Original article

Abstract: Using a bimetallic Ni-Al nanolayer as an example, molecular dynamics simulations of contact melting during annealing at 900 K were performed. The open-source LAMMPS software and the embedded-atom potential were used for this purpose. Interest in the chosen research object is due to the complexity of the phase diagram, while the temperature for the molecular dynamics experiment (900 K) was determined by considering the contact melting temperature for the macroscopic Ni-Al system and the potential size effect. Furthermore, this temperature is lower than the melting point of the lower-melting element, i.e. aluminum. During annealing for up to 100 ns, several characteristic temperatures were identified, corresponding to different stages of the diffusion process in the bimetallic Ni-Al nanolayer. The evolution of the local structure was observed using the open-source Ovito software with a modifier corresponding to the Ackland-Jones method. This approach analyzes the geometry of the angles between the bond vectors of a selected atom with its nearest neighbors. Over the selected time interval (100 ns), interface movement was identified in the Ni-Al system, but the crystalline transition layer «prevents» further «activation» of contact melting. This effect is observed for the first time for contact melting in nanoscale metallic systems.

Keywords: contact melting, bimetallic Ni-Al nanolayer, LAMMPS, molecular dynamics simulation, embedded-atom potential, local structure, Ackland-Jones method

  • Nickolay B. Kuz'min – 2nd year postgraduate student, General Physics Department, Tver State University, ORCID: 0009-0006-0634-8878
  • Pavel V. Komarov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-2138-5088
  • Vladimir M. Samsonov – Dr. Sc., Full Professor, General Physics Department, Tver State University, ORCID: 0000-0003-2929-8069
  • Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336

For citation:

Kuz'min N.B., Komarov P.V., Samsonov V.M., Sdobnyakov N.Yu. O probleme nablyudeniya kontaktnogo plavleniya v molekulyarno-dinamicheskom eksperimente na bimetallicheskom nanosloe Ni-Al [On the problem of observing contact melting in a molecular dynamics experiment in Ni-Al bimetallic nanolayer], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 401-408. DOI: 10.26456/pcascnn/2026.18.401. ⎘

Full article (in Russian): download PDF file

References:

1. Akhkubekov A.A., Orkvasov T.A., Sozaev V.A. Kontaktnoe plavlenie metallov i nanostruktur na ikh osnove: monografiya [Contact melting of metals and nanostructures based on them: monograph]. M.: Fizmatlit Publ., 2008. – 152 p. (In Russian).
2. Korotkov P.K., Orkvasov T.A., Sozaev V.A. The size effect in contact melting of metals, Technical Physics Letters, 2006, vol. 32, issue 1, pp. 61-63. DOI: 10.1134/S1063785006010202.
3. Samsonov V.M., Kuzmin N.B., Talyzin I.V. et al. Application of fractal analysis to characterize the contact melting process in a bimetallic Cu–Ag nanolayer, Theoretical Foundations of Chemical Engineering, 2025, vol. 59, issue 3, pp. 549-554. DOI: 10.1134/S0040579525601773.
4. Samsonov V.M., Kuz’min N.B., Sdobnyakov N.Yu. et al. Contact melting in bimetallic Cu-Ag nanolayer: Molecular dynamics simulation and fractal analysis, Nano-Structures & Nano-Objects, 2025, vol. 43, art. no. 101496, 10 p. DOI: 10.1016/j.nanoso.2025.101496.
5. Samsonov V.M., Kuzmin N.B., Talyzin I.V. et al. Contact melting effect in a molecular dynamics model of a noneutectic Cu–Ni bilayer, Journal of Surface Investigation: X-ray, Synchrotron and Neutron Techniques, 2025, vol. 19, issue 6, pp. 1691-1697. DOI: 10.1134/S1027451025702374.
6. Guo X., Li S., Wang G. Phase diagram of continuous binary nanoalloys: size, shape and segregation effects, Scientific Reports, 2017, vol. 7, art. №0 41990, 10 p. DOI: 10.1038/srep41990.
7. Diagrammy sostoyaniya dvojnykh metallicheskikh sistem: spravochnik: v 3 tomakh [Phase diagrams of binary metallic systems: a reference book: in 3 volumes] / ed, by N.P. Lyakishev. M.: Mashinostroenie Publ., 1996-2000, vol. 1, 1996, 992 p.; vol. 2, 1997, 1024 p.; vol. 3, book 1, 2000, 872 p.; vol. 3, book 2, 2000, 448 p. (In Russian).
8. Zhikharev A.V., Bystrov S.G., Bayankin V.Ya. et al. Vliyanie lazera na formirovanie soedinenij Ni-Al v poverkhnostnykh sloyakh nikelevoj fol'gi v zavisimosti ot plotnosti moshchnosti lazernogo izlucheniya [The laser influence on the formation of Ni-Al compounds in the nickel foil surface layers depending on the laser radiation power density], Khimicheskaya fizika i mezoskopiya [Chemical Physics and Mesoscopics], 2023, vol. 25, no. 2, pp. 239-249. DOI: 10.15350/17270529.2023.2.22. (In Russian).
9. Huang W., Chang Y.A. A thermodynamic analysis of the Ni-Al system, Intermetallics, 1998, vol. 6, issue 6 pp. 487-498. DOI: 10.1016/S0966-9795(97)00099-X.
10. Shevtsova L.I. Struktura i mekhanicheskie svojstva materialov na osnove alyuminida nikelya, poluchennykh po tekhnologii iskrovogo plazmennogo spekaniya poroshkovykh smesej [Structure and mechanical properties of nickel aluminide-based materials obtained by spark plasma sintering of powder mixtures]. Cand. tech. sci.: 05.16.09. Novosibirsk, NSTU Publ., 2015, 200 p. (In Russian).
11. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI:10.26456/sny.2025.408. (In Russian).
12. Ackland G.J., Jones A.P. Applications of local crystal structure measures in experiment and simulation, Physical Review B, 2006, vol. 73, issue 5, pp. 054101-1-054104-7. DOI: 10.1103/PhysRevB.73.054104.
13. Larsen P.M., Schmidt S., Schiøtz J. Robust structural identification via polyhedral template matching modelling, Modelling and Simulation in Materials Science and Engineering, 2016, vol. 24, no. 5, art. № 055007, 18 p. DOI: 10.1088/0965-0393/24/5/055007.
14. Polak W.Z. Efficiency in identification of internal structure in simulated monoatomic clusters: Comparison between common neighbor analysis and coordination polyhedron method, Computational Materials Science, 2022, vol. 201, art. № 110882, 8 p. DOI: 10.1016/j.commatsci.2021.110882.
15. Tsuzuki H., Branicio P.S., Rino J.P. Structural characterization of deformed crystals by analysis of common atomic neighborhood, Computer Physics Communications, 2007, vol. 177, issue 6, pp. 518-523. DOI: 10.1016/j.cpc.2007.05.018.
16. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
17. LAMMPS Molecular Dynamics Simulator. Available at: www.url: http://lammps.sandia.gov. (accessed 02.05.2026).
18. Purja Pun G.P., Mishin Y. Development of an interatomic potential for the Ni-Al system, Philosophical Magazine, 2009, vol. 89, issue 34-36, pp. 3245-3267. DOI: 10.1080/14786430903258184.
19. Svoystva elementov. Spravochnik [Properties of elements. Handbook], ed. M.E. Drits, Moscow, Metallurgiya Publ., 1985, 672 p. (In Russian).
20. Shmorgun V.G., Trykov Yu.P., Bogdanov A.I. et al. Kinetika vzaimodejstviya alyuminiya i nikelya pri zhidkofaznom formirovanii diffuzionnoj zony [Kinetics of interaction between aluminum and nickel during liquid-phase formation of a diffusion zone], Vestnik Sibirskogo gosudarstvennogo industrial'nogo universiteta [Bulletin of the Siberian State Industrial University], 2014, no. 2 (8), p. 3-6. (In Russian).
21. Lajpanov M.Z. Kontaktnoe plavlenie i fazoobrazovanie makro-, mikrorazmernykh sistem med'-alyuminij, nikel'alyuminij, nikel'-olovo [Contact melting and phase formation of macro- and micro-sized systems of copper-aluminum, nickel-aluminum, nickel-tin]. Cand. fiz.-mat. nauk: 01.04.07. Nal'chik: KBSU Publ., 2019, 103 p. (In Russian).

Content |