Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Influence of the doping method on optical properties of LiNbO3:Y single crystals

N.A. Teplyakova, S.M. Masloboeva, I.V. Biryukova

Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»

DOI: 10.26456/pcascnn/2026.18.155

Original article

Abstract: Using different doping methods (homogeneous and solid-phase) and the Czochralski method, LiNbO3:Y crystals with an yttrium concentration of 0,46 wt.% were grown. Optimal technological conditions for growing LiNbO3:Y crystals have been determined, including both the growth parameters and the melt preparation conditions. The optical and photorefractive properties of the obtained LiNbO3:Y single crystals have been studied using laser conoscopy and photoinduced light scattering methods. Comparative analysis of two LiNbO3:Y crystals showed a significant difference in their optical properties. In the LiNbO3:Y crystal grown from the homogeneous doping charge, the photorefractive effect is absent; in the LiNbO3:Y crystal grown from the solid-phase doping charge, a photorefractive response is present, and an almost instantaneous opening of the photoinduced light scattering indicatrix is observed. In addition, the homogeneously doped LiNbO3:Y crystal has a significantly higher optical homogeneity compared to the solid-phase doped LiNbO3:Y crystal. The obtained results indicate that the developed technological scheme for obtaining a single-phase lithium niobate charge doped with yttrium by the homogeneous doping method creates conditions for the growth of optically and compositionally homogeneous LiNbO3:Y single crystals, which are promising for use in electronic engineering as a nonlinear optical material with a low photorefraction effect.

Keywords: lithium niobate, single crystal, charge, homogeneous and direct doping, laser conoscopy, photoinduced light scattering

  • Natalya A. Teplyakova – Ph. D., Leading Researcher, Vibrational Spectroscopy Sector of the Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»
  • Sofia M. Masloboeva – Ph. D., Leading Researcher, Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»
  • Irina V. Biryukova – Ph. D., Leading Researcher, Electronic Engineering Materials Laboratory, Tananaev Institute of Chemistry – Subdivision of the Federal Research Centre «Kola Science Centre of the RAS»

For citation:

Teplyakova N.A., Masloboeva S.M., Biryukova I.V. Vliyanie sposoba legirovaniya na opticheskie svojstva monokristallov LiNbO3:Y [Influence of the doping method on optical properties of LiNbO3:Y single crystals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 155-163. DOI: 10.26456/pcascnn/2026.18.155. ⎘

Full article (in Russian): download PDF file

References:

1. Sidorov N.V., Palatnikov M.N., Teplyakova N.A. et al. Monokristally niobata I tantalata litiya raznogo sostava I genezisa [Monocrystals of lithium niobate and tantalate of different composition and genesis]. Moscow, RAS Publ., 2022, 288 p. (In Russian).
2. Zapadlík O., Pejchal J., Babin V. et al. GSAG:Ce scintillator: insights from yttrium admixture, RSC Advances, 2025, vol. 15, issue 3, pp. 2140-2151, DOI: 10.1039/D4RA07622B.
3. Ermochenkov I.M., Zavartsev Yu.D., Zagumennyi A.I. et al. Scintillation Lu2SiO5‒z:Y3+:Ce3+:Ca2+ crystal for positron emission tomography, Bulletin of the Lebedev Physics Institute, 2024, vol. 51, issue 1, pp. 25-29. DOI: 10.3103/S1068335623601231.
4. Belov M.V., Zavartsev Yu.D., Zavertyaev M.V. et al. Scintillation properties of large Lu2SiO5–z:Y3+:Ce3+:Ca2+ crystals, Bulletin of the Lebedev Physics Institute, 2022, vol. 49, issue 5, pp. 121-124, DOI: 10.3103/S1068335622050049.
5. Wang T., Wang Y., Weng Y. et al. Effect of yttrium doping on the properties of Nickel-Iron multiphase heterostructures at high current conditions, Chemical Engineering Science, 2025, vol. 302, part A, art.no. 120859, 10 р. DOI: 10.1016/j.ces.2024.120859.
6. Jiang Y., Zhu L., Tian J., et al. A high rate and stability O3-type cathode material based on a Y-doped NaNi1/3Fe1/3Mn1/3O2 matrix, Materials Today Communications, 2025, vol. 46, art. no. 112523, 12 р. DOI: 10.1016/j.mtcomm.2025.112523.
7. Luo Q., Wan Y., Wang Z., et al. Excellent-performing gas sensor based on Yttrium-doped ZnFe2O4 nanofibers for detection of n-Butanol, Journal of Alloys and Compounds, 2025, vol. 1027, art. no. 180605, 12 р. DOI: 10.1016/j.jallcom.2025.180605.
8. Vatnik S.M., Osipov V.V., Luk'yashin K.E.,= et al. Multiwatt lasing of Nd:YAG laser ceramics containing 0.8 % and 1 % of Nd, Quantum Electronics, 2014, vol. 44, no. 6, pp. 585-587. DOI: 10.1070/QE2014v044n06ABEH015430.
9. Kaminskii A.A. Laser crystals and ceramics: recent advances, Laser & Photonics Reviews, 2007, vol. 1, issue 2, pp. 93-177. DOI: 10.1002/lpor.200710008.
10. Goul'Kov M., Odoulov S., Naumova I. et al. Degenerate parametric light scattering in periodically poled LiNbO3:Y:Fe, Physical Review Letters, 2001, vol. 86, issue 18, pp. 4021-4024. DOI: 10.1103/PhysRevLett.86.4021.
11. Kornienko V.V., Kitaeva G.Kh., Sedlmeir F., et al. Towards terahertz detection and calibration through spontaneous parametric down-conversion in the terahertz idler-frequency range generated by a 795 nm diode laser system, APL Photonics, 2018, vol. 3, issue 5, pp051704-1-051704-8. DOI: 10.1063/1.5011201.
12. Odoulov S., Shumelyuk A., Thien R. et al. Reflection hologram recording in periodically poled LiNbO3:Y:Fe, Journal of Optics A: Pure and Applied Optics, 2004, vol. 6, no. 2, pp. 224-228. DOI: 10.1088/1464-4258/6/2/012.
13. Palatnikov M.N., Sidorov N.V., Kalinnikov V.Т. Tehnologiya upravlyaemogo sinteza monokristallicheskikh i keramicheskikh materialov na osnove niobatov-tantalatov shchelochnykh metallov [The technology of controlled synthesis of single crystal and ceramic materials on the basis of alkali metal niobates-tantalates], Czvetnye metally [Non-ferrous metals], 2000, no. 10, pp. 54-59. (In Russian).
14. Kato K. Structure refinement of H-Nb2O5, Acta Crystallographica Section B, 1976, vol. 32, issue 3, pp. 764-767. DOI: 10.1107/S0567740876003944.
15. Hsu R., Maslen E.N., Boulay D. et al. Synchrotron X-ray studies of LiNbO3 and LiTaO3, Acta Crystallographica Section B, 1997, vol. 53, issue 3, pp. 420-428. DOI: 10.1107/S010876819600777X.
16. Sidorov N.V., Pikoul O.Y., Teplyakova N.A., et al. Lazernaya konoskopiya i fotoinducirovannoe rasseyanie sveta v issledovaniyakh svojstv nelinejno-opticheskogo kristalla niobata litiya [Laser conoscopy and photoinduced light scattering in research of properties of optically nonlinear lithium niobate crystal]. Moscow, RAS Publ., 2019, 350 p. (In Russian).
17. Teplyakova N.A., Sidorov N.V., Palatnikov M.N. Osobennosti defektnoj struktury monokristalla LiNbO3:Cu(0.015 mas. %) [Features of the defect structure of a LiNbO3:Cu (0.015 wt.%) single crystal], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 215-222. DOI: 10.26456/pcascnn/2023.15.215 (In Russian).

Content |