Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Synthesis and physico-mechanical characteristics of functional Er2O3/ScSZ ceramics

I.A. Surkov1, L.A. Pasechnik2, O.I. Gyrdasova2

1 Ural Federal University named after the first President of Russia B.N. Yeltsin
2 Institute of Solid State Chemistry of the Ural Branch of RAS

DOI: 10.26456/pcascnn/2026.18.144

Original article

Abstract: Solid solutions of the Er2O3/ScSZ system were synthesized by a sol-gel method using ethylene glycol as an organic component, which ensures high homogeneity of dopant distribution in the ZrO2 matrix. Thermolysis of the intermediate sol in air at 700 °C leads to the formation of Zr0,8Sc0,2-xErxO2 (x = 0-0,04) compositions based on the tetragonal t–ZrO2 phase. Ceramic samples with a relative density of 96-98% were obtained at 1500°C. According to X‑ray diffraction data, in the range x = 0-0,01 the sintered ceramics consist of a mixture of cubic (c–ZrO2) and rhombohedral (r–ZrO2) phases, whereas at x = 0,02-0,04 a single‑phase cubic structure is formed. Scanning electron microscopy reveals a well‑sintered microstructure with grains closely adhering to each other; pores are closed and have submicron dimensions. The microhardness ranges from 12,3 to 15,6 GPa, which is comparable to that of conventional technical ceramics based on ZrO2. Co-doping with erbium almost doubles the flexural strength, raising it from 81,2 MPa (undoped ScSZ) to 150,2 MPa for the composition Zr0,8Sc0,19Er0,01O2. This value exceeds the typical strength of unstabilized ZrO2 ceramics and demonstrates a pronounced strengthening effect of erbium. The observed strengthening is attributed to the transformation toughening mechanism, as well as to reduced porosity and microstructural optimization achieved through the sol‑gel synthesis. To ensure stability of thermomechanical and thermoelectric characteristics under long‑term and cyclic operating conditions, a co-doping level of 2-3 mol.% Er (x = 0,02-0,03) is preferable, which yields a single‑phase c–ZrO2 structure that prevents unwanted phase transitions in the working temperature range. Such doping provides the best combination of strength (~154 MPa) and microhardness (~14,5-15,0 GPa), thereby reducing the risk of property degradation. Thus, the developed Er2O3/ScSZ materials represent a promising alternative to conventional electrolytes for solid oxide fuel cells, offering high density, mechanical strength, and phase stability.

Keywords: scandium stabilized zirconium oxide, co-doping, erbium oxide, sol-gel synthesis, microhardness, bending strength

  • Ilya A. Surkov – 1st year graduate student of the Institute of New Materials and Technologies, Ural Federal University named after the first President of Russia B.N. Yeltsin
  • Liliya A. Pasechnik – Ph. D., Leading Researcher, Laboratory of Heterogeneous Processes, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-0631-5287
  • Olga I. Gyrdasova – Ph. D., Leading Researcher, Laboratory of Inorganic Synthesis, Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-0680-6094

For citation:

Surkov I.A., Pasechnik L.A., Gyrdasova O.I. Sintez i fiziko-mekhanicheskie kharakteristiki funktsionalnoj keramiki sistemy Er2O3/ScSZ [Synthesis and physico-mechanical characteristics of functional Er2O3/ScSZ ceramics], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 144-154. DOI: 10.26456/pcascnn/2026.18.144. ⎘

Full article (in Russian): download PDF file

References:

1. Wang F., Lyu Y., Chu D. et al. The electrolyte materials for SOFCs of low-intermediate temperature, Materials Science and Technology, 2019, vol. 35, issue 13, pp. 1551-1562. DOI: 10.1080/02670836.2019.1639008.
2. Hossain S., Abdalla A.M., Jamain S.N.B., Zaini J.H., Azad A.K. A review on proton conducting electrolytes for clean energy and intermediate temperature-solid oxide fuel cells, Renewable and Sustainable Energy Reviews, 2017, vol. 79, pp. 750-764. DOI: 10.1016/j.rser.2017.05.147.
3. Perovskite materials: synthesis, characterisation, properties, and applications, ed. by L. Pan, G. Zhu. IntechOpen, 2016, 650 p. DOI: 10.5772/60469.
4. Medvedev D., Brouzgou A., Demin A., Tsiakaras P. Proton-conducting electrolytes for solid oxide fuel cell applications, Advanced Medium and High Temperature Solid Oxide Fuel Cell Technology, CISM International Centre for Mechanical Sciences, ed. by M. Boaro, A.A. Salvatore. Cham, Springer, 2017, vol. 574, pp. 77-118. DOI: 10.1007/978-3-319-46146-5_3.
5. Mahato N., Banerjee A., Gupta A., Omar S., Balani K. Progress in material selection for solid oxide fuel cell technology: A review, Progress in Materials Science, 2015, vol. 72, pp. 141-337. DOI: 10.1016/j.pmatsci.2015.01.001.
6. Medvedev D.A., Lyagaeva J.G., Gorbova E.V. et al. Advanced materials for SOFC application: strategies for the development of highly conductive and stable solid oxide proton electrolytes, Progress in Materials Science, 2016, vol. 75, pp. 38-79. DOI: 10.1016/j.pmatsci.2015.08.001.
7. Mahato N., Gupta A., Balani K. Doped zirconia and ceria-based electrolytes for solid oxide fuel cells: a review, Nanomaterials and Energy, 2012, vol. 1, issue 1, pp. 27-45. DOI: 10.1680/NME.11.00004.
8. Shao Z., Tadé M.O. Application of SOFC Technology, Intermediate-temperature solid oxide fuel cells. Materials and applications, ed. by Z. Shao, M.O. Tadé. Berlin, Heidelberg, Springer, 2016. pp. 247-266. DOI: 10.1007/978-3-662-52936-2.
9. Arachi Y., Asai T., Yamamoto O. et al. Electrical conductivity of ZrO2–Sc2O3 doped with HfO2, CeO2, and Ga2O3, Journal of the Electrochemical Society, 2001, vol. 148, issue 5, pp. A520-A524. DOI: 10.1149/1.1362546.
10. Brodnikovskyi Y., McDonald N., Polishko I. et al. Properties of 10Sc1CeSZ-3.5 YSZ (33-, 40-, 50-wt.%) composite ceramics for SOFC application, Materials Today: Proceedings, 2019, vol. 6, issue 2, pp. 26-35. DOI: 10.1016/j.matpr.2018.10.071.
11. Agarkov D.A., Borik M.A., Bredikhin S.I. et al. Phase compositions, structures and properties of scandia-stabilized zirconia solid solution crystals co-doped with yttria or ytterbia and grown by directional melt crystallization, Solid State Ionics, 2020, vol. 346. art. no. 115218, 7 р. DOI: 10.1016/j.ssi.2019.115218.
12. Pasechnik L.A., Pereverzev D.I., Shamsutov I.V. et al. Assessment of electrical conductivity and thermal expansion in scandium-zirconium ceramic directly derived from red mud, Inorganic Chemistry Communications, 2025, vol. 176, art. no. 114227, 8 p. DOI: 10.1016/j.inoche.2025.114227.
13. Wei X., Hou G., An Y. et al. Effect of doping CeO2 and Sc2O3 on structure, thermal properties and sintering resistance of YSZ, Ceramics International, 2021, vol. 47, issue 5, pp. 6875-6883. DOI: 10.1016/j.ceramint.2020.11.032.
14. Gyrdasova O.I., Vladimirova E.V., Dmitriev A.V. et al. Impact of formate precursor thermolysis route on the structure and photocatalytic activity of Zr0.95Sc0.05O2–δ, Inorganic Chemistry Communications, 2026, vol. 184, art. no. 116007, 11 p. DOI: 10.1016/j.inoche.2025.116007.
15. Gyrdasova O.I., Pasechnik L.A. Formation of solid solutions and composites in the ZnO-ZrO2 system [Formirovanie tverdyh rastvorov i kompozitov v sisteme ZnO-ZrO2], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 627-635. DOI: 10.26456/pcascnn/2025.17.627. (In Russian).
16. Zu J.H., Gao Y., Liu D. et al. Preparation and high-temperature performance of Sc2O3–Y2O3 co-stabilized ZrO2 thermal barrier coatings, Ceramics International, 2024, vol. 50, issue 11, pp. 20460-20472. DOI: 10.1016/j.ceramint.2024.03.169.
17. Fan W., Wang Z.Z., Bai Y. et al. Improved properties of scandia and yttria co-doped zirconia as a potential thermal barrier material for high temperature applications, Journal of the European Ceramic Society, 2018, vol. 38, issue 13, pp. 4502-4511. DOI: 10.1016/j.jeurceramsoc.2018.06.002.
18. Pasechnik L.A., Medyankina I.S., Pereverzev D.I., Chufarov A.Y., Suntsov A.Y. Scandium modified zirconia extracted from red mud as a waste of alumina production, Nanosystems: Physics, Chemistry, Mathematics, 2024, vol. 15, issue 6, pp. 768-773. DOI: 10.17586/2220-8054-2024-15-6-768-773.
19. Eichler J., Rödel J., Eisele U., Hoffman M. Effect of grain size on mechanical properties of submicrometer 3Y-TZP: fracture strength and hydrothermal degradation, Journal of the American Ceramic Society, 2007, vol. 90, issue 9, pp. 2830-2836. DOI: 10.1111/j.1551-2916.2007.01643.x.
20. Komolikov Y.I., Kashcheev I.D., Khrustov V.R., Pudov V.I. Stability of ceramics based on ZrO2 Doped with Y2O3 under hydrothermal action, Refractories and Industrial Ceramics, 2020, vol. 61, issue 4, pp. 424-427. DOI: 10.1007/s11148-020-00497-x.
21. Chien F.R., Ubic F.J., Prakash V. Stress-induced martensitic transformation and ferroelastic deformation adjacent microhardness indents in tetragonal zirconia single crystals, Acta Materialia, 1998, vol. 46, issue 6, pp. 2151-2171. DOI: 10.1016/s1359-6454(97)00444-8.
22. Borik M.A., Bublik V.T., Eremina R.M. et al. Effect of the valence state of Ce ions on the phase stability and mechanical properties of the crystals of ZrO2-based solid solutions, Physics of the Solid State, 2017, vol. 59, issue 10, pp. 1934-1939. DOI: 10.1134/S1063783417100079.

Content |