Editor’s column
Producing nanodimensional silver covering on aluminum oxide nanopowder
M.A. Kiseleva, S.Yu. Sokovnin, M.E. Balezin Ural Federal University named after the First President of Russia B. N. Yeltsin Institute of Electrophysics of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.345 Abstract: The principal possibility of the composite particles production by the radiation-chemical method was shown. ...
Method of analysis of the reversal magnetization processes using magnetic domain structure images
A.Yu. Karpenkov, G.G. Dunaeva, P.A. Rakunov, E.M. Semenova Tver State University DOI: 10.26456/pcascnn/2018.10.338 Abstract: A unique software and hardware system for obtaining and automatic analysis of the magnetic domain structure images in an external magnetic field for further study of the magnetization reversal process was ...
Sol-gel fabrication, morphology and magnetic properties of multiferroics BiFe1-xMnxO3
M.V. Kandaurov, E.V. Vladimirova, A.V. Dmitriev The Institute of Solid State Chemistry of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.330 Astract: Experimental data on the synthesis and properties of the solid solution BiFe1-xMnxO3 are given. The length of the solid solution (0 ≤ x ≤ 0,20) ...
Properties of compacts from BaF2 nano-powder obtained by pulsed electron beam evaporation
V.G. Ilves, S.Yu. Sokovnin, S.V. Zayats, A.M. Murzakaev, Т.М. Demina, M.G. Zuev Institute of Electrophysics of the Ural Branch of RAS Ural Federal University named after the First President of Russia B. N. Yeltsin The Institute of Solid State Chemistry of the Ural Branch of ...
On nanotopographic parameters of engineering surface and its profile
V.V. Izmailov, M.V. Novoselova Tver State Technical University DOI: 10.26456/pcascnn/2018.10.313 Abstract: Amplitude and spacing parameters of engineering surfaces nanotopography and some their correlations have been considered in comparison with similar parameters and correlations on a microscale level (microroughness). It is shown that on a nanoscale ...
Combined method of diffusion saturation of steel by nitrogen
Yu.F. Ivanov, Yu.A. Denisova, E.A. Petrikova, A.D. Teresov, S.V. Lykov, О.V. Ivanova, A.A. Klopotov Institute of High Current Electronics SB RAS Tomsk State University of Architecture and Building DOI: 10.26456/pcascnn/2018.10.304 Abstract: The results obtained during the study of 20H13 steel subjected to a combined treatment including ...
About «technological» properties of nano-sized nickel and copper films
D.V. Ivanov, A.S. Antonov, N.Yu. Sdobnyakov, H.N. Shimanskaya, E.V. Romanovskaia, M.S. Afanasiev Tver State University Belarusian State Technological University MIREA – Russian Technological University Fryazino Branch of V.A. Kotelnikov Institute of Radio Engineering and Electronics of Russian Academy of Sciences DOI: 10.26456/pcascnn/2018.10.291 Abstract: As an example of ...
Sedimentation of nanoparticles under the action of light pressure forces in liquid media
V.I. Ivanov, G.D. Ivanova, V.I. Krylov, V.K. Khe Far Eastern State Transport University DOI: 10.26456/pcascnn/2018.10.286 Abstract: A model of sedimentation of nanoparticles in a uniform light field is considered as an alternative to methods of precipitation in a gravitational field and centrifugation. The exact analytical ...
Thermodiffusion contribution in the thermal lens response of the nanosuspension
V.I. Ivanov, G.D. Ivanova, A.V. Mjagotin Far Eastern State Transport University DOI: 10.26456/pcascnn/2018.10.280 Abstract: A new two-beam configuration of the thermal lens method for the nonlinear optical diagnostics of nanosuspensions is presented. The proposed configuration eliminates the influence of the electrostrictive response and thus provides ...
Peculiarities of the process of switching polarization in polycrystalline thin films of lead zirconate-titanate
V.V. Ivanov, E.N. Golubeva, O.N. Sergeeva, G.M. Nekrasova, I.P. Pronin, D.A. Kiselev Tver State University Tver State Agricultural Academy Ioffe Institute National University of Science and technology «MISIS» DOI: 10.26456/pcascnn/2018.10.270 Abstract: The paper presents the results of a study of relaxation of the dielectric permittivities ...