The influence of conditions for obtaining shiny nickel coatings modified with nanodiamonds on their morphological features
E.G. Korzh1, K.M. Lopatin2, P.E. Antipov1, V.E. Burlakova1
1 Don State Technical University
2 «Etalon» LLC
DOI: 10.26456/pcascnn/2026.18.679
Original article
Abstract: In this study, bright nickel coatings modified with nanodiamonds were obtained using the electrochemical method in a bright nickel plating electrolyte at cathodic current densities of 1, 3, and 5 A/dm2. The resulting bright nickel coatings with nanodiamonds were studied using atomic force microscopy. It was found that the surface topography of the bright nickel coatings with nanodiamonds varies significantly and depends on the conditions (cathode current density) of coating production. The bright nickel coatings with nanodiamonds were studied using scanning electron microscopy. It was found that the morphological features of the nickel coatings with nanodiamonds obtained at a cathodic current density of 1 A/dm2 are characterized by an increased content of pores and irregularities compared to bright nickel coatings obtained at current densities of 3 and 5 A/dm2. The presence of inclusions in the form of rounded protrusions on the surface of shiny nickel coatings obtained at current densities of 3 and 5 A/dm2 was detected. Using energy-dispersive X-ray spectra, the presence of a carbon phase in the composite shiny nickel coating was confirmed, indicating the presence of nanodiamonds in its structure. It was found that the shiny nickel coating with nanodiamonds obtained at a cathodic current density of 5 A/dm2 contains up to 10,6% of the carbon phase.
Keywords: nanodiamonds, bright nickel coating, composite coating, surface morphology
- Ekaterina G. Korzh – PhD, Associate Professor, Department of Chemistry, Don State Technical University, ORCID: 0000-0002-4002-2082
- Kirill M. Lopatin – Founder, «Etalon» LLC
- Pavel E. Antipov – Engineer, Laboratory of Mechanics and Biocompatible Materials, Don State Technical University, ORCID: 0009-0009-8752-8572
- Victoria E. Burlakova – Dr. Sc., Professor, Department of Chemistry, Don State Technical University, ORCID: 0000-0003-3779-7079
For citation:
Korzh E.G., Lopatin K.M., Antipov P.E., Burlakova V.E. Vliyanie uslovij polucheniya blestyashchikh nikelevykh pokrytij, modifitsirovannykh nanoalmazami na ikh morfologicheskie osobennosti [The influence of conditions for obtaining shiny nickel coatings modified with nanodiamonds on their morphological features], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 679-686. DOI: 10.26456/pcascnn/2026.18.679. ⎘
Full article (in Russian): download PDF file
References:
1. Zhang W., Li B., Hong M., Li M. Effects of cerium oxide doping on microstructure and properties of Ni-GO-CeO2 nanocomposite coatings, Journal of Materials Research and Technology, 2022, vol. 21, pp. 3440-3450. DOI: 10.1016/j.jmrt.2022.10.149.
2. Köse M., Tan S., Uysal M. Graphene oxide reinforced NiPCo composite coatings: Optimum graphene oxide content for improved anticorrosion and wear resistance, Surface and Coatings Technology, 2025, vol. 504, art. no. 132021, 21 p. DOI: 10.1016/j.surfcoat.2025.132021.
3. Fatima I., Fayyaz O., Yusuf M.M. et al. Enhanced electrochemical and mechanical performance of BN reinforced Ni-P based nanocomposite coatings, Diamond and Related Materials, 2022, vol. 130, art. no. 109454, 14 p. DOI: 10.1016/j.diamond.2022.109454.
4. Song R., Zhang S., He Y. et al. Silicon nitride nanoparticles reinforced the corrosion resistance of Ni-Cu composite coating in simulated seawater solution, Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2022, vol. 649, art. no 129427, 10 p. DOI: 10.1016/j.colsurfa.2022.129427.
5. Li Z., Lin T., Jing C. et al. Effect of titanium carbide addition on the microstructure and properties of nickel‐based alloy coatings, Materialwissenschaft und Werkstofftechnik, 2025, vol. 56, issue 6, pp. 844-859. DOI: 10.1002/mawe.1744
6. Bayatlı A., Şahin E.F., Kocabaş M. Effect of boron carbide reinforcement on surface properties of electroless Ni–B and Ni–B–W coatings, Materials Chemistry and Physics, 2023, vol. 305, art. no. 127899, 11 p. DOI: 10.1016/j.matchemphys.2023.127899.
7. Górka J., Lont A., Poloczek T. The microstructure and properties of laser-cladded Ni-based self-fluxing alloy coatings reinforced by TiC particles, Coatings, 2025, vol. 15, issue 5, art. no. 527, 16 p. DOI: 10.3390/coatings15050527.
8. Maurya S.S., Grain A.K., Kumar R. et al. High temperature wear behavior of nanodiamond reinforced nickel-aluminum composite coatings, Wear, 2024, vol. 542-543, art. no. 205280, 16 p. DOI: 10.1016/j.wear.2024.205280.
9. Wintachai P., Kothanam N., Harahai K. et al. Tribological properties of diamond-reinforced electrodeposited NiP coatings: Mono-vs. bimodal particle incorporations, Diamond and Related Materials, 2025, art. no. 113169, 16 p. DOI: 10.1016/j.diamond.2025.113169.
10. Maurya S.S., Pandey K.K., Sharma S. et al. Microstructural, mechanical and tribological behavior of nanodiamonds reinforced plasma sprayed nickel-aluminum coating, Diamond and Related Materials, 2023, vol. 133, art. no. 109714, 26 p. DOI: 10.1016/j.diamond.2023.109714.
11. Mirche K.K., Pandey K.K., Pandey S.M. & Keshri A.K. Microstructure and corrosion behavior of plasma-sprayed nanodiamond-reinforced NiAl nanocomposite coating, Journal of Thermal Spray Technology, 2023, vol. 32, issue 5, pp. 1299-1310. DOI: 10.1007/s11666-023-01558-6.
12. Hong Q., Zhou R., Guo X. et al. A novel strategy for improving the wear resistance of electrodeposited Ni-diamond composite coatings by diamond surface morphology modification, Diamond and Related Materials, 2023, vol. 137, art. no. 109714, 10 p. DOI: 10.1016/j.diamond.2023.110093.
13. Zhang W., Mei T., Li B. et al. Effect of current density and agitation modes on the structural and corrosion behavior of Ni/diamond composite coatings, Journal of Materials Research and Technology, 2021, vol. 12, pp. 1473-1485. DOI: 10.1016/j.jmrt.2021.03.084.
14. Kurlovich S.A., Kovtun M.V. Sposob poluhenia vodnoi dispersii nanohastiz ugleroda [Method for obtaining an aqueous dispersion of carbon nanoparticles]. Patent RF, no 2838772, 2025.
15. Beskopylny A.N., Stel'makh S.A., Shcherban E.M. et al. Performance and mechanism of the structure formation and physical-mechanical properties of concrete by modification with nanodiamonds, Construction and Building Materials, 2024, vol. 452, art. no. 138994, 15 p. DOI: 10.1016/j.conbuildmat.2024.138994.