Film polymeric carriers of sodium carboxymethylcellulose and polyvinyl alcohol for the immobilization of nanosized calcium phosphates
O.N. Musskaya1, V.K. Krut'ko1, V. Aniya2, Ch. Patra2, E.N. Krutsko1, A.E. Doroshenko1, I.E. Glazov1, Sh. Pant2, Ch. Batsh2, H. Majeed2, P. Nagchowdhury2, A.I. Kulak1
1 Institute of General and Inorganic Chemistry of the NAS of Belarus
2 CSIR-Indian Institute of Chemical Technology
DOI: 10.26456/pcascnn/2026.18.887
Original article
Abstract: The formation features of interpolymer complexes from 0.4-7.0% aqueous solutions of sodium carboxymethyl cellulose and polyvinyl alcohol were studied. Film polymer materials were developed based on the sodium carboxymethyl cellulose / polyvinyl alcohol interpolymer complexes using the casting method. Film materials based on sodium carboxymethyl cellulose are highly soluble in aqueous media with pH of 5-7 and are more hydrophilic compared to polyvinyl alcohol and sodium carboxymethyl cellulose / polyvinyl alcohol. The possibility of increasing hydrophobic properties, as well as regulating the degree of resorption of sodium carboxymethyl cellulose / polyvinyl alcohol film composite materials, depending on their composition and heat treatment at 85ºC was demonstrated. Thermal analysis showed that the highest stability in the temperature range of 200–800ºC is characteristic of sodium carboxymethyl cellulose and sodium carboxymethyl cellulose / polyvinyl alcohol (1:1) samples. Additional treatment at 85°C for 1 hour improves the thermal stability of the materials; however, increasing the treatment time to 2 hours reduces the thermal stability of the samples. The resulting film materials are cytocompatible and hold promise as resorbable carriers for the immobilization of nanosized calcium phosphates and other bioactive components.
Keywords: film polymer materials, interpolymer complex, sodium carboxymethylcellulose, polyvinyl alcohol, calcium phosphates
- Olga N. Musskaya – Ph. D., Assistant Professor, Leading Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-9821-8969
- Valentina K. Krut'ko – Ph. D., Assistant Professor, Head of the Laboratory of Photochemistry and Electrochemistry, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-1670-207X
- Vineet . Aniya – Ph. D., Senior Scientist E, Chemical Engineering & Process Technology department, CSIR-Indian Institute of Chemical Technology, ORCID: 0000-0003-2446-2894
- Chitta Ranjan . Patra – Ph. D., Scientist G, Department of Applied Biology, CSIR-Indian Institute of Chemical Technology, ORCID: 0000-0001-9453-6524
- Evgeny N. Krutsko – Senior Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0009-0005-7441-6986
- Anna E. Doroshenko – Ph. D., Senior Researcher, Photochemistry and Electrochemistry Laboratory, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0009-0003-5034-7272
- Ilya E. Glazov – Ph. D., Senior Researcher, Laboratory of Photochemistry and Electrochemistry, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0003-2183-6715
- Shubham . Pant – Ph. D., Researcher, Chemical Engineering & Process Technology department, CSIR-Indian Institute of Chemical Technology, ORCID: 0000-0002-3965-5536
- Chandramani . Batsh – Researcher, Chemical Engineering & Process Technology department, CSIR-Indian Institute of Chemical Technology, ORCID: 0009-0003-7383-2326
- Hanana Abdul . Majeed – Researcher, Chemical Engineering & Process Technology department, CSIR-Indian Institute of Chemical Technology, ORCID: 0009-0006-0773-4420
- Proma . Nagchowdhury – Researcher, Department of Applied Biology, CSIR-Indian Institute of Chemical Technology, ORCID: 0000-0002-0152-5074
- Anatoly I. Kulak – Academician, D. Sc., Professor, Director, Institute of General and Inorganic Chemistry of the NAS of Belarus, ORCID: 0000-0002-1398-3806
For citation:
Musskaya O.N., Krut'ko V.K., Aniya V.., Patra Ch.., Krutsko E.N., Doroshenko A.E., Glazov I.E., Pant Sh.., Batsh Ch.., Majeed H.., Nagchowdhury P.., Kulak A.I. Plenochnye polimernye nositeli natrijkarboksimetiltsellyulozy i polivinilovogo spirta dlya immobilizatsii nanorazmernykh kaltsijfosfatov [Film polymeric carriers of sodium carboxymethylcellulose and polyvinyl alcohol for the immobilization of nanosized calcium phosphates], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 887-896. DOI: 10.26456/pcascnn/2026.18.887. ⎘
Full article (in Russian): download PDF file
References:
1. Bakibaev A.A., Tuguldurova V.P., Lyapunova M.V. Protivospayechnoye deystviye kompozitsionnykh plenochnykh materialov na osnove modifitsirovannoy glikolurilom natriyevoy soli karboksimetiltsellyulozy [Anti-adhesion effect of composite film materials based on glycoluril-modified sodium carboxymethyl cellulose], Sovremennye tehnologii v medicine [Modern Technologies in Medicine], 2021, vol. 13, no. 1, pp. 35-41. DOI: 10.17691/stm2021.13.1.04. (In Russian).
2. Fazel Anvari-Yazdi A., Badea I., Chen X. Biomaterials in postoperative adhesion barriers and uterine tissue engineering, Gels, 2025, vol. 11, issue 6, art. no. 441, 51 p. DOI: 10.3390/gels11060441.
3. Mudarisova R.K., Badykova L.A., Azamatova G.A. et al. Polymeric eye films based on polyvinyl alcohol and arabinogalactan with levofloxacin, Russian Journal of Applied Chemistry, 2013, vol. 86, issue 4, pp. 606-610. DOI: 10.1134/S1070427213040289.
4. Erofeeva L.N., Pankrusheva T.A., Chekmareva M.S. et al. Issledovaniya kafedry farmatsevticheskoy tekhnologii po razrabotke polimernykh lekarstvennykh plenok [Research by the department of pharmaceutical technology on the development of polymer medicinal films], Meditsinskaya nauka i obrazovaniye [Urala Medical Science and Education of Ural], 2017, no. 4, pp 179-183. (In Russian).
5. Gushchin N.A., Ostrovidova G.U., Sosnov E.A. Antimicrobial polymeric composite films for medical use, Russian Journal of Applied Chemistry, 2008, vol. 81, issue 1, pp. 128-130.
6. Kalita H., Pal P., Dhara S., Pathak A. Fabrication and characterization of polyvinyl alcohol/metal (Ca, Mg, Ti) doped zirconium phosphate nanocomposite films for scaffold-guided tissue engineering application, Materials Science and Engineering C, 2017, vol. 71, pp. 363-371. DOI: 10.1016/j.msec.2016.09.063.
7. Kesharwani R., Yadav R. et al. Polymer based biofilms: development and clinical application in medical science, Biomedical Materials & Devices, 2024, vol. 2, pp. 275-287. DOI: 10.1007/s44174-023-00114-8.
8. Thambirajoo M., Md Fadilah N.I., Maarof M. et al. Functionalised sodium–carboxymethylcellulose–collagen bioactive bilayer as an acellular skin substitute for future use in diabetic wound management: the evaluation of physicochemical, cell viability, and antibacterial effects, Polymers, 2024, vol. 16, issue 16, art. no. 2252, 27 p. DOI: 10.3390/polym16162252.
9. Yunusov K.E., Mirkholisov M.M., Azizova M.A. et al. Advances in the formation and properties of nanofiber biomaterials from polyvinyl alcohol/carboxymethylcellulose/nanosilver systems for medical applications, Chemical Review and Letters, 2025, vol. 8, pp. 20-38. DOI: 10.22034/crl.2024.473962.1409.
10. Musskaya O.N., Krut'ko V.K., Kulak A.I., Lesnikovich Yu.A. Plenochnyye kompozity na osnove gidroksiapatita i polivinilovogo spirta [Film composites based on polyvinyl alcohol and hydroxyapatite], Polimernyye materialy i tekhnologii [Polymer Materials and Technologies], 2017, vol. 3, no. 2, pp. 28-33. DOI: 10.32864/polymmattech-2017-3-2-28-33. (In Russian).
11. Krut’ko V.K., Musskaya O.N., Kulak A.I., Safronova T.V. Termicheskaya evolyutsiya kal'tsiyfosfatnoy penokeramiki, poluchennoy na osnove gidroksiapatita i monokal'tsiyfosfata monogidrata [Thermal evolution of calcium phosphate foam ceramics obtained on the basis of hydroxyapatite and monocalcium phosphate of monohydrate], Fiziko-himicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2019, issue 11, pp. 615-623. DOI: 10.26456/pcascnn/2019.11.615. (In Russian).
12. Skachkov V.М., Bogdanova E.A., Bibanaeva S.A., Shirokova A.G. Razrabotka materiala na osnove gidroksiapatita i alyumosilikatnykh tseolitov so svyazuyushchim agentom dlya bioformirovaniya pokrytiy [Development of a material based on hydroxyapatite and aluminosilicate zeolites with a binding agent for the formation of bioactive coatings], Fiziko-himicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 1004-1015. DOI: 10.26456/pcascnn/2024.16.1004. (In Russian).
13. Glazov I.E., Krut’ko V.K., Vlasov R.A. Osazhdeniye gibridnykh nanokompozitov gidroksiapatit/autofibrin v slaboshchelochnoy srede [Precipitation of hybrid hydroxyapatite / autofibrin nanocomposites], Fiziko-himicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2021, issue 13, pp. С. 818-828. DOI: 10.26456/pcascnn/2021.13.818. (In Russian).
14. Glazov I.E., Krut'ko V.K., Musskaya O.N., Kulak A.I. Calcium phosphate apatites: wet formation, thermal transformations, terminology, and identification, Russian Journal of Inorganic Chemistry, 2022, vol. 67, issue 2, pp. 173-182. DOI: 10.1134/S0036023622020048.
15. Stalder A.F., Melchior T., Müller M. et al. Low-bond axisymmetric drop shape analysis for surface tension and contact angle measurements of sessile drops, Colloids and Surfaces A: Physicochemical and Engineering Aspects, 2010, vol. 364, issue 1-3, pp. 72-81. DOI: 10.1016/j.colsurfa.2010.04.040.
16. Londhe S., Haque S., Tripathy S. et al. Silver nitroprusside nanoparticles for breast cancer therapy: in vitro and in vivo approach, Nanoscale, 2023, vol. 15, issue 23, pp. 10017-10032. DOI: 10.1039/d3nr00221g.
17. Julappagari M., Haque S., Tripathy S. et al. Gold nanoparticles-based targeted delivery of rapamycin and Olaparib to breast cancer: An in vitro and in vivo approach, Bioorganic Chemistry, 2025, vol. 158, art. no. 108322, 20 p. DOI: 10.1016/j.bioorg.2025.108322.
18. Likhomanova S.V., Kamanina N.V. Mekhanizmy vzaimodeystviya molekul polivinilovogo spirta i uglerodnykh nanochastits v vodnykh rastvorakh [Interaction mechanisms of polyvinyl alcohol molecules with carbon nanoparticles in aqueous solutions], Prikladnaya fizika [Applied Physics], 2025, no. 1, pp. 78-83. DOI: 10.51368/1996-0948-2025-1-78-83. (In Russian).
19. Rault J., Gref R., Ping Z.H. et al. Glass transition temperature regulation effect in a poly(vinyl alcohol)-water system, Polymer, 1995, vol. 36, issue 8, pp. 1655-1661. DOI: 10.1016/0032-3861(95)99011-I.
20. Tan L., Shi R., Ji Q.et al. Effect of Na+ and Ca2+ on the thermal degradation of carboxymethylcellulose in air, Polymers & Polymer Composites, 2017, vol. 25, issue 4, pp. 309-314. DOI: 10.1177/096739111702500408.