Dispersion dependences of polarization switching parameters of copper-containing triglycine sulfate crystals
N.N. Bolshakova, I.K. Galkin, A.I. Ivanova, E.M. Semenova
Tver State University
DOI: 10.26456/pcascnn/2026.18.594
Original article
Abstract: The paper presents results of an experimental study of the concentration and dispersion dependences of repolarization characteristics of copper-containing triglycine sulfate crystals. It is shown that with an increase in the impurity concentration in triglycine sulfate : Cu2+ crystals, the values of the relative and effective permittivities, switchable polarization, and unipolarity coefficient tend to increase, while the magnitudes of the coercive field, bias field, and dielectric loss tangent tend to decrease. The switching processes are significantly affected by the frequency of the alternating field, with an increase in which a transformation of the dielectric hysteresis loops is observed. As the frequency increases from 50 Hz to 2 kHz, the switchable polarization of the crystals decreases by an average of 2,5 times. At the same time, the frequency of the repolarizing field has a more significant effect on the repolarization processes of pure triglycine sulfate. A change in the repolarizing field frequency from 50 Hz to 2 kHz leads to a decrease in the dielectric viscosity coefficient of triglycine sulfate : Cu2+ crystals by an average of 3 times, which is caused by the switching off of the main switching mechanisms.
Keywords: dispersion dependences, triglycine sulfate, hysteresis properties, switchable polarization, permittivity, dielectric viscosity, domain structure
- Nataly N. Bolshakova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University, ORCID: 0009-0007-8077-6050
- Ivan K. Galkin – 2nd year graduate student, Faculty of Physics and Engineering, Tver State University, ORCID: 0009-0005-3244-5068
- Alexandra I. Ivanova – Ph. D., Docent, Applied Physics Department, Tver State University, ORCID: 0000-0002-5517-2294
- Elena M. Semenova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University, ORCID: 0000-0003-2755-6933
For citation:
Bolshakova N.N., Galkin I.K., Ivanova A.I., Semenova E.M. Dispersionnye zavisimosti parametrov pereklyucheniya polyarizatsii medsoderzhashchikh kristallov triglitsinsulfata [Dispersion dependences of polarization switching parameters of copper-containing triglycine sulfate crystals], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 594-603. DOI: 10.26456/pcascnn/2026.18.594. ⎘
Full article (in Russian): download PDF file
References:
1. Baryshnikov S.V., Milinsky A.Y., Stukova E.V. Linear and nonlinear dielectric properties of ceramics obtained from barium titanate nanopowder, Glass and Ceramics, 2024, vol. 81, issue 3-4, pp. 152-156. DOI: 10.1007/s10717-024-00674-1.
2. Gainutdinov R.V., Tolstikhina A.L., Lashkova A.K. et al. Application of scanning capacitance force microscopy for detecting impurity phases in ferroelectric triglycine sulfate, Technical Physics, 2019, vol. 64, issue 11, pp. 1602-1608. DOI: 10.1134/S1063784219110094.
3. Baryshnikov S.V., Milinsky A.Yu., Lvov A.E., Stukova E.V. Dielektricheskie svojstva kompozitov na osnove triglitsinsul'fata i nanochastits titanata bariya [Dielectric properties of composites based on triglycine sulfate and barium titanate nanoparticles], Nauchno-tekhnicheskie vedomosti SPbGPU. Fiziko-matematicheskie nauki. [St. Petersburg State Polytechnical University Journal. Physics and Mathematics.], 2025, vol. 18, no. 1, pp. 9-17. DOI: 10.18721/JPM.18101. (In Russian).
4. He H., Lu X., Hanc E. et al. Advances in lead-free pyroelectric materials: a comprehensive review, Journal of Materials Chemistry C, 2020, vol. 8 issue 5, pp. 1494-1516. DOI: 10.1039/C9TC05222D.
5. Ranu, Bharathi U., Sinha R., Agarwal P.B. CMOS compatible pyroelectric materials for infrared detectors, Materials Science in Semiconductor Processing, 2022, vol. 140, art. no. 106375, 19 p. DOI: 10.1016/j.mssp.2021.106375.
6. Physics of ferroelectrics: a modern perspective, ed by K.M. Rabe, C.H. Ahn, J.-M. Triscone. Berlin, Heidelberg, Springer-Verlag, 2007, XII + 388 p. DOI: 10.1007/978-3-540-34591-6.
7. Bogomolov A.A., Ivanov V.V. Fizika segnetoelektricheskikh yavlenij [Physics of ferroelectric phenomena], Tver, TSU Publ., 2014, 160 p. (In Russian).
8. Pecherskaya E.A. The use of the Sawyer-Tower method and its modifications to measure the electrical parameters of ferroelectric materials, Measurement Techniques, 2007, vol. 50, issue 10, pp. 1101-1107. DOI: 10.1007/s11018-007-0205-1.
9. Ivanova A.I., Grechishkin R.M., Bolshakova N.N., Belyakov V.A. Temperature observation of the evolution of the domain structure of triglycine sulphate by SEM, Journal of Surface Investigation. X-ray, Synchrotron and Neutron Techniques, 2015, vol. 9, issue 5, p. 908-912. DOI: 10.1134/S1027451015050079.
10. Kokhanchik L.S., Ponomarev B.K. Change in surface state of ferroelectric domains under electron irradiation in SEM, Bulletin of the Russian Academy of Sciences: Physics, 2005, vol. 69, issue 4, pp. 515-520.
11. Nakatani N. Observation of ferroelectric domain structure in TGS, Ferroelectrics, 2011, vol. 413, issue 1, pp. 238-265. DOI: 10.1080/00150193.2011.554269.
12. Bolshakova N., Rudyak V. Domain structure realignment processes and Barkhausen effect in TGS crystals. Ferroelectrics, 1994, vol. 157, issue 1, pp. 123-128. DOI: 10.1080/00150199408229493.
13. Golitsyna O.M., Drozhdin S.N., Chulakova V.O. et al. Evolution of the domain structure of triglycine sulphate single crystal in the vicinity of phase transition. Ferroelectrics, 2017, vol. 506, issue 1, pp. 127-135. DOI: 10.1080/00150193.2017.1282286.
14. Mihailov M.A., Shemyakin A.A., Bolshakova N.N., Gordinskaya E.N. Protsessy pereklyucheniya primesnykh kristallov triglitsinsul'fata [Switching processes in impurity-doped triglycine sulfate crystals]. Fundamental'nye problemy radioelektronnogo priborostroeniya [Fundamental problems of radioengineering and device construction], 2014, vol. 14, no. 2, pp. 171-174. (In Russian).
15. Bolshakova N.N., Druginina N.Yu., Ivanova A.I. et al. Perepolyarizatsionnye svojstva medsoderzhashchikh kristallov triglitsinsulfata [Repolarization properties of copper-containing crystals of triglycine sulfate], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 50-60. DOI: 10.26456/pcascnn/2022.14.050. (In Russian).