Editor’s column
Magnetooptical control of spatial magnetic field distribution in microelectromechanical systems
M.K. Virchenko, R.M. Eguzhokova, A.B. Zaletov, A.I. Ivanova Tver State University DOI: 10.26456/pcascnn/2017.9.128 Abstract: A study is performed of the spatial distribution of magnetic field of a microelectromechanical systems (MEMS) with the aid of magneto-optical indicator ferrite garnet films (MOIF). In order to increase the ...
Molecular dynamic study of size dependences of melting and crystallization temperatures of platinum nanoclusters
S.A. Vasilyev, A.A. Romanov Tver State University DOI: 10.26456/pcascnn/2017.9.121 Abstract: The melting and crystallization temperatures of platinum nanoclusters have been found by using results of molecular dynamics modeling, obtained employing two different computer programs and different interatomic interaction potentials. The size dependences found in computer ...
Thermally induced switching in PIN-PMN-PT single crystals
N.N. Bolshakova, V.V. Ivanov, A.I. Ivanova, E.M. Semenova, A.D. Senkovskiy, A.S. Smirnov Tver State University DOI: 10.26456/pcascnn/2017.9.114 Abstract: The results of investigation of thermally induced switching in PIN-PMN-PT single-crystal solid solutions are presented. It was found that samples have the stable unipolarity. The intensity of thermally ...
Instrumental and methodological support of the non-standard researches of the magnetic nanodispersed oils
A.N. Bolotov, V.V. Novikov, O.O. Novikova Tver State Technical University DOI: 10.26456/pcascnn/2017.9.108 Abstract: In the present work we submit an equipment and research technique to study corrosive and tribotechnical properties of the nanodispersed media. The proposed equipment allows to examine the processes which are taking ...
The influence of fluoride ions on the strength properties of hydroxyapatite and based on it composite materials
E.A. Bogdanova, O.V. Skachkova, V.M. Skachkov, N.A. Sabirzyanov The Institute of Solid State Chemistry of the Ural Branch of RAS DOI: 10.26456/pcascnn/2017.9.099 Abstract: The article discusses the possibility of hardening of stoichiometric hydroxyapatite (HAP) obtained by deposition from a solution by means of the partial ...
The effect of calcium-containing reagents on Bayer leaching of bauxites
S.А. Bibanaeva1, N.А. Sabirzyanov1, V.N. Koryukov2 1The Institute of Solid State Chemistry of the Ural Branch of RAS 2Ural Federal University named after the first President of Russia B.N. Yeltsin DOI: 10.26456/pcascnn/2017.9.094 Abstract: The results of the experimental study of the effect of calcium-containing reagents ...
Field desorption of sesium atoms from nanostructured rhenium surface
D.P. Bernatskii, V.G. Pavlov Ioffe Institute DOI: 10.26456/pcascnn/2017.9.089 Abstract: Using method of the field desorption microscopy, desorption of cesium atoms from quasi-spherical surface of a rhenium microcrystal in the electric field has been investigated. The dependence of the desorbing electric field strength vs cesium coverage ...
Molecular dynamics and thermodynamic simulations of segregation phenomena in binary Au-Ag nanoparticles
A.G. Bembel Tver State University DOI: 10.26456/pcascnn/2017.9.081 Abstract: A complex approach combining atomistic molecular dynamics (MD) and thermodynamic simulations was applied to predict segregation in binary Au-Ag nanoparticles consisting of 2000 atoms (of about 4 nm in size). Both approaches predict the surface segregation of Ag ...
The structure of body after manufacturing selective laser melting of iron powder
B.K. Barakhtin1, A.S. Zhukov2, M.V. Staritsin2, N.A. Vershinina1 1Saint Petersburg State Marine Technical University 2Central Research Institute of Structural Materials «Prometey» named by I.V. Gorynin of National Research Center «Kurchatov Institute» DOI: 10.26456/pcascnn/2017.9.071 Abstract: The structure investigation results of selective laser melting (SLM) samples of iron ...
Modeling of CuAu nanoparticle formation during the gas phase synthesis
V.S. Baidyshev, V.А. Tsura, I.V. Chepkasov N.F. Katanov Khakas State University DOI: 10.26456/pcascnn/2017.9.064 Abstract: In this work computer simulation of the cluster condensation from a high-temperature gas phase containing pairs of copper and gold atoms was carried out by the molecular dynamics method. The average ...