Editor’s column
The use of SiO2 – MnO2 nanopowders for targeted drug delivery
O.A. Zlygosteva, S.Yu. Sokovnin, V.G. Il’ves Ural Federal University named after the First President of Russia B. N. Yeltsin Institute of Electrophysics of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.262 Abstract: Application of manganese-doped mesoporous silica nanopowders SiO2 – MnO2 for targeted drug delivery was researched. ...
Microstructure, phase states, dielectric and elastic properties of ceramic solid solutions Li0,17Na0,83NbyTa1-yO3 obtained at high pressure
V.V. Efremov, O.B. Shcherbina, Yu.V. Radyush, M.N. Palatnikov I.V. Tananaev Institute of Chemistry and Technology of the Federal Research Centre Kola Science Centre of the RAS Scientific and Practical Center of the National Academy of Sciences of Belarus for Materials Science DOI: 10.26456/pcascnn/2018.10.252 Abstract: Microstructure ...
Investigation of size dependences of melting and crystallization temperatures and specific excess surface energy of nickel nanoparticles under melting / crystallization phase transition
P.M. Ershov, A.Yu. Kolosov, V.S. Myasnichenko, D.N. Sokolov, A.A. Khort, S.S. Bogdanov, H.N. Shimanskaya, N.Yu. Sdobnyakov Tver State University A.V. Luikov Heat and Mass Transfer Institute of NAS of Belarus Scientific Investigation Center «Structural Ceramic Nanomaterials», National University of Science and Technologу «MISIS» Belarusian State Technological ...
The influence of the intercalated silicon on the graphene electronic structure
G.S. Grebenyuk, E.Yu. Lobanova, I.I. Pronin Ioffe Institute Saint Petersburg National Research University of Information Technologies, Mechanics and Optics DOI: 10.26456/pcascnn/2018.10.234 Abstract: Intercalation of the graphene-cobalt system with silicon was investigated experimentally. The ab initio calculation of the electronic structure of a low-dimensional graphene-silicon-cobalt system was ...
Using nanoparticles of Ag-Cu alloy as separate bits of PCM memory
Yu.Ya. Gafner, D.A. Bashkova, S.L. Gafner N.F. Katanov Khakas State University DOI: 10.26456/pcascnn/2018.10.226 Abstract: One of the promising areas of application of metallic nanoparticles is the creation of devices on their basis with a high information recording density that generates interest in the study of ...
Evaluation of applicability of small silver nanoparticles as the cells of PCM memory
Yu.Ya. Gafner, D.A. Bashkova, S.L. Gafner, L.V. Redel N.F. Katanov Khakas State University DOI: 10.26456/pcascnn/2018.10.219 Abstract: In this paper, one of the aspects of using metallic nanoclusters was considered, namely the use of silver nanoparticles as separate bits of information in memory devices based on ...
Nanostructures as a material for phase-inverse memory
Yu.Ya. Gafner, S.L. Gafner, L.V. Redel N.F. Katanov Khakas State University DOI: 10.26456/pcascnn/2018.10.210 Abstract: Despite on long researches, chalcogenide alloys are still generally used in the contemporary PCM layouts as the operating layer material undergoing structural transformations. However, the evolution of the technique aimed at ...
Melting of metal nanowires: molecular dynamics simulation
S.A. Vasilyev, A.Yu. Kartoshkin, M.V. Samsonov, E.V. Dyakova Tver State University DOI: 10.26456/pcascnn/2018.10.204 Abstract: A comparative molecular dynamics study has been carried out of the melting of infinite metallic nanowires and free spherical metallic nanoparticles of the same diameter. It was found that the nanowire ...
Antioxidant properties of cerium dioxide nanoparticles
R.A. Vazirov, S.Yu. Sokovnin, V.G. Ilves Ural Federal University named after the First President of Russia B. N. Yeltsin Institute of Electrophysics of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.196 Abstract: Studies of biological activity of cerium dioxide nanoparticles show that this compound exhibits antioxidant, ...
Modeling fractal crystals forming on the surface of stainless steel by cellular automata
A.A. Burtsev, O.Ya. Butkovskii Vladimir State University named after Alexander and Nikolay Stoletovs DOI: 10.26456/pcascnn/2018.10.187 Abstract: In this paper experiments on crystallization from melts and results of analysis of the morphology of formed crystal structures are discussed. Some examples of forming complex dendritic formations are ...