Abstract: In this work, we carried out a comparative study of the surface structure of bariumstrontium titanate Ba1-xSrxTiO3 ceramics of various compositions (x = 0,1; 0,2; 0,25; 0,3; 0,4 and 0,5) and the dielectric characteristics of samples in a wide temperature range. It has been found that with increasing the strontium content, a decrease in the density of ceramic samples is observed. An increase in the strontium concentration in the composition of the ceramics under study leads to a reduction in the average grain size by an order of magnitude, and fine grains from 2 μm to 200 nm. For all ceramic samples of barium-strontium titanate, there is a deviation of the elemental composition from the stoichiometric at the nanoscale. The closest to the stoichiometric composition in terms of the molar content of elements is the composition of the Ba0,75Sr0,25TiO3 samples. It was found that the samples of this composition have the highest value of the permittivity at room temperature. Temperature studies of the dielectric permittivity showed the existence of two maxima: at a temperature of 130°C, corresponding to the Curie temperature of pure barium titanate ceramics, and at lower temperatures in the range from 10 to 100°C, the second depends on the strontium content. The low-temperature maximum for the ε value corresponds to the diffuse transition of the solid solution Ba1-xSrxTiO3, whose relaxor properties are confirmed by deviation of the temperature dependence from the Curie–Weiss law. The samples of Ba0,75Sr0,25TiO3 composition have the most pronounced relaxor behavior.

Keywords: piezoelectric ceramics, barium– strontium titanate, lead-free materials, grain structure, permittivity

  • Vladislav V. Ivanov – 1st year postgraduate student, Tver State University
  • Olga V. Malyshkina – Dr. Sc., Professor, Full Professor, Department of Computer Security and Mathematical Control Methods, Tver State University
  • Inna L. Kislova – Ph. D., Docent, Condensed Matter Physics Department, Tver State University
  • Alexandra I. Ivanova – Ph. D., Docent, Applied Physics Department, Tver State University
  • Alexandr V. Solnyshkin – Dr. Sc., Full Professor, Condensed Matter Physics Department, Tver State University

Reference:

Ivanov, V.V. Structural features and dielectric response of barium-strontium titanate ceramics / V.V. Ivanov, O.V. Malyshkina, I.L. Kislova, A.I. Ivanova, A.V. Solnyshkin // Physical and chemical aspects of the study of clusters, nanostructures and nanomaterials. — 2023. — I. 15. — P. 108-118. DOI: 10.26456/pcascnn/2023.15.108. (In Russian).

Full article (in Russian): download PDF file

References:

1. Marshall M., Malashevich A., Disa A. et al. Conduction at a Ferroelectric interface, Physical Review Applied, 2014, vol. 2, issue 5, pp. 051001-1-051001-6. DOI: 10.1103/PhysRevApplied.2.051001.
2. Smolenskij G.A., Isupov V.A., Pasynkov R.E. et al. Fizika segnetoelektricheskikh yavlenij [Physics of ferroelectric phenomena], ed. by G.A. Smolenskij. Leningrad, Nauka Publ., 1985, 396 p. (In Russian).
3. Jackson C. A., Stemmer S. Interface-induced magnetism in perovskite quantum wells, Physical Review B, 2013, vol. 88, issue 18, pp. 180403-1-180403-4. DOI: 10.1103/PhysRevB.88.180403.
4. Acosta M., Novak N., Rojas V. BaTiO3-based piezoelectrics: Fundamentals, current status, and perspectives, Applied Physics Reviews, 2017, vol. 4, issue 4, pp. 041305-1-041305-53. DOI: 10.1063/1.4990046.
5. Golovnin V.А., Kaplunov I.А., Ped'ko B.B. et al. Fizicheskie osnovy, metody issledovaniya i prakticheskoe primenenie p'ezomaterialov [Physical foundations, research methods and practical application of piezomaterials]. – Moscow, TEKHNOSFERА Publ., 2013. – 272 p. (In Russian).
6. Fu C., Yang C., Chen H. et al. Microstructure and dielectric properties of BaxSr1−xTiO3 ceramics, Materials Science and Engineering: B, 2005, vol. 119, issue 2, pp. 185-188. DOI: 10.1016/j.mseb.2005.02.056.
7. Thakur O.P., Prakash C., Agarwal D.K. Dielectric behavior of Ba0.95Sr0.05TiO3 ceramics sintered by microwave, Materials Science and Engineering: B, 2002, vol. 96, issue 3, pp. 221-225. DOI: 10.1016/S0921-5107(02)00159-9.
8. Mahani R.M., Battisha I.K., Aly M., Abou–Hamad A.B. Structure and dielectric behavior of nanostructure ferroelectric BaxSr1−xTiO3 prepared by sol–gel method, Journal of Alloys and Compounds, 2010, vol. 508, issue 2, pp. 354-358. DOI: 10.1016/j.jallcom.2010.05.060.
9. Jonscher A.K. Universal relaxation law: a sequel to dielectric relaxation in solids. London, Chelsea Dielectrics Press Limited, 1996, xvi, 415 p.
10. Cross L.E. Relaxor ferroelectrics, Ferroelectrics, 1987, vol. 76, issue 1, pp. 241-267. DOI: 10.1080/00150198708016945.
11. Kleemann W., Samara G.A., Dec J. Relaxor ferroelectrics–from random field models to glassy relaxation and domain states, Polar Oxides: Properties, Characterization, and Imaging, ed. by. R. Waser, U. Böttger, S. Tiedke. Weinheim, Wiley‐VCH Verlag GmbH & Co, 2004, сhаpter 15, pp. 275-301. DOI: 10.1002/3527604650.ch15.
12. Martirena H.T., Burfoot J.C. Grain-size and pressure effects on the dielectric and piezoelectric properties of hot-pressed PZT-5, Ferroelectrics, 1974, vol. 7, issue 1, pp. 151-152. DOI: 10.1080/00150197408237979.

⇐ Prevoius journal article | Content | Next journal article ⇒