Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Surface modification of single-crystal germanium by femtosecond laser radiation

I.A. Kaplunov1, S.A. Tretiakov1, A.I. Ivanova1, A.D. Vasilyev1, K.B. Yushkov2, V.E. Rogalin3, N.Ya. Vaysburg1

1 Tver State University
2 National Research Technological University MISIS
3 Institute of Electrophysics and Power Engineering of the RAS

DOI: 10.26456/pcascnn/2026.18.646

Original article

Abstract: This paper presents the results of a study examining the effects of femtosecond laser radiation on polished germanium single crystal surfaces with varying crystallographic orientations. In the experiments used a 1030 nm laser with an average power of 5 W and a pulse duration of 330 fs, as well as an optical setup with an automated sample position control system, enabling the radiation stability and repeatability of experimental conditions to be monitored. The resulting surface irregularities, which consisted of craters or a structure consisting of a series of peaks and valleys with the midline maintained in the plane of the original surface, were fixed using optical microscopy and subsequently examined using a profilometer and a scanning electron microscope. Morphological and 3D surface profile analysis of the obtained data at the impact points revealed features of the resulting relief depending on the crystallographic orientation of the samples and the energy characteristics of the laser radiation, where the peak pulse power, and therefore the fluence, was controlled through the average power or pulse repetition rate. Irreversible change of the surface (laser-induced damage) for single-crystal germanium is 20-30 MW in peak power per pulse with a beam diameter of 0,31 mm and an exposure duration of 20 ms, which corresponds to an fluence of 8,7-13,1 mJ/cm2.

Keywords: femtosecond laser, critical values, profilometric analysis, germanium

  • Ivan A. Kaplunov – Dr. Sc., Professor, Head of the Department of Applied Physics, Tver State University
  • Sergei A. Tretiakov – Ph. D., Associate Professor, Department of Applied Physics, Tver State University, ORCID: 0000-0002-4134-5609
  • Alexandra I. Ivanova – Ph. D., Associate Professor, Department of Applied Physics, Tver State University, ORCID: 0000-0002-5517-2294
  • Alexey D. Vasilyev – 3rd year postgraduate student, Department of Condensed Matter Physics, Tver State University
  • Konstantin B. Yushkov – Ph. D., Leading Researcher, Scientific and Technological and Educational Center of Acousto-Optics, National Research Technological University MISIS, ORCID: 0000-0001-9015-799X
  • Vladimir E. Rogalin – Dr. Sc., Head of the Laboratory, Institute of Electrophysics and Power Engineering of the RAS, ORCID: 0000-0002-2980-5385
  • Natalia Ya. Vaysburg – 2nd year postgraduate student, Department of Condensed Matter Physics, Tver State University

For citation:

Kaplunov I.A., Tretiakov S.A., Ivanova A.I., Vasilyev A.D., Yushkov K.B., Rogalin V.E., Vaysburg N.Ya. Modifikatsiya poverkhnosti monokristallicheskogo germaniya izlucheniem femtosekundnogo lazera [Surface modification of single-crystal germanium by femtosecond laser radiation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 646-656. DOI: 10.26456/pcascnn/2026.18.646. ⎘

Full article (in Russian): download PDF file

References:

1. Khomich V.Y., Shmakov V.A. Mechanisms of direct laser nanostructuring of materials, Physics–Uspekhi, 2015, vol. 58, issue 5, pp. 455-465. DOI: 10.3367/UFNe.0185.201505c.0489.
2. Kochuev D.A., Chkalov R.V., Prokoshev V.G., Khor’kov K.S. Effect of laser radiation on the surface of a solid body and the formation of micro- and nanostructures, Bulletin of the Russian Academy of Sciences: Physics, 2020, vol. 84, issue 3, pp. 343-345. DOI: 10.3103/S1062873820030120.
3. Bronnikov K.A., Gladkikh S.A., Okotrub K.A. et al. Formation of laser-induced periodic structures on thin films of transition metal nitrides and semiconductors, Kvantovaya Elektonika [Quantum Electronics], 2022, vol. 52, no. 11, pp. 1012-1017. (In Russian).
4. Libensov M.N., Yakovlev E.B., Shandybina G.D. Vzaimodejstvie lazernogo izlucheniya s veshchestvom (silovaya optika). Konspekt lektsij. Chast' I. Pogloshchenie lazernogo izlucheniya v veshchestve [Interaction of laser radiation with matter (power optics). lecture notes. Part I. Absorption of laser radiation in matter], ed. by V.P. Veiko. St. Petersburg, St. Petersburg State University of Information Technologies, Mechanics, and Optics Publ., 2008. – 141 p. (In Russian).
5. Iqbal M.H., Basir S., Rafique M.S. et al. Pulsed laser ablation of germanium under vacuum and hydrogen environments at various fluences, Applied Surface Science, 2015, vol. 344, pp. 146-158. DOI: 10.1016/j.apsusc.2015.03.117.
6. Kumar M., Mavi H.S., Rath S. et al. Fabrication of nanopatterned germanium surface by laser-induced etching: AFM, Raman and PL studies, Physica E: Low-dimensional Systems and Nanostructures, 2008, vol. 40, issue 9, pp. 2904-2910. DOI: 10.1016/j.physe.2008.02.007.
7. Chumakov A.N., Luchkouski V.V., Nikonchuk I.S., Matsukovich A.S. Silicon ablation in air by mono- and bichromatic laser pulses with wavelength 355 and 532nm, Technical Physics, 2022, vol. 67, no. 1, pp. 16-24. DOI: 10.21883/TP.2022.01.52527.202-21.
8. Dostovalov A.V. Sozdanie periodicheskikh struktur femtosekundnym izlucheniem vnutri svetovodov i na poverkhnosti metallov [Creation of periodic structures by femtosecond radiation inside light guides and on the surface of metals]. Cand. chem. sci. diss.: 02.00.04. Novosibirsk, Institute of Automation and Electrometry SB RAS Publ., 2015, 120 p. (In Russian).
9. Bespalov V.G., Kozlov S.A., Petrov N.V. et al. Femtosekundnaya optika i femtotekhnologii [Femtosecond optics and femtotechnologies]. St. Petersburg, ITMO University, 2018, 136 p. (In Russian).
10. Birnbaum M. Semiconductor surface damage produced by ruby lasers, Journal of Applied Physics, 1965, vol. 36, issue 11, pp. 3688-3689. DOI: 10.1063/1.1703071.
11. Rogalin V.E., Zheleznov V.Y., Malinsky T.V. et al. Poluchenie poristoj poverkhnosti na germanii putem vozdejstviya infrakrasnymi nanosekundnymi lazernymi impul'sami [Obtaining a porous surface on germanium by exposure to infrared nanosecond laser pulses], Fizika Tverdogo Tela [Solid State Physics], 2025, vol. 67, issue 12, pp. 2412-2415. DOI: 10.61011/FTT.2025.12.62438.8061k-25. (In Russian).
12. Zheleznov V.Yu., Malinskiy T.V., Mikolutskiy S.I. et al. Impact treatment of the surface of oxygen-free copper with nanosecond laser pulses in water, Inorganic Materials, 2024, vol. 60, issue 9, pp. 1083-1088. DOI: 10.1134/S0020168524701437.
13. Zheleznov V.Yu., Malinskii T.V., Rogalin V.E. et al. Effect of nanosecond ultraviolet laser pulses on the surface of germanium single crystals, Russian Microelectronics, 2023, vol. 52, issue 8, pp. 741-749. DOI: 10.1134/S1063739723080073.
14. Ozkan A. M., Malshe A.P., Railkar T.A. et al. Femtosecond laser-induced recording of periodic structures on diamond crystals and microclusters, Applied Physics Letters, 1999, vol. 75, issue 23, pp. 3716-3718. DOI: 10.1063/1.125439.
15. Okamura K., Hashida M., Miyasaka Y. et al. Laser fluence dependence of periodic grating structures formed on metal surfaces under femtosecond laser pulse irradiation, Physical Review B, 2010, vol. 82, issue 16, pp. 165417-1-165417-5. DOI: 10.1103/PhysRevB.82.165417.
16. Vorobyev A.Y., Guo C. Direct femtosecond laser surface nano/microstructuring and its applications, Laser & Photonics Reviews, 2012, vol. 7, issue 3, pp. 385-407. DOI: 10.1002/lpor.201200017.
17. Dostovalov A.V., Korolkov V.P., Golubtsov S.K., Kondrat’ev V.I. Specific features of formation of self-induced gratings on metal foils during scanning by a tightly focused femtosecond laser beam, Quantum Electronics, 2014, vol. 44, issue 4, pp. 330-334. DOI: 10.1070/QE2014v044n04ABEH015376.
18. Micromachining, Ultrafast lasers technology and applications, ed. by M.E. Fermann, A. Galvanauskas, G. Such, 1st ed. Boca Raton, CRC Press, 2002, chapter 7, 30 p. DOI: 10.1201/9780203910207.
19. GOST 11141-84. Detali opticheskie. Klassy chistoty poverkhnostej. Metody kontrolya [Optical parts. Classes of cleanness of surfaces. Methods of control]. Moscow, Izdatel'stvo standartov Publ., 1985, 20 p. (In Russian).
20. GOST 2789-73. Sherokhovatost' poverkhnosti. Parametry i kharakteristiki [Surface roughness. Parameters and characteristics]. Moscow, Izdatel'stvo standartov Publ., 1985, 41 p. (In Russian).

Content |