Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Investigation of the process of stabilization of nanoparticles of mixed iron oxide by beta-glucan

M.A. Pirogov, A.V. Blinov, A.V. Samovolov, A.V. Tatov, Z.A. Rekhman, N.M. Bocharov

North Caucasus Federal University

DOI: 10.26456/pcascnn/2026.18.897

Original article

Abstract: In this work, samples of mixed iron oxide nanoparticles stabilized with beta-glucan were prepared by chemical precipitation in an aqueous medium from iron (III) chloride and iron (II) sulfate using ammonia as the precipitating agent. This material is of interest due to its magnetic and biocompatible properties, as well as to combination of a magnetite core and a polysaccharide shell. The Fourier transform infrared spectroscopy and diffuse reflectance spectroscopy studies were conducted, along with quantum chemical computer modeling of the elementary act of interaction of beta-glucan with iron (II) and iron (III) oxides using the QChem software. The modeling revealed that the interaction of the beta-glucan site with iron oxides is energetically favorable (the difference in the total energy of beta-glucan and the elementary act of interaction is > 1335 (for iron (II)) oxide and > 2744 kcal/mol (for iron (III) oxide)) and chemically stable (chemical hardness of 0,140-0,161 eV and 0,156-0,170 eV, respectively), with the optimal interaction being via the hydroxyl group attached to C3 of the B-linked glucopyranose residue. Infrared spectral analysis confirmed this mechanism: the intensity of the hydroxyl stretching band in the spectrum of stabilized nanoparticles is reduced compared to that of pure beta-glucan, while the appearance of a Fe–O stretching band in the 533-656 cm–¹ region confirms the formation of a magnetite crystal lattice. Analysis of the diffuse reflectance spectrum revealed that the optical properties of the sample in the visible region are determined predominantly by mixed iron oxide, with an absorption band at 450-600 nm associated with the electron transitions of Fe2+ and Fe3+ ions.

Keywords: nanoparticles, iron oxide, beta-glucan, quantum chemical modeling, diffuse reflection, Fourier transform infrared spectroscopy

  • Maxim A. Pirogov – assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0001-9217-6262
  • Andrey V. Blinov – Ph. D., Associate Professor, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0002-4701-8633
  • Artem V. Samovolov – assistant, Department of Oil Refining Technology and Industrial Ecology, Faculty of Petroleum Engineering, North Caucasus Federal University, ORCID: 0000-0001-5570-6201
  • Alexey V. Tatov – Laboratory Assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0009-0003-8842-232X
  • Zafar A. Rekhman – Teacher, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0003-2809-4945
  • Nikita M. Bocharov – Laboratory Assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0009-0005-7286-0995

For citation:

Pirogov M.A., Blinov A.V., Samovolov A.V., Tatov A.V., Rekhman Z.A., Bocharov N.M. Issledovanie protsessa stabilizatsii nanochastits smeshannogo oksida zheleza beta-glyukanom [Investigation of the process of stabilization of nanoparticles of mixed iron oxide by beta-glucan], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 897-907. DOI: 10.26456/pcascnn/2026.18.897. ⎘

Full article (in Russian): download PDF file

References:

1. Akhmedzhanova Z.I., Zhiemuratova G.K., Danilova E.A. et al. Makro-i mikroelementy v zhiznedeyatel'nocti organizma i ikh vzaimosvyaz' s immunnoj sistemoj (obzor literatury) [Macro- and microelements in the body's vital functions and their relationship with the immune system (literature review)], Zhurnal teoreticheskoi i klinicheskoi meditsiny [Journal of Theoretical and Clinical Medicine], 2020, no. 1, pp. 16-21. (In Russian).
2. Spivakovsky Yu.M., Spivakovskaya A.Yu. Mikroelementy i ikh rol' v zhizni cheloveka [Microelements and their role in human life], Meditsinskaya sestra [The Nurse], 2005, issue 5, pp. 19-22. (In Russian).
3. Churin B.V., Astashov V.V., Trunova V.A. et al. Essentsial'nye mikroelementy (Fe, Cu, Mn, Zn, Se, As) v pecheni i legkikh pri alimentarnom ozhirenii v eksperimente [Essential elements (Fe, Cu, Mn, Zn, Se, As) in the liver and lungs with alimentary obesity in the experiment], Eksperimental'naya i klinicheskaya gastroenterologiya [Experimental and Clinical Gastroenterology], 2011, issue 6, pp. 59-63. (In Russian).
4. López-Alonso M., Rivas I., Miranda M. Trace mineral imbalances in global health: challenges, biomarkers, and the role of serum analysis, Nutrients, 2025, vol. 17, issue 13, art. no 2241, 39 p. DOI: 10.3390/nu17132241.
5. Zakharova I.N., Skorobogatova E.V., Obynochnaya E.G., Korovina N.A. Defitsit vitaminov i mikroelementov u detej i ikh korrektsiya [Deficiency of vitamins and trace elements in children and their correction], Pediatriya. Zhurnal im. G.N. Speranskogo [Pediatrics Journal named after G.N. Speransky], 2007, vol. 86, issue 3, pp. 112-118. (In Russian).
6. Bel’mer S., Gasilina T. Mikroelementy i mikroelementozy i ikh znachenie v detskom vozraste [Microelements and microelementosis and their significance in childhood], Voprosy sovremennoi pediatrii [Current Pediatrics], 2008, vol. 7, no. 6, pp. 91-96. (In Russian).
7. Yagupova V.T., Vezirova D.R. Vliyanie mikroelementa zheleza na organizm cheloveka [The effect of the trace element iron on the human body], Poisk (Volgograd) [Search (Volgograd)], 2019, no. 1 (10), pp. 74-77. (In Russian).
8. Torshin I.Y., Gromova O.A., Grishina T.R., Rudakov K.V. Ierarkhiya vzaimodejstvij tsinka i zheleza: fiziologicheskie, molekulyarnye i klinicheskie aspekty [Hierarchy of zinc and iron interactions: physiological, molecular and clinical aspects], Trudnyi patsient [A difficult patient], 2010, vol. 8, no. 3, pp. 45-53. (In Russian).
9. Shamov I.A., Gasanova P.O. Zhelezo, absorbtsiya, transport [Ferrum, absorption, transport], Vestnik gematologii [Bulletin of Hematology], 2016, vol. 12, no. 1, pp. 31-38. (In Russian).
10. Rozhentsev D.A., Mansurov R.R., Tkachev N.K. et al. Kataliticheskie svoistva v geterogennoi reaktsii Fentona poverkhnosti nanoporistogo zheleza, poluchennogo posredstvom ehlektrokhimicheskogo dealloinga v rasplavlennykh khloridnykh smesyakh [Catalytic properties in the heterogeneous fenton reaction of the surface of nanoporous iron obtained by electrochemical dealoiyng in melted chloride mixtures], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. 919-927. DOI: 10.26456/pcascnn/2021.13.919. (In Russian).
11. Sokur T.N., Burlev V.A., Konovodova E.N., Fedorova Yu.V. Zhelezodefitsitnaya anemiya i beremennost'. Rol' medi i margantsa v metabolizme zheleza [Iron deficiency anemia and pregnancy. The role of copper and manganese in iron metabolism], Poliklinika [Polyclinic], 2013, vol. 1, no. 1, pp. 57-60. (In Russian).
12. Andreichev N.A., Baleyeva L.V. Zhelezodefitsitnye sostoyaniya i zhelezodefitsitnaya anemiya [Iron deficiency and iron deficiency anemia], Vestnik Sovremennoi Klinicheskoi Mediciny [The Bulletin of Contemporary Clinical Medicine], 2009, vol. 2, issue 3, pp. 60-65. (In Russian).
13. Tarasova I.S. Zhelezodefitsitnaya anemiya u detej i podrostkov [Iron deficiency anemia in children and adolescents], Voprosy sovremennoi pediatrii [Current Pediatrics], 2011, vol. 10, no. 2, pp. 40-48. (In Russian).
14. Dvoretsky L.I. Sul'fat zheleza v lechenii zhelezodefitsitnoj anemii: pozitsii sokhranyayutsya [Ferrous sulfate in the treatment of iron deficiency anemia: the positions continue], Terapevticheskii arkhiv [Therapeutic Archive], 2017, vol. 89, issue 10, pp. 108-112. DOI: 10.17116/terarkh20178910108-112. (In Russian).
15. Stuklov N.I., Kunina M.Yu., Semenova E.N. Effektivnost' i perenosimost' preparatov zheleza. Chto vazhnee? Sushchestvuet li optimal'noe reshenie [Efficacy and tolerability of iron preparations. What is more important? Is there an optimal solution], Poliklinika [Polyclinic], 2014, vol. 2, no. 1, pp. 48-53. (In Russian).
16. Kamzin A.S., Obaidat I.M., Kozlov V.S. et al. Graphene oxide/iron oxide (gro/feox) nanocomposites for biomedicine: synthesis and study, Physics of the Solid State, 2021, vol. 63, issue 6, pp. 856-865. DOI: 10.1134/S1063783421060123.
17. Baranova O.V., Kiyaeva E.V., Notova S.V. Ispol'zovanie razlichnykh form zheleza v kormlenii zhivotnykh (obzor) [Different forms of iron in feeding of animals], Zhivotnovodstvo i kormoproizvodstvo [Animal Husbandry and Fodder Production], 2025, vol. 108, no. 4, pp. 217-233. DOI: 10.33284/2658-3135-108-4-217. (In Russian).
18. Nagdalian A.A., Leontiev P.S., Golik A.B. Issledovanie protsessa polimernoj stabilizatsii smeshannogo oksida zheleza amilopektinom [Investigation of the process of polymer stabilization of mixed iron oxide with amylopectin], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 951-959. DOI: 10.26456/pcascnn/2024.16.951. (In Russian).
19. IQmol Molecular Viewer. Available at: www.url: http://www.iqmol.org/ (accessed 12.06.2026).
20. Q-Chem 6.3 User’s Manual. Available at: https://manual.q-chem.com/6.3/ (accessed 12.06.2026).
21. Strens, R.G.J., Wood B.J. Diffuse reflectance spectra and optical properties of some iron and titanium oxides and oxyhydroxides, Mineralogical Magazine, 1979, vol. 43, issue 327, pp. 347-354. DOI: 10.1180/minmag.1979.043.327.06.
22. Sherman, D.M., Waite T.D. Electronic spectra of Fe3+ oxides and oxide hydroxides in the near IR to near UV, American Mineralogist, 1985, vol. 70, issue 11-12, pp. 1262-1269.

Content |