PhC-2018
Electronic integral characteristics of groups in the fluoro-substituted of isobutan and neopentan
A.V. Kotomkin, N.P. Rusakova, V.V. Turovtsev, Yu.D. Orlov Tver State University Tver State Medical University DOI: 10.26456/pcascnn/2018.10.368 Abstract: Within a «quantum theory of atoms in molecules» (QTAIM) the equilibrium geometry and the electron structure of fluoro-substituted molecules (CH3)2−CH−CH(3-n)Fn and (CH3)3−C−CH(3-n)Fn, where 1 ≤ n ≤ 3, ...
On the regularities of formation of mono- and bimetallic nanoparticles in the coalescence process
A.Yu. Kolosov, V.S. Myasnichenko, S.S. Bogdanov, V.I. Romanovskiy, N.I. Nepsha, K.R. Shcherbatykh, N.Yu. Sdobnyakov Tver State University Scientific Investigation Center «Structural Ceramic Nanomaterials», National University of Science and Technologу «MISIS» Belarusian State Technological University DOI: 10.26456/pcascnn/2018.10.359 Abstract: The simulation was carried out using two alternative Monte ...
Violation of the energy distribution of desorbiting ions Na+ in thermal ionization on the surface of NaAuy alloy
M.V. Knat’ko, M.N. Lapushkin Ioffe Institute DOI: 10.26456/pcascnn/2018.10.352 Abstract: The effect of the applied external electric field on the energy distribution of desorbed from the alloys are presented. It is shown that the energy distributions of the desorbed depend on the distribution of positive charge ...
Producing nanodimensional silver covering on aluminum oxide nanopowder
M.A. Kiseleva, S.Yu. Sokovnin, M.E. Balezin Ural Federal University named after the First President of Russia B. N. Yeltsin Institute of Electrophysics of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.345 Abstract: The principal possibility of the composite particles production by the radiation-chemical method was shown. ...
Method of analysis of the reversal magnetization processes using magnetic domain structure images
A.Yu. Karpenkov, G.G. Dunaeva, P.A. Rakunov, E.M. Semenova Tver State University DOI: 10.26456/pcascnn/2018.10.338 Abstract: A unique software and hardware system for obtaining and automatic analysis of the magnetic domain structure images in an external magnetic field for further study of the magnetization reversal process was ...
Sol-gel fabrication, morphology and magnetic properties of multiferroics BiFe1-xMnxO3
M.V. Kandaurov, E.V. Vladimirova, A.V. Dmitriev The Institute of Solid State Chemistry of the Ural Branch of RAS DOI: 10.26456/pcascnn/2018.10.330 Astract: Experimental data on the synthesis and properties of the solid solution BiFe1-xMnxO3 are given. The length of the solid solution (0 ≤ x ≤ 0,20) ...
Properties of compacts from BaF2 nano-powder obtained by pulsed electron beam evaporation
V.G. Ilves, S.Yu. Sokovnin, S.V. Zayats, A.M. Murzakaev, Т.М. Demina, M.G. Zuev Institute of Electrophysics of the Ural Branch of RAS Ural Federal University named after the First President of Russia B. N. Yeltsin The Institute of Solid State Chemistry of the Ural Branch of ...
On nanotopographic parameters of engineering surface and its profile
V.V. Izmailov, M.V. Novoselova Tver State Technical University DOI: 10.26456/pcascnn/2018.10.313 Abstract: Amplitude and spacing parameters of engineering surfaces nanotopography and some their correlations have been considered in comparison with similar parameters and correlations on a microscale level (microroughness). It is shown that on a nanoscale ...
Combined method of diffusion saturation of steel by nitrogen
Yu.F. Ivanov, Yu.A. Denisova, E.A. Petrikova, A.D. Teresov, S.V. Lykov, О.V. Ivanova, A.A. Klopotov Institute of High Current Electronics SB RAS Tomsk State University of Architecture and Building DOI: 10.26456/pcascnn/2018.10.304 Abstract: The results obtained during the study of 20H13 steel subjected to a combined treatment including ...
About «technological» properties of nano-sized nickel and copper films
D.V. Ivanov, A.S. Antonov, N.Yu. Sdobnyakov, H.N. Shimanskaya, E.V. Romanovskaia, M.S. Afanasiev Tver State University Belarusian State Technological University MIREA – Russian Technological University Fryazino Branch of V.A. Kotelnikov Institute of Radio Engineering and Electronics of Russian Academy of Sciences DOI: 10.26456/pcascnn/2018.10.291 Abstract: As an example of ...