PhC-2026
The effect of NiO doping on the phase composition and ferroelectric properties of lead-free ceramics based on sodium and potassium niobate
S.V. Torianik1, T.S. Ilina1, E.A. Skryleva1, B.R. Senatulin1, M.I. Voronova1, A.V. Pavlenko2, D.A. Kiselev1, Yu.N. Parkhomenko1
1 University of Science and Technology MISIS
2 Federal Research Centre The Southern Scientific Centre of the RAS
Keywords: potassium-sodium niobate, lead-free ceramics, atomic force microscopy, X-ray photoelectron spectroscopy, X-ray phase analysis
Simulating the evaporation process of magnetic nanofluid to estimate the service life of magnetic fluid devices
A.N. Bolotov, O.O. Novikova
Tver State Technical University
Keywords: magnetic fluid, evaporation, dispersion medium, friction unit life, viscosity, plain bearing
Determination of the surface energy of the phase components of structural steel by the fatigue crack growth kinetics
L.P. Aref'eva, V.V. Kovaleva
Don State Technical University
Keywords: surface energy, tensile strength, crack, structural steel, ferrite, martensite, two-phase structure
A planar array of GST225-based memristor elements
V.A. Mikhalevsky1, A.A. Burtsev1, V.V. Ionin1, A.A. Nevzorov1,2, A.V. Kiselev1, N.N. Eliseev1, A.A. Lotin1,3
1 National Research Centre «Kurchatov Institute»
2 National University of Science and Technology MISIS
3 Mendeleev University of Chemical Technology
Keywords: memristor, chalcogenides, phase change materials, thin films, amorphization
Liquid-phase oxidation of ethylene glycol with hydrogen peroxide using nanostructured silver catalysts
S.Yu. Menshikov1, V.S. Kurmacheva1, S.A. Fedorov2,1, A.N. Malyshev3,1, Yu.V. Mikushina4, A.B. Shishmakov4, A.A. Tumashov3,4, A.E. Permyakova3, A.A. Ostroushko3
1 Ural State Mining University
2 Vatolin Institute of Metallurgy of the Ural Branch of the RAS
3 Ural Federal University named after the first President of Russia B.N. Yeltsin
4 I.Ya. Postovsky Institute of Organic Synthesis of the Ural Branch of the RAS
Keywords: nanoscale silver, catalytic properties, oxidation, hydrogen peroxide, gas and liquid chromatography, nuclear magnetic resonance spectroscopy, kinetics
Formation of the porous structure of the NiTi intermetallic compound during vacuum sintering of mechanically milled powder
S.S. Volodko1, G.V. Markova2, A.V. Kasimtsev1, D.V. Permyakova2, A.D. Gusev2
1 METSINTEZ LLC
2 Tula State University
Keywords: NiTi, porous materials, pore structure, mechanical milling, planetary mill, vacuum sintering
Features of zirconium carbonitride formation under multistage reduction-carburization-nitridation of ZrO2
S.N. Yudin1, A.V. Kasimtsev2, S.S. Volodko1, D.O. Moskovskikh1
1 National University of Science and Technology MISIS
2 METSINTEZ LLC
Keywords: zirconium carbonitride, zirconium carbide, calcium hydride synthesis, reduction-carburization, nitridation, ZrO2
Modeling of light propagation in silicon nitride and zinc selenide photonic integrated circuit elements with a switchable phase-change material film
A.A. Burtsev1, V.V. Ionin1, A.V. Kiselev1, A.A. Nevzorov1,2, V.A. Mikhalevsky1, N.N. Eliseev1, A.A. Lotin1
1 National Research Centre «Kurchatov Institute»
2 University of Science and Technology MISIS
Keywords: photonic integrated circuits, optical waveguides, phase-change materials, thin films
The influence of synthesis temperature on the structural and electrical properties of metal-dielectric-semiconductor structures based on hafnium oxide films
M.S. Afanasiev, D.A. Belorusov, E.I. Goldman, D.A. Kiselev, A.A. Sivov, G.V. Chucheva
Fryazino branch of the Kotelnikov Institute of Radioengineering and Electronics of RAS
Keywords: ferroelectric films, hafnium oxide (HfO2), structures metal-dielectric-semiconductor, electrophysical properties, polarization