PhC-2026
Production of a titanium-containing composite material with a wide spectrum of action based on ultradisperse hydroxyapatite
N.S. Kozhevnikova1, E.A. Bogdanova2, V.M. Skachkov1, A.Yu. Chufarov1, A.A. Yushkov3, I.V. Baklanova1, Y.A. Avdeeva1
1 Institute of Solid State Chemistry of the Ural Branch of RAS
2 JSC «Giredmet»
3 Ural Federal University named after the first President of Russia B.N. Yeltsin
Keywords: hydroxyapatite, titanium-containing hydroxyapatite, synthesis, precipitation from solution, sol-gel method, titanium oxide, functional materials
Size effect in the formation of fractal nickel films
V.A. Anofriev1, A.S. Antonov1, E.M. Semenova1, M.S. Afanasiev2,3, N.Yu. Sdobnyakov1
1 Tver State University
2 Fryazino Branch of V.A. Kotelnikov Institute of Radio Engineering and Electronics of RAS
3 MIREA – Russian Technological University
Keywords: size effect, degradation and growth, atomic force microscopy, scanning tunneling microscopy, fractal relief, nickel films
Formation of supramolecular particles of polyoxometalate {Mo72Fe30}-doxorubicin-biocompatible polymer: interaction of components and properties
M.O. Tonkushina, I.D. Gagarin, B.T.M.A.. Sharadgah, A.A. Ostroushko
Ural Federal University
Keywords: {Mo72Fe30}, doxorubicin, polyethylene glycol, polyvinylpyrrolidone, particle size, supramolecular systems
Dependence of the interfacial energy of molybdenum faces at the boundary with organic liquids on the dielectric constant
A.M. Apekov1, I.G. Shebzukhova2, L.A. Khamukova1
1 North-Caucasus Center for Mathematical Research, North-Caucasus Federal University
2 Kabardino-Balkarian State University named after H.M. Berbekov
Keywords: molybdenum, interfacial energy, polarization correction, dispersion correction, electron statistical method, nonpolar organic liquid
Study of nanoparticle coalescence mechanisms using Pt and Pb as an example
A.A. Cherepovskaya1,2, D.A. Ryzhkova1, Y.Ya. Gafner1, M.D. Starostenkov2
1 Katanov Khakass State University
2 Polzunov Altai State Technical University
Keywords: coalescence, platinum, lead, nanoparticles, structure, computer simulations, molecular dynamics, tight-binding
Hydrogen embrittlement of high-entropy rare-earth alloys: structure and magnetic properties of the resulting trihydrides
P.A. Krot, Y.A. Ovchenkova, N.Yu. Pankratov, I.S. Tereshina, V.N. Verbetsky
Lomonosov Moscow State University
Keywords: high-entropy alloys, rare earths, hydrides, magnetic properties, crystal structure, lanthanide contraction
Hydrothermal and solvothermal syntheses of calcium phosphates in the form of cotton wool
V.K. Krut'ko1, L.Yu. Maslova1, O.N. Musskaya1, E.N. Krutsko1, I.E. Glazov1, T.V. Safronova2, A.I. Kulak1
1 Institute of General and Inorganic Chemistry of the NAS of Belarus
2 Lomonosov Moscow State University
Keywords: fibrous calcium phosphates, hydrothermal synthesis, octacalcium phosphate, solvothermal synthesis, hydroxyapatite, calcium phosphate wool
Formation of fractal nanostructures of Ge2Sb2Te5 phase-change material by laser-induced transfer
A.A. Burtsev1, D.N. Bukharov2, V.V. Ionin1, V.A. Mikhalevsky1, A.V. Kiselev1, A.A. Nevzorov1,3, N.N. Eliseev1, M.R. Konnikova1, A.A. Lotin1,4
1 National Research Centre «Kurchatov Institute»
2 Vladimir State University named after Alexander and Nikolay Stoletovs
3 University of Science and Technology MISIS
4 Mendeleev University of Chemical Technology
Keywords: chalcogenides, phase change materials, nanoparticles, clustering, laser-induced transfer, fractal dimension