Creation of mesoscale models of aged polymer nanoparticles using the Rosenbluth algorithm
I.K. Patrenkov1, M.D. Malyshev1,2, P.V. Komarov1,2
1 Tver State University
2 Yaroslav-the-Wise Novgorod State University
DOI: 10.26456/pcascnn/2026.18.428
Original article
Abstract: This paper presents a three-stage approach to constructing mesoscale models of aged polymer nanoparticles. The initial nanoparticle configuration is constructed using the lattice Rosenbluth algorithm, which has been adapted to address the current issue. This algorithm creates dense globules composed of a specified number of polymer chains, which are constructed from coarse-grained particles (beads) of a single type. Increasing the size of the nanoparticles, as determined by the number of beads they contain, results in increased polydispersivity of the polymer chains. This also results in increased shape anisotropy. For nanoparticles containing more than 100 beads, this anisotropy is preserved even after long-term relaxation, which is the second stage in the construction process. The third step involves transforming some beads into different types using a specific ratio. The type of bead, its location in the polymer chain, and its ratio are determined from literature sources. Some intra-chain bonds are broken, and new inter-chain bonds are formed. These changes form the basis of the nanoparticle aging algorithm. Applying the aging algorithm has been found to lead to the formation of large numbers of low-molecular-weight fragments inside nanoparticles. These degraded products easily desorb from nanoparticle surfaces into the surrounding environment.
Keywords: Rosenbluth algorithm, coarse-grained modeling, polymers, degradation, nanoparticles
- Ivan K. Patrenkov – 2nd year postgraduate student, Department of General Physics, Tver State University
- Maxim D. Malyshev – Ph. D., Associate Professor of Physical Chemistry Department, Tver State University, Researcher, Microplastics Research Center Yaroslav-the-Wise Novgorod State University, ORCID: 0000-0002-2799-7512
- Pavel V. Komarov – Dr. Sc., Docent, General Physics Department, Tver State University, Leading Researcher, Microplastics Research Center Yaroslav-the-Wise Novgorod State University, ORCID: 0000-0003-2138-5088
For citation:
Patrenkov I.K., Malyshev M.D., Komarov P.V. Postroenie mezomasshtabnykh modelej sostarennykh polimernykh nanochastits s ispolzovaniem algoritma Rozenbluta [Creation of mesoscale models of aged polymer nanoparticles using the Rosenbluth algorithm], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 428-438. DOI: 10.26456/pcascnn/2026.18.428. ⎘
Full article (in Russian): download PDF file
References:
1. Kim M.-S. Modeling study on fate of micro/nano-plastics in micro/nano-hydrodynamic flow of freshwater, Journal of Hazardous Materials, 2021, vol. 419, art. no. 126397, 14 p. DOI: 10.1016/j.jhazmat.2021.126397.
2. Martín J., Santos J.L., Aparicio I., Alonso E. Microplastics and associated emerging contaminants in the environment: Analysis, sorption mechanisms and effects of co-exposure, Trends in Environmental Analytical Chemistry, 2022, vol. 35, art. no. e00170, 15 p. DOI: 10.1016/j.teac.2022.e00170.
3. Hoseini M., Stead J., Bond T. Ranking the accelerated weathering of plastic polymers, Environmental Sciences: Processes and Impacts, 2023, vol. 25, issue 12, pp. 2081-2091, DOI: 10.1039/d3em00295k.
4. Shyichuk A.V., White J.R., Craig I.H., Syrotynska I.D. Comparison of UV-degradation depth-profiles in polyethylene, polypropylene and an ethylene–propylene copolymer, Polymer Degradation and Stability, 2005, vol. 88, pp. 415-419, DOI: 10.1016/j.polymdegradstab.2004.12.006.
5. White J.R., Shyichuk A.V. Macromolecular scission and crosslinking rate changes during polyolefin photo-oxidation, Polymer Degradation and Stability, 2007, vol. 92, issue 7, pp. 1161-1168, DOI: 10.1016/j.polymdegradstab.2007.04.011.
6. Ruan X., Xie L., Liu J. et al. Rapid detection of nanoplastics down to 20 nm in water by surface-enhanced Raman spectroscopy, Journal of Hazardous Materials, 2024, vol. 462, art. no. 132702, 10 p. DOI: 10.1016/j.jhazmat.2023.132702.
7. Roy S., Bhattacharjee J. Nano-scale computational modeling: challenges, limitations, and emerging trends, Advanced Nanomaterials in Biomedical Implants: Processing, Structures, Properties and, Applications. Amsterdam, Elsevier, 2025, pp. 471-494, DOI: 10.1016/B978-0-443-27378-0.00018-0.
8. Ranby B.G., Rabek J.F. Photodegradation, photo-oxidation, and photostabilization of polymers: principles and applications. London, John Wiley & Sons, 1975, 590 p.
9. Adams J.H. Analysis of nonvolatile oxidation products of polypropylene. III. Photodegradation, Journal of Polymer Science. Part A1, 1970, vol. 8, issue 5, pp. 1279-1288, DOI: 10.1002/pol.1970.150080520.
10. Costa, L., Luda M.P., Trossarelli L. Ultra-high molecular weight polyethylene – II. Thermal- and photo-oxidation, Polymer Degradation and Stability, 1997, vol. 58, issue 1-2, pp. 41-54, DOI: 10.1016/s0141-3910(97)00010-4.
11. Wu Q., Qu B., Xu Y., Wu Q. Surface photo-oxidation and photostabilization of photocross-linked polyethylene, Polymer Degradation and Stability, 2000, vol. 68, issue 1, pp. 97-102, DOI: 10.1016/s0141-3910(99)00171-8.
12. Gardette M., Perthue A., Gardette J.-L. et al. Photo- and thermal-oxidation of polyethylene: Comparison of mechanisms and influence of unsaturation content, Polymer Degradation and Stability, 2013, vol. 98, issue 11, pp. 2383-2390, DOI: 10.1016/j.polymdegradstab.2013.07.017.
13. Scacchi A., Vuorte M., Sammalkorpi M. Multiscale modelling of biopolymers, Advances in Physics: X, 2024, vol. 9, issue 1, art. no. 2358196, 55 p. DOI: 10.1080/23746149.2024.2358196.
14. Hsu H.-P., Grassberger P. A review of Monte Carlo simulations of polymers with PERM, Journal of Statistical Physics, 2011, vol. 144, pp. 597-637, DOI: 10.1007/s10955-011-0268-x.
15. Binder K., Paul W. Recent developments in Monte carlo simulations of lattice models for polymer systems, Macromolecules, 2008, vol. 41, issue 13, pp. 4537-4550, DOI: 10.1021/ma702843z.
16. Paquet E., Viktor H.L. Molecular dynamics, Monte Carlo simulations, and Langevin dynamics: A computational review, Biomed Research International, 2015, vol. 2015, art. no. 183918, 18 p. DOI: 10.1155/2015/183918.
17. Liwo A., Czaplewski C., Sieradzan A.K. et al. Theory and practice of coarse-grained molecular dynamics of biologically important systems, Biomolecules, 2021, vol. 11, art. no. 1347, 31 p. DOI: 10.3390/biom11091347.
18. Glagolev M., Volgin I., Malyshev M. et al. Probing the structural evolution and stability of aged polyethylene nanoparticles through coupled atomistic-mesoscale simulations, Macromolecules, 2026, vol. 59, issue 12, pp. 6629-6643, DOI: 10.1021/acs.macromol.6c00213.
19. Voevodin Vl., Antonov A., Nikitenko D. et. al. Supercomputer Lomonosov-2: large scale, deep monitoring and fine analytics for the user community, Supercomputing Frontiers and Innovations, 2019, vol. 6, issue 2, pp. 4-11. DOI: 10.14529/jsfi190201.