Study of properties of selenium nanoparticles stabilized with K-17 polyvinyl pyrrolidone
Z.A. Rekhman, M.A. Pirogov, A.V. Blinov, A.V. Samovolov, A.Yu. Andiralov, Ya.A. Oblogin, A.V. Tatov
North Caucasus Federal University
DOI: 10.26456/pcascnn/2026.18.934
Original article
Abstract: In this work, samples of selenium nanoparticles stabilized with polyvinylpyrrolidone K-17 were obtained by chemical reduction of selenious acid with ascorbic acid in an aqueous medium in the presence of a stabilizer. The samples were studied by Fourier transform infrared spectroscopy, dynamic and electrophoretic light scattering. Computational quantum-chemical modeling of the interaction between polyvinylpyrrolidone K-17 and a selenium atom was performed using the QChem software package. The modeling results showed that the interaction of polyvinylpyrrolidone K-17 with selenium via the ionized amino group is energetically favorable (a decrease the total energy of 2397,942 kcal/mol) and chemically stable (the chemical rigidity of the molecular system is 0,160 eV). Analysis of the infrared spectra showed a match between the main diagnostic absorption bands of polyvinylpyrrolidone (3400, 1660, and 1460 cm-1) before and after stabilization of the selenium nanoparticles, with no new absorption bands appearing, indicating that the chemical structure of the polymer is preserved during synthesis. A study of colloidal stability by dynamic and electrophoretic light scattering over a pH range of 3-11, temperatures of 25-95°C, and holding times of 5-25 min showed that the average hydrodynamic diameter of the particles ranged from 45,44 to 197,67 nm, and the ζ-potential ranged from -6,05 to -83,06 mV, with the system exhibiting the highest stability in an alkaline medium at 25°C and the lowest stability in an acidic medium and at elevated temperature (95°C).
Keywords: selenium nanoparticles, polyvinyl pyrrolidone, quantum chemical modeling, infrared spectroscopy, colloidal stability
- Zafar A. Rekhman – Teacher, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0003-2809-4945
- Maxim A. Pirogov – Assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0001-9217-6262
- Andrey V. Blinov – Ph. D., Associate Professor, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0000-0002-4701-8633
- Artem V. Samovolov – Junior Research Assistant, International Research Laboratory of Functional Materials and Food Systems of the Department of Science, North Caucasus Federal University, ORCID: 0000-0001-5570-6201
- Alexander Yu. Andiralov – Research Engineer, International Research Laboratory of Functional Materials and Food Systems of the Department of Science, North Caucasus Federal University, ORCID: 0009-0006-1303-0083
- Yaroslav A. Oblogin – Laboratory Assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0009-0003-5180-9045
- Alexey V. Tatov – Laboratory Assistant, Department of Functional Materials and Engineering Design, North Caucasus Federal University, ORCID: 0009-0003-8842-232X
For citation:
Rekhman Z.A., Pirogov M.A., Blinov A.V., Samovolov A.V., Andiralov A.Yu., Oblogin Ya.A., Tatov A.V. Issledovanie svojstv nanochastits selena, stabilizirovannykh polivinilpirrolidonom marki K-17 [Study of properties of selenium nanoparticles stabilized with K-17 polyvinyl pyrrolidone], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 934-942. DOI: 10.26456/pcascnn/2026.18.934. ⎘
Full article (in Russian): download PDF file
References:
1. Akhmedzhanova Z.I., Zhiemuratova G.K., Danilova E.A. et al. Makro-i mikroelementy v zhiznedeyatel'nocti organizma i ikh vzaimosvyaz' s immunnoj sistemoj (obzor literatury) [Macro- and microelements in the body's vital functions and their relationship with the immune system (literature review)], Zhurnal teoreticheskoi i klinicheskoi meditsiny [Journal of Theoretical and Clinical Medicine], 2020, no. 1, pp. 16-21. (In Russian).
2. Li Q., Yu X., Liu H. et al. Emerging Insights into the role of trace elements in human health and disease prevention, Nutrients, 2025, vol. 17, issue 23, art. no. 3678, 4 p. DOI: 10.3390/nu17233678.
3. Vasilenko A.M., Sharipova M.M. Defitsit mikroehlementov i problema komorbidnosti [Deficiencies of trace elements and the problem of comorbidity], Mikroelementy v meditsine [Trace Elements in Medicine], 2019. vol. 20., no. 1, pp. 4-12. DOI: 10.19112/2413-6174-2019-20-1-4-12. (In Russian).
4. Drozdov V.N. Ratsional'noe vozmeshchenie defitsita vitaminov i mikroehlementov [Rational compensation of vitamins and microcells deficiency], Lechebnoe delo [Lechebnoe Delo Journal], 2009, no. 3, pp. 34-41. (In Russian).
5. Burtseva T.I., Burlutskaya O.I. Selen: essentsial'nyj mikroelement (obzor) [Selenium: an essential trace element (review)], Vestnik Orenburgskogo gosudarstvennogo universiteta [Vestnik of the Orenburg State University], 2006, no. 2 (52), pp. 7-9. (In Russian).
6. Gmoshinski I.V., Mazo V.K., Tuteljan V.A., Hotimchenko S.A. Mikroehlement selen: rol' v protsessakh zhiznedeyatel'nosti [Elenium microelement: its role in vitality processes], Ekologiya morya [Ecology of the sea], 2000, no. 54, pp. 5-19. (In Russian).
7. Zhang Y., Y.J. Roh, S.J. Han. Role of selenoproteins in redox regulation of signaling and the antioxidant system: a review, Antioxidants, 2020, vol. 9, issue 5, art. no. 383, 17 p. DOI: 10.3390/antiox9050383.
8. Shestakova T.P. Ispol'zovanie selena v meditsinskoi praktike [The use of selenium in medical practice], Russkij Meditsinskij Zhurnal [Russian Medical Journal], 2017, vol. 25, no. 22, pp. 1654-1659. (In Russian).
9. Golubkina N.A., Kapitalchuk I.P., Kapitalchuk M.V. Selen v pochvakh na raznykh vysotnykh urovnyakh rel'efa Dnestrovsko-Prutskogo mezhdurech'ya [Selenium in soils at different altitudes of the terrain between the rivers dniester and prut], Vestnik Moskovskogo gosudarstvennogo oblastnogo universiteta. Seriya: Estestvennye nauki [Bulletin of Moscow state regional university. Series: natural sciences], 2012, no. 1, pp. 98-101. (In Russian).
10. Reshetnik L.A., Parfjonova E.O. Selen i zdorov'e cheloveka (obzor literatury) [Selenium and people’s health (literary review)], Ekologiya morya [Ecology of the sea], 2000, vol. 54, pp. 20-25. (In Russian).
11. Reshetnik L.A., Parfenova E.O. Biogeokhimicheskoe i klinicheskoe znachenie selena dlya zdorov'ya cheloveka [Biogeochemical and clinical significance of selenium for human health], Mikroelementy v meditsine [Trace Elements in Medicine], 2001, vol. 2, no. 2, pp. 2-8. (In Russian).
12. Liu L., Luo P., Wen P., Xu P. Effects of selenium and iodine on Kashin-Beck disease: an updated review, Frontiers in Nutrition, 2024, vol. 11, art. no. 1402559, 11 p. DOI: 10.3389/fnut.2024.1402559.
13. Egorova E.A., Gmoshinskii I.V., Zorin S.N., Mazo V.K. Izuchenie vsasyvaniya i deponirovaniya selena v sostave biomassy selenosoderzhashchikh laktobatsill i selenita natriya u laboratornykh zhivotnykh [Studies on essential trace element selenium absorption and lay up from selenium containing lactobacillus biomass in laboratory animals], Voprosy detskoi dietologii [Pediatric Nutrition], 2006, vol. 4, no. 2, pp. 14-16. (In Russian).
14. Skorinova K.D., Kuzmenko V.V., Vasilenko I.A. Perspektiva sozdaniya lekarstvennykh preparatov na osnove nanochastits selena (obzor) [The prospect of creating medicines based on selenium nanoparticles (review)], Razrabotka i registratsiya lekarstvennykh sredstv [Drug development & registration], 2020, vol. 9, no. 2, pp. 33-44. DOI: 10.33380/2305-2066-2020-9-2-33-44. (In Russian).
15. Nikitenko O.V., Putalova I.N. Strukturno-kletochnye perestroiki limfoidnykh organov posle vnutribryushinnogo vvedeniya selenita natriya v toksicheskoi doze [Structural and cellular changes in lymphoid organs after intraperitoneal of sodium selenite introductions in the toxic dose in the cavity peritoneale], Vestnik novykh meditsinskikh tekhnologij [Bulletin of new Medical Technologies], 2010, vol. 17, no. 2, pp. 32-35. (In Russian).
16. IQmol Molecular Viewer. Available at: www.url: http://www.iqmol.org/ (accessed 12.06.2026).
17. Q-Chem 6.3 User’s Manual. Available at: https://manual.q-chem.com/6.3/ (accessed 12.06.2026).