PhC-2026
Can the presence of a cavity alter the nature of structural transformations during a cycle of thermally induced treatment, taking Ag-Ni-Pd ternary nanoparticles as an example?
E.S. Mitinev, K.G. Savina, O.V. Polev, M.G. Gostintsev, A.Yu. Kolosov, D.N. Sokolov, I.A. Vzglyadov, I.S. Dmitriev, P.M. Ershov, N.Yu. Sdobnyakov
Tver State University
Keywords: molecular dynamics method, MDSym, tight-binding potential, ternary nanoparticles, cavity, phase transition, segregation, local structure
Creation of mesoscale models of aged polymer nanoparticles using the Rosenbluth algorithm
I.K. Patrenkov1, M.D. Malyshev1,2, P.V. Komarov1,2
1 Tver State University
2 Yaroslav-the-Wise Novgorod State University
Keywords: Rosenbluth algorithm, coarse-grained modeling, polymers, degradation, nanoparticles
Synthesis and physicochemical study of pectin-stabilized selenium nanoparticles
A.B. Golik, N.A. Rusev, A.V. Blinov, Y.A. Oblogin, A.V. Tatov, A.M. Serov, M.A. Pirogov
North-Caucasian Federal University
Keywords: pectin-stabilized selenium nanoparticles, optimization of the synthesis method, stability at different pH levels, average hydrodynamic diameter, ζ potential
Changes in the mass composition of alkali metal clusters caused by the geometry of the field source surface changes
D.P. Bernatskii, V.G. Pavlov
Ioffe Institute
Keywords: field desorption, cesium, potassium, sodium, tungsten, rhenium, electric field, ion clusters
Influence of synthesis method on functional characteristics of materials based on ultradispersed hydroxyapatite
N.A. Sabirzyanov1, E.A. Bogdanova2, V.M. Skachkov1, S.A. Bibanaeva1, I.S. Medyankina1
1 Institute of Solid State Chemistry of the Ural Branch of RAS
2 JSC «Giredmet»
Keywords: biomaterials, hydroxyapatite, synthesis, autoclave, precipitation from solution, functional properties, strength characteristics
Dielectric properties of Pt/0,91NaNbO3-0,09SrZrO3/SrRuO3/MgO(001) antiferroelectric thin films
D.S. Pavlenko1, A.L. Bulanova1, A.V. Pavlenko1,2
1 Southern Federal University
2 Southern Scientific Center of the RAS
Keywords: antiferroelectric, dielectric properties, thin films, polarization, high-frequency magnetron sputtering method
Equation of polymolecular adsorption on a flat homogeneous surface of an adsorbent for a finite number of layers
A.V. Tvardovskiy
Tver State Medical University
Keywords: adsorption, adsorbent, absorption, thermodynamics of phase equilibria, Henry equation, Langmuir equation, Brunauer – Emmett – Teller equation, equation of polymolecular adsorption, flat homogeneous surface
Features of structural transformations in four-component Cu-Au-Pt-Pd nanoalloys: multi-shell structure and alloy with uniform distribution of components
S.V. Serov, K.G. Savina, A.Yu. Kolosov, D.N. Sokolov, S.A. Veresov, D.R. Zorin, A.V. Zaytsev, N.N. Simchuk, N.Yu. Sdobnyakov
Tver State University
Keywords: quaternary Cu-Au-Pt-Pd nanoparticles, multi-shell structure, alloy with uniform distribution of components, molecular dynamics method, tight-binding potential, segregation
Study of the parameters of carbon nanostructures synthesis in microwave co-pyrolysis of polystyrene and microcrystalline cellulose
A.N. Zaritovskii1, E.N. Kotenko1, S.V. Grishchuk1, V.A. Glazunova2,1, G.K. Volkova2,1
1 L.M. Litvinenko Institute of Physical Organic and Coal Chemistry
2 Galkin Donetsk Institute for Physics and Engineering
Keywords: microwave pyrolysis, carbon nanostructures, polystyrene, microcrystalline cellulose, nickel and iron oxalates, activated carbon
Quantum-chemical calculation of the zinc(II) glycine complex: synthesis, structure, properties, determination of stability constants
D.V. Bespalov, O.A. Golovanova
Omsk State University named after F.M. Dostoevsky
Keywords: synthesis, amino acids, zinc complexes, glycine, density functional method, molecular simulation