Original article

Abstract: The article discusses changes in the structure and microhardness of diffusion-hardening solder based on low-melting alloy gallium (68%) -indium (23,5%) -tin (8,5%) and a solid component from copper-tin alloy powder (5%) depending on the dosage of stainless steel powder. Stainless steel powder was added in an amount of 5, 10, 15, 20% by weight, solder samples were heat treated at temperatures of 125 and 600°C, and compared with a base solder composition of 30% by weight of gallium-indium-tin alloy and 70% by weight of copper-tin alloy powder. The X-ray phase analysis method determines the phases formed as a result of the interaction of solder components under different heat treatment modes. The method of differential thermal analysis revealed thermal effects in the formation of solid solutions and intermetallic compounds of gallium with transition metals in the temperature range of 17-600°C. It has been shown that thermal treatment at temperatures above 450°C promotes the transition of the solder to an equilibrium state, which leads to an increase in hardness, in particular, due to the uniform distribution of nanoscale inclusions. Scanning electron microscopy revealed that stainless steel has limited solubility in the composition of diffusion-hardening solder, but after high-temperature treatment (600°C) reduces its hardness due to violation of the composition of the gallium-copper solid solution.

Keywords: composite diffusion-hardening solders, metal powder, properties, microhardness, differential thermal analysis

  • Vladimir M. Skachkov – Ph. D., Senior Researcher, Laboratories of heterogeneous processes chemistry, The Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0003-2551-3235
  • Svetlana A. Bibanaeva – Researcher, Laboratories of heterogeneous processes chemistry, The Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-1181-8735
  • Nail A. Sabirzyanov – Dr. Sc., Chief Researcher, Laboratories of heterogeneous processes chemistry, The Institute of Solid State Chemistry of the Ural Branch of RAS, ORCID: 0000-0002-0304-8160

For citation:

Skachkov V.M., Bibanaeva S.A., Sabirzyanov N.A. Izmenenie svojstv diffuzionno-tverdeyushchego kompozitsionnogo pripoya pri modifikatsii poroshkom iz nerzhaveyushchej stali [Change in properties of diffusion-hardening composite solder when modified with stainless steel powder], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 761-770. DOI: 10.26456/pcascnn/2026.18.761. ⎘

Full article (in Russian): download PDF file

References:

1. Devitsky O.V. Sovremennie metodi polucheniya tonkih pleonok GaAs1-X-YNXBiY: obzor [Advanced methods for growth thin films of GaAs1-X-YNXBiY: a review], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 636-648. DOI: 10.26456/pcascnn/2025.17.636. (In Russian).
2. Mineral commodity summaries 2026, Mineral Commodity Summaries. Reston, VA, U.S. Geological Survey, 2026, 222 p. DOI: 10.3133/mcs2026.
3. Maraeva E.V., Permiakov N.V., Moshnikov V.A. Osobennosti primeneniya e`vtekticheskix rasplavov na osnove indiya i galliya [The features of application of eutectic melts based on indium and gallium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 760-776. DOI: 10.26456/pcascnn/2023.15.760. (In Russian).
4. Yatsenko S.P., Hayak V.G. Kompozitsionnye pripoi na osnove legkoplavkikh splavov [Composite solders based on low-melting alloys]. Ekaterinburg, Ural Branch of RAS Publ., 1997, 186 p. (In Russian).
5. Yatsenko S.Р., Pasechnik L.A., Skachkov V.M., Rubinshtein G.V. Gallii: Gallij: Tekhnologii polucheniya i primenenie zhidkikh splavov: Monografiya [Technologies for the production and application of liquid alloys]. Moscow, RAS Publ., 2020, 344 p. (In Russian).
6. Skachkov V.M. Osobennosti dinamiki izmeneniya svoistv diffuzionno-tverdeyushchij pripoj v razlichnih uslovijah [Features of dynamics change of properties of diffusion-hardening solder at various conditions], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 699-706. DOI: 10.26456/pcascnn/2022.14.699. (In Russian).
7. Pashkov I.N., Gadzhiev M.R., Morozov V.A., Bazlova T.A. Vy`bor pripoya pri proizvodstve rezczov dorozhny`x mashin i issledovanie mikrostruktury` payany`x soedinenij [Selection of solder in the production of cutters for road machines and study of the microstructure of soldered joints], Svarochnoe proizvodstvo [Welding International], 2024, no. 2, pp. 56-63. (In Russian).
8. Galushka I.A., Afanasiev-Khodikin A.N., Panteleev M.D., Zotov S.D. Optimizaciya kompozicii pripoya dlya soedineniya raznoimennogo sochetaniya splavov E`P975 i VKNA-25 s ispol`zovaniem sovremenny`x vy`chislitel`ny`x sistem [Optimization of the solder composition for joining dissimilar EP975 and VKNA-25 alloys using modern computational systems] Trudy` VIAM [Proceedings of VIAM], 2026, no. 2 (156), pp. 37-48. DOI: 10.18577/2307-6046-2026-0-2-37-48. (In Russian).
9. Skachkov V.M., Pasechnik L.A., Skachkova O.V., Yatsenko S.P. Diffuzionno-tverdeyushchij pripoj na osnove splava gallij-indij-olovo i poroshka metallov PMOSF5, uprochnennyj titanom [Diffuzionno-hardening solders based alloy gallium-indium-tin and powder of metal PCTSP5 reinforced with titanium], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2018, issue 10, pp. 600-608. DOI: 10.26456/pcascnn/2018.10.600. (In Russian).
10. Skachkov V.M. Svoistva diffuzionno-tverdeyushchij kompozitsionnogo pripoj modifizirovannogo porosckom vanadij [Properties of diffusion-hardening composite solder modified with vanadium powder], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 823-830. DOI: 10.26456/pcascnn/2023.15.823. (In Russian).
11. Skachkov V.M., Pasechnik L.A., Medyankina I.S., Sabirzyanov N.A. Svojstva diffuzionno-tverdeyushchego kompozitsionnogo pripoya modifitsirovannogo poroshkami vol'frama [Properties of diffusion-hardening composite solder modified with tungsten powders], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 707-716. DOI: 10.26456/pcascnn/2022.14.707. (In Russian).
12. Dubov L.Yu., Shtotsky Yu.V., Ilyukhina O.V. et al. Pozitronnaja diagnostika Fe–Ga splavov [Positron diagnostics of Fe–Ga alloys], Yadernaya fizika i inzhiniring [Physics of Atomic Nuclei], 2026, issue 17, no 1, pp. 12-21. DOI: 10.56304/S2079562926010082. (In Russian).
13. Powder Diffraction File JCPDS-ICDD PDF-2 (Set 1-47). (Release, 2016). Available at: www.url: https://www.icdd.com/pdf-2/ (accessed 15.03.2026).
14. Speyer R.F. Thermal Analysis of Materials. New York, Marcel Dekker Publ., 1994, 298 p.
15. Poroshok splava med'-olovo sfericheskoi formy. Tekhnicheskie usloviya [Spherical copper-tin alloy powder. Specifications]. Specifications RF, no. 48-1318-03-89. Мoscow, 1989. 9 p. (In Russian).
16. Poroshki korrozionnostojkikh stalei. Tekhnicheskie usloviya [Powders of corrosion-resistant steels]. Specifications RF, no. 14-1-3540-83. Мoscow, 1983. 9 p. (In Russian).
17. Vasilev A.A., Nefedov D.Yu., Charnaya E.V. et al. Vliyanie magnitnogo polya na napravlennuyu kristallizaciyu galliya [Impact of magnetic field on directional crystallization in gallium], Fizika tverdogo tela [Physics of the solid state], 2025, issue 67, no 10, pp. 1830-1836. DOI: 10.61011/FTT.2025.10.61958.272-25. (In Russian).
18. Semenov A.A., Ukhov S.A., Semenov S.A. Problemy` i perspektivy` izvlecheniya indiya i proizvodstva vy`sokochistogo metalla [Problems and prospects of indium recovery and production of high-purity metal], Voprosy` atomnoj nauki i texniki. Seriya: materialovedenie i novy`e materialy` [Issues of atomic science and technology. Series: Materials Science and New Materials], 2025, no 2 (128), pp. 98-117. (In Russian).

Content |