Adsorption of a beryllium monolayer on the surface of GaN(0001)
M.N. Lapushkin
Ioffe Institute
DOI: 10.26456/pcascnn/2026.18.409
Original article
Abstract: The density functional method was used to calculate the adsorption of a monolayer of beryllium atoms on a GaN(0001) surface. The surface was modeled within the framework of a 2×2 supercell geometry containing 10 GaN bilayers. The initial GaN(0001) surface exhibits a metallic conductivity caused by the presence of a band of surface states near the Fermi level. One beryllium monolayer corresponded to a concentration of one Be atom per one surface Ga atom. Calculations of the electron density of states and the adsorption energy were performed for a stable configuration during the adsorption of Be atoms over surface Ga atoms (on-top position) and during the formation of trimer Be clusters with a side length of 2,036 Å within the hexagonal GaN cell. It was found that adsorption is energetically most favorable in the trimer configuration. This non-standard configuration became possible due to the small size of the Be atom. The adsorption energy of Be is 2,125 eV. It was shown that the deposition of a Be monolayer causes only minor structural reconstruction of the substrate: the distance between the Ga and N layers in the surface GaN bilayer increases by 0,102 Å. The adsorption of beryllium leads to the formation of a wide band of surface states below the Fermi level, and the chemical bond with the GaN(0001) substrate is covalent in nature and is provided by the hybridization of the valence electrons of Be and the surface Ga atoms.
Keywords: density functional method, electronic structure, interface, surface, adsorption, beryllium, GaN
- Mikhail N. Lapushkin – Ph. D., Docent, Senior Researcher, Ioffe Institute, ORCID: 0000-0002-9042-7889
For citation:
Lapushkin M.N. Adsorbtsiya monosloya berilliya na poverkhnosti GaN(0001) [Adsorption of a beryllium monolayer on the surface of GaN(0001)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 409-417. DOI: 10.26456/pcascnn/2026.18.409. ⎘
Full article (in Russian): download PDF file
References:
1. Qian X., Zhou J., Chen G. Phonon-engineered extreme thermal conductivity materials, Nature Materials, 2021, vol. 20, issue 9, pp. 1188-1202. DOI: 10.1038/s41563-021-00918-3.
2. Buffolo M., Caria A., Piva F. et al. Defects and reliability of GaN‐based LEDs: review and perspectives, Physica Status Solidi (a), 2022, vol. 219, issue 8, art. no. 2100727, 25 p. DOI: 10.1002/pssa.202100727.
3. Emon A.I., Mirza, A. B., Kaplun, J. et al. A review of high-speed GaN power modules: state of the art, challenges, and solutions, IEEE Journal of Emerging and Selected Topics in Power Electronics, 2022, vol. 11, issue 3, pp. 2707-2729. DOI: 10.1109/JESTPE.2022.3232265.
4. Zhang Y., Xu R., Kang Q. et al. Recent advances on gan-based micro-leds, Micromachines, 2023, vol. 14, issue 5, art. no. 991, 19 p. DOI: 10.3390/mi14050991.
5. Sun R., Lai J., Chen W., Zhang B. GaN power integration for high frequency and high efficiency power applications: a review, IEEE Access, 2020, vol. 8, pp. 15529-15542. DOI: 10.1109/ACCESS.2020.2967027.
6. Bermudez V.M. The fundamental surface science of wurtzite gallium nitride, Surface Science Reports, 2017, vol. 72, issue 4, pp. 147-315. DOI: 10.1016/j.surfrep.2017.05.001.
7. Lyons J.L., Alkauskas A., Janotti A., Van de Walle C.G. First‐principles theory of acceptors in nitride semiconductors, Physica Status Solidi (b), 2015, vol. 252, issue 5, pp. 900-908. DOI: 10.1016/j.cossms.2024.101148.
8. Reshchikov M.A. Photoluminescence from vacancy‐containing defects in GaN, Physica Status Solidi (a), 2023, vol. 220, issue 10, art. no. 2200402, 8 p. DOI: 10.1002/pssa.202200402.
9. Yeoh K.H., Yoon T.L., Lim T.L, Rusi, Ong D.S., Monolayer GaN functionalized with alkali metal and alkaline earth metal atoms: A first-principles study, Superlattice Microstructures, 2019, vol. 130, pp. 428-436. DOI: 10.1016/j.spmi.2019.05.011.
10. Northrup J. E.. Incorporation of beryllium on the clean and indium-terminated GaN(0001) surface, Applied Physics Letters, 2001, vol. 78, issue 19, pp. 2855-2857. DOI: 10.1063/1.1368369.
11. Tian J., Liu L., Lu F., Theoretical research on p-type doping two-dimensionalGaN based on first-principles study, International Journal of Energy Research, 2020, vol. 44, issue 7, pp. 6058-6067. DOI: 10.1002/er.5380
12. Van de Walle C. G., Limpijumnong S., Neugebauer J. First-principles studies of beryllium doping of GaN, Physical Review B, 2001, vol. 63, issue 24, pp. 245205-17. DOI: 10.1103/PhysRevB.63.245205.
13. Lapushkin M.N. Adsorbtsiya bariya na poverhnosti GaN(0001) [Adsorption of barium on the surface of GaN(0001)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 210-218. DOI: 10.26456/pcascnn/2024.16.210. (In Russian).
14. Lapushkin M.N. Adsorbtsiya monosloya magniya na poverhnosti GaN(0001) [Adsorption of a magnesium monolayer on the surface of GaN(0001)], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 447-454. DOI: 10.26456/pcascnn/2025.17.447. (In Russian).
15. Giannozz, P., Baroni S., Bonini N. QUANTUM ESPRESSO: a modular and open-source software project for quantum simulations of materials, Journal of Physics: Condensed Matter, 2009, vol. 21, no. 39, art. no. 395502, 19 p. DOI: 10.1088/0953- 8984/21/39/395502.
16. Perdew J.P., Zunger A. Self-interaction correction to density-functional approximations for many-electron systems, Physical Review B, 1981, vol. 23, issue 10, pp. 5048-5079. DOI: 10.1103/PhysRevB.23.5048.
17. Nishihara S. BURAI 1.3 A GUI of Quantum ESPRESSO. Available at: https://nisihara.wixsite.com/burai (accessed 20.06.2026).
18. Nielsen D.O., Van de Walle C.G., Pantelides S.T. et al. First-principles approach to closing the 10–100 eV gap for charge-carrier thermalization in semiconductors, Physical Review B, 2023, vol. 108, issue 15, pp. 155203-1-155203-20. DOI: 10.1103/PhysRevB.108.155203.