Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. Founded at 2009


PhC-2026


Influence of the nature of the organo-ligand complex of transition metals and thermochemical activation on the effectiveness of metal oxide catalysts for carbon nanotube growth in the CVD process

A.P. Prudchenko, O.Yu. Poliakova, J.S. Protasevich
L.M. Litvinenko Institute of Physical Organic and Coal Chemistry

Abstract: This paper presents the results of a study of the effect of the nature of organic ligands, the composition of organo-ligand complexes of 3d-metals, and the conditions of their thermal degradation in the synthesis of metal oxide catalysts for the growth of carbon nanotubes on their effectiveness of the processes of catalytic chemical deposition of carbon from the gas phase. Metal oxide catalysts were synthesized using a technique combining the approaches of polymerized complex precursors, the chelation method of sol-gel technology, as well as thermal decomposition and thermochemical activation of the carrier. It has been established that the effectiveness of catalysts of the general composition Me2CO/CaCO3 (Me–Fe, Ni) in the CCVD synthesis of carbon nanotubes depends both on the nature of organic ligands of transition metal complexes and on the composition of active metals. The effect of the structure of the ligands used in the synthesis of metal oxide catalysts for both the Fe–Co and Ni–Co combinations is similar and consists in increasing the effectiveness in the following sequence: glycols < polyglycols < polyalcohols < carbohydrates (mono- and disaccharides) < branched polyalcohols (pentaerythritol). Replacing Fe with Ni in the organo-ligand complex can significantly reduce the optimal process temperature from 800°С to 500°С, as well as increase the specific yield of the carbon product. Based on the results of the analysis of temperature dependences using the example of catalysts where the ligands were sucrose, fructose, pentaerythritol and citric acid, it was assumed that the decrease in productivity observed with increasing temperature may be due to an increase in the mobility of catalytic particles, their agglomeration, sintering and, as a result, loss of activity. It has been established that, in case of significant excess, organic ligands can play the role of additional fuel in the process of thermochemical activation of the carrier, affecting its morphology, composition, surface texture, and energy efficiency.
Keywords: carbon nanotubes, metal oxide catalysts, organic ligands, chelates, CVD synthesis, carbon nanomaterials

Thermal phenomena induced by pulsed current in titanium during tensile deformation

A.A. Misochenko, O.E. Korolkov
Mechanical Engineering Research Institute of RAS

Abstract: The study analyzes the thermal effect of pulsed current during tensile testing in Grade 2 and Grade 4 titanium in coarse‑grained and ultrafine‑grained states. The work demonstrates the determining role of the current duty cycle in the manifestation of electroplastic and thermal effects. It is shown that in the single‑pulse mode (duty cycle 5000-10000), there is a correspondence between the onset of the temperature peak and the yield stress jump. In the multi‑pulse current mode (duty cycle 10), the maximum temperatures increase linearly with increasing current density above 40 A/mm2 and can reach approximately 170°C at a current density of 100 A/mm2. When the duty cycle is below 5000, thermal effects become the dominant mechanisms. The results of comparing the electroplastic effect manifestation in coarse‑grained and ultrafine‑grained Grade 4 titanium are presented, demonstrating the structural sensitivity of the effect to grain size. A comparison was made of the reduction in the flow stress under the influence of current versus heating by an external source, demonstrating the presence of other contributions to the electroplastic effect besides the thermal one. At the same time, the thermal contribution of the current to the reduction of the flow stress in ultrafine‑grained titanium is smaller than in coarse‑grained titanium.
Keywords: electroplastic effect, tension, pulsed current, titanium, thermal effect of pulsed current

Problems and strategies of epitaxial growth of III-V-Bi semiconductor thin films: a review

O.V. Devitsky1,2
1 Federal Research Center Southern Scientific Center of the RAS
2 North Caucasus Federal University

Abstract: This review article systematically summarizes fundamental and applied research concerning the epitaxy of metastable III-V–Bi solid solutions. The main challenge in obtaining thin films of III-V–Bi is their thermodynamic instability, which results from a wide miscibility gap and extremely low equilibrium solubility of bismuth in III-V compounds. It is demonstrated that overcoming these limitations is only possible through kinetic stabilization methods. Key strategies to enhance bismuth incorporation are identified, including lowering the substrate temperature to 200-350°C, manipulating surface stoichiometry by shifting to gallium-rich regimes, and employing surface reconstructions such as the 2×1 pattern. Additional approaches involve engineering tensile strain to increase bismuth solubility by up to 100 times and using high-index substrates like (115)A and (311)B, along with congruent transfer techniques. The paper also thoroughly discusses strategies for improving structural quality, such as suppressing bismuth droplet formation, implementing two-temperature growth procedures, and performing in-situ and post-growth annealing. A comparative analysis of molecular beam epitaxy, metal-organic vapor phase epitaxy, and pulsed laser deposition methods is presented within the context of producing high-quality III-V–Bi thin films. The review concludes that further progress in developing devices based on III-V–Bi requires shifting from empirical process optimization to precise control of surface kinetics and atomic-level defect management.
Keywords: GaAsBi, thin films, III-V-Bi, molecular beam epitaxy, metal-organic vapor phase epitaxy, pulsed laser deposition

On the problem of observing contact melting in a molecular dynamics experiment in Ni-Al bimetallic nanolayer

N.B. Kuz'min, P.V. Komarov, V.M. Samsonov, N.Yu. Sdobnyakov
Tver State University

Abstract: Using a bimetallic Ni-Al nanolayer as an example, molecular dynamics simulations of contact melting during annealing at 900 K were performed. The open-source LAMMPS software and the embedded-atom potential were used for this purpose. Interest in the chosen research object is due to the complexity of the phase diagram, while the temperature for the molecular dynamics experiment (900 K) was determined by considering the contact melting temperature for the macroscopic Ni-Al system and the potential size effect. Furthermore, this temperature is lower than the melting point of the lower-melting element, i.e. aluminum. During annealing for up to 100 ns, several characteristic temperatures were identified, corresponding to different stages of the diffusion process in the bimetallic Ni-Al nanolayer. The evolution of the local structure was observed using the open-source Ovito software with a modifier corresponding to the Ackland-Jones method. This approach analyzes the geometry of the angles between the bond vectors of a selected atom with its nearest neighbors. Over the selected time interval (100 ns), interface movement was identified in the Ni-Al system, but the crystalline transition layer «prevents» further «activation» of contact melting. This effect is observed for the first time for contact melting in nanoscale metallic systems.
Keywords: contact melting, bimetallic Ni-Al nanolayer, LAMMPS, molecular dynamics simulation, embedded-atom potential, local structure, Ackland-Jones method

Magnetic nanofluids in tribology: achievements, challenges, and future research directions

A.N. Bolotov, O.O. Novikova
Tver State Technical University

Abstract: This article presents a systematic review of current research on magnetic lubricating nanofluids (ferrofluids) as a class of intelligent tribological media whose properties are controlled by an external magnetic field. The aim of the work is to summarize and critically analyze scientific concepts regarding the colloidal structure, synthesis methods, tribological characteristics, and engineering applications of such fluids. The classification of magnetic lubricants, the historical evolution of approaches (including studies from 1988–1991 that established the magnetotribological effect and the role of structural components), and current trends are discussed. The mechanisms of colloidal stabilization, the influence of Fe3O4 nanoparticle size and concentration, the magnetoviscous effect, and field-induced structure formation are analyzed in detail. It is shown that an optimal particle concentration (approximately 5 wt.%) reduces wear by up to 90%, while exceeding this concentration leads to abrasive wear. Four main mechanisms for reducing friction and wear are identified: rolling bearing, tribochemical film formation, self-healing of microcracks, and magnetic removal of wear debris. It was established that the effectiveness of a magnetic field depends significantly on its orientation and gradient, as well as the material of the friction pair. The main areas of application (magnetic seals, bearings, controlled tribosystems, heat transfer), limitations (aggregate instability, particle abrasion, scaling), and development prospects, including active feedback systems and hybrid compositions, are discussed. It is concluded that the main value of magnetic lubricating nanofluids lies in their ability not only to simply lubricate but also to control lubrication, opening up new operating principles for friction units in precision, vacuum, and microengineering.
Keywords: magnetic lubricating nanofluids, ferrofluids, tribology, Fe3O4 nanoparticles, magnetically viscous effect, boundary lubrication, wear, magnetic field, smart lubricants

Synthesis and thermal stability of high-entropy oxide (CuZnNiCoFeCrAl)xOy nanoparticles obtained by joint exploding wires

A.V. Pervikov, A.I. Sagun, E.E. Ryumin, K.V. Suliz, M.I. Lerner
National Research Tomsk State University

Abstract: For the first time, a high-entropy oxide nanoparticle-based powder was synthesized via a single-step method based on the co-electrical explosion of various metal/alloy wires in an oxygen-containing atmosphere. The particle size distribution and crystal structure were characterized using transmission electron microscopy and X-ray diffraction analysis. It was shown that particle sizes varied from 10 nm to 3 μm. The particles exhibited a spherical morphology with a relatively uniform distribution of metals throughout their volume. Their crystal structure was represented by spinel and rock-salt phases. Thermal stability of the powder was also investigated. Sintering at 800°C was found to lead to the emergence of weak reflections of the CuO phase. Increasing the sintering temperature to 1000°C resulted in grain growth up to 2-5 μm and the formation of distinct copper-enriched grains. The synthesized powder was used to prepare polymer pellets for the extrusion-based 3D printing of high-entropy oxide ceramic products. The obtained pellets were applied to print a block structure with gyroidal channels. The results of this study demonstrate that co-electrical explosion of wires made of different metals/alloys enables the production of particles with a controlled structure and elemental composition. Tailoring the structure, elemental composition, and metal segregation both during particle synthesis and during sintering of the extrusion-printed part opens new avenues for developing ceramic products with novel or enhanced functional properties.
Keywords: nanoparticles, high-entropy oxide, aluminum oxide, thermal stability, segregation, electrical explosion of wires, current, spinel, rock-salt, gyroid structure

Spectral-luminescent properties of Nd-containing perovskite quantum dots in a pseudocumene matrix and the effect of 2,5-diphenyloxazole

A.M. Pshukov, A.A. Kokoeva, D.N. Ermolenko, Kh.R. Akhmedova, M.U. Shokumova, M.M. Shogenova
Kabardino-Balkarian State University named after H.M. Berbekov

Abstract: It has been experimentally demonstrated that Nd-containing mixed-halide perovskite quantum dots retain an optically active luminescent state after incorporation into a pseudocumene matrix. Dilutions of the dispersion at 1:10, 1:20, and 1:30 were compared without 2,5-diphenyloxazole and with 2,5-diphenyloxazole at a concentration of 2 g/L. Emission spectra and excitation-emission matrices were recorded under identical settings. In all compositions, a dominant band at 501,5-505,5 nm was observed and 2,5-diphenyloxazole changed the peak position by no more than 1,0 nm. Upon addition of PPO, the maximum intensity and the band area decreased by 2,2 and 2,3% for 1:10, by 20,3 and 15,9% for 1:20, and by 48,8 and 35,3% for 1:30, respectively. Consequently, pseudocumene is a viable organic matrix for the quantum dots under study during photoluminescence diagnostics, whereas 2,5-diphenyloxazole at a concentration of 2 g/L does not sensitize their photoluminescence. This result establishes the conditions for further optimization but does not replace measurements of radioluminescence and γ-excited light yield.
Keywords: perovskite quantum dots, neodymium, pseudocumene matrix, 2,5-diphenyloxazole, photoluminescence, energy transfer, self-absorption, liquid organic scintillator

Charge transfer effects in Me-Al2O3-SiO2-Si structures

G.A. Mustafayev1, N.V. Cherkesova1, A.G. Mustafayev2
1 Kabardino-Balkarian State University
2 Dagestan State University of National Economy

Abstract: The aim of the work is to experimentally study the effects of charge transfer and flat-band voltage shift in metal-Al2O3-SiO2-Si structures under high-temperature treatment and applied bias. It was found that a negative bias resulted in the formation of an «instantaneous» polarization component of the shift, while a positive bias additionally produced a thermally activated «slow» component with a delay time of ~10 min at 125°C. The dependence of the shift on applied voltage at 190°C is linear. It was determined that charge transfer from the metal-Al2O3 interface to the Si-SiO2 interface was caused by the thermal release of carriers from bulk traps with an activation energy of 1,2 eV. A correlation was found between aluminum oxide thickness and the stability of the structure’s parameters, with the minimum mobile charge density observed at a layer thickness of 70 nm. Practical significance is as follows: optimizing the Al2O3 layer thickness to 70 nm ensures maximum stability of the electrical characteristics of metal-insulator-semiconductor structures under combined thermal and electrical loads. The obtained patterns and physical model of charge transport can be used in the technological design of reliable microelectronic devices.
Keywords: metal-insulator-semiconductor-structures, flat-band voltage, capacitance-voltage characteristics, high-temperature processing, multilayer dielectric, charge traps, stability of parameters

Calculation of P-ρ-T properties of noble gases using the fractal state equation in the temperature range from 500 to 3000 K

R.A. Magomedov, E.N. Akhmedov
Institute for Geothermal Research and Renewable Energy of the Joint Institute for High Temperatures of the Russian Academy of Sciences

Abstract: This paper presents a calculation of the state equation isotherms for noble gases: neon, argon, krypton, and xenon in the temperature range from 500 to 3000 K. The calculation was performed using a mathematical model based on a fractal state equation, which has previously demonstrated high efficiency in calculating the P-ρ-T properties of other substances. The obtained results are in good agreement with literature reference data. The dependence of the fitting parameter α of the fractal state equation on density is determined for various temperatures. It is found that for neon, krypton, and xenon, the density dependence is small, but the temperature dependence is noticeable. For argon, the opposite is true: the density dependence is more pronounced, and the temperature dependence is almost absent. To evaluate the effectiveness of the fractal state equation, a comparative analysis of the calculation accuracy is performed and compared to the classical equation of state of a real gas. It is shown that the accuracy of the classical equation decreases with increasing pressure. The fractal equation has high calculation accuracy over the entire studied range of temperatures and pressures.
Keywords: mathematical modeling, fractal equation of state, thermophysical properties of inert gases, neon, argon, krypton, xenon, fractional integro-differentiation, software calculation module

Adsorption of a beryllium monolayer on the surface of GaN(0001)

M.N. Lapushkin
Ioffe Institute

Abstract: The density functional method was used to calculate the adsorption of a monolayer of beryllium atoms on a GaN(0001) surface. The surface was modeled within the framework of a 2×2 supercell geometry containing 10 GaN bilayers. The initial GaN(0001) surface exhibits a metallic conductivity caused by the presence of a band of surface states near the Fermi level. One beryllium monolayer corresponded to a concentration of one Be atom per one surface Ga atom. Calculations of the electron density of states and the adsorption energy were performed for a stable configuration during the adsorption of Be atoms over surface Ga atoms (on-top position) and during the formation of trimer Be clusters with a side length of 2,036 Å within the hexagonal GaN cell. It was found that adsorption is energetically most favorable in the trimer configuration. This non-standard configuration became possible due to the small size of the Be atom. The adsorption energy of Be is 2,125 eV. It was shown that the deposition of a Be monolayer causes only minor structural reconstruction of the substrate: the distance between the Ga and N layers in the surface GaN bilayer increases by 0,102 Å. The adsorption of beryllium leads to the formation of a wide band of surface states below the Fermi level, and the chemical bond with the GaN(0001) substrate is covalent in nature and is provided by the hybridization of the valence electrons of Be and the surface Ga atoms.
Keywords: density functional method, electronic structure, interface, surface, adsorption, beryllium, GaN