Using nanoparticles of Ag-Cu alloy as separate bits of PCM memory

Yu.Ya. Gafner, D.A. Bashkova, S.L. Gafner
N.F. Katanov Khakas State University

DOI: 10.26456/pcascnn/2018.10.226

Abstract: One of the promising areas of application of metallic nanoparticles is the creation of devices on their basis with a high information recording density that generates interest in the study of their magnetic, optical and structural-phase properties. In this paper, one of the aspects of using metallic nanoclusters. Namely we mean the use of silver-copper nanoparticles as separate bits of information in memory devices based on the phase-change memory.
Keywords: phase transition, memory cells, silver, copper, nanoclusters.

Bibliography link:
Gafner, Yu.Ya. Using nanoparticles of Ag-Cu alloy as separate bits of PCM memory / Yu.Ya. Gafner, D.A. Bashkova, S.L. Gafner // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 226-233.

Full text (in Russian): download PDF file