Hydrogen embrittlement of high-entropy rare-earth alloys: structure and magnetic properties of the resulting trihydrides
P.A. Krot, Y.A. Ovchenkova, N.Yu. Pankratov, I.S. Tereshina, V.N. Verbetsky
Lomonosov Moscow State University
DOI: 10.26456/pcascnn/2026.18.687
Original article
Abstract: The synthesis and investigation of the structural and magnetic properties of the trihydrides of high entropy rare-earth alloys was carried out. It was determined that the alloys containing only heavy rare-earth elements adopted the magnesium-type structure (space group P63/mmc), while the one made of both heavy and light rare-earth elements had the rhombohedral lattice of samarium type (Rm). For all the studied trihydrides the complex hexagonal holmium trihydride-type structure (Pc1) was found. Hydrogen uptake in the alloys led to the lattice expansion, the occurrence of stress and spontaneous cracking along the grain boundaries, as a result of which the ingot crumbled into powder without mechanical grinding. Lanthanide contraction effect for both the studied alloys and their trihydrides was observed. The paramagnetic Curie temperatures, effective magnetic moments, and the prevailing type of exchange interaction were determined for each trihydride. It was found out that hydrogen uptake suppressed magnetic ordering down to 2 K.
Keywords: high-entropy alloys, rare earths, hydrides, magnetic properties, crystal structure, lanthanide contraction
- Pavel A. Krot – 4th year postgraduate student, Department of Chemistry, Lomonosov Moscow State University
- Yulia A. Ovchenkova – Ph. D., Associate Professor, Department of Physics, Lomonosov Moscow State University, ORCID: 0000-0002-2278-9191
- Nikolay Yu. Pankratov – Ph. D., Senior Lecturer, Department of Physics, Lomonosov Moscow State University, ORCID: 0000-0003-1565-2661
- Irina S. Tereshina – Dr. Sc., Leading Researcher, Department of Physics, Lomonosov Moscow State University, ORCID: 0000-0003-3633-3440
- Viktor N. Verbetsky – Dr. Sc., Professor, Department of Chemistry, Lomonosov Moscow State University
For citation:
Krot P.A., Ovchenkova Y.A., Pankratov N.Yu., Tereshina I.S., Verbetsky V.N. Vodorodnoe okhrupchivanie vysokoentropijnykh splavov redkozemelnykh elementov: struktura i magnitnye svojstva obrazuyushchikhsya trigidridov [Hydrogen embrittlement of high-entropy rare-earth alloys: structure and magnetic properties of the resulting trihydrides], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 687-704. DOI: 10.26456/pcascnn/2026.18.687. ⎘
Full article (in Russian): download PDF file
References:
1. Tsai M.-H., Yeh J.-W. High-entropy alloys: a critical review, Materials Research Letters, 2014, vol. 2, issue 3, pp. 107-123. DOI: 10.1080/21663831.2014.912690.
2. Miracle D.B., Senkov O.N. A critical review of high entropy alloys and related concepts, Acta Materialia, 2017, vol. 122, pp. 448-511. DOI: 10.1016/j.actamat.2016.08.081.
3. Gromov V.E., Konovalov S.V., Ivanov Y.F., Osintsev K.A. Structure and properties of high-entropy alloys, Advanced Structured Materials, vol. 107. Cham, Springer, 2021, X+110 p. DOI: 10.1007/978-3-030-78364-8.
4. Yang C. Advances in high-entropy alloys’ microstructure, properties and preparation, Metals, 2026, vol. 16, issue 6, pp. 607-610. DOI: 10.3390/met16060607.
5. Miracle D.B. High-entropy alloys: a current evaluation of founding ideas and core effects and exploring «nonlinear alloys», The Journal of the Minerals, Metals and Materials Society, 2017, vol. 69, issue 11, pp. 2130-2136. DOI: 10.1007/s11837-017-2527-z.
6. Pickering E.J., Jones N.G. High-entropy alloys: a critical assessment of their founding principles and future prospects, International Materials Reviews, 2016, vol. 61, issue 3, pp. 183-202. DOI: 10.1080/09506608.2016.1180020.
7. Wang X., Guo W., Fu Y. High-entropy alloys: emerging materials for advanced functional applications, Journal of Materials Chemistry A, 2020, vol. 9, issue 2, pp. 663-701. DOI: 10.1039/D0TA09601F.
8. Wang J., Jia D., Gao Q., Fu Y., Wu X. High-entropy alloy coatings: a systematic review on composition design, microstructural mechanisms, and multifunctional application, Materials & Design, 2025, vol. 258, art. no. 114715, 5 p. DOI: 10.1016/j.matdes.2025.114715.
9. Mikheeva V.I., Kost M.E. The hydrides of the rare-earth metals, Russian Chemical Reviews, 1960, vol. 29, issue 1, pp. 28-37. DOI: 10.1070/RC1960v029n01ABEH001216.
10. Bos W.G., Gayer K.H. The rare earth hydrides, Journal of Nuclear Materials, 1966, vol. 18, issue 1, pp. 1-30. DOI: 10.1016/0022-3115(66)90092-4.
11. Korst W.L., Warf J.C. Rare earth-hydrogen systems. I. Structural and thermodynamic properties, Inorganic Chemistry, 1966, vol. 5, issue 10, pp. 1719-1726. DOI: 10.1021/ic50044a018.
12. Jiang Z., Wang J. Cao D. Research progress of rare earth-based hydrogen storage alloys, Key Engineering Materials, 2020, vol. 861, pp. 354-362. DOI: 10.4028/www.scientific.net/KEM.861.354.
13. Xu Y., Yang X., Li Y. et al. Rare-earth metal-based materials for hydrogen storage: progress, challenges, and future perspectives, Nanomaterials, 2024, vol. 14, issue 20, pp. 1671-1690. DOI: 10.3390/nano14201671.
14. Sahlberg M., Karlsson D., Zlotea C. Jansson U. Superior hydrogen storage in high entropy alloys, Scientific Reports, 2016, vol. 6, art. no. 36770, 6 p. DOI: 10.1038/srep36770.
15. Karlsson D., Ek G., Cedervall J. et al. Structure and hydrogenation properties of a HfNbTiVZr high-entropy alloy, Inorganic Chemistry, 2018, vol. 57, issue 4, pp. 2103-2110. DOI: 10.1021/acs.inorgchem.7b03004.
16. Zlotea C., Sow M.A., Ek G. et al. Hydrogen sorption in TiZrNbHfTa high entropy alloy, Journal of Alloys and Compounds, 2019, vol. 775, pp. 667-674. DOI: 10.1016/j.jallcom.2018.10.108.
17. Zhang C., Song A., Yuan Y. et al. Study on the hydrogen storage properties of a TiZrNbTa high entropy alloy, International Journal of Hydrogen Energy, 2020, vol. 45, issue 8, pp. 5367-5374. DOI: 10.1016/j.ijhydene.2019.05.214.
18. Li T., Xie Z., Zhou W. et al. Study on the hydrogen absorption properties of a YGdTbDyHo rare-earth high-entropy alloy, International Journal of Minerals, Metallurgy and Materials, 2025, vol. 32, issue 1, pp. 127-135. DOI: 10.1007/s12613-024-2933-5.
19. Ragg O.M., Keegan G., Nagel H., Harris I.R. The HD and HDDR processes in the production of Nd-Fe-B permanent magnets, International Journal of Hydrogen Energy, 1997, vol. 22, issues 2-3, pp. 333-342. DOI: 10.1016/S0360-3199(96)00174-7.
20. Poenaru I., Patroi E.A., Patroi D., Iorga A., Manta E. HDDR as advanced processing method and recycling technology to address the rare-earth resource criticality in high performance Nd2Fe14B magnets production, Journal of Magnetism and Magnetic Materials, 2023, vol. 577, art. no. 170777, 19 p. DOI: 10.1016/j.jmmm.2023.170777.
21. Liu R., Bulyk I.I., Yang M., Wang Y., Wang H. Features of the solid HDDR process in sintered (Nd,Pr,Gd)-Fe-B magnets at low hydrogen pressure and low temperature, Materials, 2025, vol. 18, issue 17, pp. 4019-4036. DOI: 10.3390/ma18174019.
22. Huot J., Cuevas F., Deledda S. et al. Mechanochemistry of metal hydrides: recent advances, Materials, 2019, vol. 12, issue 17, art. no. 2778, 44 p. DOI: 10.3390/ma12172778.
23. Duwal S., Stavila V., Spataru C. et al. Enhancement of hydrogen absorption and hypervalent metal hydride formation in lanthanum using cryogenic ball milling, arXiv:2506.23980, 2025, 24 p. DOI: 10.48550/arXiv.2506.23980.
24. Pommerin A., Felderhoff M., Schüth F., Weidenthaler C. Influence of the ball milling conditions on the preparation of rare earth aluminum hydrides, Scripta Materialia, 2010, vol. 63, issue 11, pp. 1128-1131. DOI: 10.1016/j.scriptamat.2010.08.020.
25. Zaluski L., Zaluska A., Ström-Olsen J.O. Nanocrystalline metal hydrides, Journal of Alloys and Compounds, 1997, vols. 253-254, pp. 70-79. DOI: 10.1016/S0925-8388(96)02985-4.
26. Nielsen T.K., Besenbacher F., Jensen T.R. Nanoconfined hydrides for energy storage, Nanoscale, 2011, vol. 3, issue 5, pp. 2086-2098. DOI: 10.1039/c0nr00725k
27. Palmero P. Structural ceramic nanocomposites: a review of properties and powders’ synthesis methods, Nanomaterials, 2015, vol. 5, issue 2, pp. 656-696. DOI: 10.3390/nano5020656.
28. Luo Y., Wang Q., Li J. et al. Enhanced hydrogen storage/sensing of metal hydrides by nano-modification, Materials Today Nano, 2019, vol. 9, art. no. 100071, 87 p. DOI: 10.1016/j.mtnano.2019.100071.
29. Preiur D., Bonani W., Popa K. et al. Size dependence of lattice parameter and electronic structure in CeO2 nanoparticles, Inorganic Chemistry, 2020, vol. 59, issue 8, pp. 5760-5767. DOI: 10.1021/acs.inorgchem.0c00506.
30. Jagiello K., Chomicz B., Avromopoulos A. et al. Size-dependent electronic properties of nanomaterials: how this novel class of nanodescriptors supposed to be calculated?, Structural Chemistry, 2017, vol. 28., issue 3, pp. 635-643. DOI: 10.1007/s11224-016-0838-2.
31. Caizer C. Nanoparticle size effect on some magnetic properties, Handbook of Nanoparticles. Amsterdam, Springer, 2015, pp. 475-519. DOI: 10.1007/978-3-319-15338-4_24.
32. Issa B., Obaidat I.M., Albiss B.A., Yousef H. Magnetic Nanoparticles: Surface Effects and Properties Related to Biomedicine Applications, International Journal of Molecular Sciences, 2013, vol. 14, issue 11, pp. 21266-21305. DOI: 10.3390/ijms141121266.
33. Vajda P., Andre G. Commensurate and incommensurate magnetic structures in rare-earth hydrides, Journal of Alloys and Compounds, 2001, vol. 326, issues 1-2, pp. 151-156. DOI: 10.1016/S0925-8388(01)01251-8.
34. Piquer C., Grandjean F., Isnard O., Long G.J. A phenomenological model for the rare-earth contribution to the magnetic anisotropy in RFe11Ti and RFe11TiH, Journal of Physics: Condensed Matter, 2006, vol. 18, no. 1, pp. 221-242, DOI: 10.1088/0953-8984/18/1/016.
35. Skomski R. RKKY interactions between nanomagnets of arbitrary shape, EDP Sciences Europhysics Letters, 1999, vol. 48, issue 4, pp. 455-460. DOI: 10.1209/epl/i1999-00504-y.
36. Mi S., Yuan S.-H., Lyu P. Size effect of Ruderman–Kittel–Kasuya–Yosida interaction mediated by electrons in nanoribbons, Journal of Applied Physics, 2011, vol. 109, issue 8, art. no. 083931, 4 p. DOI: 10.1063/1.3575338.
37. Lundin C.E. Research on the samarium-type intermediate phases of intra-rare-earth binary systems, 633558 (also Given as DRI-2326, Final Report), Denver Research Institute, University of Denver, CO, USA, 1966, 32 p.
38. Jayaraman A., Sherwood R.C., Williams H.J., E. Corenzwit. Pressure-induced phase transformations and magnetic ordering in some intra-rare-earth alloys and samarium, Physical Review, 1966, vol. 148, issue 2, pp. 502-508. DOI: https://doi.org/10.1103/PhysRev.148.502.
39. Ellner M., Reule H., Mittemeijet E.J. The structure of the trihydride GdH3, Journal of Alloys and Compounds, 2000, vol. 309, issues 1-2, pp. 127-131. DOI: https://doi.org/10.1016/S0925-8388(00)01055-0.
40. Mansmann M., Wallace W.E. The structure of HoD3, Journal de Physique, 1964, vol. 25, issues 5, pp. 454-459. DOI: 10.1051/jphys:01964002505045400.
41. Uporov S.A., Estemirova S.Kh., Sterkhov E.V. et al. Magnetocaloric effect in ScGdTbDyHo high-entropy alloy: impact of synthesis route, Intermetallics, 2022, vol. 151, art. no. 107678, 10 p. DOI: 10.1016/j.intermet.2022.107678.
42. Qiao J.W., Bao M.L., Zhao Y.J. et al. Rare-earth high entropy alloys with hexagonal close-packed structure, Journal of Applied Physics, 2018, vol. 124, issue 19, art. no. 195101, 7 p. DOI: 10.1063/1.5051514.
43. Soler R., Evirgen A., Yao M. Microstructural and mechanical characterization of an equiatomic YGdTbDyHo high entropy alloy with hexagonal close-packed structure, Acta Materialia, 2018, vol. 156, pp. 86-96. DOI: 10.1016/j.actamat.2018.06.010.
44. Jordan R.B. The lanthanide contraction: what is abnormal and why?, Inorganic Chemistry, 2025, vol. 64, issue 5, pp. 2207-2216. DOI: 10.1021/acs.inorgchem.4c03698.
45. Mugiraneza S., Hallas A.M. Tutorial: a beginner’s guide to interpreting magnetic susceptibility data with the Curie-Weiss law, Communications Physics, 2022, vol. 5, art. no. 95, 12 p. DOI: 10.1038/s42005-022-00853-y.
46. Wang L., Lu H., Guo H. Multi-principal rare-earth Gd-Tb-Dy-Ho-Er alloys with high magnetocaloric performance near room temperature, Journal of Alloys and Compounds, 2023, vol. 960, art. no. 170901, 10 p. DOI: 10.1016/j.jallcom.2023.170901.
47. Kudrevatykh N.V., Volegov A.S. Magnetizm redkhozemelnykh metallov i ikh intermetallicheskikh soedineniy [Magnetism of rare-earth metals and their intermetallic compounds]. Yekaterinburg, Ural University Publ., 2015, 198 p. (In Russian).
48. Yuan Y., Wu X., Tong X. et al. Rare-earth high-entropy alloys with giant magnetocaloric effect, Acta Materialia, 2017, vol. 125, pp. 481-489. DOI: 10.1016/j.actamat.2016.12.021.
49. Lu S.F., Ma L., Rao G.H. et al. Magnetocaloric effect of high-entropy rare-earth alloy GdTbHoErY, Journal of Materials Science: Materials in Electronics, 2021, vol. 32, issue 8, pp. 10919-10926. DOI: 10.1007/s10854-021-05749-1.
50. Svalov A.V., Neznakhin D.S., Arkhipov A.V. et al. Magnetocaloric effect in powder of GdTbDyHoEr high-entropy alloy, Physics of the Solid State, 2024, vol. 66, issue 12, pp. 2120-2124. DOI: 10.61011/PSS.2024.12.60204.313.
51. Nikitin S.A. Magnitnye svoystva redkozemelnykh metallov i splavov [Magnetic properties of rare earth metals and their alloys]. Moscow, Moscow State University Publ., 1989, 248 p. (In Russian).
52. Pankratov N.Yu., Tereshina I.S., Krot P.A., Verbetsky V.N., Nikitin S.A. Structure and magnetic properties of the medium-entropy GdTbDyY alloy, Bulletin of the Russian Academy of Sciences: Physics, 2025, vol. 89, issue 4, pp. 572-577. DOI: 10.1134/S1062873825710785.
53. Flood D.J. Crystal fields and magnetic properties of ErH3, Journal of Applied Physics, 1978, vol. 49, issue 3, pp. 1495-1497. DOI: 10.1063/1.324933.
54. Carlin R.L., Chirico R.D., Joung K.O. et al. Magnetic ordering in GdH3, Physics Letters A, 1980, vol. 75, issue 5, pp. 413-414. DOI: 10.1016/0375-9601(80)90858-0.
55. Carlin, R.L., Krause L.J. Magnetic ordering in DyH2 and DyH3, Chemical Physics Letters, 1981, vol. 82, issue 2, pp. 323-326. DOI: 10.1016/0009-2614(81)85165-2.