Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


Carbon nanotubes with impurity nitrogen atoms as promising filters for harmful gases

A.D. Grigoriev, S.V. Boroznin, I.V. Zaporotskova

Volgograd State University

DOI: 10.26456/pcascnn/2026.18.233

Original article

Abstract: Carbon nanotubes modified with nitrogen atoms are one of the promising materials for the development of electronic devices in the modern world. They are characterized by the presence of structural distortions and increased nucleophilicity, which significantly distinguishes them from primitive graphene structures. These facilities exhibit abnormally high stability in aggressive environments and low overvoltage. Their uniqueness lies in the synergy of the mechanical strength of the carbon backbone and the chemical activity of nitrogen-containing centers, which makes it possible to solve the problems of creating effective sorbents and heterogeneous catalysts. To study the interaction of nanotubes with harmful gases and obtain the energy characteristics of adsorption, some semi-empirical calculations using the Gaussian software package were used in the framework of the density functional theory using the B3LYP method with a 6-31G baseline set. The nanotube model was built using GaussView 6.0. Every second carbon atom of the nanotube was replaced by a nitrogen atom. To obtain the adsorption energy, the gas molecule approached the surface of the nanotube perpendicular to the axis of the nanotube with 0,2 nm increments. The energy was calculated at each step, which made it possible to build profiles of the potential energy of interaction of chlorine, fluorine and carbon dioxide. During the theoretical experiment, interaction energies were obtained for each step of the approach of Cl, F, and CO2. Based on the results, the potential energy interaction curves were constructed, which made it possible to determine the most effective distance for the sorption of harmful gases onto the surface of a carbon nanotube modified with nitrogen atoms. Sorption occurs at various distances. For chlorine, it is 1,4-1,8 Å, and for fluorine and carbon dioxide, it is 2-3 angstroms. The interaction graphs clearly demonstrate the possibility of sorption of hazardous gases by the nanocomposite. Fluorine forms a stable chemical bond with the carbon atom of the nanotube, while chlorine is physically sorbed onto the nitrogen atom, which indicates the high potential of the material under study for reusable filters. The experiments conducted demonstrate the possibility of using carbon nanotubes with substituting nitrogen atoms as filters. The assessment of the energy properties shows a high potential for application in microelectronic technology.

Keywords: carbon-nitrogen nanotubes, filters, density functional theory, gas adsorption, harmful gases

  • Alexandr D. Grigoriev – Senior Lecturer, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0009-0004-8999-7552
  • Sergey V. Boroznin – Dr. Sc., Head of the Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0003-0110-2271
  • Irina V. Zaporotskova – Dr. Sc., Professor, Department of Forensic Science and Physical Materials Science, Institute of Physics and Technology, Volgograd State University, ORCID: 0000-0002-9486-2482

For citation:

Grigoriev A.D., Boroznin S.V., Zaporotskova I.V. Uglerodnye nanotrubki s primesnymi atomami azota, kak perspektivnye filtry vrednykh gazov [Carbon nanotubes with impurity nitrogen atoms as promising filters for harmful gases], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 233-243. DOI: 10.26456/pcascnn/2026.18.233. ⎘

Full article (in Russian): download PDF file

References:

1. Onyancha R.B., Ukhurebor K.E., Aigbe U.O. et al. A systematic review on the detection and monitoring of toxic gases using carbon nanotube-based biosensors, Sensing and Bio-Sensing Research, 2021, vol. 34, art. no. 100463, 19 p. DOI: 10.1016/j.sbsr.2021.100463.
2. Shalina T.I., Vasil'eva L.S. Obshchie voprosy toksicheskogo dejstviya ftora [General problems of toxic effect of fluorine], Bajkal'skij meditsinskij zhurnal [Baikal Medical Journal], 2009, vol. 88, no. 5, pp. 5-9. (In Russian).
3. Donskikh I.V. Vliyanie ftora i ego soedinenij na zdorov'e naseleniya (obzor dannykh literatury) [The influence of fluorine and its compounds on people’s health (literature review)], Acta Biomedica Scientifica, 2013, vol. 3, no. 2, pp. 179-185. (In Russian).
4. Xie M., Wang J., Du X-L. et al. Metal-organic framework derived single-atom catalysts for electrochemical CO2 reduction, RSC Advances, 2022, vol. 12, issue 50, pp. 32518-32525. DOI: 10.1039/D2RA06302F.
5. Hinds B.J., Chopra N., Rantell T. et al. Aligned multiwalled carbon nanotube membranes, Science, 2004, vol. 303, no. 5654, pp. 62-65. DOI: 10.1126/science.1092048.
6. Casavant M.J., Walters D.A., Schmidt J.J., Smalley R.E. Neat macroscopic membranes of aligned carbon nanotubes, Journal of Applied Physics, 2003, vol. 93, issue 4, pp. 2153-2156. DOI: 10.1063/1.1536732.
7. Miller S.A., Young V.Y., Martin C.R. Electroosmotic flow in template-prepared carbon nanotube membranes, Journal American Chemical Society, 2001, vol. 123, issue 49, pp. 12335-12342. .
8. Bogdanovskaya V.A., Radina M.V., Korchagin O.V. et al. Carbon nanotubes modified with oxygen- and nitrogen-containing groups as perspective catalysts for the oxygen electroreduction reaction, Russian Journal of Electrochemistry, 2020, vol. 56, issue 10, pp. 809-820. DOI: DOI: 10.1134/S1023193520100043.
9. Bogdanova D.A. Upravlenie svojstvami poluprovodnikovykh odnostennykh uglerodnykh nanotrubok [Controlling the properties of semiconducting single-walled carbon nanotubes], Cand. phys.-math. sci. diss.: 1.4.4. Ulyanovsk, Ulyanovsk State University Publ., 2013, 137 p. (In Russian).
10. Nesov S.N., Korusenko P.M., Bolotov V.V. et al. Electronic structure of nitrogen-containing carbon nanotubes irradiated with argon ions: XPS and XANES studies, Physics of the Solid State, 2017, vol. 59, issue 10, pp. 2030-2035. DOI: 10.1134/S1063783417100286.
11. Boroznina N.P., Zaporotskova I.V., Murugadoss G. Issledovanie vzaimodejstviya modifitsirovannykh BC-nanotrubok s uglerodosoderzhashchimi molekulami [Investigation of the interaction of modified bc-nanotubes with carbon-containing molecules], NBI-technologies, 2024, vol. 18, no. 3, pp. 17-27. DOI: 10.15688/NBIT.jvolsu.2024.3.2. (In Russian).
12. Liang S., Niu H.Y., Guo H. et al. Incorporating Fe3C into B, N co-doped CNTs: non-radical-dominated peroxymonosulfate catalytic activation mechanism, Chemical Engineering Journal, 2021, vol. 405, art. no 126686, 13 p. DOI: 10.1016/j.cej.2020.126686.
13. Nesov S.N. Sravnitel'nyj analiz struktury i khimicheskogo sostoyaniya mnogostennykh uglerodnykh nanotrubok, legirovannykh azotom [Comparative analysis of structure and chemical state of nitrogen-doped multi-walled carbon nanotubes], Omskiy nauchnyy vestnik [Omsk Scientific Bulletin], 2020, no. 4 (172), pp. 94-97. DOI: 10.25206/1813-8225-2020-172-94-97. (In Russian).
14. Tian L., Li J., Liang F. et al. Molten salt synthesis of tetragonal carbon nitride hollow tubes and their application for removal of pollutants from wastewater, Applied Catalysis B: Environmental, 2018, vol. 225, pp. 307-313. DOI: 10.1016/j.apcatb.2017.11.082.
15. Zhu Y., Feng Y., Chen S. et al. Carbon nitride nanotube-based materials for energy and environmental applications: a review of recent progresses, Journal of Materials Chemistry A, 2020, vol. 8, issue 48, pp. 25626-25648. DOI: 10.1039/d0ta08892g.
16. Wu B., Ouro-Koura H., Lu S.-H. et al. Functional materials for powering and implementing next-generation miniature sensors, Materials Today, 2023, vol. 69, pp. 333-354. DOI: 10.1016/j.mattod.2023.09.001.
17. Elbakyan L.S. Kvantovo-khimicheskie raschety s primeneniem programmnogo paketa GAUSSIAN i graficheskogo redaktora GAUSSVIEW: uchebnoe posobie [Quantum-chemical calculations using the GAUSSIAN software package and the GAUSSVIEW graphical editor: a study guide]. Volgograd, Volgograd State University Publ., 2022, 79 p. (In Russian).
18. Zhang I. Y., Wu J., Xu X. Extending the reliability and applicability of B3LYP, Chemical Communications, 2010, vol. 46, issue 18, pp. 3057-3070. DOI: 10.1039/c000677g.

Content |