Manjón-Sanz A. et al. Atomic structural mechanism for ferroelectric-antiferroelectric transformation in perovskite NaNbO3, Physical Review B, 2022, vol. 105, issue 17, pp. 174113-1-174113-13. DOI: 10.1103/PhysRevB.105.174113.
7. Guo H., Shimizu H., Mizuno Y., Randall C.A. Strategy for stabilization of the antiferroelectric phase (Pbma) over the metastable ferroelectric phase (P21ma) to establish double loop hysteresis in lead-free (1−x)NaNbO3−xSrZrO3 solid solution, Journal of Applied Physics, 2015, vol. 117, issue 21, pp. 214103-1-214103-6. DOI: 10.1063/1.4921876.
8. Yuzyuk Yu.I., Zakharchenko I.N., Alyoshin V.A. et al. Influence of the growth mechanism and thermoelastic stresses on the lattice dynamics of heteroepitaxial films of barium strontium titanate, Physics of the Solid State, 2007, vol. 49, issue 9, pp. 1759-1765. DOI: 10.1134/S1063783407090247.
9. Pavlenko A.V., Zinchenko S.P., Stryukov D.V., Kovtun A.P. Nanorazmernye plenki niobata bariya-strontsiya: osobennosti polucheniya v plazme vysokochastotnogo razryada, struktura i fizicheskie svojstva [Nanosized films of barium-strontium niobate: features of production in plasma of high-frequency discharge, structure and physical properties]. Rostov-on-Don, The Southern Scientific Centre of the RAS Publ., 2022, 242 p. (In Russian).
10. Bogatin A.S., Turik A.V. Protsessy relaksatsionnoj polyarizatsii v dielektrikakh s bol'shoj skvoznoj elektroprovodnost'yu [Processes of relaxation polarization in dielectrics with large through-current conductivity]. Rostov-on-Don, Publishing House «Feniks», 2013, 256 p. (In Russian).
11. Ma C., Tan X. Phase diagram of unpoled lead-free (1−x)(Bi1/2Na1/2) TiO3–xBaTiO3 ceramics, Solid State Communications, 2010, vol. 150, issues 33-34, pp. 1497-1500. DOI: 10.1016/j.ssc.2010.06.006.
12. Nguyen M.D. Effect of substrate and electrode on the crystalline structure and energy storage performance of antiferroelectric PbZrO3 films, Thin Solid Films, 2021, vol. 717, art. no. 138441, 33 p. DOI: 10.1016/j.tsf.2020.138441.