Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


PhC-2026


Phase and structural evolution of red muds during chemical looping reforming of methane

I.V. Shamsutov, L.A. Pasechnik, O.V. Merkulov
Institute of Solid State Chemistry of the Ural Branch of RAS

Abstract: The accumulation of red mud – a large‑tonnage waste from alumina production – poses a serious environmental challenge: with an annual waste output exceeding 150 million tons, the global utilisation rate remains below 5%. At the same time, the polymetallic oxide composition of red muds (Fe2O3 up to 45–49 %, Al2O3, SiO2, CaO, TiO2, Na2O) provides opportunities for their use as oxygen carriers in chemical reforming of methane, thereby combining waste utilization with syngas production. Two types of materials were investigated: the original red mud from the Bogoslovsk Aluminum Smelter and a magnetite‑enriched mud with reduced aluminum content, obtained by hydrothermal leaching of the original red mud. Granules (3-5 mm) prepared by sintering at 1050°C were tested in cyclic «methane reduction – air oxidation» runs at 900°C in a fixed‑bed reactor; the evolution of phase composition and microstructure was monitored. It is established that, during cycling, iron oxides are reduced to metallic Fe, while aluminosilicate phases (gehlenite Ca2Al2SiO7, CaFeAlSiO6) acted as structural stabilisers, preventing particle sintering. For red mud, a steady‑state regime with CH4 conversion of ~75% and CO selectivity of ~85-90% is reached after 6-7 cycles; for magnetite‑enriched mud this occurs after 10 cycles, which is attributed to larger aggregates of iron oxides and their sintering, as well as to the formation of a layered porous structure. At the same time, magnetite‑enriched mud exhibits a slightly higher overall oxygen capacity. In both cases, the H2/CO ratio in the products remains at 1,75-1,80. It is shown that the key factor for long‑term stability is the balance between the content of the active component (iron oxides) and the amount of aluminosilicate stabilizers. The obtained results open up prospects for the targeted modification of red mud composition to create efficient and durable oxygen carriers for cyclic hydrocarbon processing.
Keywords: bauxite residue of red mud, oxygen carriers, methane reforming, chemical looping, synthesis gas, magnetite, hematite, cyclic stability, structural evolution

Ferromagnetic nanoclusters in austenite: nature, role, characteristics, and controllability

V.N. Pustovoit, Yu.V. Dolgachev
Don State Technical University

Abstract: This article examines the nature of magnetic inhomogeneities in austenite steels and their fundamental role in phase transformations. It is shown that austenite, being a paramagnetic phase, contains spontaneously emerging regions of short-range ferromagnetic order (ferromagnetic nanoclusters), the existence of which has been confirmed experimentally using neutron magnetic diffraction methods. The dependence of the magnetic susceptibility of austenite is described by the Langevin function for superparamagnets, which reflects the fluctuation nature of these magnetic inhomogeneities localized in nanometer-sized regions. The magnetic state of the initial phase crucially determines the nature of the γ→α transformation. Using computer simulation based on the Ising model, the effect of an external magnetic field on the characteristics of nanoclusters over a wide temperature range was studied. It has been established that a magnetic field of up to 2,4 MA/m can increase the average cluster size, their total number by two orders of magnitude (most effectively at low temperatures, where the increase reaches 1,4 nm), and increase the proportion of large clusters, as well as extend their stable existence by up to 25%. Experiments with quenching in a constant magnetic field for a range of steels demonstrated a significant reduction in the volume fraction of retained austenite, comparable to cold treatment, and an acceleration of the bainitic transformation kinetics by 1,5-1,8 times. The magnetic field enhances the magnetic heterogeneity of austenite, activates new nucleation centers, and stimulates the multiplicative mechanism of α-phase formation, providing a practical tool for targeted phase transition control during heat treatment of steels in a magnetic field.
Keywords: austenite, magnetic state, nanocluster, steel, hardening, external magnetic field

Modeling the thermal effect on the surface energy and electron work function of a monocrystal thallium

I.G. Shebzukhova1, L.P. Aref`eva2
1 Kabardino-Balkarian State University named after H.M. Berbekov
2 Don State Technical University

Abstract: The aim of this work was to carry out numerical modeling of thermal influence on energy and force characteristics of monocrystal thallium. The surface energies and work function of faces of thallium crystals are calculated using the electron-statistical method taking into account quantum corrections. The influence of polymorphic transformations and temperature on anisotropy of these properties is analyzed. The cohesive energy of α- and β- thallium has also been estimated based on the values of surface and interfacial energies, which include the average configuration energy and the energy of chemical interaction between two parts of the metal, and the temperature dependence of the chemical interaction energy has been investigated. The contact potential difference for pairs of close-packed faces has been calculated. Computer simulations of the mechanical properties have been performed using the Griffiths model, and the tensile strength of thallium has been obtained, which allows for the prediction of the material’s service life.
Keywords: surface energy, electron work function, anisotropy, polymorphic modifications of thallium, cohesive energy, crack resistance

Coalescence and sintering in a ternary nanosystem Pt+Cu+Pd: molecular dynamics simulation

V.V. Puytov, V.M. Samsonov, S.A. Vasilyev
Tver State University

Abstract: Using the LAMMPS soft-ware and the embedded atom method, molecular dynamics simulation has been performed of sintering and coalescence in a system of three monometallic nanoparticles (Pd1700 + Cu5100 + Pt1700), whose centers of mass were located on the same straight line. The process was carried out during uniform heating of the system up to a temperature of 2300 K, corresponding to the daughter nanodroplet, and subsequent cooling (quenching) it to the initial temperature of 300 K. We found that as a result of low-temperature sintering (heating to 500-900 K), a ternary analogue of the Janus structure was formed. Solidification of the nanodroplet resulted in the ternary nanocrystal formation. Temperature dependences of radial distributions of atomic fractions of the components were found and analyzed. It was established that during both sintering solid nanoparticles and cooling (quenching) nanodroplets, Pd atoms migrate to the outer atomic monolayer, whereas in solidified nanodroplets, Pt atoms have segregated toward the second monolayer and the center of the nanoparticle. In addition to chemical segregation, i.e., the spatial separation of components, structural segregation was observed in the solidified nanodroplets. This segregation yields grains in the form of bands with a defective fcc structure, separated from each other by boundaries represented by atoms identified by the Ovito program as a local hcp structure.
Keywords: LAMMPS, molecular dynamics, embedded atom potential, sintering, coalescence, surface segregation

Phase-structural design of TiSiBN nanocomposite coating synthesized by vacuum-arc plasma-assisted method

Y.F. Ivanov1, A.A. Klopotov2, N.A. Prokopenko1, E.A. Petrikova1
1 Institute of High Current Electronics of the Siberian Branch of RAS
2 Tomsk State University of Architecture and Building

Abstract: The paper considers the phase and structural conditions of the formation of a nanostructured TiSiBN coating synthesized by the vacuum-arc plasma-assisted method on a 321 steel substrate. It is shown that analysis of the ternary systems Ti-Si-N, Ti-B-N and Ti-Si-B allows one to predict in advance the limited solubility of the components and the predominant formation of some individual nitride phases. Based on the size factor, Pauling electronegativity and valence of the elements, it was established that nitrogen and boron have a significant size mismatch with titanium, which prevents the formation of extended substitutional solid solutions and enhances the tendency to form TiN- and BN-containing phases. Experimental data obtained by electron microscopy confirm the formation of a multilayer coating without a pronounced columnar structure. The main volume of the coating is represented by TiN and BN nanocrystallites 2,5-3,5 nm in size, and a transition layer up to 100 nm thick is revealed between the coating and the substrate. The average coating hardness is 32 GPa, with a range of 21-49 GPa. A physical interpretation of the hardening is proposed, based on a modified Hall-Petch dependence, suppression of dislocation nucleation in nanocrystallites, and consideration of the contribution of interphase and intraphase boundaries.
Keywords: film/substrate system, vacuum-arc plasma-assisted method, phase composition, defect substructure, phase diagram

The study of the interaction of L-cysteine methyl ether with silver salts

E.S. Burlakov1, D.V. Vishnevetskii1, E.E. Polyakova1, D.V. Averkin2, A.A. Efimov3, M.Yu. Aleshina3
1 Tver State University
2 All-Russian Scientific Research Institute of Physical-Technical and Radiotechnical Measurements
3 Moscow Institute of Physics and Technology

Abstract: In this work, the effect of silver salts on the self-assembly process in aqueous solutions of L-cysteine methyl ester hydrochloride was studied using UV–visible spectroscopy, dynamic light scattering, electrophoretic light scattering, pH measurements, transmission electron microscopy, and selected-area electron diffraction. The nitrate- and acetate-based systems remained visually stable after storage in the dark for 2 months, whereas the nitrite-based systems began to precipitate after several days. The UV-visible spectra showed no characteristic absorption bands and no pronounced scattering region, indicating the stability and homogeneity of the samples. According to the zeta-potential values, the solutions with L-cysteine methyl ester hydrochloride:silver salt ratios of 1:1,5 and 1:1,75 were the most stable in both systems. The dynamic light scattering results showed that only a small number of nanoparticles formed under conditions of silver ion deficiency, whereas an excess of silver ions produced sufficient scattering intensity for reliable particle-size determination. The pH measurements revealed different trends for the acetate- and nitrate-based systems. transmission electron microscopy and selected-area electron diffraction data showed that the obtained systems form predominantly amorphous, polydisperse, spherical nanoparticles ranging from 5 to 60 nm in size, with some particles reaching approximately 200 nm.
Keywords: L-cysteine methyl ester, silver nitrate, silver nitrite, silver acetate, self-assembly, nanostructured systems

Hybrid materials based on d-element hexacyanoferrates modified with nanosized gold

I.M. Shevchenko1, M.A. Yasnaya2, A.A. Blinova1, A.V. Prasolova1, A.D. Goncharov1, T.N. Glizhova1
1 North Caucasus Federal University
2 Branch of JSC NPO «Mikrogen» in Stavropol «Allergen»

Abstract: For the first time, we present the results of a study on the influence of the composition and ratio of components in the synthesis process of hybrid materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), modified with gold nanoparticles, on the elemental and phase composition of these hybrid materials and on the microstructure of their surface. According to the results of investigations using scanning electron microscopy and energy dispersive X-ray microscopy, it was found that gold was identified in samples of hexacyanoferrates (III) of d-elements (Co, Ni, Fe) containing from 0,1 to 5,0 masses.% gold. Analysis of the phase composition of samples of hexacyanoferrates of d‑elements (Co, Ni, Fe) modified with gold showed that the main crystalline phases were the corresponding hexacyanoferrates of d‑elements with a face‑centered cubic crystal lattice (Fm3m); impurity phases of mixed hexacyanoferrates were also present. According to the results of X‑ray phase analysis, the phases of metallic gold cannot be identified. The obtained experimental data will be useful for the development and use of promising materials based on hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron) as sensitive elements in glucose sensors. Additional modification of the matrix of hexacyanoferrates (III) of d‑elements (cobalt, nickel, iron), for example, with nanoparticles of noble metals, helps to increase the conductivity, selectivity, and stability of composite materials when creating sensors for assessing blood glucose levels.
Keywords: hybrid nanomaterials, hexacyanoferrates of d‑elements, gold nanoparticles, elemental composition, phase composition, surface microstructure

Imprint effect in spherulitic lead zirconate titanate thin films

S.V. Senkevich1,2, V.P. Pronin2, I.V. Ryzhov2, M.V. Staritsyn3, A.R. Dunkabash4, E.Yu. Kaptelov1, I.P. Pronin1
1 Ioffe Institute
2 The Herzen State Pedagogical University of Russia
3 NRC Kurchatov Institute, CRISM Prometey
4 Saint Petersburg State University of Industrial Technologies and Design

Abstract: We investigated the microstructure and imprint (internal field) of spherulitic lead zirconate titanate thin films formed via a two-stage radio frequency magnetron sputtering process on Pt/TiO2/SiO2/Si substrates at various perovskite phase crystallization temperatures (Tann = 580–650°C). The films were subjected to a thermal treatment and application of a strong external field, and prolonged aging. Microstructural analysis using scanning electron microscopy revealed that increasing Tann led to a sharp increase (by a factor of 5-10) in the crystal lattice rotation rate; this effect is attributed to the recrystallization of the perovskite phase, accompanied by an increase in its density. It was found that the magnitude and orientation of the internal field in the films, determined from dielectric hysteresis loops, depended on the «phase» state of the films. Long-term aging (~ 108 s) had little effect on the internal field in the loose phase. In the dense phase, aging led to a significant change in the magnitude and direction of the internal field vector. The observed changes are attributed to strong bending deformation of the crystal lattice and the resulting directed diffusion of charged oxygen vacancies toward the upper film interface. The study discusses the role of the electronic subsystem and charged oxygen vacancies in the formation of the imprint (internal field) and in charge redistribution across the film thickness under the influence of external factors and the passage of time.
Keywords: radio frequency magnetron sputtering, lead zirconate titanate thin films, spherulitic microstructure, oxygen vacancies, Gorsky effect

Model of the diffusion process in a nanostructured system as a generator of pseudorandom sequences

A.V. Shishulin, A.V. Shishulina
Nizhny Novgorod State Technical University n.a. R.E. Alekseev

Abstract: Complex random number generators that combine rapid pseudorandom sequence generation with hardware entropy sources have numerous practical applications in stochastic process modeling, machine learning, and information security. This paper presents a method for generating pseudorandom sequences based on a physical model of particle diffusion within a nanoscale periodic structure featuring a nonlinear potential and thermal noise, which serve as sources of dynamic chaos. The sequence of thermally activated transitions between potential minima exhibits irregular and chaotic behavior. The sequence generation is achieved through the digitalization of the particle’s stochastic motion along the energy landscape of the nanostructure. Particle diffusion in a nanostructured medium is described by the Langevin equation and is integrating by using the Verlet method. Additionally, a software implementation of the suggested algorithm is provided in the Ruby programming language. The obtained results demonstrate the potential for using a «pseudophysical» approach, which is based on nonlinear potentials of various physical natures, as a viable alternative to a «purely mathematical» methodology in the tasks involving the generation of random number sets.
Keywords: nanostructures, diffusion, nonlinear potential, dynamic chaos, pseudorandom numbers

Atomistic simulation of segregation in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations

K.G. Savina, S.V. Serov, A.Yu. Kolosov, D.N. Sokolov, D.A. Kravchenko, R.E. Grigoryev, S.S. Bogdanov, E.E. Arakcheev, N.Yu. Sdobnyakov
Tver State University

Abstract: In this work, the molecular dynamics method was used to study modeling quaternary Ni-Cu-Fe-Co nanoparticles (containing 4000 atoms) with different initial configurations: a particle with a mixed three-component core and a nickel shell, a four-shell structure with concentric shells, a nanoalloy with a uniform distribution of components, a four-layer planar structure, two symmetrical variants with seven layers of atoms. The interatomic interaction was described by the tight-binding potential. The molecular dynamics experiment was carried out according to the following scheme: 1) heating from 300 to 1800 K, and then cooling to 300 K with relaxation at each step of 10 ps, 2) relaxation for 100 ps at temperature 300 K. For the first stage, two rates of thermally induced action were selected. The temperature ranges of hysteresis of the melting and crystallization processes were determined. Segregation patterns in quaternary Ni-Cu-Fe-Co nanoparticles with different initial configurations are described using radial density distributions. The temperature parameters of the hysteresis associated with melting and crystallization processes have been evaluated. The obtained results demonstrate the variability of the properties of multicomponent nanoparticles, determined by both the initial conditions (morphology, composition, size) and the conditions of the molecular dynamics experiment (rate of thermally induced action).
Keywords: molecular dynamics, MDSym, tight-binding potential, quaternary nanoparticles, segregation, nickel, copper, cobalt, iron, local density