Microstructure and electrophysical properties of barium ferrite-based ceramics with bismuth impurity
M.A. Belyavsky, I.L. Kislova, A.Yu. Karpenkov, A.I. Ivanova, R.F. Izmailov, E.A. Pis'merova, A.V. Solnyshkin
Tver State University
DOI: 10.26456/pcascnn/2026.18.541
Original article
Abstract: In this work, bismuth-doped barium ferrite ceramic BaFe12O19 samples were synthesized. Scanning electron microscopy of the samples microstructure revealed that increasing the bismuth content in the ceramics BaBixFe12-xO19 leads to a decrease in the grain size. It should be noted that this also increases the density of the synthesized ceramics. The effect of Bi doping on the electrical properties of the obtained samples was studied. Adding the bismuth oxide into the barium ferrite during solid-phase synthesis reduces the sample conductivity significantly. This effect is due to a decrease in the mobility of charge carriers because of the potential relief change. Furthermore, in the low-frequency region, the dispersion dependences of the permittivity and dielectric loss tangent change significantly with increasing frequency, further indicating increased sample conductivity. Moreover, the low-frequency dispersion significantly decreases with the addition of bismuth ions to the ceramic samples, further indicating a decrease in electrical conductivity. For all compositions BaBixFe12-xO19 at x ≥ 0,2 full magnetic hysteresis loops and partial dielectric hysteresis loops were obtained for x = 0,6 and 1. It was found that the effect of an external magnetic field reveals a clear correlation between the permittivity and the amount of introduced impurity.
Keywords: ceramics based on barium ferrite, microstructure, multiferroic, dielectric constant, magnetic hysteresis loops, dielectric hysteresis loops
- Mikhail A. Belyavsky – 3rd year postgraduate student, Condensed Matter Physics Department, Tver State University
- Inna L. Kislova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University, ORCID: 0000-0003-3418-7929
- Aleksey Yu. Karpenkov – Ph. D., Head of Condensed Matter Physics Department, Tver State University
- Alexandra I. Ivanova – Ph. D., Docent, Applied Physics Department, Tver State University
- Ruslan F. Izmailov – 4th year student, Faculty of Physics and Technology, Tver State University
- Evgeniya A. Pis'merova – 4th year student, Faculty of Physics and Technology, Tver State University
- Alexander V. Solnyshkin – Professor of Condensed Matter Physics Department, Tver State University, ORCID: 0000-0002-4044-8761
For citation:
Belyavsky M.A., Kislova I.L., Karpenkov A.Yu., Ivanova A.I., Izmailov R.F., Pis'merova E.A., Solnyshkin A.V. Mikrostruktura i elektrofizicheskie svojstva keramiki na osnove ferrita bariya s primesyu vismuta [Microstructure and electrophysical properties of barium ferrite-based ceramics with bismuth impurity], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 541-549. DOI: 10.26456/pcascnn/2026.18.541. ⎘
Full article (in Russian): download PDF file
References:
1. Pullar R.C. Hexagonal ferrites: a review of the synthesis, properties and applications of hexaferrite ceramics. Progress in Materials Science, 2012, vol. 57, issue 7, pp. 1191-1334. DOI: 10.1016/j.pmatsci.2012.04.001.
2. Harris V.G. Modern microwave ferrites, IEEE Transactions on Magnetics, 2012, vol. 48, issue 3, pp. 1075-1104. DOI: 10.1109/TMAG.2011.2180732.
3. Turik A.V., Pavlenko A.V. Magnetodielectric effect and magnetoelectricity in multiferroics and heterogeneous systems: modeling and experiment, Ferroelectrics, 2013, vol. 444, issue 1, pp. 53-59. DOI: 10.1080/00150193.2013.786308.
4. Pavlenko A.V., Turik A.V., Reznichenko L.A. et al. The magnetodielectric effect in Bi1/2La1/2MnO3 ceramics, Technical Physics Letters, 2013, vol. 39, issue 1, pp. 78-80. DOI: 10.1134/S1063785013010215.
5. Ram S., Krishnan H., Rai K.N., Narayan K.A. Magnetic and electrical properties of Bi₂O₃ modified BaFe₁₂O₁₉ hexagonal ferrite, Japanese Journal of Applied Physics, 1989, vol. 28, issue 4R, pp. 604-608. DOI: 10.1143/JJAP.28.604.
6. Pal M., Brahma P., Chakravorty D., Agrawal D.C. Magnetic properties of Ba hexaferrites doped with bismuth oxide, Journal of Magnetism and Magnetic Materials, 1995, vol. 147, issues 1-2, pp. 208-212. DOI: 10.1016/0304-8853(95)00061-5.
7. Ghasemi A., Hossienpour A., Morisako A., Saatch A. Cation distribution in bismuth-doped M-type barium hexaferrite, Materials Research Bulletin, 2000, vol. 35, issue 11, pp. 847-859. DOI: 10.1016/S0025-5408(00)00382-2.
8. Sehar F., Anjum S., Mustafa Z., Atiq S. Co-existence of ferroelectric and ferromagnetic properties of Bi³⁺ substituted M-type barium hexaferrites, Journal of Superconductivity and Novel Magnetism, 2020, vol. 33, issue 7, pp. 2073-2086. DOI: 10.1007/s10948-020-05452-y.
9. Yao Y., Hrekau I.A., Tishkevich D.I. et al. Correlation of the chemical composition, phase content, structural characteristics and magnetic properties of the Bi-substituted M-type hexaferrites, Ceramics International, 2023, vol. 49, issue 22, part B, pp. 37009-37016. DOI: 10.1016/j.ceramint.2023.09.033.
10. Duglet R., Chauhan A., Sharma D. et al. Investigation on microwave absorption properties of bismuth ions doped barium hexaferrites, Journal of Materials Science: Materials in Electronics, 2024, vol. 35, issue 9, art. no. 654, 33 p. DOI: 10.1007/s10854-024-12418-6.
11. Catalan G., Scott J.F. Advances in magnetoelectric multiferroics, Advanced Materials, 2009, vol. 21, issue 24, pp. 2463-2485. DOI: 10.1002/adma.200802849.
12. Mott, N.F., Davis, E.A. Electronic properties of non-crystalline materials, 2nd ed. Oxford, Clarendon Press, 1979, 604 p.
13. Poplavko Yu.M., Pereverzeva L.P., Raevskii I.P. Fizika aktivnykh dielektrikov: uchebnoe posobie [Physics of Active Dielectrics: Textbook], ed. by V.P. Sakhnenko. Rostov-on-Don, Southern Federal University Publ., 2009, 480 p.