Liquid-phase oxidation of ethylene glycol with hydrogen peroxide using nanostructured silver catalysts
S.Yu. Menshikov1, V.S. Kurmacheva1, S.A. Fedorov2,1, A.N. Malyshev3,1, Yu.V. Mikushina4, A.B. Shishmakov4, A.A. Tumashov3,4, A.E. Permyakova3, A.A. Ostroushko3
1 Ural State Mining University
2 Vatolin Institute of Metallurgy of the Ural Branch of the RAS
3 Ural Federal University named after the first President of Russia B.N. Yeltsin
4 I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS
DOI: 10.26456/pcascnn/2026.18.877
Original article
Abstract: The catalytic activity of nanoscale silver-containing compositions in the oxidation of ethylene glycol with hydrogen peroxide, as well as the selectivity of the processes, were studied. The reactions were carried out at a temperature of 60°C using L-micro laboratory setup The degree of ethylene glycol conversion was determined by gas chromatography. The composition of the ethylene glycol oxidation products and, in addition, the oxidation products of glyoxal upon reaction with H2O2 in the presence of the same nanoscale silver-containing samples were determined by liquid chromatography and nuclear magnetic resonance spectroscopy. For comparison, colloidal silver samples and nanoscale silver samples supported on a carbon material and on a mineral support (aluminum oxide) were used as catalysts in the reactions investigated. It was established that, under the same catalyst-to-substrate mass ratio and identical conditions, the conversion of ethylene glycol was higher in the presence of the colloidal silver samples. Comparing the catalytic activity of the silver samples supported on aluminum oxide and on a carbon material, the conversion of ethylene glycol in the presence of the carbon–silver catalyst was found to be lower. Under the studied conditions of catalytic liquid-phase oxidation of ethylene glycol on silver samples of various types, the main oxidation product in the presence of an excess of the oxidant was oxalic acid.
Keywords: nanoscale silver, catalytic properties, oxidation, hydrogen peroxide, gas and liquid chromatography, nuclear magnetic resonance spectroscopy, kinetics
- Sergei Yu. Menshikov – Ph. D., Associate Professor, Chemistry Department, Ural State Mining University, ORCID: 0009-0004-0390-0108
- Vera S. Kurmacheva – 1st year postgraduate student, Chemistry Department, Engineer, Research Laboratory of Analytical Chemistry, Ural State Mining University, ORCID: 0009-0005-5925-021X
- Sergei A. Fedorov – Ph. D., Senior Researcher, Laboratory of Pyrometallurgy of Non-Ferrous Metals; Associate Professor, Chemistry Department, Vatolin Institute of Metallurgy of the Ural Branch of the RAS, Associate Professor, Chemistry Department Ural State Mining University, ORCID: 0000-0002-4201-5177
- Alexander N. Malyshev – 3rd year postgraduate student, Department of Life Safety, Engineer and Researcher, Ural Federal University named after the first President of Russia B.N. Yeltsin, Engineer and Researcher, Research Laboratory of Analytical Chemistry Ural State Mining University
- Yuliya V. Mikushina – Junior Researcher, Laboratory of Organic Materials, I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS, ORCID: 0000-0002-0873-7483
- Andrey B. Shishmakov – Ph. D., Researcher, Laboratory of Organic Materials, I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS, ORCID: 0000-0001-5880-2370
- Andrey A. Tumashov – Ph. D., Senior Researcher, Laboratory of Asymmetric Synthesis, Ural Federal University named after the first President of Russia B.N. Yeltsin; I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS, Associate Professor, Department of Organic Chemistry and High Molecular Weight Compound I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS
- Anastasia E. Permyakova – 3rd year postgraduate student; Junior Researcher, Ural Federal University named after the first President of Russia B.N. Yeltsin
- Alexander A. Ostroushko – Dr. Sc., Professor, Head of the Department of Chemical Materials Science, Ural Federal University named after the first President of Russia B.N. Yeltsin
For citation:
Menshikov S.Yu., Kurmacheva V.S., Fedorov S.A., Malyshev A.N., Mikushina Yu.V., Shishmakov A.B., Tumashov A.A., Permyakova A.E., Ostroushko A.A. Zhidkofaznoe okislenie etilenglikolya peroksidom vodoroda s ispolzovaniem nanostrukturirovannykh serebryanykh katalizatorov [Liquid-phase oxidation of ethylene glycol with hydrogen peroxide using nanostructured silver catalysts], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 877-886. DOI: 10.26456/pcascnn/2026.18.877. ⎘
Full article (in Russian): download PDF file
References:
1. Shi H., Yin X., Subramaniam B., Chaudhari R.V. Liquid-phase oxidation of ethylene glycol on Pt and Pt-Fe catalysts for the production of glycolic acid: remarkable bimetallic effect and reaction mechanism, Industrial and Engineering Chemistry Research, 2019, vol. 58, issue 40, pp. 18561-18568. DOI: 10.1021/acs.iecr.9b03419.
2. Xu Y., Liu W., Xu B. et al. Synthesis of glycolic acid by selective oxidation of ethylene glycol over Pt/Sn-beta in a base-free medium, reaction chemistry & engineering, 2024, vol. 9, issue 12, pp. 3122-3132. DOI: 10.1039/d4re00243a.3.
3. Wu S., Quan Y., Ren J. Density functional theory study on the selective oxidation of ethylene glycol to glycolic acid over Ptn (n = 4-5) clusters, Frontiers of Chemical Science and Engineering, 2025, vol. 19, issue 8, art. no. 72, 11 p. DOI: 10.1007/s11705-025-2585-7.
4. Olvera-Vargas H., Jaramillo-Quintero O.A., AlarcónLeón L.D.et al. Green synthesis of glycolic acid through the electrocatalytic reduction of oxalic acid over black TiO2: An experimental and theoretical study, Journal of Energy Chemistry, 2024, vol. 100, pp. 544-556. DOI: 10.1016/j.jechem.2024.09.011.
5. Bleger F., Simon O., Shuteten A. Sposob polucheniya vodnogo rastvora glioksilovoj kisloty [Method for obtaining an aqueous solution of glyoxylic acid]. Patent RF, no. 2481322, 2013. (In Russian).
6. Vodyankina O.V., Kurina L.N., Petrov L.A., Knyazev A.S. Glioksal': monografiya [Glyoxal: monograph]. Moscow, Academia Publ., 2007, 248 p. (In Russian).
7. Olenin A.Y., Mingalev P.G., Lisichkin G.V. Partial catalytic oxidation of alcohols: catalysts based on metals and metal coordination compounds (a review), Petroleum Chemistry, 2018, vol. 58, issue 8, pp. 577-592. DOI: DOI: 10.1134/S0965544118080182.
8. Zakharova A.M., Kartsova L.A., Grinstein I.L. Opredelenie organicheskikh kislot, uglevodov i podslastitelej v pishchevykh produktakh i biologicheski aktivnykh dobavkakh metodom vysokoeffektivnoj zhidkostnoj khromatografii [Determination of organic acids, carbohydrates and sweeteners in food products and biologically active additives by HPLC], Analitika i kontrol [Analytics and Control], 2013, vol. 17, no. 2, pp. 204-210. (In Russian).
9. Menshikov S.Yu., Vurasko A.V., Driker B.N. et al. Vliyanie primesej v antrakhinone na ego kataliticheskuyu aktivnost' v protsesse delignifikatsii [The effect of impurities in anthraquinone on its catalytic activity during delignification], Zhurnal prikladnoj himii [Journal of Applied Chemistry], 2010, no. 5, pp. 849-853. (In Russian).
10. Savel'ev E.A., Cherepanova A.D., Sapunov V.N. Formation of formic acid and its esters in oxidation of fatty acid methyl esters, Russian Journal of Applied Chemistry, 2023, vol. 96, issue 1, pp. 91-98. DOI: 10.1134/s1070427223010123.
11. Shishmakov A.B., Mikushina Yu.V., Koryakova O.V. Sintez granulirovannykh serebrosoderzhashchikh uglej pirolizom kompozita poroshkovaya tsellyuloza-sakharoza-AgNO3 [Synthesis of granulated silver-containing coals by pyrolysis of cellulose-sucrose-AgNO3 composite], Vestnik tekhnologicheskogo universiteta [Bulletin of the Technological University], 2023, vol. 26, no. 1, pp. 22-27. DOI: 10.55421/1998-7072_2023_26_1_22. (In Russian).
12. Ostroushko A.A., Permyakova A.E., Zhulanova T.Yu. et al. Preparation and antibacterial properties of alumina-silver nanocomposites, Russian Journal of Inorganic Chemistry, 2025, vol. 70, issue 1, pp. 10-19. DOI: 10.1134/S0036023624602265.
13. Menshikov S.Yu., Kurmacheva V.S., Fedorov S.A. et al. Vozdejstvie nanorazmernykh obraztsov serebra i polioksometallata {Mo72Fe30} na reaktsii perekisnogo okisleniya organicheskikh soedinenij [The effect of nanoscale samples of silver and polyoxometallate {Mo72Fe30} on the reactions of peroxidation of organic compounds], Rasplavy [Melts], 2025, no. 4, pp. 394-404. DOI: 10.7868/S3034571525040106. (In Russian).
14. Bogachev N.V., Tarbeeva K.A., Ogorodova N.Yu. Razrabotka poshagovoj metodiki polucheniya nanochastits serebra tsitratnym metodom [Development of step-by-step method for producing silver nanoparticles by citrate method], Izvestiya Vysshikh Uchebnykh Zavedenii, Seriya Khimiya i Khimicheskaya Tekhnologiya [The Journal ChemChemTech], 2020, vol. 63, no. 5, pp. 65-69. DOI: 10.6060/ivkkt.20206305.6171. (In Russian).
15. Glioksal', 40% rastvor [Glyoxal, 40% solution]. Available at: : https://novochem.ru/products/raw/glioksal-40-rastvor/ (accessed 15.04.2026).
16. Menshikov S.Yu., Malyshev A.N., Kurmacheva V.S. et al. Vozdejstvie FeSO4 i nanoklasternykh polioksometallatov na okislenie fenola persul'fatom v spirtovoj srede [The effect of FeSO4 and nanocluster polyoxometalates on the oxidation of phenol persulfate in an alcohol medium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 992-999. DOI: 10.26456/pcascnn/2023.15.992. (In Russian).