Equation of polymolecular adsorption on a flat homogeneous surface of an adsorbent for a finite number of layers

A.V. Tvardovskiy

Tver State Medical University

DOI: 10.26456/pcascnn/2026.18.282

Original article

Abstract: To date, a large number of different adsorption and absorption equations have been proposed, describing a variety of equilibrium situations on homogeneous and inhomogeneous surfaces of adsorbents as well as polymers, micro-, meso- and macroporous adsorbents. However, the most valuable works are those in which attempts are made to build a general theory of adsorption (and absorption). At least the well-known classical adsorption equations should follow from such a general equation as special cases. Such an equation was previously proposed, and it was shown that the classical Henry, Langmuir, and Brunauer – Emmett – Teller equations with constants having a clear physical meaning follow from the general equation as special cases. Thus, the constant in the Henry equation is determined by the temperature as well as by the specific surface of the adsorbent, the size of the adsorbate molecules, the molar mass of the adsorbate, and the isosteric heat of adsorption (the energy of interaction of the adsorbate molecules with the surface of the adsorbent). In the derived Brunauer – Emmett – Teller partial equation, in contrast to its classical version, a clear dependence of the equation constant on the specific physical characteristics of the adsorption system is provided for the first time. The dependence in question is determined by the concentration of adsorbate molecules in the liquid phase at the temperature under consideration, the concentration of adsorbate molecules during the formation of a dense monolayer on the surface of the adsorbent, and by the energy of interaction of adsorbate molecules with the surface of the adsorbent and the heat of condensation. The presented approach can serve as a basis for modeling a variety of adsorption and absorption phenomena, including adsorption on microporous and deformable adsorbents. In this paper, based on previous investigation, the equation of polymolecular adsorption on a flat homogeneous surface for a limited number of layers is derived.

Keywords: adsorption, adsorbent, absorption, thermodynamics of phase equilibria, Henry equation, Langmuir equation, Brunauer – Emmett – Teller equation, equation of polymolecular adsorption, flat homogeneous surface

  • Andrey V. Tvardovskiy – Dr. Sc., Professor, Professor of the Department of Medical Biophysics, Tver State Medical University

For citation:

Tvardovskiy A.V. Uravnenie polimolekulyarnoj adsorbtsii na ploskoj odnorodnoj poverkhnosti adsorbenta dlya konechnogo chisla sloev [Equation of polymolecular adsorption on a flat homogeneous surface of an adsorbent for a finite number of layers], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 282-288. DOI: 10.26456/pcascnn/2026.18.282. ⎘

Full article (in Russian): download PDF file

References:

1. Tvardovskiy A.V. Obshchij fenomenologicheskij podkhod dlya opisaniya adsorbtsionnykh i absorbtsionnykh ravnovesij [General phenomenological approach for the description of adsorption and absorption equilibria], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 321-330. DOI: 10.26456/pcascnn/2022.14.321. (In Russian).
2. Sanchez-Varretti F.O. Adsorption of interacting binary mixtures on heterogeneous surfaces: theory, Monte Carlo simulations and experimental results, Adsorption, 2019, vol. 25, issue 7, pp. 1317-1328. DOI: 10.1007/s10450-019-00093-7.
3. Pérez-Chávez N.A., Albesa A.G., Longo G.S. Molecular theory of glyphosate adsorption to pH-responsive polymer layers, Adsorption, 2019, vol. 25, issue 7, pp. 1307-1316. DOI: 10.1007/s10450-019-00091-9.
4. Abbasi A., Abdelrasoul A., Sardroodi J.J. Adsorption of CO and NO molecules on Al, P and Si embedded MoS2 nanosheets investigated by DFT calculations, Adsorption, 2019, vol. 25. issue 5, pp. 1001-1017. DOI: 10.1007/s10450-019-00121-6.
5. Sladekova K., Campbell C., Grant C. et al. The effect of atomic point charges on adsorption isotherms of CO2 and water in metal organic frameworks, Adsorption, 2021, vol. 27, issue 6, pp. 995-1000. DOI: 10.1007/s10450-021-00301-3.
6. Sastre G.J., Kärger J., Ruthven D.M. Surface barriers and symmetry of adsorption and desorption processes, Adsorption, 2021, vol. 27, issue 5 (Topical issue: Diffusion in nanoporous solids, vol. 2), pp. 777-785. DOI: 10.1007/s10450-020-00260-1.
7. Van Assche T.R.C., Baron G.V., Denaye J.F.M. An explicit multicomponent adsorption isotherm model: accounting for the size-effect for components with Langmuir adsorption behavior, Adsorption, 2018, vol. 24, issue 6, pp. 517-530. DOI: 10.1007/s10450-018-9962-1.
8. Dastani N., Arab A., Raiss H. Adsorption of Ampyra anticancer drug on the graphene and functionalized graphene as template materials with high efficient carrier, Adsorption, 2020, vol. 26, issue 6, pp. 879-893. DOI: 10.1007/s10450-019-00142-1.
9. Avijegon G., Xiao G., Li G., May E.F. Binary and ternary adsorption equilibria for CO2/CH4/N2 mixtures on Zeolite 13X beads from 273 to 333 K and pressures to 900 kPa, Adsorption, 2018, vol. 24, issue 4, pp. 381-392. DOI: 10.1007/s10450-018-9952-3.
10. Ghasemi A.S., Mashhadban F., Ravari F. A DFT study of penicillamine adsorption over pure and Al-doped C60 fullerene, Adsorption, 2018, vol. 24, issue 5, pp. 471-480. DOI: 10.1007/s10450-018-9960-3.
11. Berezovsky V., Öberg S. Computational study of the CO adsorption and diffusion in zeolites: validating the Reed–Ehrlich model, Adsorption, 2018, vol. 24, issue 4, pp. 403-413. DOI: 10.1007/s10450-018-9948-z.
12. Henry D.C. A kinetic theory of adsorption, The London, Edinburgh, and Dublin Philosophical Magazine and Journal of Science. Series 6, 1922, vol. 44, issue 262, pp. 689-705. DOI: 10.1080/14786441108634035.
13. Langmuir I. The adsorption of gases on plane surfaces of glass, mica and platinum, Journal of the American Chemical Society, 1918, vol. 40, issue 9, pp. 1361-1403. DOI: 10.1021/ja02242a004.
14. Brunauer S., Emmett P.H., Teller E. Adsorption of gases in multimolecular layers, Journal of the American Chemical Society, 1938, vol. 60, issue 2, pp. 309-319. DOI: 10.1021/ja01269a023.
15. Tvardovskiy A.V. Sorbent deformation. Oxford, Elsevier, 2007, 278 p.
16. Shkolin A.V. Adsorbtsionno – stimulirovannaya deformatsiya mikroporistogo uglerodnogo adsorbenta c uzkim raspredeleniem por po razmeram pri adsorbtsii uglevodorodov v shirokih intervalah davlenij [Adsorption-stimulated deformation of a microporous carbon adsorbent with a narrow pore size distribution during hydrocarbon adsorption in wide ranges of pressures and temperatures], Сand. chem. sci. diss.: 02.00.04. Moscow, A.N. Frumkin Institute of Physical Chemistry and Electrochemistry of the Russian Academy of Sciences, 2008, 276 p. (In Russian).
17. Nabiulin V.V., Tvardovskiy A.V., Fomkin A.A. Adsorption deformation of a microporous AR-V carbon adsorbent during the adsorption of N-hexane, Russian Journal of Physical Chemistry A, 2011 vol. 85, issue 11, pp. 1960-1964.DOI: 10.1134/S0036024411110227.

Content |