Abstract: Using two initial configurations (a multi-shell structure and an alloy with a uniform distribution of components) as an example, a molecular dynamics study was conducted to investigate the structure formation processes in quaternary Cu-Au-Pt-Pd nanoparticles (with a total of 10,000 atoms) during a sequential cycle of thermally induced exposure, including phase transitions corresponding to melting and crystallization. The thermally induced exposure was performed at three cooling/heating rates: 0,25 K/ps (typical rate), 0,5 K/ps (median rate), and 1 K/ps (high rate). For each initial configuration, the temperature dependences of the potential component of the specific internal energy were obtained during heating and cooling, and the hysteresis parameters of the melting and crystallization temperatures were determined. Additionally, the regularities of chemical and structural segregation in the configurations corresponding to the end of cooling are described. Furthermore, the component distributions in the final configurations of the Cu-Au-Pt-Pd nanoparticles were constructed and analyzed to verify the hypothesis of a specific segregation behavior of the components. It is shown that the patterns of local crystalline ordering and the width of the temperature hysteresis corresponding to melting and crystallization are determined mainly by the rate of thermally induced action, while the initial morphology has a predominant effect on the distribution of atoms between fcc and hcp local environments.
Keywords: quaternary Cu-Au-Pt-Pd nanoparticles, multi-shell structure, alloy with uniform distribution of components, molecular dynamics method, tight-binding potential, segregation
- Sergei V. Serov – 2nd year postgraduate student, General Physics Department, Tver State University, ORCID: 0009-0004-6219-6309
- Kseniya G. Savina – 4th year postgraduate student, General Physics Department, Tver State University, ORCID: 0000-0002-4916-4968
- Andrei Yu. Kolosov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-3805-0567
- Denis N. Sokolov – Ph. D., Researcher, General Physics Department, Tver State University, ORCID: 0000-0003-2411-0143
- Sergey A. Veresov – 4th year postgraduate student, General Physics Department, Tver State University
- Danila R. Zorin – 1st year postgraduate student, General Physics Department, Tver State University
- Alexander V. Zaytsev – 4th year student, General Physics Department, Tver State University
- Nickolay N. Simchuk – 4th year student, General Physics Department, Tver State University
- Nickolay Yu. Sdobnyakov – Dr. Sc., Docent, Professor, General Physics Department, Tver State University, ORCID: 0000-0003-1749-0336
For citation:
Serov S.V., Savina K.G., Kolosov A.Yu., Sokolov D.N., Veresov S.A., Zorin D.R., Zaytsev A.V., Simchuk N.N., Sdobnyakov N.Yu. Osobennosti strukturnykh prevrashchenij v chetyrekhkomponentnykh nanosplavakh Cu-Au-Pt-Pd: mnogoobolochechnaya struktura i splav s ravnomernym raspredeleniem komponentov [Features of structural transformations in four-component Cu-Au-Pt-Pd nanoalloys: multi-shell structure and alloy with uniform distribution of components], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2026, issue 18, pp. 439-454. DOI: 10.26456/pcascnn/2026.18.439. ⎘
Full article (in Russian): download PDF file
References:
1. Samsonov V.M., Vasilev S.A., Talyzin I.V. et al. Nanothermodynamics on the example of metallic nanoparticles, Russian Journal of Physical Chemistry A, 2023, vol. 97, issue 8, pp. 1751-1760. DOI: 10.1134/S003602442308023X.
2. Ferrando R., Jellinek J., Johnston R.L. Nanoalloys: from theory to applications of alloy clusters and nanoparticles, Chemical Reviews, 2008, vol. 108, issue 3, pp. 845-910. DOI: 10.1021/cr040090g.
3. Dahale C., Srinivasan S., Mishra S. et al. Surface segregation in AgAuCuPdPt high entropy alloy: insights from molecular simulations, Molecular Systems Design & Engineering, 2022, vol. 7, issue 8, pp. 878-888. DOI: 10.1039/D2ME00045H.
4. Tang Z., Yeo B.C., Han S.S. et al. Facile aqueous-phase synthesis of Ag–Cu–Pt–Pd quadrometallic nanoparticles, Nano Convergence, 2019, vol. 6, art. no. 38, 7 p. DOI: 10.1186/s40580-019-0208-z.
5. Lu X.-Z., Shao G.-F., Xu L.-Y. et al. Structural optimization and segregation behavior of quaternary alloy nanoparticles based on simulated annealing algorithm, Chinese Physics B, 2016, vol. 25, no. 5, pp. 053601-1-053601-8. DOI: 10.1088/1674-1056/25/5/053601.
6. Veresov S.A., Savina K.G., Veselov A.D. et al. K voprosu izucheniya protsessov strukturoobrazovaniya v chetyrekhkomponentnykh nanochastitsakh [To the problem of studying structure formation processes in quaternary nanoparticles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 371-382. DOI: 10.26456/pcascnn/2022.14.371. (In Russian).
7. Kolosov A.Yu., Savina K.G., Veresov S.A. et al. Stsenarii strukturoobrazovaniya v chetyrekhkomponentnykh nanochastitsakh: atomisticheskoe modelirovanie [Structure formation scenarios in quaternary nanoparticles: atomistic simulation], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2023, issue 15, pp. 432-443. DOI: 10.26456/pcascnn/2023.15.432. (In Russian).
8. Kolosov A.Yu., Veresov S.A., Serov S.V. et al. Razmernyi effekt v chetyrekhkomponentnykh nanochastitsakh Au–Cu–Pd–Pt i ikh stabil’nost’ [Size effect in quaternary Au–Cu–Pd–Pt nanoparticles and their stability], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2024, issue 16, pp. 361-372. DOI: 10.26456/pcascnn/2024.16.361. (In Russian).
9. Serov S.V., Nepsha N.I., Kolosov A.Yu. et al. Strukturnye prevrashcheniya v chetyrekhkomponentnykh nanosplavakh Cu–Au–Pt–Pd razlichnoi morfologii pri posledovatelnykh termoindutsirovannykh tsiklakh [Structural transformations in quaternary Cu–Au–Pt–Pd nanoalloys of different morphology under successive thermally induced cycles], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2025, issue 17, pp. 466-484. DOI: 10.26456/pcascnn/2025.17.466. (In Russian).
10. Eom N., Messing M.E., Johansson J. et al. General trends in core–shell preferences for bimetallic nanoparticles, ACS Nano, 2021, vol. 15, issue 5, pp. 8883-8895. DOI: 10.1021/acsnano.1c01500.
11. Samsonov V.M., Talyzin I.V., Kartoshkin A.Yu. et al. On the problem of stability/instability of bimetallic core-shell nanostructures: molecular dynamics and thermodynamic simulations, Computational Materials Science, 2021, vol. 199, art. no. 110710, 11 p. DOI: 10.1016/j.commatsci.2021.110710.
12. Bochicchio D., Ferrando R. Morphological instability of core-shell metallic nanoparticles, Physical Review B, 2013, vol. 87, issue 16, pp. 165435-1-165435-13. DOI: 10.1103/PhysRevB.87.165435.
13. Shibuta Y., Suzuki T. A molecular dynamics study of cooling rate during solidification of metal nanoparticles, Chemical Physics Letters, 2011, vol. 502, issues 1–3, pp. 82-86. DOI: 10.1016/j.cplett.2010.12.020.
14. Van Dung M. Heating-rate and size-dependent melting, structural disorder, and diffusion in Au–Cu alloys: a molecular dynamics study, Physical Chemistry Chemical Physics, 2026, vol. 28, issue 11, pp. 6800-6810. DOI: 10.1039/D5CP04851F.
15. Liu H.B., Pal U., Perez R., Ascencio J.A. Structural transformation of Au–Pd bimetallic nanoclusters on thermal heating and cooling: a dynamic analysis, The Journal of Physical Chemistry B, 2006, vol. 110, issue 11, pp. 5191-5195. DOI: 10.1021/jp056060e.
16. Cuba-Supanta G., Amao P., Quispe-Huaynasi F. et al. The composition effect on the structural and thermodynamic properties of Cu–Ag–Au ternary nanoalloys: a study via molecular dynamics approach, Modelling and Simulation in Materials Science and Engineering, 2024, vol. 32, issue 4, art. no. 045003, 22 p. DOI: 10.1088/1361-651X/ad332f.
17. Yıldırım H., Garip A.K. Heating rate effects for the melting transition of Pt–Ag–Au nanoalloys, Chinese Physics B, 2021, vol. 30, issue 10, pp. 108201-1-108201-7. DOI: 10.1088/1674-1056/abee09.
18. Sdobnyakov N.Yu. [Modelirovanie strukturnykh prevrashchenij v odnokomponentnykh i mnogokomponentnykh metallicheskikh nanosistemakh: uchebnik] Simulation of structural transformations in single-component and multi-component metallic nanosystems: a textbook. Tver, Tver State University Publ., 2025, 408 p. DOI: 10.26456/sny.2025.408. (In Russian).
19. Sdobnyakov N.Yu., Kolosov A.Yu., Sokolov D.N., Savina K.G. MDSym. Certificate RF, no. 2025683621, 2025. (In Russian).
20. Cleri F., Rosato V. Tight binding potentials for transition metals and alloys, Physical Review B, 1993, vol. 48, issue 1, pp. 22-33. DOI: 10.1103/PhysRevB.48.22.
21. Paz Borbón L.O. Computational studies of transition metal nanoalloys. Doctoral Thesis accepted by University of Birmingham, United Kingdom. Berlin, Heidelberg, Springer-Verlag, 2011, 155 p. DOI: 10.1007/978-3-642-18012-5.
22. Leimkuhler B., Noorizadeh E., Theil F. A gentle stochastic thermostat for molecular dynamics, Journal of Statistical Physics, 2009, vol. 135, issue 2, pp. 261-277. DOI: 10.1007/s10955-009-9734-0.
23. Ackland G.J., Jones A.P. Applications of local crystal structure measures in experiment and simulation, Physical Review B, 2006, vol. 73, issue 5, pp. 054104-1-054104-7. DOI: 10.1103/PhysRevB.73.054104
24. Polak W.Z. Efficiency in identification of internal structure in simulated monoatomic clusters: comparison between common neighbor analysis and coordination polyhedron method, Computational Materials Science, 2022, vol. 201, art. no. 110882, 8 p. DOI: 10.1016/j.commatsci.2021.110882.
25. Larsen P.M., Schmidt S., Schiøtz J. Robust structural identification via polyhedral template matching, Modelling and Simulation in Materials Science and Engineering, 2016, vol. 24, no. 5, art. no. 055007, 18 p. DOI: 10.1088/0965-0393/24/5/055007.
26. Stukowski A. Visualization and analysis of atomistic simulation data with OVITO – the open visualization tool, Modelling and Simulation in Materials Science and Engineering, 2010, vol. 18, issue 1, pp. 015012-1-015012-7. DOI: 10.1088/0965-0393/18/1/015012.
27. Safaltin Ş., Gürmen S. Molecular dynamics simulation of size, temperature, heating and cooling rates on structural formation of Ag-Cu-Ni ternary nanoparticles (Ag34-Cu33-Ni33), Computational Materials Science, 2020, vol. 183, art. no. 109842, 12 p. DOI: 10.1016/j.commatsci.2020.109842.
28. Chen J., Fan X., Liu J. et al. Heating-rate and particle-size effects on melting process of Au nanoparticles, The Journal of Physical Chemistry C, 2020, vol. 124, issue 13, pp. 7414-7420. DOI: 10.1021/acs.jpcc.9b10769.
29. Talyzin I.V., Samsonov V.M., Bogdanov S.S. et al. Identifikatsiya slozhnykh nanostruktur yadro-obolochka po radialnym raspredeleniyam lokalnoj plotnosti komponentov [Identification of complex core-shell nanostructures from the radial distributions of the local density of components], Fiziko-khimicheskie aspekty izucheniya klasterov, nanostruktur i nanomaterialov [Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials], 2022, issue 14, pp. 307-320. DOI: 10.26456/pcascnn/2022.14.307. (In Russian).