Formation of fractal nanostructures of Ge2Sb2Te5 phase-change material by laser-induced transfer
A.A. Burtsev1, D.N. Bukharov2, V.V. Ionin1, V.A. Mikhalevsky1, A.V. Kiselev1, A.A. Nevzorov1,3, N.N. Eliseev1, M.R. Konnikova1, A.A. Lotin1,4
1 National Research Centre «Kurchatov Institute»
2 Vladimir State University named after Alexander and Nikolay Stoletovs
3 University of Science and Technology MISIS
4 Mendeleev University of Chemical Technology
DOI: 10.26456/pcascnn/2026.18.021
Original article
Abstract: This work is devoted to the study of the synthesis of Ge2Sb2Te5 phase-change material nanoparticles via direct laser-induced forward transfer using sub-nanosecond pulses with durations of the order of hundreds of picoseconds. Thin Ge2Sb2Te5 films deposited by thermal vacuum evaporation onto silicon substrates were used as the initial targets. It is shown that the temperature regime, governed by the high melting temperature of the crystalline Ge2Sb2Te5 phases (approximately 600 °C) and their ability to rapidly recrystallize, plays a key role in determining the efficiency of the cluster formation and morphology of the resulting aggregates. These factors create specific conditions for nucleation and growth of particles from the molten material. A detailed morphological analysis of the synthesized nanoparticles and their aggregates was performed using scanning electron microscopy. It was found that depending on the laser pulse fluence and the initial film thickness, structures of varying complexity can be formed, ranging from isolated spherical particles to highly branched dendritic clusters. To quantitatively describe the aggregation processes, the diffusion-limited aggregation model was employed, which explains the observed morphological features in terms of random walks of particles in the gas phase and their subsequent adhesion to the substrate. It is demonstrated that by varying the experimental parameters (pulse energy and duration, film thickness, and target-to-substrate distance), clusters with tailored morphology and, consequently, controllable optical and electrical properties can be synthesized. This opens up the possibility of creating switchable elements based on Ge2Sb2Te5 nanoparticles with predictable characteristics, which could potentially replace conventional thin-film devices in a number of applications. The fractal dimension of the aggregates is identified as a key parameter correlating with their functional properties and can serve as a criterion for evaluating their performance.
Keywords: chalcogenides, phase change materials, nanoparticles, clustering, laser-induced transfer, fractal dimension
- Anton A. Burtsev – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0280-7943
- Dmitry N. Bukharov – Ph. D., Senior Researcher, Head of the Youth Research Laboratory, Vladimir State University named after Alexander and Nikolay Stoletovs, ORCID: 0000-0002-4536-8576
- Vitaly V. Ionin – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-1253-2261
- Vladimir A. Mikhalevsky – Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-6234-1084
- Alexey V. Kiselev – Ph. D., Senior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-0292-9553
- Alexey A. Nevzorov – Ph. D., Researcher, National Research Centre «Kurchatov Institute», Researcher, Laboratory of Photonic Gas Sensors University of Science and Technology MISIS, ORCID: 0000-0001-5602-6355
- Nikolay N. Eliseev – Junior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0002-8864-3961
- Maria R. Konnikova – Junior Researcher, National Research Centre «Kurchatov Institute», ORCID: 0000-0003-4701-6483
- Andrey A. Lotin – Sc. D., Deputy Head of the branch, National Research Centre «Kurchatov Institute», Deputy Director of the Department of Scientific and Technical Policy Mendeleev University of Chemical Technology, ORCID: 0000-0001-9051-7158
For citation:
Burtsev A.A., Bukharov D.N., Ionin V.V., Mikhalevsky V.A., Kiselev A.V., Nevzorov A.A., Eliseev N.N., Konnikova M.R., Lotin A.A. Formirovanie fraktalnykh nanostruktur fazoizmenyaemogo materiala Ge2Sb2Te5 pri lazerno-indutsirovannom perenose [Formation of fractal nanostructures of Ge2Sb2Te5 phase-change material by laser-induced transfer], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 21-30. DOI: 10.26456/pcascnn/2026.18.021. ⎘
Full article (in Russian): download PDF file
References:
1. Zhang W., Mazzarello R., Wuttig M., Ma E. Designing crystallization in phase-change materials for universal memory and neuro-inspired computing, Nature Reviews Materials, 2019, vol. 4, issue 3, pp. 150-168. DOI: 10.1038/s41578-018-0076-x.
2. Kolobov A.V., Tominaga J. Chalcogenides: Metastability and Phase Change Phenomena. Berlin Heidelberg, Springer-Verlag, 2012, XVI, 284 p. DOI: 10.1007/978-3-642-28705-3.
3. Kozyukhin S.A., Lazarenko P.I., Popov A.I. et al. Phase change memory materials and their applications, Russian Chemical Reviews, 2022, vol. 91, issue 9, art. no. RCR5033, 37 p. DOI: 10.1070/RCR5033.
4. Phase change materials. science and applications, ed. by S. Raoux, M. Wutting. New York, Springer Science+Business Media, LLC, 2009, 450 p. DOI: 10.1007/978-0-387-84874-7.
5. Papandreou N., Pantazi A., Sebastian A. et al. Multilevel phase-change memory, 17th IEEE International Conference on Electronics, Circuits and Systems, 2010, pp. 1017-1020. DOI: 10.1109/ICECS.2010.5724687.
6. Guo P., Sarangan A. M., Agha I. A review of germanium-antimony-telluride phase change materials for non-volatile memories and optical modulators, Applied Sciences, 2019, vol. 9, issue 3, art. no. 530, 26 p. DOI: 10.3390/app9030530.
7. Nevzorov A.A., Burtsev A.A., Kiselev A.V. et al. Chaotic computing cell based on nanostructured phase-change materials, Journal of Computational Electronics, 2024, vol. 23, issue 6, pp. 1448-1454. DOI: 10.1007/s10825-024-02221-1.
8. Caretta A., Casarin B., Chen B. et al. Ultrafast response of Ge2Sb2Te5 nanoparticles: The benefits of low energy amorphization switching with the same read/write speed of bulk memories, APL Materials, 2023, vol. 11, Art no 071117, 5 p. DOI: 10.1063/5.0156207.
9. Casarin B., Caretta A., Chen B. et al. Ultralow-fluence single-shot optical crystalline-to-amorphous phase transition in Ge–Sb–Te nanoparticles, Nanoscale, 2018, vol. 10, issue 35, pp. 16574-16580. DOI: 10.1039/c8nr04350g.
10. Sarwat S.G. Materials science and engineering of phase change random access memory, Materials Science and Technology, 2017, vol. 33, issue 16, pp. 1890-1906. DOI: 10.1080/02670836.2017.1341723.
11. Nicolis G., Prigogine I. Exploring complexity: an introduction, New York, St. Martin's Press, 1989, 328 p.
12. Suzdalev I.P. Nanotekhnologiya: Fiziko-khimiya nanoklasterov, nanostruktur i nanomaterialov [Nanotechnology: Physical chemistry of nanoclusters, nanostructures and nanomaterials]. Moscow, URSS Publ., 2017, 592 p. (In Russian).
13. Bukharov D.N., Kucherik A.O., Arakelyan S.M., Lotin A.A. Modeling of a profile of a PbTe semiconductor nanofilm, Journal of Physics: Conference Series, 2019, vol. 1331, art no. 012002, 8 p. DOI: 10.1088/1742-6596/1331/1/012002.
14. Burtsev A.A., Butkovskii O.Ya. Analiz kristallicheskikh struktur na poverkhnosti nerzhaveyushchej stali [Analysis of crystal structures on stainless steel surface], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 107-114. DOI: 10.26456/pcascnn/2019.11.107. (In Russian).
15. Brylkin Yu.V., Kusov A.L. Issledovanie zavisimosti fizicheskikh svojstv poverkhnosti ot fraktal'noj razmernosti [Research of the dependence of surface physical properties from the fractal dimension], Fizikokhimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2015, issue 7, pp. 142-149. DOI: 10.26456/pcascnn/2015.7.142 (In Russian).
16. Antonov A.S., Sdobnyakov N.Yu., Ivanov D.V. et al. Issledovanie fraktal'nykh svojstv nanorazmernykh plenok zolota, serebra i medi: atomno-silovaya i tunnel'naya mikroskopiya [Investigation of fractal properties of nanosized gold, silver and copper films: atomic force and tunnelling microscopy], Khimicheskaya fizika i mezoskopiya [Chemical Physics and Mesoscopy], 2017, vol. 19, no. 3, pp. 473-486. (In Russian).
17. Sdobnyakov N.Yu., Antonov A.S., Ivanov D.V. Morfologicheskie kharakteristiki i fraktal'nyj analiz metallicheskikh plenok na dielektricheskikh poverkhnostyakh: monografiya [Morphological characteristics and fractal analysis of metal films on dielectric substrates: monography], Tver, Tver State University Publ., 2019, 168 p. (In Russian).
18. Burtsev A.A., Mikhalevsky V.A. et al. Poluchenie nanochastits fazoizmenyaemogo materiala Ge2Sb2Te5 metodom pryamogo lazerno-indutsirovannogo perenosa [Synthesis of phase-change material Ge2Sb2Te5 nanoparticles by laser-induced forward transfer techniques], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 612-620. DOI: 10.26456/pcascnn/2024.16.612. (In Russian).
19. Burtsev A.A., V.A. Mikhalevsky, V.V. Ionin et al. Klasterizatsiya nanochastits fazoizmenyaemogo materiala Ge2Sb2Te5, poluchennykh metodom lazerno-indutsirovannogo perenosa [Clustering of phase-change material Ge2Sb2Te5 nanoparticles obtained by laser-induced forward transfer techniques], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 598-605. DOI: 10.26456/pcascnn/2025.17.598. (In Russian).
20. Witten T.А., Sander L.M. Diffusion limited aggregation, Physical Review В, 1983, vol. 27, issue 9, pp. 5686-5697. DOI: 10.1103/PhysRevB.27.5686.
21. Mroczka J., Woźniak M., Onofri F.R.A. Algorithms and methods for analysis of the optical structure factor of fractal aggregates, Metrology and Measurement Systems, 2012, vol. XIX, issue 3, pp. 459-470. DOI: 10.2478/v10178-012-0039-2.
22. Zaitsev D.A. A generalized neighborhood for cellular automata, Theoretical Computer Science, 2017, vol. 666, pp. 21-35. DOI: 10.1016/j.tcs.2016.11.002.
23. Wu J., Jin X., Mi S., Tang J. An effective method to compute the box-counting dimension based on the mathematical definition and intervals, Results in Engineering, 2020, vol. 6, pp. 100-106, DOI: 10.1016/j.rineng.2020.100106.