Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


PhC-2026


Dispersion dependences of polarization switching parameters of copper-containing triglycine sulfate crystals

N.N. Bolshakova, I.K. Galkin, A.I. Ivanova, E.M. Semenova
Tver State University

Abstract: The paper presents results of an experimental study of the concentration and dispersion dependences of repolarization characteristics of copper-containing triglycine sulfate crystals. It is shown that with an increase in the impurity concentration in triglycine sulfate : Cu2+ crystals, the values of the relative and effective permittivities, switchable polarization, and unipolarity coefficient tend to increase, while the magnitudes of the coercive field, bias field, and dielectric loss tangent tend to decrease. The switching processes are significantly affected by the frequency of the alternating field, with an increase in which a transformation of the dielectric hysteresis loops is observed. As the frequency increases from 50 Hz to 2 kHz, the switchable polarization of the crystals decreases by an average of 2,5 times. At the same time, the frequency of the repolarizing field has a more significant effect on the repolarization processes of pure triglycine sulfate. A change in the repolarizing field frequency from 50 Hz to 2 kHz leads to a decrease in the dielectric viscosity coefficient of triglycine sulfate : Cu2+ crystals by an average of 3 times, which is caused by the switching off of the main switching mechanisms.
Keywords: dispersion dependences, triglycine sulfate, hysteresis properties, switchable polarization, permittivity, dielectric viscosity, domain structure

Change in properties of diffusion-hardening composite solder when modified with stainless steel powder

V.M. Skachkov, S.A. Bibanaeva, N.A. Sabirzyanov
The Institute of Solid State Chemistry of the Ural Branch of RAS

Abstract: The article discusses changes in the structure and microhardness of diffusion-hardening solder based on low-melting alloy gallium (68%) -indium (23,5%) -tin (8,5%) and a solid component from copper-tin alloy powder (5%) depending on the dosage of stainless steel powder. Stainless steel powder was added in an amount of 5, 10, 15, 20% by weight, solder samples were heat treated at temperatures of 125 and 600°C, and compared with a base solder composition of 30% by weight of gallium-indium-tin alloy and 70% by weight of copper-tin alloy powder. The X-ray phase analysis method determines the phases formed as a result of the interaction of solder components under different heat treatment modes. The method of differential thermal analysis revealed thermal effects in the formation of solid solutions and intermetallic compounds of gallium with transition metals in the temperature range of 17-600°C. It has been shown that thermal treatment at temperatures above 450°C promotes the transition of the solder to an equilibrium state, which leads to an increase in hardness, in particular, due to the uniform distribution of nanoscale inclusions. Scanning electron microscopy revealed that stainless steel has limited solubility in the composition of diffusion-hardening solder, but after high-temperature treatment (600°C) reduces its hardness due to violation of the composition of the gallium-copper solid solution.
Keywords: composite diffusion-hardening solders, metal powder, properties, microhardness, differential thermal analysis

Study of properties of selenium nanoparticles stabilized with K-17 polyvinyl pyrrolidone

Z.A. Rekhman, M.A. Pirogov, A.V. Blinov, A.V. Samovolov, A.Yu. Andiralov, Ya.A. Oblogin, A.V. Tatov
North Caucasus Federal University

Abstract: In this work, samples of selenium nanoparticles stabilized with polyvinylpyrrolidone K-17 were obtained by chemical reduction of selenious acid with ascorbic acid in an aqueous medium in the presence of a stabilizer. The samples were studied by Fourier transform infrared spectroscopy, dynamic and electrophoretic light scattering. Computational quantum-chemical modeling of the interaction between polyvinylpyrrolidone K-17 and a selenium atom was performed using the QChem software package. The modeling results showed that the interaction of polyvinylpyrrolidone K-17 with selenium via the ionized amino group is energetically favorable (a decrease the total energy of 2397,942 kcal/mol) and chemically stable (the chemical rigidity of the molecular system is 0,160 eV). Analysis of the infrared spectra showed a match between the main diagnostic absorption bands of polyvinylpyrrolidone (3400, 1660, and 1460 cm-1) before and after stabilization of the selenium nanoparticles, with no new absorption bands appearing, indicating that the chemical structure of the polymer is preserved during synthesis. A study of colloidal stability by dynamic and electrophoretic light scattering over a pH range of 3-11, temperatures of 25-95°C, and holding times of 5-25 min showed that the average hydrodynamic diameter of the particles ranged from 45,44 to 197,67 nm, and the ζ-potential ranged from -6,05 to -83,06 mV, with the system exhibiting the highest stability in an alkaline medium at 25°C and the lowest stability in an acidic medium and at elevated temperature (95°C).
Keywords: selenium nanoparticles, polyvinyl pyrrolidone, quantum chemical modeling, infrared spectroscopy, colloidal stability

Temperature dependence of the ellipsometric parameters of thin films of the AIST phase-change chalcogenide

A.A. Nevzorov1,2, V.A. Mikhalevsky1, A.A. Burtsev1, V.V. Ionin1, A.V. Kiselev1, N.N. Eliseev1, A.A. Lotin1,3
1 National Research Centre «Kurchatov Institute»
2 University of Science and Technology MISIS
3 Mendeleev University of Chemical Technology

Abstract: This work is devoted to the study of the temperature dependences of the refractive index (n) and extinction coefficient (k) of thin films of the phase-change chalcogenide AIST (Ag5In5Sb60Te30) in the spectral range of 380-1000 nm. Using spectroscopic ellipsometry, a direct comparison of optical properties of the amorphous and crystalline phases was performed during heating from room temperature to 170°C. It was found that heating the amorphous film to 100°C leads to a decrease in n by 3,2% and an increase in k by 2,55% at a wavelength of 780 nm, as well as a decrease in n by 5,0% and a decrease in k by 4,2% at a wavelength of 910 nm. The observed behavior indicates a notable instability of both the amorphous and crystalline phases of the investigated AIST material. The quantitative data obtained provide a necessary experimental basis for accurate thermal and optical modeling of phase-change memory devices operating in the near-infrared range. The effective application of this material requires optimization and control of synthesis methods, thin-film properties, and the precise kinetics of phase transformations. Nevertheless, AIST can be recommended for applications where high switching speed is a priority, rather than requirements for stability and multilevel state storage.
Keywords: chalcogenides, phase change materials, thin films, crystallization, optical properties

The effect of irradiation on the dynamic instability of dislocation slip in metals

V.V. Malashenko
Galkin Donetsk Institute for Physics and Engineering

Abstract: Within the framework of the theory of dynamic interaction of defects, the above-barrier motion of edge dislocations in an irradiated metal containing radiation point and nanoscale defects (prismatic dislocation loops) is analyzed. Intense external loads generate high strain rate deformation of irradiated metals. During high strain rate deformation, dislocations accelerate to high velocities, and their kinetic energy exceeds the height of potential barriers generated by structural defects. During above-barrier motion of dislocations, the energy of external loads is converted into the energy of dislocation oscillations. This dissipation mechanism differs significantly from the dissipation mechanism in the low-velocity region. The presence of a gap in the dislocation oscillation spectrum significantly affects the efficiency of this mechanism. This paper considers the case where the gap is generated by the collective interaction of radiation point defects. An analytical expression defining the rate dependence of the dynamic yield strength in irradiated metal is obtained. A new region of dynamic instability of dislocation motion was predicted, caused by a high concentration of prismatic dislocation loops. This dynamic instability is the cause of plastic deformation jumps. Some analytical expressions defining the boundaries of the dynamic instability region are obtained, and numerical estimates of the boundary values are performed.
Keywords: irradiated metals, dislocations, dislocation loops, radiation defects, high-speed deformation

Modeling the temperature dependence of the energy gap of a subnanocluster of titanium dioxide

G.P. Mikhailov1, Yu.G. Voronova2
1 Ufa University of Science and Technology
2 Ufa State Petroleum Technological University

Abstract: Using quantum-chemical modeling methods, the temperature dependence of the energy gap of the (TiO2)15 subnanocluster was studied in the range from 10 to 900 K. Within the framework of density functional theory (M06/6-31G(d,p) approximation), it was found that the (TiO2)15 subnanocluster has a quasi-spherical shape (C2h symmetry, diameter of 0,9 nm), and its inner core exhibits the atomic order of rutile. Thermostable structures (TiO2)15 were obtained by the non-empirical molecular dynamics method using the Atom-Centered Density Matrix Propagation scheme. For each temperature, the energy gap Egap between the lowest vacant and highest occupied molecular orbitals was calculated using the M06/6-31G(d,p) approximation. The obtained data were analyzed using the Eg(T) model dependencies developed for crystalline solids. The qualitative similarity of the temperature dependencies of Eg(T) for the (TiO2)15 cluster and bulk semiconductors has been established, namely, a non-linear monotonic decrease of the Eg with increasing temperature. As the temperature increases, significant anharmonicity of the (TiO2)15 cluster vibrations is observed, and the temperature sensitivity of the O 2p (highest occupied molecular orbital) and Ti 3d (lowest unoccupied molecular orbital) molecular orbitals is different, with the titanium orbitals showing a weak dependence. The most adequate and physically interpretable results are obtained using the O’Donnell-Chen model, which takes into account the quantum nature of the subnanocluster vibrations and allows us to determine the average energy of the vibrational modes that determine the temperature dependence of the energy gap.
Keywords: nanocluster, titanium dioxide, density functional theory, energy gap

Sorption analysis and photocatalytic activity of graphitic carbon nitride powder

C.D. Bui1, Z.V. Shomakhov2, S.S. Nalimova1, E.V. Maraeva1, A.A. Naimark1, E.S. Popov1, A.I. Maximov1, V.A. Moshnikov1
1 Saint Petersburg Electrotechnical University «LETI»
2 Kabardino-Balkarian State University named after H.M. Berbekov

Abstract: Graphitic carbon nitride (g‒C3N4) is considered a promising metal-free photocatalyst for the efficient degradation of stable organic dyes in wastewater, however, the relationship between its structural-dispersive characteristics and photocatalytic activity remains insufficiently studied. In this work, a comprehensive characterization was performed on g‒C3N4 powder synthesized via thermal polycondensation of urea at 550°C, followed by treatment with hydrochloric acid and ultrasonic exfoliation. The specific surface area, determined by the Brunauer-Emmett-Teller method, was 52 m2/g. Based on experimental sorption data, geometric parameters of the particles were evaluated within the framework of the nanosheet model. It is shown that the nanosheet thickness depends only weakly on the aspect ratio and is 17 nm, which corresponds to approximately 50 atomic layers under partial exfoliation of blocks. The photocatalytic activity of the material was investigated during the degradation of Rhodamine 6G dye under ultraviolet irradiation (395 nm). The degradation process obeys pseudo-first-order kinetics. As the catalyst loading is increased from 12 to 26 mg, the degradation degree of the dye over 120 minutes rises from 23,2% to 67,9%, and the rate constant increases from 2,1·10-3 to 9,3·10-3 min-1 due to the growth in the number of available active sites.
Keywords: graphitic carbon nitride, Brunauer-Emmett-Teller method, specific surface area, nanosheets, photocatalytic degradation of rhodamine 6G

Investigation of magnetic properties of cobalt nanofilms and their potential for spintronic device applications

A.Yu. Fedotov, O.Yu. Severyukhina, A.Yu. Salomatina
Udmurt Federal Research Center of the Ural Branch of the RAS

Abstract: In this study, performed using a hybrid method of molecular dynamics and spin modeling within the LAMMPS software package with the SPIN module, the influence of the thickness of crystalline cobalt films on their magnetic properties was investigated. The thickness varied from 1,8 to 7,1 nm. It is shown that the film thickness significantly affects its magnetic behavior due to the interplay between surface and bulk effects. In ultrathin films (less than 4,5 nm in thickness), inhomogeneity of the magnetic response is observed. This is attributed to the dominance of the surface effects and atomic-scale roughness, which creates local demagnetizing fields. As a result, domain walls behave chaotically, leading to some stepwise changes in the magnetization and inhomogeneity of its distribution. The normalized magnetic energy is the highest in such films. At thicknesses of 4,5-7,1 nm, the films exhibit the bulk magnetic behavior. Reducing the proportion of surface atoms allows the bulk properties of cobalt to dominate. The magnetization becomes more stable, and its distribution becomes uniform. The magnetic energy, normalized to the number of atoms, approaches a value characteristic of bulk cobalt. A direct proportionality was observed between this energy and the proportion of the surface atoms, clearly indicating the decisive contribution of the surface to the formation of increased energy and spatial heterogeneity of magnetic properties at the nanoscale. The obtained data can be used in the creation of spintronic elements and magnetic recording devices.
Keywords: mathematical modeling, thin films, cobalt, molecular dynamics, spin dynamics, ferromagnet, magnetic properties

Temperature-catalytic control over the formation of a layered sp/sp2-carbon nanomaterial under palladium-free Sonogashira cross-coupling conditions

D.S. Ryashentsev, D.S. Polyakov, N.V. Chernikov
Chelyabinsk State University

Abstract: The possibility of replacing the palladium catalyst with 3d metals (iron, cobalt, nickel, and copper) in the synthesis of a layered sp/sp2-carbon nanomaterial via the Sonogashira cross-coupling reaction has been investigated. Acetates of the corresponding metals were used as precatalysts, o-phenanthroline served as the ligand, and copper iodide as the cocatalyst. The synthesis was carried out in dimethyl sulfoxide at 100℃ and 140℃ for 24 hours under an argon atmosphere using hexaiodobenzene and calcium carbide as sources of aromatic and acetylenic fragments. The products were subjected to multi-stage purification, including sequential washing with solutions of ammonium chloride, nitric acid, and sodium thiosulfate, followed by thermal treatment at 200℃. Using X-ray diffraction, infrared and Raman spectroscopy, it was established that the synthesis temperature and the nature of the transition metal jointly determine the structural characteristics and the degree of defectiveness of the final material. Raman spectroscopy confirmed the presence of acetylenic bridges between benzene rings. The ratio of the D– and G–band intensities varies from 0,17 to 0,31, indicating a tunable defectiveness of the sp2 matrix, while the IY/IG intensity ratios vary from 0,06 to 0,13. The obtained results demonstrate the fundamental possibility of temperature-catalytic control over the structure of graphyne-like materials without the use of a palladium catalyst.
Keywords: γ-graphyne, Sonogashira reaction, palladium-free catalysis, transition metals, layered nanostructures

Dependence of sintering parameters for nanosized complex oxide powders on intensity of charge generation during synthesis from nitrate-organic precursors

A.A. Ostroushko, A.E. Permyakova, T.Yu. Zhulanova
Ural Federal University named after the first President of Russia B.N. Yeltsin

Abstract: Parameters of the sintering process for compacted complex oxide powders based on lanthanum strontium manganite with a perovskite-type structure were studied: the temperature of intensive sintering and the achieved shrinkage of the workpiece. The studied complex oxide samples were obtained in the combustion reactions of nitrate-organic precursors (the so-called solution combustion method). During the synthesis, the composition of the precursors was varied: the nature of the organic component (polyvinyl alcohol, polyvinylpyrrolidone, glycine) and its relative content in relation to the stoichiometry of the combustion reaction with the formation of water vapor, molecular nitrogen and carbon dioxide as gaseous products. At the same time, positive or negative electric charges were generated in the precursors due to the formation and carry-over with the released gases of ionized molecular groups. The intensity of this process was monitored using an electrostatic field meter. The ground-precursor potential difference, depending on the composition of the initial composition, ranged from values close to zero to several tens of volts. With intensive generation due to the accumulation of the excess surface energy of mutually repulsive nanoparticles of the complex oxide, the temperature of intensive sintering decreased by 350 degrees compared to that (1050°C) for materials obtained from precursors with a low intensity of charge formation. The relative shrinkage of samples of the first type increased from 3 to 23%. The established correlation was universal and practically independent of the sign of the generated charge.
Keywords: nanosized powders, synthesis of nitrate-organic precursors in combustion reactions, charge generation, sintering, complex oxides, lanthanum-strontium manganite