Hybrid materials based on d-element hexacyanoferrates modified with nanosized gold
I.M. Shevchenko1, M.A. Yasnaya2, A.A. Blinova1, A.V. Prasolova1, A.D. Goncharov1, T.N. Glizhova1
1 North Caucasus Federal University
2 Branch of JSC NPO «Mikrogen» in Stavropol «Allergen»
DOI: 10.26456/pcascnn/2026.18.985
Original article
Abstract: For the first time, we present the results of a study on the influence of the composition and ratio of components in the synthesis process of hybrid materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), modified with gold nanoparticles, on the elemental and phase composition of these hybrid materials and on the microstructure of their surface. According to the results of investigations using scanning electron microscopy and energy dispersive X-ray microscopy, it was found that gold was identified in samples of hexacyanoferrates (III) of d-elements (Co, Ni, Fe) containing from 0,1 to 5,0 masses.% gold. Analysis of the phase composition of samples of hexacyanoferrates of d‑elements (Co, Ni, Fe) modified with gold showed that the main crystalline phases were the corresponding hexacyanoferrates of d‑elements with a face‑centered cubic crystal lattice (Fm3m); impurity phases of mixed hexacyanoferrates were also present. According to the results of X‑ray phase analysis, the phases of metallic gold cannot be identified. The obtained experimental data will be useful for the development and use of promising materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron) as sensitive elements in glucose sensors. Additional modification of the matrix of hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), for example, with nanoparticles of noble metals, helps to increase the conductivity, selectivity, and stability of composite materials when creating sensors for assessing blood glucose levels.
Keywords: hybrid nanomaterials, hexacyanoferrates of d‑elements, gold nanoparticles, elemental composition, phase composition, surface microstructure
- Irina M. Shevchenko – Ph. D., Associate Professor, Head of the Department of Standardization, Metrology and Quality Management, Faculty of Food Engineering and Biotechnology Academician A.G. Khramtsova, North Caucasus Federal University, ORCID: 0009-0005-9113-9335
- Maria A. Yasnaya – Ph. D., Associate Professor, Head of the Department of Registration of Medicines, Branch of JSC NPO «Mikrogen» in Stavropol «Allergen», ORCID: 0000-0002-4486-4834
- Anastasia A. Blinova – Ph. D., Associate Professor, Department of Pharmacy and Pharmacognosy, Faculty of Medicine and Biology, North Caucasus Federal University, ORCID: 0000-0001-9321-550X
- Alina V. Prasolova – Lecturer, Department of Pharmacy and Pharmacognosy, Faculty of Medicine and Biology, North Caucasus Federal University, ORCID: 0009-0003-7629-4391
- Artem D. Goncharov – Laboratory Assistant, Department of Theoretical and Mathematical Physics, Faculty of Physics and Technology, North Caucasus Federal University
- Tamara N. Glizhova – Ph. D., Associate Professor, Head of the Department of Pharmacy and Pharmacognosy, Faculty of Medicine and Biology, North Caucasus Federal University, ORCID: 0000-0003-4311-5636
For citation:
Shevchenko I.M., Yasnaya M.A., Blinova A.A., Prasolova A.V., Goncharov A.D., Glizhova T.N. Gibridnye materialy na osnove geksatsianoferratov d-elementov, modifitsirovannykh nanorazmernym zolotom [Hybrid materials based on d-element hexacyanoferrates modified with nanosized gold], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 985-995. DOI: 10.26456/pcascnn/2026.18.985. ⎘
Full article (in Russian): download PDF file
References:
1. Bruns D.E., Metzger B.E., Sacks D.B. Diagnosis of gestational diabetes mellitus will be flawed until we can measure glucose, Clinical Chemistry, 2020. vol. 66, issue 2, pp. 265-267. DOI: 10.1093/clinchem/hvz027.
2. Elmaleh-Sachs A., Schwartz J.L., Bramante C.T. et al. Obesity management in adults: a review, The Journal of the American Medical Association, 2023, vol. 330, issue 20, pp. 2000-2015. DOI: 10.1001/jama.2023.19897.
3. Mariadoss A.V.A., Sivakumar A.S., Lee C.H., Kim S.J. Diabetes mellitus and diabetic foot ulcer: etiology, biochemical and molecular based treatment strategies via gene and nanotherapy, Biomedicine & Pharmacotherapy, 2022, vol. 151, art. no. 113134, 14 p. DOI: 10.1016/j.biopha.2022.113134.
4. Mutluer T., Genç H.A., Demir T. et al. The effect of problem-solving skills on blood glucose regulation and disease management in children with type 1 diabetes mellitus, Journal of Pediatric Endocrinology and Metabolism, 2023, vol. 36, issue 10, pp. 949-956. DOI: 10.1515/jpem-2023-0282.
5. García-Moreno R.M., Benítez-Valderrama P., Barquiel B. et al. Predictors of postpartum glucose metabolism disorders in women with gestational diabetes mellitus, Diabetes & Metabolic Syndrome: Clinical Research & Reviews, 2022, vol. 16, issue 10, art. no. 102629, 7 p. DOI: 10.1016/j.dsx.2022.102629.
6. Itiola A.J., Cheng L., Zhang W. et al. The impact of blood glucose test strips reimbursement limits on utilization, costs, and health-care utilization in British Columbia, Canadian Journal of Diabetes, 2024, vol. 48, issue 1, pp. 10-17. DOI: 10.1016/j.jcjd.2023.08.005.
7. Nikitina V.N., Karastsialiova A.R., Karyakin A.A. Glucose test strips with the largest linear range made via single step modification by glucose oxidase-hexacyanoferrate-chitosan mixture, Biosensors and Bioelectronics, 2023, vol. 220, art. no. 114851, 7 p. DOI: 10.1016/j.bios.2022.114851.
8. Torné-Morató H., Donati P., Pompa P.P. Nanoplasmonic strip test for salivary glucose monitoring, Nanomaterials (Basel), 2022, vol. 12, issue 1, art. no. 105, 8 p. DOI: 10.3390/nano12010105.
9. Theyagarajan K., Lakshmi B.A., Kim C., Kim Y.-J. A nanohybrid-based smartphone-compatible high performance electrochemical glucose sensor, Materials Today Chemistry, 2024, vol. 41, art. no 102282, 10 p. DOI: 10.1016/j.mtchem.2024.102282.
10. Si P., Razmi N., Nur O. et al. // Gold nanomaterials for optical biosensing and bioimaging, Nanoscale Advances, 2021, vol. 3, issue 10, pp. 2679-2698. DOI: 10.1039/d0na00961j.