Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Laser annealing of doped amorphous silicon films obtained by high frequency sputtering

G.A. Mustafayev1, N.V. Cherkesova1, A.G. Mustafayev2

1 Kabardino-Balkarian State University
2 Dagestan State University of National Economy

DOI: 10.26456/pcascnn/2026.18.714

Short communication

Abstract: The effect of pulsed laser annealing on the structural and electrical properties of arsenic-doped amorphous silicon films (50-200 nm thick) obtained by high frequency ion sputtering is studied. It is shown that at an energy density of 1,4 J/cm2, an oxidized amorphous layer up to 75 nm thick forms on the surface, under which a crystalline layer with an As concentration exceeding the solubility limit, is detected. It is found that As diffusion into the single-crystal substrate occurs only upon melting of the latter (threshold >1,0 J/cm²) and increases with decreasing the amorphous film thickness and increasing the number of pulses. Moreover, evaporation of the material leads to a loss of up to 20% As and the formation of craters up to 100 nm deep, which is associated with the release of Ar bubbles. It was found that the minimum surface resistance (<10 Ω/□) is achieved with three pulses and a thickness of 50-100 nm, corresponding to the maximum electrical activation of the impurity. Diode structures with a saturation current density of 6,5⋅10-10 A/cm² and a leakage current density of 2,5⋅10-8 A/cm2 were formed using laser annealing, demonstrating the potential of this method for creating shallow p-n junctions.

Keywords: laser processing, amorphous films, impurity concentration, film thickness, diffusion, substrate, energy density, surface resistance, doped layer

  • Gasan A. Mustafayev – Dr. Sc., Professor, Department of Electronics and Digital Information Technologies, Kabardino-Balkarian State University
  • Natalya V. Cherkesova – Ph. D., Associate Professor, Department of Electronics and Digital Information Technologies, Kabardino-Balkarian State University
  • Arslan G. Mustafayev – Dr. Sc., Professor, Department of Information Technologies and Information Security, Dagestan State University of National Economy, ORCID: 0000-0003-3463-4303

For citation:

Mustafayev G.A., Cherkesova N.V., Mustafayev A.G. Lazernyj otzhig legirovannykh amorfnykh plenok kremniya, poluchennykh vysokochastotnym raspyleniem [Laser annealing of doped amorphous silicon films obtained by high frequency sputtering], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 714-721. DOI: 10.26456/pcascnn/2026.18.714. ⎘

Full article (in Russian): download PDF file

References:

1. Fogarassy E., Stuck R., Toulemonde M., Bruyere J.C., Siffert P. Pulsed laser annealing of RF sputtered amorphous Si-H films doped with arsenic, Journal of Applied Physics, 1982, vol. 53, issue 4, pp. 3261-3266. DOI: 10.1063/1.331029.
2. Laser and electron beam processing of materials, ed. by C.W. White, P.S. Peercy. New York, Academic Press, 1980, XVIII+769 p. DOI: 10.1016/B978-0-127-46850-1.X5001-4.
3. Arduino D., Stassi S., Spano C. et al. Silicon and silicon carbide recrystallization by laser annealing: a review, Materials (Basel), 2023, vol. 16, issue 24, art. no. 7674. DOI: 10.3390/ma16247674.
4. Huet K., Mazzamuto F., Tabata T. et al. Doping of semiconductor devices by laser thermal annealing, Materials Science in Semiconductor Processing, 2017, vol. 62, pp. 92-102. DOI: 10.1016/j.mssp.2016.11.008.
5. Komarov F.F., Mil’chanin O.V., Parchomenko I.N. et al. Influence of the laser pulse annealing of the silicon implanted with indium and arsenic ions on its optical and structural properties, Journal of Engineering Physics and Thermophysics, 2024, vol. 97, issue 3, pp. 745-752. DOI: 10.1007/s10891-024-02946-7.
6. Scanlon P.J., Barfoot K.M., Skensved P. et al. Channeling and high-resolution backscattering studies of laser-annealed low-energy arsenic-implanted silicon, Ion Implantation: Equipment and Techniques, ed. by H. Ryssel, H. Glawischnig. Berlin, Heidelberg, Springer, 1983, pp. 549-553. DOI: 10.1007/978-3-642-69156-0_63.
7. White C.W., Wilson S.R., Appleton B.R., Young F.W. Jr. Supersaturated substitutional alloys formed by ion implantation and pulsed laser annealing of group-III and group-V dopants in silicon, Journal of Applied Physics, 1980, vol. 51, issue 1, pp. 738-749. DOI: 10.1063/1.327334.
8. Tan H.S., Ong C.K. Green function approach to the calculations of dopant redistribution in multi-pulse laser irradiation of silicon, Journal of Physics C: Solid State Physics, 1985, vol. 18, no. 14, pp. 2799-2807. DOI: 10.1088/0022-3719/18/14/011.
9. Kim C.-D., Ishihara R., Matsumura M. Excimer-laser annealing technology for hydrogenated amorphous-silicon devices, Japanese Journal of Applied Physics, 1995, vol. 34, no. 11R, pp. 5971-5976. DOI: 10.1143/JJAP.34.5971.
10. Heise H., Nickel N.H. Hydrogen bonding in laser-crystallized poly-Si, Journal of Non-Crystalline Solids, 2002, vol. 299-302, part 1, pp. 226-230. DOI: 10.1016/S0022-3093(01)00979-6.
11. Wang H., Lusquiños F., Yao Y.L. Effect of hydrogen on surface texturing and crystallization of a-Si:H thin film irradiated by excimer laser, Applied Physics A, 2012, vol. 107, issue 2, pp. 307-320. DOI: 10.1007/s00339-012-6843-4.
12. Fair R.B. Modeling laser-induced diffusion of implanted arsenic in silicon, Journal of Applied Physics, 1979, vol. 50, issue 10, pp. 6552-6555. DOI: 10.1063/1.325716.

Content |