Sol-gel fabrication, morphology and magnetic properties of multiferroics BiFe1-xMnxO3

M.V. Kandaurov, E.V. Vladimirova, A.V. Dmitriev
The Institute of Solid State Chemistry of the Ural Branch of RAS

DOI: 10.26456/pcascnn/2018.10.330

Astract: Experimental data on the synthesis and properties of the solid solution BiFe1-xMnxO3 are given. The length of the solid solution (0 ≤ x ≤ 0,20) was established, the morphology of the particles and magnetic properties of the samples were investigated in dependence on the content of a dopant. Nonlinear concentration dependences of magnetic characteristics for BiFe1-xMnxO3 with a maximum at the manganese 5 – 7 mol. %. content were found.
Keywords: bismuth ferrite, doping, sol-gel method, morphology, agglomerates, solid solution, phase composition, magnetic properties.

Bibliography link:
Kandaurov, M.V. Sol-gel fabrication, morphology and magnetic properties of multiferroics BiFe1-xMnxO3 / M.V. Kandaurov, E.V. Vladimirova, A.V. Dmitriev // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials: Interuniversity collection of proceedings / Ed. by V.M. Samsonov, N.Yu. Sdobnyakov. – Tver: TSU, 2018. – I. 10. – P. 330-337.

Full text (in Russian): download PDF file